Studies on the fabrication and properties of $La_ 0.7Sr_0.3MnO_3$cathode contact prepared by glycine-nitrate process and solid state reaction method for the high efficient solid oxide fuel cells applications 0.3/Mn $O_{3}$ (고효율 고체산화물 연료전지 개발을 위한 자발 착화 연소 합성법과 고상반응법에 의한 $La_ 0.7Sr_0.3MnO_3$ 양극재료 제조 및 물성에 관한 연구)

  • Shin, Woong-Shun;Park, In-Sik;Kim, Sun-Jae;Park, Sung
    • Electrical & Electronic Materials
    • /
    • v.10 no.2
    • /
    • pp.141-149
    • /
    • 1997
  • L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ powders were prepared by both GNP(Glycine-Nitrate Process) and solid state reaction method in various of calcination temperature(800-1000.deg. C) and time in air. Also, L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ cathode contacts on YSZ(Yttria-Stabilized Zirconia) substrate were prepared by screen printing and sintering method as a function of sintering temperature(1100-1450.deg. C) in air. Sintering behaviors have been investigated by SEM(Scanning Electron Microscope) and porosity measurement. Compositional and structural characterization were carried out by X-ray diffractometer and ICP AES(Inductively Coupled Plasma-Atomic Emission Spectrometry) analysis. Electrical characterization was carried out by the electrical conductivity with linear 4 point probe method. As the calcination period increased in solid state reaction method, L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ phase increased. Although L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ single phase was obtained only for 48hrs at 1000.deg. C, in GNP method it was easy to get single and ultra-fine L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ powders with submicron particle size at 650.deg. C for 30min. The particle size and thickness of L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ cathode contact by solid state reaction method did not change during the heat treatment, while those by GNP method showed good sintering characteristics because initial powder size fabricated from GNP method is smaller than that fabricated from solid state reaction method. Based on enthalpy change from thermodynamic data and ICP-AES analysis, it was suggested to make cathode contact in composition of (L $a_{0.7}$S $r_{0.3}$)$_{0.91}$ Mn $O_{3}$ which have little second phase (L $a_{2}$Z $r_{2}$ $O_{7}$) for high efficient solid oxide fuel cells applications. As (L $a_{0.7}$S $r_{0.3}$)$_{0.91}$Mn $O_{3}$ cathode contact on YSZ substrate was sintering at 1250.deg. C the temperature that liquid phase sintering did not occur. It was possible to obtain proper cathode contacts with electrical conductivity of 150(S/cm) and porosity content of 30-40%.m) and porosity content of 30-40%.

  • PDF

The Synthesis of $ZrO_2+12 mol% CeO_2$ Powders by Coprecipitation Technique and Their Sintering Behaviors (공침법을 이용한 $ZrO_2+12 mol% CeO_2$ 분말합성 및 소결특성)

  • 강희복;김윤호
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.8
    • /
    • pp.879-885
    • /
    • 1994
  • Coprecipitation technique was used to synthesize ZrO2+12 mol% CeO2 powders with ZrOCl2.8H2O and Ce(NO3)3.6H2O as starting materials. The powders were dried on different conditions such as distilled water, ethanol, and azeotropic distillation. The powders prepared by azeotropic distillation showed weak aggregation of particles and the average particle size of powders calcined at 85$0^{\circ}C$ for 1 hour was 0.19 ${\mu}{\textrm}{m}$. The optimum sintering temperature and holding time are 130$0^{\circ}C$ and 2.5~10 hours, respectively. Beyond the optimum conditions, a phase transition from tetragonal to monoclinic causes to produce cracks in the sintered bodies and to decrease the density.

  • PDF

Studies on the Control of Porosity and Mean Pore Size in Cordierite Ceramics (Cordierite의 기공률 및 기공경조절에 관한 연구)

  • Yang, Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.4
    • /
    • pp.399-405
    • /
    • 1998
  • The effect of each factor on the porosity and mean pore size of cordierite(2Mg$.$2{{{{ {Al}_{2 } {O }_{3 } }}$.$5{{{{ {SiO}_{2 } }}) ceram-ics which have been mainly used for hot gas filter was investigated by using orthogonal array. The poros-ity was observed to increase with the content of graphite added as pore-forming material and decrease with increasing talc size. The effects of the other factors the graphite size sintering temperature and hold-ing time at sintering temperature were observed to be small relatively. In case of mean pore size the ef-fect of talc size on the mean pore size of cordierity was investigated to be the largest. The mean pore size was observed to increase with increasing talc size.

  • PDF

Electrical Properties of Ultrafine $(CeO_2)_{0.9}(Gd_2O_3)_{0.1}$ Powders Prepared by Glycine Nitrate Process for the High Efficient Solid Oxide Fuel Cell Applications

  • Lee, Kang-Ryeol;Park, Sung
    • The Korean Journal of Ceramics
    • /
    • v.7 no.1
    • /
    • pp.6-10
    • /
    • 2001
  • Ultrafine $(CeO_2)_{0.9}(Gd_2O_3)_{0.1}$ solid solution powders synthesized by the glycine-nitrate process, with specific surface areas of $19-23\;\textrm{m}^2$/g were sintered at $1500^{\circ}C$ for various sintering times and then their electrical characteristics were investigated using AC impedance and four-point probe measurements. The electrical resistivity of the sintered $(CeO_2)_{0.9}(Gd_2O_3)_{0.1}$ bodies showed the minimum value at the sintering time of 10 hrs. The minimum total resistivity of the $(CeO_2)_{0.9}(Gd_2O_3)_{0.1}$ bodies sintered at $1500^{\circ}C$ for 10 hrs seems to result from the lowest activation energy for the electrical resistivity by the combination between the activation energies for the resistivities at the grain interior and grain boundary.

  • PDF

Development of Cast Iron Bonded Grinding Wheel by Using Spheroidization Mechanism of Graphite (흑연의 구상화기구를 이용한 주철본드 다이어몬드 숫돌의 개발)

  • 유기태;정해도;전형일
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1995.10a
    • /
    • pp.61-64
    • /
    • 1995
  • Grinding has been adapted as a finishing process,which can carry out form and surface integrity at the same time. Recently, high efficient and precise grinding technique is required bacause the needs for functional parts such as silicon wafer,ceramic,and electric materials are increasing. Accordingly, the development of grinding wheel appropriate to that purpose is very important. So, in this paper we newly developed a diamond grinding wheel by applying the superior characteristics of spheroidal graphite of the cast iron sintered product. Especially, a electric resistance sintering method was applied in which rapid heat treatment is possible. Finally, we have achieved successful results that the grinding wheel has high hardness,durability and grinding ability,and satisfies above conditions.

  • PDF

Characteristics of Sintering Densification of Co and Fe+Co Fine Powders (Co와 Fe+Co혼합미분의 소결치밀화 특성)

  • 임태환
    • Journal of Powder Materials
    • /
    • v.3 no.2
    • /
    • pp.97-103
    • /
    • 1996
  • The densification of the compacts of pure Co, Fe+50%.Co and Fe+25% Co sintered under H$_2$ gas or in vacuum was investigated. The effects of AL, Nb, Ti, and V additions on the densification were also studied. The sintered compact of Co was fully-dense when the density of the compact was lower than $Dg^c$. However, above $Dg^{c}$, it was never fully-dense regardless of sintering atmosphere, temperature, and time. The densification of sintered compacts of Fe-50% Co and Fe-25% Co were always incomplete. While the addition of AL made all compacts fully-dense, the addition of Ti was effective for the compacts of Co and Fe-25% Co. V was effective only for the Fe-25% Co. These results tell us that the particle size of Co powder, the amount of Fe, and the amount of additives forming stable oxides play on important role for the complete densification. Therefore it is desirable to reduce or eliminate the equilibrium pressure of H$_{2}$O or CO in isolated pores to obtain a fully-dense sintered compact.

  • PDF

The Piezoelectric Characteristics Depending on the GrainSize of the PT-PZ-PNN Ceramics (압전변압기용 PT-PZ-PNN 세라믹스의 그레인 크기에 따른 압전특성)

  • 박정호;김철수;김성곤;이상렬
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.10
    • /
    • pp.815-820
    • /
    • 2001
  • The piezoelectric properties of the PT-PZ-PNN system ceramics were investigated depending on the variati on of the grain size. The grain size was varied by sintering temperature, and additive. The effect of the grain size on the electrical, dielectric, and piezoelectric properties was studied with respect to the feasibility of the application for the piezoelectric transformer. Grain size increased as the PMW contents increased. The smaller the particle size used, the smaller the grain size obtained. Specimens are densily sintered. Dielectric and piezoelectric properties are not always improved in proportion to the grain sizes. When he particle size are fine and the grain size are increased properly with the optimum additives, the piezoelectric preperties have good values. the specimen sintered at 1200$\^{C}$ with PMW 2 mol% and MnO$\_$2/ 0.5wt% contents exhibited good piezoelectric properties for a piezoelectric transformer.

  • PDF

A study on the Microwave Dielectric Properties of Ba(Mg,Co)(Ta,Nb)$O_3$ Ceramics (Ba(Mg,Co)(Ta,Nb)$O_3$ 세라믹의 마이크로파 유전특성에 관한 연구)

  • Lee, Moon-Kee;Chung, Jang-Ho;Bae, Seon-Gi;Lee, Young-Hi
    • Proceedings of the KIEE Conference
    • /
    • 1998.11c
    • /
    • pp.752-754
    • /
    • 1998
  • $Ba(Mg_{(1-x)}Co_x)_{1/3}(Ta_{(1-x)}Nb_x)_{2/3}O_3$ ($x=0.3{\sim}0.6$) ceramics were prepared by the conventional mixed oxide method. The sintering temperature and time were of $1400{\sim}1575[^{\circ}C]$,5[hr.] respectively. The structural and microwave dielectric Properties were investigated with composition ratio and sintering temperature. And then the application for the microwave dielectric resonator was investigated.

  • PDF

Study on the Dielectric and Voltage-Current Properties of $(Sr{\cdot}Ca)TiO_3$-based Ceramics ($(Sr{\cdot}Ca)TiO_3$계 세라믹의 유전 및 V-I 특성에 관한 연구)

  • Kang, Jae-Hun;Choi, Woon-Shik;Kim, Tae-Wan;Song, Min-Jong
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.09a
    • /
    • pp.72-75
    • /
    • 2001
  • In this paper, the $Sr_{1-x}Ca_{x}TiO_{3}(0{\leq}x{\leq}0.2)$ 2)-based grain boundary layer ceramics were fabricated to measured dielectric properties and voltage-current properties. The sintering temperature and time were $1420\sim1520^{\circ}C$, 4hours, in $N_{2}$ gas, respectively. The structural and the dielectric properties were investigated by SEM, X-ray, HP4194A and K6517. The 2nd phase formed by thermal diffusion from the surface lead to a very high apparent dielectric constant, $\varepsilon_r$ > 50000. X-ray diffraction patterns exhibited cubic structure for all specimens. Increasing content of Ca, the peak intensity were decreased.ﱇﶖ⨀ਆᘍ܀㘱㔮㠹㬅K䍄乍

  • PDF

Cation Ordering and Microwave Dielectric Properties of $Ba(Mg_{1/3}Nb_{2/3})O_3$Ceramics: I. Long-Range Order Parameter ($Ba(Mg_{1/3}Nb_{2/3})O_3$ 세라믹스의 양이온 규칙구조와 유전특성: I. 장거리 규칙도)

  • 김영웅;박재환;김윤호;박재관
    • Korean Journal of Crystallography
    • /
    • v.12 no.2
    • /
    • pp.76-80
    • /
    • 2001
  • We have studied the effect of sintering conditions on the long-range order parameter of the 1 : 2 cation ordering in Ba(Mg/sub 1/3/Nb/sub 2/3/)O₃microwave dielectrics prepared through a columbite precursor method. It is found that the order parameter depends strongly on the sintering conditions. As the heat-treatment time increases at 1350℃, the long-range order parameter decreases. When sintered at 1500℃ for 4 hours, BMN shows a high long-range order parameter of 0.94.

  • PDF