• Title/Summary/Keyword: Sintered Preform

Search Result 26, Processing Time 0.022 seconds

Structure and Properties of EN AC AlSi12 Alloy Reinforced by Ceramic Fibre and Particles

  • Dobrzanki, Leszek A.;Kremzer, Marek
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1078-1079
    • /
    • 2006
  • The paper presents the possibilities of obtaining new composite materials based on sintered porous ceramics with particles and fibre of $Al_2O_3$ infiltrated by aluminum alloy. The EN AC - AlSi12 alloy features the matrix material, whereas the RF50AX-301 preform, of Saffil Automotive, was used as the reinforcement. Examinations of ceramics preforms permeability were made. Metallographic examination of composite materials made on light microscope and in scanning electron microscope show that aluminum alloys fill micropores in the matrix. New composite materials show twice higher value of hardness in comparison with matrix. Results indicate that it is possible to infiltrate porous ceramic with liquid aluminum alloy to obtain new composite materials were advantageous properties of each component are connected.

  • PDF

Fabrication and Properties of SiC Candle Filter by Vacuum Extrusion and Ramming Process (II) (진공 압출성형 및 래밍성형 공정에 의한 탄화규소 캔들 필터 제조 및 특성 (II))

  • Han, In-Sub;Seo, Doo-Won;Kim, Se-Young;Hong, Ki-Seog;Woo, Sang-Kuk;Kim, Young-Wook
    • Journal of the Korean Ceramic Society
    • /
    • v.47 no.6
    • /
    • pp.515-523
    • /
    • 2010
  • Porous SiC candle filter preforms were fabricated by extrusion and ramming process. To fabricate SiC candle filter preform, commercially available F180 mesh ($85\;{\mu}m$) $\alpha$-SiC powder and $44\;{\mu}m$ mullite, $CaCO_3$ powder were used as the starting materials. The candle type preforms were fabricated by vacuum extrusion and ramming process, and sintered at $1400^{\circ}C$ 2 h in air atmosphere. Corrosion test of the sintered candle filter specimens as forming method was performed at $600^{\circ}C$ for 2,400 h in simulated IGCC syngas atmosphere. The effect of forming method on mechanical properties, pore distribution, microstructure and crystalline phase was investigated.

forming of High Density Bevel Gear for Industrial Machinery (산업기계용 고밀도 Bevel Gear 제품화를 위한 성형성 연구)

  • 임성주;윤덕재;최석우;박훈재;김승수;나경환
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.2 no.1
    • /
    • pp.1-6
    • /
    • 2001
  • This study is concerned with the cold forging of sintered preform by rotary forging process and direct powder compacting process. An experiment has been carried out using the rotary powder forging press (500kN) which had been designed and equipped with the rotational conical die inclined to the central axis of the press at certain angle The effect of process variables was observed and measured by several mechanical test, such as hardness distribution density, and microstructure of the specimens. It is found that the highly densified P/M parts can be obtained and this process is very effective for improving quality of the powder products.

  • PDF

Microstructure and Mechanical Properties of TiC-Ni/Al Composites by the Reaction-Bonding Method (반응결합법에 의한 TiC-Ni/Al 복합체의 미세구조 및 기계적 특성)

  • 한인섭;우상국;김흥수;양준환;정윤중
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.5
    • /
    • pp.536-546
    • /
    • 1996
  • The TiC-Ni/Al reaction-bonding composites were prepared by the infiltration of Ni/Al melt into the TiC preforms. The microstructure the reaction composition crystalline phase and the mechanical properties of the composites were investigated. During the reaction-bonding Ni/Al mixture had a good wettability and per-meability with TiC preform and pore-free and fully dense sintered bodies were produced. In the case of the Ni/Al atomic ratio of 0.3 and 0.5 TiC raw particle shape was changed to irregular particles because of the decomposition in the liquid matrix and its phenomena was more distinguished in the Al-rich liquid matrix. With increasing more than 1 of the Ni/Al atomic ratio the sample of TiC grain shape was changed from spherical to palatelet particles. Also with increasing the atomic ratio of Ni/Al bending strength and fracture spherical to palatelet particles. Also with increasing the atomic ratio of Ni/Al bending strength and fracture toughness were increased and its maximum value was 1073 MPa and 11 MPa.m1/2 respectively.

  • PDF

Effect of Green Microstructure on Sintered Microstructure and Mechanical Properties of Reaction-Bonded Silicon Carbide (성형미세구조가 반응소결 탄화규소체의 소결미세구조 및 기계적 특성에 미치는 영향)

  • 박현철;김재원;백운규;최성철
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.1
    • /
    • pp.97-105
    • /
    • 1999
  • In the binary system of SiC and carbon, porosity and pore size distribution of green body was controlled by varying pH, by the addition of polyelectrolyte dispersants, and by using different particle size of starting powders. The preforms having different green microstructure were fabricated by slip casting from suspensions having different dispersion condition. The reaction bonding process was carried out for these preforms. The condition of reaction bonding was 1600$^{\circ}C$ and 20 min. under vacuum atmosphere. The analyses of optical and SEM were studied to investigate the effect of green microstructure on that of reaction bonded silicon carbide and subsequently the mechanical properties of sintered body was investigated. Different green microstructures were obtained from suspensions having different dispersion condition. It was found that the pore size could be remarkably reduced for a fine SiC(0.5$\mu\textrm{m}$). The bimodal microstructure was not found in the present study, which is frequently observed in the typical reaction bonded silicon carbide. It is considered that the ratio between SiC and C was responsible for the formation of bimodal microstructure. For the preform fabricated from the well dispersed suspension, the 3-point bending strength of reaction-bonded silicon carbide was 310${\pm}$40 MPa compared to the specimen fabricated from relatively agglomerated particles having lower value 260${\pm}$MPa.

  • PDF

Evaluation of Mechanical Properties and Microstructural Behavior of Sintered WC-7.5wt%Co and WC-12wt%Co Cemented Carbides

  • Raihanuzzaman, Rumman Md.;Song, Jun-U;Tak, Byeong-Jin;Hong, Hyeon-Seon;Hong, Sun-Jik
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.05a
    • /
    • pp.58.1-58.1
    • /
    • 2011
  • WC-Co and other similar cemented carbides have been widely used as hard materials in industrial cutting tools and as mould metals; and a number of techniques have been applied to improve its microstructural characteristics, hardness and ear resistance. Cobalt is used primarily to facilitate liquid phase sintering and acts as a matrix, i.e. a cementing phase between WC grains. A uniform distribution of metal phase in a ceramic is beneficial for improved mechanical properties of the composite. WC-Co, starting from initial powders, is vastly used for a variety of machining, cutting, drilling, and other applications because of its unique combination of high strength, high hardness, high toughness, and moderate modulus of elasticity, especially with fine grained WC and finely distributed cobalt. In this study, that started with two different compositions of initial powders, WC-7.5wt%Co and WC-12wt%Co with initial powder size being 1~3 ${\mu}m$, magnetic pulsed compaction followed by subsequent vacuum sintering were carried out to produce consolidated preforms. Magnetic Pulsed Compaction (MPC), a very short duration (~600 ${\mu}s$), high pressure (~4 Gpa), high-density preform molding method was used with varied pressure between 0.5 and 3.0 Gpa, in order to reach an initial high density that would help improve the sintering behavior. For both compositions and varied MPC pressure, before and after sintering, changes in microstructural behavior and mechanical properties were analyzed. With proper combination of MPC pressure and sintering, samples were obtained with better mechanical properties, densification and microstructural behavior, and considerably improved than other conventional processes.

  • PDF