Preparation of High Purity ZnO Powder from zinc-bearing waste by the Hydrometallurgical Process (함아연 폐기물로부터 습식법에 의한 고순도 ZnO 분말의 제조)

  • 이재천;이강인;유효신
    • Resources Recycling
    • /
    • v.1 no.1
    • /
    • pp.58-68
    • /
    • 1992
  • A process development for direct synthesis of high pure ZnO powders from zinc-bearing waste was investigated. This waste contains a 55% of zinc and it was extracted by the sulfuric acid(leaching). After removal of iron ion by precipitation from the zinc solution, the purification through a solvent extraction by the use of D2EHPA as an extractant was carried out. Then, loaded zinc in organic solution was stripped and precipitated simultaneously using a precipitant such as oxalic acid. Then, loaded zinc in organic solution was stripped and precipitated simulataneously using a precipitant such as oxalic acid. The synthesized $ZnC_2O_4$ powders by the precipitation stripping method was calcined to obtain more than 99.9% of ZnO powders. The effect of sulfuric acid concentration, leaching time, pulp density on the extraction of zinc was studied and the optimum conditions for the solvent extraction were obtained through the investigation of purification of zinc solution. The size, morphology and size distribution of synthesized $ZnC_2O_4$ powders were studied in terms of oxalic acid concentration, temperature, surfactant added, precipitation time, etc.

  • PDF

Formation Mechanism of Ultrafine $TiO_2$ Powders from Aqueous $TiOCl_2$ Solution by Homogeneous Precipitation Process at Low Temperature (저온 균일침전법으로 $TiOCl_2$ 수용액에서 얻은 $TiO_2$ 초미분체의 형성기구)

  • 김선재;이희균;박순동;전치중;이창규;김흥회;이은구
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.5
    • /
    • pp.473-478
    • /
    • 2000
  • The TiO2 powder with the values of the large specific surface area more than 150$m^2$/g has been prepared with the homogeneous precipitation process below 5$0^{\circ}C$ and its formation mechanism was investigated using the SEM, TEM and Raman Spectroscopy. With the spontaneous hydrolysis of aqueous TiOCl2 solutions, all the precipitates were fully and homogeneously crystallized with the rutile TiO2 phase simply by heating, which as transformed to the anatase TiO2 phase as increasing the addition of SO42- ions to the aqueous TiOCl2 solution. The precipitates were formed with spherical secondary particles which consisted of acicular, spherical and mixed primary particles corresponding to the rutile, anatase and mixed phases, respectively. It can be thought that the formation and phase determination of crystalline TiO2 powders even at ambient temperature would be related with the existence of the capillary force. This force might be varied depending on the shape change of the primary particles.

  • PDF

Influence of "Historical Effects" on the Rheological Properties of a Polyacrylonitrile Copolymer Solution

  • Cheng, Yumin;Zhang, Huibo;Zhang, Shuangkun;Liu, Weiwei;Wang, Jing;Cheng, Run;Ryu, SeungKon;Jin, Riguang
    • Carbon letters
    • /
    • v.14 no.1
    • /
    • pp.45-50
    • /
    • 2013
  • Polyacrylonitrile (PAN) copolymers of different molecular weights were synthesized by a suspension polymerization and precipitation polymerization method. The rheology behaviors of the synthesized PAN copolymers were investigated in relation to their molecular weight, solid content and melting temperature. The influence of "historical effects" on the spinning solution of PAN was studied by analyzing the laws of viscosity considering the diversification time and temperature. The viscosity disciplines of each spinning solution conformed well to the rheological universal laws in a comparison of the suspension polymerization product with that of precipitation polymerization. Viscosity changes in the swelling process of dissolution were gentler in the suspension polymerization product; a small amount of water will quickly debase the solution viscosity, and high-speed mixing can greatly shorten the time required by the spinning solution to reach the final viscosity.

Process Study on Alumina-zirconia Nanocomposite via Ammonolysis Route

  • Naoya Enomoto;Tang, Jun-Mu;Masato Uehara;Hideaki Maeda;Junichi Hojo;Nakagawa, Zenbe-e
    • Proceedings of the Korea Association of Crystal Growth Conference
    • /
    • 2000.06a
    • /
    • pp.143-150
    • /
    • 2000
  • Wet-chemical process using ammonia to precipitate aluminum ion dissolved in a zirconia sol solution is examined. Formation of crystalline bayerite is unfavorable for fine dispersion of zirconia nanoparticles in alumina matrix after heat treatment. To avoid the bayerite formation, it was preferred to make a precipitation with a diluted ammonia or with an ammonia gas flow at high temperature. By optimizing the precipitation process and the calcination temperature, we successfully prepared the uniform microstructure in which tetragonal zirconia particles of ∼30nm is finely dispersed within the alumina grains.

  • PDF

Chemical Precipitation Treatment for the Disperse Dyes Removal (분산성 염료의 제거를 위한 응집처리)

  • 한명호;박종득;허만우
    • Textile Coloration and Finishing
    • /
    • v.14 no.2
    • /
    • pp.40-50
    • /
    • 2002
  • In order to remove the pollutants effectively in the dye wastewater by chemical precipitation process, coagulation arid flocculation test were carried out using several coagulants on various reaction conditions. It was found that the Ferrous sulfate was the most effective coagulant for the removal of disperse dye(B79), and we could get the best result lot the removal of disperse dye(B56) in the aspects of TOC removal efficiency and sludge field. When the Ferrous sulfate dosage was $800mg/\ell$, the sludge settling velocity was very fast>, and the color was effectively removed in the disperse dye(B79) solution. Although the color removal was ineffective when the Alum was used as a coagulant, the sludge field was decreased in comparison with the Ferrous sulfate or the Ferric sulfate was used in the disperse dye(B56) solution. The general color removal effect for the disperse dye(B56 and B79) solutions, the Ferric sulfate was more proper coagulant than the Alum. It was showed that TOC removal was improved 5% and over by the addition of Calcium hydroxide, and $30mg/\ell$ of sludge yield was decreased(B79). When Alum or Ferric sulfate was used as a coagulant, pH condition for most effective color removal was 5 in B56 solution. In case of Ferrous sulfate as a coagulant, most effective pH condition for color removal was 9. When Ferric sulfate or Ferrous sulfate was used as a coagulant, pH condition for most effective color removal was 9 in B79 solution.

Dynamic Precipitation and Substructure Stablility of Cu Alloy during High Temperature Deformation

  • Han, Chang-Suk;Choi, Dong-Nyeok;Jin, Sung-Yooun
    • Korean Journal of Materials Research
    • /
    • v.29 no.6
    • /
    • pp.343-348
    • /
    • 2019
  • Structural and mechanical effects of the dynamical precipitation in two copper-base alloys have been investigated over a wide range of deformation temperatures. Basing upon the information gained during the experiment, also some general conclusion may be formulated. A one concerns the nature of dynamic precipitation(DP). Under this term it is commonly understood decomposition of a supersaturated solid solution during plastic straining. The process may, however, proceed in two different ways. It may be a homogeneous one from the point of view of distribution and morphological aspect of particles or it may lead to substantial difference in shape, size and particles distribution. The effect is controlled by the mode of deformation. Hence it seems to be reasonable to distinguish DP during homogeneous deformation from that which takes place in heterogeneously deformed alloy. In the first case the process can be analyzed solely in terms of particle-dislocation-particle interrelation. Much more complex problem we are facing in heterogeneously deforming alloy. Deformation bands and specific arrangement of dislocations in form of pile-ups at grain boundaries generate additional driving force and additional nucleation sites for precipitation. Along with heterogeneous precipitation, there is a homogeneous precipitation in areas between bands of coarse slip which also deform but at much smaller rate. This form of decomposition is responsible for a specially high hardening rate during high temperature straining and for thermally stable product of the decomposition of alloy.

Green Synthesis of Colloidal and Nanostructured MnO2 by Solution Plasma Process (용액 플라즈마를 이용한 콜로이드 및 나노 구조 MnO2의 친환경 합성)

  • Hyemin Kim
    • Korean Journal of Materials Research
    • /
    • v.33 no.7
    • /
    • pp.315-322
    • /
    • 2023
  • In the present work, we address the new route for the green synthesis of manganese dioxide (MnO2) by an innovative method named the solution plasma process (SPP). The reaction mechanism of both colloidal and nanostructured MnO2 was investigated. Firstly, colloidal MnO2 was synthesized by plasma discharging in KMnO4 aqueous solution without any additives such as reducing agents, acids, or base chemicals. As a function of the discharge time, the purple color solution of MnO4- (oxidation state +7) was changed to the brown color of MnO2 (oxidation state +4) and then light yellow of Mn2+ (oxidation state +2). Based on the UV-vis analysis we found the optimal discharging time for the synthesis of stable colloidal MnO2 and also reaction mechanism was verified by optical emission spectroscopy (OES) analysis. Secondly, MnO2 nanoparticles were synthesized by SPP with a small amount of reducing sugar. The precipitation of brown color was observed after 8 min of plasma discharge and then completely separated into colorless solution and precipitation. It was confirmed layered type of nanoporous birnessite-MnO2 by X-ray powder diffraction (XRD), fourier-transform infrared spectroscopy (FT-IR), and electron microscopes. The most important merits of this approach are environmentally friendly process within a short time compared to the conventional method. Moreover, the morphology and the microstructure could be controllable by discharge conditions for the appropriate potential applications, such as secondary batteries, supercapacitors, adsorbents, and catalysts.

Separation of Cobalt and Nickel from Aqueous Solution (수용액(水溶液)에서 코발트와 니켈 분리(分離))

  • Liu, Yang;Lee, Manseung
    • Resources Recycling
    • /
    • v.22 no.1
    • /
    • pp.11-19
    • /
    • 2013
  • Recovery of pure cobalt and nickel from diverse resources is important due to the increased demand for these metals. In order to get cobalt and nickel with high purity, separation of them from other metal ions is necessary. In this review, several methods to obtain pure cobalt or nickel solution, such as solvent extraction, ion exchange, precipitation were introduced and compared. For solvent extraction, the advantage and disadvantage of the separation process together with detailed process conditions were investigated.

Study of the Changes in Composition of Ammonium Diuranate with Progress of Precipitation, and Study of the Properties of Ammonium Diuranate and its Subsequent Products Produced from both Uranyl Nitrate and Uranyl Fluoride Solutions

  • Manna, Subhankar;Kumar, Raj;Satpati, Santosh K.;Roy, Saswati B.;Joshi, Jyeshtharaj B.
    • Nuclear Engineering and Technology
    • /
    • v.49 no.3
    • /
    • pp.541-548
    • /
    • 2017
  • Uranium metal used for fabrication of fuel for research reactors in India is generally produced by magnesio-thermic reduction of $UF_4$. Performance of magnesio-thermic reaction and recovery and quality of uranium largely depends on properties of $UF_4$. As ammonium diuranate (ADU) is first product in powder form in the process flow-sheet, properties of $UF_4$ depend on properties of ADU. ADU is generally produced from uranyl nitrate solution (UNS) for natural uranium metal production and from uranyl fluoride solution (UFS) for low enriched uranium metal production. In present paper, ADU has been produced via both the routes. Variation of uranium recovery and crystal structure and composition of ADU with progress in precipitation reaction has been studied with special attention on first appearance of the precipitate Further, ADU produced by two routes have been calcined to $UO_3$, then reduced to $UO_2$ and hydroflorinated to $UF_4$. Effect of two different process routes of ADU precipitation on the characteristics of ADU, $UO_3$, $UO_2$ and $UF_4$ were studied here.

Phase transformation and grain boundary precipitation related to the age-hardening of an Au-Ag-Cu-Pt-Zn alloy for crown and bridge fabrication (관교의치용 Au-Ag-Cu-Pt-Zn 합금의 시효경화성과 관련된 상변태와 입계석출)

  • Cho, Mi-Hyang
    • Journal of Technologic Dentistry
    • /
    • v.34 no.4
    • /
    • pp.345-352
    • /
    • 2012
  • Purpose: The age-hardening mechanism of an Au-Ag-Cu-Pt-Zn alloy for crown and bridge fabrication was investigated by means of hardness test, X-ray diffraction study and field emission scanning electron microscopic observation. Methods: Before hardness testing, the specimens were solution treated and then were rapidly quenched into ice brine, and were subsequently aged isothermally at $400-450^{\circ}C$ for various periods of time in a molten salt bath and then quenched into ice brain. Hardness measurements were made using a Vickers microhardness tester. The specimens were examined at 15 kV using a field emission scanning electron microscope. Results: By the isothermal aging of the solution-treated specimen at $450^{\circ}C$, the hardness increased rapidly in the early stage of aging process and reached a maximum hardness value. After that, the hardness decreased slowly with prolonged aging. However, the relatively high hardness value was obtained even with 20,000 min aging. By aging the solution-treated specimen, the f.c.c. Au-Ag-rich ${\alpha}_0$ phase was transformed into the Au-Ag-rich ${\alpha}_1$ phase and the AuCu I ordered phase. Conclusion: The hardness increase in the early stage of aging process was attributed to the formation of lattice strains by the precipitation of the Cu-rich phase and then subsequent ordering into the AuCu I-type phase. The decrease in hardness in the later stage of aging process was due to the release of coherency strains by the coarsening of tweed structure in the grain interior and by the growth and coarsening of the lamellar structure in the grain boundary. The increase of inter-lamellar space contributed slightly to the softening compared to the growth of lamellar structure toward the grain interior.