Burning Characteristics of Wood-based Materials using Cone Calorimeter and Inclined Panel Tests

  • Park, Joo-Saeng;Lee, Jun-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.30 no.3
    • /
    • pp.18-25
    • /
    • 2002
  • Research to discuss the fire performance of materials requires tools for measuring their burning characteristics and validated fire growth models to predict fire behavior of the materials under specific tire scenarios using the measured properties as input for the models. In this study, burning characteristics such as time to ignition, weight loss rate, flame spread, heat release rate, total heat evolved, and effective heat of combustion for four types of wood-based materials were evaluated using the cone calorimeter and inclined panel tests. Time to ignition was affected by not only surface condition and specific gravity of the tested materials but also the type and magnitude of heat source. Results of weight loss rate, measured by inclined panel tests, indicated that heat transfer from the contacted flame used as the heat source into the inner part of the specimen was inversely proportional to specific gravity of material. Flame spread was closely related with ignition time at the near part of burning zone. Under constant and severe external heat flux, there was little difference in weight loss rate and total heat evolved between four types of wood-based panels. More applied heat flux caused by longer ignition time induced a higher first peak value of heat release rate. Burning characteristics data measured in this study can be used effectively as input for fire growth models to predict the fire behavior of materials under specific fire scenarios.

Studies on Plywood Treated Fire-Retardant - III. The Fire-Retardant Degree of Monoammonium Phosphate Treated Plywood (합판(合板)의 내화처리(耐火處理)에 관(關)한 연구(硏究) - III. 제1인산(第一燐酸)암모늄처리합판(處理合板)의 내화도(耐火度))

  • Kim, Jong-Man
    • Journal of the Korean Wood Science and Technology
    • /
    • v.14 no.4
    • /
    • pp.21-28
    • /
    • 1986
  • Plywood used for construction as a decorative inner material is inflammable and can fire accident, causing destruction of human life and property. In this study, 3.5mm Kapur plywoods were soaked in the 23% monoammonium phosphate solutions by cold soaking method 3, 6, 9hrs and hot-cold bath method for 3/3hrs, and redrying was carried out by press-drying at the platen temperature of 110, 130, 160, 180$^{\circ}C$, and then fire test was carried out to investigate burning point, flame exhausted length, frame spread length, back side carbonized area and weight loss. The results are as follows; 1. In cold soaking method for 3, 6, 9hrs. retentions of monoammonium phosphate were 0.377, 0.448, 0.498kg/(30cm)$^3$ respectively, and in hot-cold bath method for 3/3hrs, the retention was 1.331kg(30cm)$^3$ that exceeded the minimum retention 1.124kg/(30cm)$^3$. 2. Correlation coefficients among the variable were shown in table 2. From the table, it could be recognized that there were close negative correlations between the treatment and burning point, flame spread length, back side carbonized area, flame exhausted time and weight loss, and there was negative correlation between treating time and back side carbonized area, but there was positive correlation between platen temperature and burning point. 3. From table 3, it can be observed that there were highly significant differences for burning point, flame spread length, flame exhausted time, back side carhonized area, weight loss between treatments. And in 2-way interactions, there were also highly significant for burning point, flame spread length, flame exhausted time, weight loss between time x treatment. 4. It was observed that burning point, flame exhausted time, flame spread length, back side carbonized area, and weight loss in fire-retardant treated plywood were the best effects in fire-retardant treated plywood, water treated plywood and nontreated plywood. In conclusion, I can estimate that absorbed chemical contents by hot-cold bath method for 3/3hrs, have a lot of effects on fire-retardant factors such as burning point, flame spread length, flame exhausted time, backside carbonized area and weight loss, but platen temperatures have a little effects on the fire factors.

  • PDF

Igniter and Thickness Effects on Upward Flame Spread

  • J.Q. Quintiere;Lee, C.H.
    • Proceedings of the Korea Institute of Fire Science and Engineering Conference
    • /
    • 1997.11a
    • /
    • pp.154-161
    • /
    • 1997
  • Several studies have developed upward flame spread models which use somewhat different features. However, the models have not considered the transient effects of the igniter and the burning rate. Thus, the objective of this study is to examine a generalized upward flame spread model which includes these effects. We shall compare the results with results from simpler models used in the past in order to examine the importance of the simplifying assumptions. We compare these results using PMMA, and we also include experimental results for comparison. The results of the comparison indicate that flame velocity depends on the thermal properties of a material, the specific model for flame length and transient burning rate, as well as other variables including the heat flux by igniter and flame itself. The results from the generalized upward flame spread model can provide a prediction of flame velocity, flame and pyrolysis height, burnout time and position, and rate of energy output as a function of time.

  • PDF

Studies on Press Drying and Dynamic Elastic Modulus of Plywood Treated with Boric Acid (붕산처리(硼酸處理) 합판(合板)의 열판건조(熱板乾燥) 및 동적(動的) 탄성율(彈性率)에 관(關)한 연구(硏究))

  • Kim, Jong-Man
    • Journal of the Korean Wood Science and Technology
    • /
    • v.15 no.3
    • /
    • pp.56-67
    • /
    • 1987
  • Plywoods used for construction as a decorative interior material are inflammable and can make fire accidents, causing destruction of human life and property. Therefore, it is indeed required to make fire-retardant treated plywood. In this study, 3.7mm yellow meranti plywoods were soaked in 18% boric acid solutions and tap water by hot-cold bath for 1/2, 2/2, 4/2, 6/2 hours and redrying of treated plywoods was carried out by press drying at the platen temperature of 110, 130, 160, $180^{\circ}C$ and then it was conducted to investigate solution absorption, drying rates, dynamic young's modulus. specific gravity and fire-retardant factors such as burning point, flame spread length. flame exhausted time, back side carbonized area and weight loss by treating time, treating solutions and platen temperature. The results are as follows; 1. When plywood was impregnated with the hot bath temperature of $70^{\circ}C$ for 1. 2, 4, 6 hours and the cold bath temperature of $15^{\circ}C$ for 2 hours respectively, retentions of boric acid were 1.565, l.597, 1.643, 1.709kg/$(30cm)^3$ and all of them exceeded the minimum retention [1.125kg/$(30cm)^3$] even in the shortest treatment. 2. In hot-cold bath method for 1/2 hours, the drying rates of treated plywood remarkably increased with the extension of platen temperature of 110, 130, 160, $180^{\circ}C$ and the values of boric acid treated plywood were 5.900, 10.196, 45.42, 54.958m.c%/min and the values of water treated plywood were 6.014, 12.373, 46.520, 55.730m.c%/min and drying rates of water treated plywood were faster than those of boric acid treated plywood. 3. The values of boric acid treated plywoods in dynamic young's modulus were widely higher than those of water treated plywoods. And it can be observed that there were highly significant differences for treating time between dynamic young's modulus, and the values of boric acid plywoods increased with the extension of treating time but on the contrary water treated plywoods were decreased values with prolonged time 4. It was observed that there were highly significant differences for platen temperature between dynamic young's modulus. When the values of water treated plywoods in dyna nic young's modulus were abruptly decreased according to the rise of platen temperature. boric acid treated plywoods showed rather increased values at $160^{\circ}C$ of platen temperature. And in 2- way interactions, there were also highly significant for dynamic young's modulus between treating time x treating solutions and platen temperature x treating solutions. 5. Correlation coefficients of fire-retardant factors were shown in table 5. It could be recognized that there were close correlations between the treating solutions and burning point, flame spread length, back side carbonized area, flame exhausted time and weight loss, but there was no correlation between fire-retardant factors and treating time and platen temperature. 6. From table 6, it can be observed that there were highly significant differences for burning point, flame spread length, flame exhausted time, back side carbonized area, weight loss between treating solutions. And in 2-way interactions, there were highly significant for burning point, flame spread length, weight loss between treating time $\times$ treating solutions.

  • PDF

Experimental Studies on the Burning Forms of Flammable Liquids (인화성액체의 연소 형태에 관한 실험적 연구)

  • Choi, Seung-Bok;Choi, Don-Mook
    • Proceedings of the Safety Management and Science Conference
    • /
    • 2010.04a
    • /
    • pp.247-251
    • /
    • 2010
  • The victims of fire are increasing steadily. Fires have been occurred by arson, spontaneous combustion and various causes. As a result of that, the damages of fire got out of hand. Especially, the fires of flammable liquids are can be spreaded easily because of high calorific value and fire loads. These rapid fire spread cause the huge losses of both life and property and the malfunction of extinguishing systems. In these studies, we examined the spread pattern of surface fire on the water surface by the reappearance experiment.

  • PDF

Study on the Combustion Characteristics of Flammable materials and Combustion Accelerants in an Arson (방화 범죄에서 가연성 물질과 연소촉진제의 연소 특성에 관한 연구)

  • Park, Hye-Jeong;Nam, Ki-Hun;Kim, Kwang-Il
    • Fire Science and Engineering
    • /
    • v.31 no.5
    • /
    • pp.7-11
    • /
    • 2017
  • The purpose of this study is to recognize the necessity for the management of the available materials in cases of arsons and to prevent arson gaining an understanding of the combustion characteristics of the flammable materials and combustion accelerants in arson cases. We investigated and analyzed the statistical data on arsons and selected flammable materials (wood, paper, synthetic textiles, synthetic resins), and combustion accelerants (gasoline, diesel, solvent) that are frequently used in cases of arson. We conducted a thermogravimetric analysis to assess the thermal properties of the flammable materials. Also, we conducted burning and flame spread rate tests for the purpose of comparing and analyzing the combustion characteristics of the flammable materials and combustion accelerants.

Analysis of forest fire danger rating on the forest characteristic of thinning area and non-thinning area (숲 가꾸기 실행 및 미실행지의 임분특성에 따른 산불위험도 분석)

  • Lee, Si-Young;Lee, Myung-Woog;Chae, Hee-Min;Won, Myoung-Soo;Yeom, Chan-Ho
    • 한국방재학회:학술대회논문집
    • /
    • 2007.02a
    • /
    • pp.217-222
    • /
    • 2007
  • Since 1973, we attain a successful achievement of nation-wide afforestation such as a thick forest and heaped-up leaves. However, the higher of the formation density in forest, the more dangerous to be a large-scale forest fire whenever fire occurs. According to the type of forest in the country, 42% of the forest is occupied by conifer forest that are highly flammable, and the distribution of forest age is in a transition period from immature forest to mature one. And the structure is too weak to the forest fire for the occurrence and spread because there are too many scrub and shrub trees in the forest. As a matter of course, it is on the increase of the thinning-forest that can shift the forest structure from a weak on forest fire to a strong one nowaday. In other words, thinning-forest has primary purposes such as the promotion of producing forest trees, production of excellent timbers, and build-up of public forest area. Furthermore, in some reports, the reduction of ladder fuel by eliminating the vertical/horizontal fuel in a forest and ensuring spaces in the forest can decrease the occurrence of forest fire and the risk of spread of burning as by-effect. Therefore, this study is designed to clarify the relation with the risk of forest fire by an on-spat-investigation of the characteristics of forest composition on the thinning and the non-thinning area.

  • PDF

Burning Tests for Interior Flooring Materials (건축용 바닥재의 연소성능 시험)

  • Lee, Bong-Woo;Lee, Jang-Won;SaKong, Seong-Ho;Kim, Hee-Soo;Lee, Byoung-Ho;Kim, Hyun-Joong
    • Fire Science and Engineering
    • /
    • v.22 no.2
    • /
    • pp.30-37
    • /
    • 2008
  • We have performed the inflammability test for various flooring materials through a radiant heat panel tester by using the specification KSISO 9239-1 (an examination method of flooring materials) that has been set as an international standard for the fire prevention means of interior flooring materials. We have measured the flame spread distance, critical heat flux and smoke density generated by the fire of various flooring materials while using the radiant heat panel tester. The measurement result has shown the burning characteristics different from each other by the respective flooring materials and we could see that the surface materials and construction elements influence greatly on the heat release and smoke generation. We could see that the evaluation method above is an important test method in evaluating the critical heat flux, smoke generation and flame spread distance that are Important factors in studying for fire risks and it is judged that setting and applying a fire evaluation method of flooring materials suitable for the domestic construction use would be relevant.

Characteristics and Risk Assessment of Flame Spreading Over Metal Dust Layers (퇴적금속 분진층을 전파하는 화염의 연소특성과 위험성 평가)

  • Han, Ou-Sup
    • Korean Chemical Engineering Research
    • /
    • v.43 no.1
    • /
    • pp.47-52
    • /
    • 2005
  • The wide use of metal dusts have been found in industrial field and many dust explosion accidents occur by fire spread of dust layer. In this study, we developed a new experimental device to examine fire and explosion characteristics of the dust layer. Aspects of the burning zone over metals(Mg, Zr, Ta, Ti, etc) and PMMA(Polymethyl methacrylate) dust layers have been investigated experimentally to clarify behaviors (Spread rate and quenching distance) and effects of $N_2$ surrounding gas on the fire spread over metal dust layers. From the experimental result, it was found that the spread rate of metal dusts is larger than PMMA, the dependability of spread rate over the thickness of dust layer is small, and the minimum oxygen concentration of spread flame over Mg dust layer is 3.6-3.7 vol%. Since high correlation between the spread rate and the reciprocal of quenching distance was seen, relative risk prediction in those inflammable parameters can be predicted.

A Study on Flash Over Delay Effects on Applied Plate-Fire Spread Prevention Method at Sandwich Panels Structure (샌드위치패널 건축물 플래시오버 지연을 위한 화재확산방지플레이트 시공방법 연구)

  • Kim, Do-hyun;Cho, Nam-Wook
    • Fire Science and Engineering
    • /
    • v.31 no.3
    • /
    • pp.79-87
    • /
    • 2017
  • Sandwich panels which are having the both sides are bonded with a heat insulating material with an iron plate are used as factories, warehouse structures as advantages of convenience in construction at economic efficiency of material cost. However, in a panel structure constructed by continuous joining of sandwich panels, a joint portion where a panel and a panel are connected is generated. The joint part is a part which is easily vulnerable to fire because flames easily flow into the melting and deformation of the iron plate during fire. The flames flowing into the panel induce diffusion of fire by rapid burning, causing damage of human life and property. In this research, we developed a flame spread prevention plate to prevent spreading of sandwich panel. This is an improvement of the workability by the anti-spreading construction method of the existing previous research, it can be applied independently to the connecting part where the panel and the panel are coupled, designed to prevent inflow and spreading of flame did. The actual fire test of the test method of KS F ISO 13784-1 of the sandwich panel specimen was conducted and the burning behavior corresponding to the presence or absence of application of the flame spread prevention plate was grasped at the panel connection part and its effect was measured. Inserting a fire spreading plate into the test result panel connecting part is measured by delaying the flashover, prevention of collapse of the specimen, and temperature rise of the opening, effectively improving the fire safety of the panel structure It was confirmed as a method that can be secured. It is judged that panel structure will contribute to ensuring fire safety by applying the fire spread prevention construction method of various methods ensuring the workability and economy of panel connection vulnerable to fire.