• Title/Summary/Keyword: SiC particle size

Search Result 330, Processing Time 0.026 seconds

A Study on the Mechanism for the Formation of Partices in electroless Ni Composite Coating(II) (무전해 Ni 복합도금 과정에서 분말의 공석기구에 대한 연구(II))

  • 이원해;이승평
    • Journal of the Korean institute of surface engineering
    • /
    • v.22 no.2
    • /
    • pp.78-87
    • /
    • 1989
  • Mechanism of formation of electroless composite coatings is similar to that of electrodeposited composite coating, but the amount of particles entraped in electroless coating is higher that the one of electrodeposited coatings. The methol of entrapment by the metal for SiC and Al2O3 particles is different from that for WC particles. In the former case the particles are gracually engulfed by the depositing metal, wheran with WC a metal envelope is rapidly fomed around each particles. This difference can be attributed to the difference in electrical resistivity of the particles. Inclusion density of SiC and Al2O3 particles during copeposition depend on the particle size, agitation condition, vabration conditions and electrolyte temperatures.

  • PDF

Morphological Study on the Soot Transition in a Propane/Air Laminar Diffusion Flame (프로판 층류확산화염의 그을음 천이에 대한 형태학적 연구)

  • Shim, Sung-Hoon;Yoo, Chang-Jong;Shin, Hyun-Dong
    • Journal of the Korean Society of Combustion
    • /
    • v.7 no.2
    • /
    • pp.24-33
    • /
    • 2002
  • The morphology of deposits on $15-{\mu}m$ thin SiC filaments has been investigated with SEM in a co-flowing, propane/air laminar diffusion flame. The average size of mature soot particles deposited in the luminous flame edge is strongly dependent on their axial position in a typical heavily sooting flame. The surface growth of liquid-phase PAHs molecules and the transition to soots from fully-developed precursors could be observed in the radial deposition of the flame. Two sooting regimes were found: one is the transition from the condensed-phase precursors; the other is the aggregation of smaller soot particles (or chains of them) to be carried along particle path lines. In the high temperature flame edge outside the soot luminous flame surface, the very thin fiber-like structures, which are about 10 nm thick, were found.

  • PDF

New Application of Clay Filler for Carbon/Carbon Composites and Improvement of Filler Effect by Clay Size Reduction

  • Jeong, Eui-Gyung;Kim, Jin-Hoon;Lee, Young-Seak
    • Carbon letters
    • /
    • v.11 no.4
    • /
    • pp.293-297
    • /
    • 2010
  • To investigate new potential application of a clay material for C/C composites, illite added C/C composites were prepared with various illite contents. The improvement of filler effect by illite size reduction was also investigated using wet ballmilling by evaluating illite/phenolic resin infiltration using bulk density and porosity measurements, chemical structural changes of the composites using XRD, and thermal oxidation stability in air of the composites using TGA. The size reduction of illite resulted in narrower particle size distribution and improved illite infiltration into carbon preform. And the resultant C/C composites prepared with illite had even more improved thermal oxidation stability in air, showing more increased IDTs up to $100^{\circ}C$, compared to those of the C/C composites with pristine illite, due to the SiC formation through carbothermal reduction between illite and carbon materials. The illite induced delay in oxidation of the illite-C/C composites was also observed and the delayed oxidation behavior was attributed to the layered structure of illite, which improved illite/phenol resin infiltration. Therefore, the potential use of illite as filler to improve oxidation stability of C/C composite can be promising. And the size reduction of illite can improve its effect on the desired properties of illite-C/C composites even more.

THE EFFECT OF SURFACE TREATMENTS ON THE SHEAR BOND STRENGTH OF REPAIRED COMPOSITES (광중합형 복합레진 수리시 표면처리가 전단결합강도에 미치는 영향)

  • Moon, Jang-Won;Lee, Kwang-Won;Park, Soo-Joung
    • Restorative Dentistry and Endodontics
    • /
    • v.24 no.1
    • /
    • pp.156-165
    • /
    • 1999
  • The purpose of this study was to evaluate the effect of surface treatments on the shear bond strength between new and old composites. Circular cavities prepared on the center of acrylic resin mold and the prepared cavities were filled with composite resin. They randomly assigned into control group and 8 groups according to the difference in surface treatments of old composites; Control group: no surface treatment, Group 1: surface treated with #120 SiC paper & bonding agent, Group 2: surface treated with #400 SiC paper & bonding agent, Group 3: surface treated with #120 SiC paper, 32% $H_3PO_4$ & bonding agent, Group 4: surface treated with #400 SiC paper, 32% $H_3PO_4$ & bonding agent, Group 5: surface treated with #120 SiC paper, primer & bonding agent, Group 6: surface treated with #400 SiC paper, primer & bonding agent, Group 7: surface treated with #120 SiC paper, 32% $H_3PO_4$, primer & bonding agent, Group 8: surface treated with #400 SiC paper, 32% $H_3PO_4$, primer & bonding agent. New composites were applicated on the old composites of experimental groups. The shear bond strengths for the experimental specimen were measured and the results were analyzed by using one way ANOVA. The observations of surface morphology after SiC paper roughening and debonded surface morphology after shear bond strength test were done by SEM. The results were as follows; 1. Shear bond strengths for specimens roughened with #120 SiC paper matching with the particle size of coarse diamond bur were significantly higher than those for the specimens with #400 SiC paper(P<0.05). By SEM, the surface of the specimens roughened with #120 SiC paper was more irregular than the specimens with #400 SiC paper. 2. Shear bond strengths for specimens treated with 32% $H_3PO_4$ etchant, primer, bonding resin were significantly higher than those for specimens treated with 32% $H_3PO_4$ and bonding resin(P<0.05). 3. Shear bond strengths for the specimens treated with 32% $H_3PO_4$ etchant and bonding resin were significantly higher than those for specimens treated with only bonding resin(P<0.05). There was no remarkable change of surface morphology after 32% $H_3PO_4$ etching. 4. It was possible to observe mixed fracture patterns (the cohesive fracture of old composite and the adhesive fracture between old and new composite) in the specimens roughened with #120 SiC paper, but almost adhesive fracture in the specimens roughened with #400 SiC paper.

  • PDF

Strength Properties and Elastic Waves Characteristics of Silicon Carbide with Damage-Healing Ability (손상치유 능력을 가지는 탄화규소의 강도 특성과 탄성파 특성)

  • KIM MI-KYUNG;AHN BYUNG-GUN;KIM JIN-WOOK;PARK IN-DUCK;AHN SEOK-HWAN;NAM KI-Woo
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2004.05a
    • /
    • pp.337-341
    • /
    • 2004
  • Engineering ceramics have superior heat resistance, corrosion resistance, and wear resistance. Consequently, these art significant candidates for hot-section structural components of heat engine and the inner containment of nuclear fusion reactor. Besides, some of them have the ability to heal cracks and great benefit can be anticipated with great benefit the structural engineering field. Especially, law fracture toughness of ceramics supplement with self-healing ability. In the present study, we have been noticed some practically important points for the healing behavior of silicon nitride, alumina, mullite with SiC particle and whisker. The presence of silicon carbide (SiC) in ceramic compound is very important for crack-healing behavior. However, self-healing of SiC has not been investigated well in detail yet. In this study, commercial SiC was selected as sample, which can be anticipated in the excellent crack healing ability. The specimens were produced three-point bending specimen with a critical semi-circular crack of which size that is about $50-700{\mu}m$. Three-point bending test and static fatigue test were performed cracked and healed SiC specimens. A monotonic bending load was applied to cracked specimens by three-point loading at different temperature. The purpose of this paper is to report Strength Properties and Elastic Waves Characteristics of Silicon Carbide with Crack Healing Ability.

  • PDF

Fabrication of SiCp/Al Alloy Composites by In-situ Vacuum Hot Press Process (In-situ Vacuum Hot Press 공정을 이용한 SiCp/Al 복합재료의 제조)

  • Choe, Se-Won;Hong, Seong-Gil;Kim, Yeong-Man;Jang, Si-Yeong;Gang, Chang-Seok
    • Korean Journal of Materials Research
    • /
    • v.11 no.7
    • /
    • pp.590-598
    • /
    • 2001
  • SiCp/pure Al and SiCp/2024Al MMCs were fabricated by in-situ VHP process designed specially just in this study which is composed of the vacuum hot press at range from R.T. to $500^{\circ}C$ and the continuous extrusion without canning process at $520^{\circ}C$. It was investigated the effect of SiC particle size, volume fraction and extrusion ratio on the tensile properties and micro structure in auf composites. In case of the 10:1 extrusion ratio, but SiCp/pure Al and SiCp/2024Al composites were shown a sound appearance and a good micro structure without crack of SiCp as well as uniform distribution of SiCp. However, in case of the 16:1 extrusion ratio, the number of cracked SiC particles more than increased in a higher volume fraction composite and 2024Al matrix composite compared with pure Al matrix one. The tensile strength of the composites reinforced smaller SiCp was higher than that of the bigger SiCp reinforced in same volume fraction and extrusion ratio.

  • PDF

The Crystallization of $Li_2O-MgO-MgF_2-SiO_2$ Glass System by $B_2O_3$ addition (B$_2$O$_3$의 첨가에 따른 저온 소결기판용 $Li_2O-MgO-MgF_2-SiO_2$)

  • 박대현;강원호
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1997.11a
    • /
    • pp.39-43
    • /
    • 1997
  • Effects of B$_2$O$_3$ addition in the Li$_2$O-MgO-MgF$_2$-SiO$_2$g1ass system were investigated in order to make glass-ceramics for low temperature firing substrate. Base glass was made by melting at 145$0^{\circ}C$ . This glass was analyzed by THA and DTA to settle nucleation and crystallization temperature. After crystallization. crystal phase and microstructure were absorvated by XRD and SEM. Glass powders were made by water swelling method. Average particle size was 5.44${\mu}{\textrm}{m}$

  • PDF

Microstructural changes during semi-solid state processing of hypereutectic Al-Si alloys (고액공존 과공정 Al-Si합금의 교반응고시 미세조직변화)

  • Ryoo, Young-Ho;Kim, Do-Hyang
    • Journal of Korea Foundry Society
    • /
    • v.15 no.5
    • /
    • pp.483-493
    • /
    • 1995
  • The microstructural changes during semi-solid state processing of hypereutectic Al-Si alloy has been investigated in the present study. Stirring of semi-solid slurry results in the morphological changes of the primary Si particles, i.e. from angular rod shape to near-spherical shape. Besides the spherodization of primary Si particles, the average particle size increases, especially, at much higher rate in the final stage than that in the early stage of stirring. Various microstructure characterization techniques, such as anisotropic etching, SEM imaging and ECP analysis, reveal that the spherodization of primary Si particles occurs by the combinations of the mechanisms of coalescence, fracture, and wear of the individual particles. Isothermal shearing of hypereutectic Al-Si at $580^{\circ}C$ shows that spherical ${\alpha}-Al$ particles are formed by the dissociation of Al-Si eutectic structure at the early stage of isothermal shearing. The spherical ${\alpha}-Al$ particles gradually grow by the mechanisms of Ostwald ripening and coalescence of the particles.

  • PDF

A study on the properties of artificial aggregates containing bottom ash from the power plant and waste catalyst slag (화력발전소 바닥재와 폐촉매 슬래그로 제조된 인공골재의 특성 연구)

  • Jo, Si-Nae;Kang, Seung-Gu
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.22 no.4
    • /
    • pp.200-206
    • /
    • 2012
  • The artificial aggregate composing of coal bottom ash and waste catalyst slag (7 : 3, wt%) were fabricated using direct sintering method and, the bloating properties of aggregates were investigated as a function of raw material particle size and sintering temperature. Most of the artificial aggregates sintered at over $1150^{\circ}C$ showed the bloating phenomenon regardless of particle size of the raw materials. Consequently, the specific gravity of the aggregates was drastically decreased to below 1.4. The aggregates containing waste catalyst slag of $90{\mu}m$ under among the W-series specimens, however, did not show the noticeable bloating phenomenon. For the aggregates sintered at lower temperature as $1050{\sim}1150^{\circ}C$, the specific gravity increased with particle size of raw materials. Also, the water absorption of all aggregates decreased with the sintering temperature. The aggregates fabricated in this study met the lightweight aggregate standard showing the specific gravity 1.7~1.4 and water absorption 8~19 % and, therefore, can be applicable for the various fields.

Influence of Melt Processing Factors on Microstructures of SiCp/Ma-Al Composites (SiCp/Mg-Al 복합재료의 조직에 미치는 용융가공의 영향)

  • Yoon, Yeo-Chang;Choi, Jeong-Cheol;Nam, Tae-Woon;Park, Ik-Min
    • Journal of Korea Foundry Society
    • /
    • v.13 no.4
    • /
    • pp.359-368
    • /
    • 1993
  • Mg-9wt.%Al and Mg-9wt.%-1.6wt%Zn/SiCp(particle size $40{\mu}m$) metal-matrix-composite specimens were manufactured by rheo-compocasting method, known for its effect of improving the wettability. The ceramic reinforcement particles(SiCp) were dispersed in the semi-solid magnesium alloy matrix slurry being vigorously stirred in a high frequency induction furnace under inert atmosphere. A microstructural study of the dispersed particles in the specimens, prepared under different conditions as regards the time(10min, 20min, 30min) and temperature of the stirring, was made with the aid of optical microscope and SEM. The effect of superheating was also observed. It is revealed that 30 minutes' stirring time of the semi-solid at 40% solid fraction temperature(Mg-9wt.%Al : $590^{\circ}C$, AZ91 : $576^{\circ}C$), as determined by the lever rule, gives a satisfactorily uniform distribution of the particles. The superheating is observed to enhance further the uniformity.

  • PDF