공간주파수대역에서 기저대역 확장을 통한 원전 대비시험편과 대비 보정 시험편의 초음파 영상 개선 (Ultrasonic Images Enhancement of the SS Reference Specimen and the Reference Calibration Block for NPPs by the Combining Bases of Support for Spatial Frequency)

  • 박치승;김선진
    • 한국재료학회지
    • /
    • 제13권10호
    • /
    • pp.651-657
    • /
    • 2003
  • Ultrasonic microscope has been used to detect the defects on surface or inner solid. Conventionally, it has used at a single operating frequency. The resolution and quality of the measured images are determined by a characteristic of the transducer of the ultrasonic microscope. The conventional ultrasonic microscope has been used envelope detector to detect the amplitude of reflected signal, but the changes in amplitude is not sensitive enough for specimen with microstructure that in phase. In this paper, we have studied multi-frequency depth resolution enhancement with ultrasonic reflection microscope for the reflectors of a stainless steel reference specimen and a reference calibration block to be used as the material in nuclear power plants for ISI, PSI. Increased depth resolution can be obtained by taking two, three-dimensional images at more that one frequency and numerically combining the results. As results of the experiment, we could get enhanced images with the rate of contrast in proportion and high quality signal distribution for the image to the changing rate of depth for the reflectors of the two kinds of specimens.

7175Al 링롤단조재의 미세조직과 기계적 성질에 미치는 공정조건의 영향 (Effect of Process Conditions on the Microstructure and Mechanical Properties of 7175Al Ring Roll Forgings)

  • 이인기;강락경;이오연
    • 열처리공학회지
    • /
    • 제17권1호
    • /
    • pp.10-16
    • /
    • 2004
  • The aim of this study is to investigate the process conditions on the microstructual changes and mechanical properties of large 7175 aluminum ring roll forgings. The billets range from 370 mm to 720 mm in diameter were homogenized and ring roll forged after direct chill casting. The tensile properties of ring roll forged specimen manufactured with ${\Phi}370mm$ billets were superior to those of ${\Phi}720mm$ billets under $T_6$ condition. Also, these properties showed better than those of military specification under $T_{74}$ treatment. The impact value of ring roll forged specimen under $T_{74}$ treatment increased up to 20% than that of $T_6$ condition. The fracture toughness of ring roll forged specimen manufactured with ${\Phi}370mm$ cast billet showed nearly same level of ${\Phi}720mm$ billet which was processed using MF or Cog free forging followed by ring roll forging.

압연강판(壓延鋼板)의 피로균열(被虜龜裂) 전파거동(傳播擧動)에 대(對)한 연구(硏究) (A Study on the Propagation Behaviour of the Fatigue Cracks in Rolled Steel Plates)

  • 강창수
    • 대한조선학회지
    • /
    • 제12권2호
    • /
    • pp.43-58
    • /
    • 1975
  • There are many reports on fatigue crack of metallic materials but most of them relate crack propagation rate to stress intensity factor. The problem of crack propagation is not yet clarified, especially the bridge between micro and macro phenomena In this experiment rotating bending fatigue tests have been carried out with smoothed specimen of rolled steel plates including 0.2% carbon under application of three stress conditions to investigate the slip band and the crack propagation behaviour. The results obtained are as follows; 1) The length of cracks which have grown at initial crack tips can be expressed as follows; $l=Ae^{BNr}$(A,B: constant, $N_r$: cycle ratio) $\frac{dl}{dN}=\frac{AB}{N_f}{\cdot}e^{BNr}$($N_f$:fatigue life) 2) The ratio of slipped grain number to total grain number is $S_f=7{\sigma}-5.6$-5.6{\sigma}_c$($\sigma$: stress amplitude) (${\sigma}_c$: fatigue limit) 3) When the fatigue process transfers from Stage I to Stage II, the crack which propagates into specimen changes its direction from that of the maximum shear stress to the direction of perpendicular to principal stress and this is same in the circumferential direction of specimen. the crack propagation behaviors of both sides of a crack are different each other when they approach to the grain boundary.

  • PDF

폴리프로필렌/마이카 복합재료의 물성에 미치는 고상압출 배향의 영향 (Effects of Orientation via Solid-State Extrusion on Properties of Polypropylene/Mica Composites)

  • 이재춘;하창식
    • 접착 및 계면
    • /
    • 제15권1호
    • /
    • pp.9-13
    • /
    • 2014
  • 본 연구는 폴리프로필렌/마이카 복합재료의 고상압출에 의한 배향에 따른 기계적 물성의 변화에 관한 연구이다. 마이카 함량이 증가할수록 복합재료의 비중이 증가하였다. 하지만 고상압출에 따른 배향에 의해 복합재료의 비중은 미세공극의 발생으로 말미암아 비중은 배향 전에 비해 현저히 감소하는 것으로 나타났다. 이러한 미세공극의 존재는 복합재료의 인장 및 굴곡물성에 큰 영향을 미치는 것으로 나타났다. 고상압출 여부에 관계없이 마이카 함량이 10 wt%일 때 최대 굴곡 물성이 관찰되었다.

36개월간 국내 옥외폭로시험에 따른 아연도강의 표면외관 변화 (Surface Appearance of Galvanized Steel with Outdoor Exposure Testing in Korea for 36 Months)

  • 김기태;김영식
    • Corrosion Science and Technology
    • /
    • 제17권6호
    • /
    • pp.301-309
    • /
    • 2018
  • If galvanized steel is exposed to an outdoor environment, atmospheric corrosion will occur with time and red rust will form when the sacrificial protection capacity of zinc reaches its limit. With corrosion, the surface appearance of steel changes, and the properties of the exterior materials degrade. In this study, two kinds of galvanized steel, (GA and GI specimens) were subjected to an outdoor exposure test for 36 months in six regions of Korea. Chrominance (color, chroma, and brightness) and glossiness surface analyses were performed. The color change was not significant, regardless of the exposed area or the specimens tested. With increasing exposure times, the GA specimen became blackened by the formation of zinc oxide, and red coloration was increased by the formation of red rust. As the exposure time of GI specimen increased, the surface proceeded to blacken, but no red rust was formed and the color did not change significantly. Regardless of the outdoor exposure area or the specimen, longer exposure times led to lower glossiness, and this behavior appears to be influenced by the formation of zinc oxide.

Predicting Damage in a Concrete Structure Using Acoustic Emission and Electrical Resistivity for a Low and Intermediate Level Nuclear Waste Repository

  • Hong, Chang-Ho;Kim, Jin-Seop;Lee, Hang-Lo;Cho, Dong-Keun
    • 방사성폐기물학회지
    • /
    • 제19권2호
    • /
    • pp.197-204
    • /
    • 2021
  • In this study, the well-known non-destructive acoustic emission (AE) and electrical resistivity methods were employed to predict quantitative damage in the silo structure of the Wolsong Low and Intermediate Level Radioactive Waste Disposal Center (WLDC), Gyeongju, South Korea. Brazilian tensile test was conducted with a fully saturated specimen with a composition identical to that of the WLDC silo concrete. Bi-axial strain gauges, AE sensors, and electrodes were attached to the surface of the specimen to monitor changes. Both the AE hit and electrical resistance values helped in the anticipation of imminent specimen failure, which was further confirmed using a strain gauge. The quantitative damage (or damage variable) was defined according to the AE hits and electrical resistance and analyzed with stress ratio variations. Approximately 75% of the damage occurred when the stress ratio exceeded 0.5. Quantitative damage from AE hits and electrical resistance showed a good correlation (R = 0.988, RMSE = 0.044). This implies that AE and electrical resistivity can be complementarily used for damage assessment of the structure. In future, damage to dry and heated specimens will be examined using AE hits and electrical resistance, and the results will be compared with those from this study.

암석코어시편의 절리면 직접전단시험을 위한 겉보기 면적 계산방법 (Calculation Method for Nominal Area of Rock Core Specimen During Direct Shear Test)

  • 강훈;박정욱;박찬;오태민;조정우
    • 터널과지하공간
    • /
    • 제30권6호
    • /
    • pp.551-558
    • /
    • 2020
  • 기존 시험법은 암석시편의 절리면 직접전단시험시 겉보기 면적의 변화를 고려해야 한다고 명시하고 있다. 본 기술보고는 암석코어 시편의 절리면 직접전단시험시 겉보기 면적 계산방법을 제시하였다. 암석코어 시편의 초기 절리면을 타원으로 가정하고, 타원의 중첩면적 감소를 계산하는 수식을 정리하였다. 전단변위와 겉보기 면적을 정규화하면 타원형상에 관계없이 일정한 변화 비율을 가지는 것을 확인하였다. 암석코어 시편 전단시험을 위한 정규화 실험상수를 제안하여 일반화된 계산방법을 제안하였다. 그 방법을 실제 전단시험의 데이터에 적용하여 결과 변화값을 확인하고, 정확도에 대해 간략히 토의하였다.

A novel dual stress/strain-controlled direct simple shear apparatus to study shear strength and shear creep of clay

  • Chen Ge;Zhu Jungao;Wang Tao;Li Jian;Lou Qixun;Li Tao
    • Geomechanics and Engineering
    • /
    • 제37권6호
    • /
    • pp.615-627
    • /
    • 2024
  • Direct simple shear test is an effective method to measure strength and deformation properties of soil. However, existing direct simple shear apparatus have some shortcomings. The paper has developed a novel dual stress/strain-controlled direct simple shear apparatus. The novel apparatus has the following advantages: A rectangular specimen is used that effectively avoid common issues associated with conventional cylindrical specimens, such as specimen tilting. The utilization of deformation control rods ensures a uniform shear deformation of the specimen. Vertically integrated force transmission structure is improved that avoids issues arising from changes in pivot points due to lever tilting. Incorporating this novel direct simple shear apparatus, shear strength and shear creep tests of clay were performed. Shear strength parameters and shear creep behaviors are analyzed. The results of these experiments show that the novel apparatus can measure accurately the shear rheological properties of soil. This study provides strong guidance for studying the mechanical properties of soil in engineering practice.

The Peculiarities of New Textile Hand Evaluation Method

  • Eugenija, Strazdiene;Matas, Gutauskas
    • Fibers and Polymers
    • /
    • 제7권4호
    • /
    • pp.414-419
    • /
    • 2006
  • The paper presents information concerning metrological and technical characteristics of KTU-Griff-Tester device, the optimization of its parameters and the cases of its application. It was defined that the behaviour of textile material during its extraction through a rounded hole depends upon its structure. Variations of geometrical shape of woven and knitted specimens can be described by mathematical expressions of shortened epicycloids and Cassini ovals. It is shown that waving process of disc shaped specimen can be predicted on the basis of the law of sine curve. The examples of textiles treatment with different types of commercial softeners are presented, herewith showing the suitability (sensitiveness) of the new device to detect the changes of textile hand. Meantime it is shown that the level of materials anisotropy can be decided on the basis of transformations of specimen's geometrical shape.

미세 구조가 Mg-페라이트 소결체의 자성에 미치는 영향 (Effects of Microstructure on the Magnetic Properties of Mg-ferrite Sintered Body)

  • 김성재;정명득;백종규
    • 한국세라믹학회지
    • /
    • 제32권4호
    • /
    • pp.436-440
    • /
    • 1995
  • Effects of microstructure of two Mg-ferrite specimens with the same starting composition and relative density but with different grain size on B-H hysteresis loop, natural resonance frequency, and ferromagnetic resonance line width are reported. Such properties as B-H hysteresis loop, saturation magnetization, natural resonance frequency, and ferromagnetic resonance line width were influenced by the microstructure development during sintering. Large grain size specimen showed high saturation magnetization, low coercive force, low natural resonance frequency, and low ferromagnetic resonance line width compared with the specimen of small grain size. The main reason for the changes in properties can be explained by the variation in anisotropic characteristics due to Fe+2 content generated during sintering process.

  • PDF