Total reflection X-ray fluorescence spectroscopy using synchrotron radiation source called as TRSFA was explored to achieve high sensitivities to impurity metals on Si wafer surface. It consists of monochromating part to select a specific wavelength, slit part to shield direct beam and to control monochromated beam, and main chamber to dectect fluorescent X-ray counts of impurities on si wafer. Monochromated X-ray of 10.90 KeV was selected and the optimum total reflection condition on silicon wafer was obtained through tuning the dead time and fluorescent X-ray count of Si and Fe. TRSFA system could increase the sensitivity as high as 50 times in comparision with TRXFA using normal X-ray source. But the trend was varied since the surface conditions of Si wafers and, therefore, the reflectivities were different. Furthemore, there seems to be a promising path to reaching a detection limit useful to the next generation metal impurities control, because Fe impurity below to the $5\times10^{9}\textrm{atomas/cm}^2$ can be detectable through the developed TRSFA system.
Journal of the Korean Society of Manufacturing Technology Engineers
/
v.6
no.4
/
pp.34-38
/
1997
This paper presents a joining method by using the silicon wafer in order to apply to joint to the 3-dimensional structures of semiconductor device, high-speed , high integration, micro machine, silicon integrated sensor, and actuator. In this study, the high atomic beam, stabilized by oxidation film and organic materials at the material surface, is investigated, and the purified is obtained by removing the oxidation film and pollution layer at the materials. And the unstable surface is obtained, which can be easily joined. In order to use the low temperatures for the joint method, the main subjects are obtained as follows: 1) In the case of the silicon wafer and the silicon wafer and the silicon wafer of alumina sputter film, the specimens can be jointed at 2$0^{\circ}C$, and the joining strength is 5Mpa. 2) The specimens can not always be joined at the room temperatures in the case of the silicon wafer and the silicon wafer of alumina sputter film.
Si wafer direct bonding(SDB) technology is very attractive for both Si-on-insulator(SOI) electronic devices and MEMS applications. This paper presents on pre-bonding according to HF pre-treatment conditions in Si wafer direct bonding. The characteristics of bonded sample were measured under different bonding conditions of HF concentration and applied pressure. The bonding strength was evaluated by tensile strength method. A bond characteristic on the interface was analyzed by using FT-IR, and surface roughness according to HF concentration was analyzed by AFM. Si-F bonds on Si surface after HF pre-treatment are replaced by Si-OH during a DI water rinse. Consequently, hydrophobic wafer was bonded by hydrogen bonding of Si-OH$\cdots$(HOH$\cdots$HOH$\cdots$HOH)$\cdots$OH-Si. The pre-bonding strength depends on the HF pre-treatment condition before pre-bonding. (Min : $2.4kgf/cm^2{\sim}$Max : $14.9kgf/cm^2$)
Kim, Seon-Un;Sin, Dong-Seok;Lee, Jeong-Yong;Choe, In-Hun
Korean Journal of Materials Research
/
v.8
no.10
/
pp.890-897
/
1998
The direct wafer bonding between n-InP(001) wafer and the ${Si}_3N_4$(200 nm) film grown on the InP wafer by PECVD method was investigated. The surface states of InP wafer and ${Si}_3N_4$/InP which strongly depend upon the direct wafer bonding strength between them when they are brought into contact, were characterized by the contact angle measurement technique and atomic force microscopy. When InP wafer was etched by $50{\%}$ HF, contact angle was $5^{\circ}$ and RMS roughness was $1.54{\AA}$. When ${Si}_3N_4$ was etched by ammonia solution, RMS roughness was $3.11{\AA}$. The considerable amount of initial bonding strength between InP wafer and ${Si}_3N_4$/InP was observed when the two wafer was contacted after the etching process by $50{\%}$ HF and ammonia solution respectively. The bonded specimen was heat treated in $H^2$ or $N^2$, ambient at the temperature of $580^{\circ}C$-$680^{\circ}C$ for lhr. The bonding state was confirmed by SAT(Scannig Acoustic Tomography). The bonding strength was measured by shear force measurement of ${Si}_3N_4$/InP to InP wafer increased up to the same level of PECVD interface. The direct wafer bonding interface and ${Si}_3N_4$/InP PECVD interface were chracterized by TEM and AES.
In this study, surface roughness and interfacial defect characteristics were analyzed after forming a high-k oxide film on the surface of a prime wafer and a test wafer, to study the possibility of improving the quality of the test wafer. As a result of checking the roughness, the deviation in the test after raising the oxide film was 0.1 nm, which was twice as large as that of the Prime. As a result of current-voltage analysis, Prime after PMA was 1.07 × 10 A/cm2 and Test was 5.61 × 10 A/cm2, which was about 5 times lower than Prime. As a result of analyzing the defects inside the oxide film using the capacitance-voltage characteristic, before PMA Prime showed a higher electrical defect of 0.85 × 1012 cm-2 in slow state density and 0.41 × 1013 cm-2 in fixed oxide charge. However, after PMA, it was confirmed that Prime had a lower defect of 4.79 × 1011 cm-2 in slow state density and 1.33 × 1012 cm-2 in fixed oxide charge. The above results confirm the difference in surface roughness and defects between the Test and Prime wafer.
Song, Inhyeop;Lee, Minjae;Kim, Sungdong;Kim, Sarah Eunkyung
Journal of the Microelectronics and Packaging Society
/
v.20
no.4
/
pp.81-85
/
2013
Wafer stacking technology becomes more important for the next generation IC technology. It requires new process development such as TSV, wafer bonding, and wafer thinning and also needs to resolve wafer warpage, power delivery, and thermo-mechanical reliability for high volume manufacturing. In this study, Cu CMP which is the key process for wafer bonding has been studied using Cu CMP and oxide CMP processes. Wafer samples were fabricated on 8" Si wafer using a damascene process. Cu dishing after Cu CMP and oxide CMP was $180{\AA}$ in average and the total height from wafer surface to bump surface was approximately $2000{\AA}$.
The reaction mechanisms of dry cleaning with UV-excited chlorine radical for Zn, Fe and Ti trace contaminants on the Si wafer have been studied by SEM, AFM and XPS analyses in this work. The patterned Zn, Fe and Ti films were deposited on the Si wafer surface by thermal evaporation and changes in the surface morphology after dry cleaning with $Cl_2$and UV/$Cl_2$at $200^{\circ}C$ were studied by optical microscopy and SEM. In addition, changes in the surface roughness of Si wafer with the cleaning was observed by AFM. The chemical bonding states of the Zn, Fe and Ti deposited silicon surface were observed with in-line XPS analysis. Zn and Fe were easily cleaned in the form of volatile zinc-chloride and iron-chloride as verified by the surface morphology changes. Ti which forms involatile oxides was not easily removed at room temperature but was slightly removed by UV/$Cl_2$at elevated temperature of $200^{\circ}C$. It was also found that the surface roughness of the Si wafer increased after $Cl_2$and UV/$Cl_2$cleaning. Therefore, the metallic contaminants on the Si wafer can be easily removed at lower temperature without surface damage by a continuous process using wet cleaning followed by UV/$Cl_2$dry cleaning.
Proceedings of the Materials Research Society of Korea Conference
/
2010.05a
/
pp.27.2-27.2
/
2010
In recent years, there is a strong requirement of low cost, stable microelectro mechanical systems (MEMS) for resonators, microswitches and sensors. Most of these devices consist of freely suspended microcantilevers, which are usually made by the etching of some sacrificial materials. Herein, we have attempted to use Si nanowires, inherited from the parent Si wafer, as a sacrificial material due to its porosity, low cost and ease of fabrication. Prior to the fabrication of the Si nanowires silver nanoparticles were continuously formed on the surface of Si wafer. Vertically aligned Si nanowires were fabricated from the parent Si wafers by aqueous chemical route at $50^{\circ}C$. Afterwards, the morphological and structural characteristics of the Si nanowires were investigated. The morphology of nanowires was strongly modulated by the resistivity of the parent wafer. The 3-step etching of nanowires in diluted KOH solution was carried out at room temperature in order to control the fast etching. A layer of $Si_3N_4$ (300 nm) was used for the selective fabrication of nanowires. Finally, a freely suspended bridge of zinc oxide (ZnO) was fabricated after the removal of nanowires from the parent wafer. At present, we believe that this technique may provide a platform for the inexpensive fabrication of futuristic MEMS.
Park Ji-hwan;Park So-yeon;Lee Jong-kwon;Song Tae-hwa;Ryoo Kun-kul;Lee Yoon-bae;Lee Mi-Young
Journal of the Korea Academia-Industrial cooperation Society
/
v.5
no.5
/
pp.458-461
/
2004
In order to improve the adhesion properties of copper, MPS(3-mercaptopropyltrimethoxysilane) organic film were employed. The plasma pretreatment in pure He or $He/O_{2}$ mixed gas environment greatly increased adhesion force. Adhesion force was measured by scratch test with nano indenter. Microstructures and surface roughness were observed with scanning electron microscope(SEM). The characteristics of MPS layer for pretreatment were studied with flourier transform infrared spectroscope(FT-IR) and contact angle tester. The heighest adhesion was achieved in the specimen pretreated with mixed plasma and NPS coating, which was 56mN. Other specimen showed lower value by $20{\%}$ to $30{\%}$. The roughness of substrate was not affected by the bonding strength of copper plating.
Dopant-free silicon heterojunction solar cells using Transition Metal Oxide(TMO) such as Molybdenum Oxide($MoO_X$) and Vanadium Oxide($V_2O_X$) have been focused on to increase the work function of TMO in order to maximize the work function difference between TMO and n-Si for a high-efficiency solar cell. One another way to increase the work function difference is to control the silicon wafer resistivity. In this paper, dopant-free silicon heterojunction solar cells were fabricated using the wafer with the various resistivity and analyzed to understand the effect of n-Si work function. As a result, it is shown that the high passivation and junction quality when $V_2O_X$ deposited on the wafer with low work function compared to the high work function wafer, inducing the increase of higher collection probability, especially at long wavelength region. the solar cell efficiency of 15.28% was measured in low work function wafer, which is 34% higher value than the high work function solar cells.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.