• 제목/요약/키워드: Si addition

Search Result 2,820, Processing Time 0.03 seconds

TiAl 금속간화헙물의 공식거동에 미치는 합금원소의 영향 (Effects of Alloying Elements on the Pitting Behavior of Ti-Al Intermetallic Compounds)

  • 이호종;최한철
    • 한국표면공학회지
    • /
    • 제31권3호
    • /
    • pp.157-164
    • /
    • 1998
  • Effects of alloying elements on the pitting behavior of Ti-Al intermetalic compounds in the electrolytic soution containing Cl- were investigated through electrochemical tets and corrosion morphologies. Corrosion potential increased in the case of Cr addition to Ti-48%Al, whereas it decreased in the case of Si and B addition. The simultaneous addition of Cr and Si increased passive current density and decrosion corrosion potential. The passive current density of N addtion was higher than that of B addition in H2SO4 solution. With the addition of alloying elements, The pitting resistance decreased in order of TiAl>TiAlSi>TiAlN>TiAlB>TiAlCr and whin siumultaneous addition, it decreased in order of TiAlCrSi>TiAlCrBN>TiAlCrrN. The surface merohology after pitting test showed that the TiAl coataining Si had for fewer pits than that containing Cr and N simultaneously.

  • PDF

$SiO_2$가 첨가된 산화아연 바리스터의 미세구조 및 전기적 특성 (Microstructure and Electrical Properties of $SiO_2$-Doped Zinc Oxide Varistors)

  • 남춘우;정순철
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권7호
    • /
    • pp.659-667
    • /
    • 1997
  • The influence of SiO$_2$on the microstructure and electrical properties of zinc oxide varistor was investigated. Zn$_2$SiO$_4$third phase in the sintered body was found at grain boundaries, multiple grain junctions, and occasionally within ZnO grains. This phase acted as a grain growth inhibitor, which retard the grain growth of the ZnO matrix by impeding migration on the grain boundaries. As SiO$_2$ addition increases, average grain size decreased from 40.6${\mu}{\textrm}{m}$ to 26.9${\mu}{\textrm}{m}$ due to the pinning effect by Zn$_2$SiO$_4$ and drag effect by Si segregation at grain boundaries, the breakdown voltage consequently increased. When SiO$_2$ addition is increased, interface state density decreased, however, the barrier height increased by decrease of donor concentration, as a result, the nonlinear exponent increased and leakage current decreased. While, as SiO$_2$ addition increase, it was found that the apparent dielectric loss factor shows a tendency of decrease. Wholly, electrical properties of zinc oxide varistor can be said to be improved by SiO$_2$addition.

  • PDF

Mg 첨가에 따른 A356 합금의 열처리 및 기계적 특성 변화 (Effects of Mg Addition on Heat Treatment and Mechanical Properties of A356 Alloy)

  • 조재찬;김광삼;임인택;김대환;심성용;임수근
    • 한국주조공학회지
    • /
    • 제36권6호
    • /
    • pp.195-201
    • /
    • 2016
  • The effects of Mg addition on heat treatment and mechanical properties of A356 alloy were investigated. With increased amounts of Mg addition to A356 alloy, the grain size decreased and eutectic Si was refined. And, this process can improve the mechanical properties. Solid solution heat treatment causes the spheroidizing of eutectic Si. In this study, although eutectic Si was refined with Mg addition, solid solution time increased from 2 hours to 6 hours with Mg addition, and aging time also increased, from 4 hours to 8 hours. After heat treatment, Mg2Si remained in a formation of Chinese script. And, Chinese script Mg2Si formed with Mg addition caused a reduction of the elongation of the alloys according to the stress concentration.

Flexural Strength of Polysiloxane-Derived Strontium-Doped SiOC Ceramics

  • Eom, Jung-Hye;Kim, Young-Wook
    • 한국세라믹학회지
    • /
    • 제52권1호
    • /
    • pp.61-65
    • /
    • 2015
  • The effect of Sr addition on the flexural strength of bulk SiOC ceramics was investigated in polymer-derived SiOC ceramics prepared by conventional hot pressing. Crack-free, dense SiOC discs with a 30 mm diameter were successfully fabricated from commercially available polysiloxane with 1 mol% strontium isopropoxide derived Sr as an additive. Agglomerates formed after the pyrolysis of polysiloxane led to the formation of domain-like structures. The flexural strength of bulk SiOC was strongly dependent on the domain size formed and Sr addition. Both the minimization of the agglomerate size in the starting powders by milling after pyrolysis and the addition of Sr, which reinforces the SiOC structure, are efficient ways to improve the flexural strength of bulk SiOC ceramics. The typical flexural strength of bulk Sr-doped SiOC ceramics fabricated from submicron-sized SiOC powders was ~209 MPa.

Nickel silicide에 대한 Pd 첨가 효과 : ab initio 계산 (Effect of Pd addition on nickel silicide : ab initio calculation)

  • 김대희;서화일;김영철
    • 반도체디스플레이기술학회지
    • /
    • 제7권1호
    • /
    • pp.7-10
    • /
    • 2008
  • Effect of Pd addition on crystal structures of two nickel silicides, NiSi and $NiSi_2$, is investigated by using an ab initio calculation. A Pd atom substitutes a Ni and Si site, respectively, to evaluate the preferable site between them. Pd prefers Ni site to Si site in NiSi, while it prefers Si site to Ni site in $NiSi_2$. The calculated total energy also indicates that the Pd substitution to Si site stabilizes the $NiSi_2$ structure. This calculated data matches well with the experimental data obtained from Atom probe.

  • PDF

과공정 Al-Si 합금의 반고상 재가열시 미세조직 변화 (Microstructural Changes during Semi-solid State in Hypereutectic Al-Si Alloy)

  • 김인준;김도향
    • 한국주조공학회지
    • /
    • 제18권6호
    • /
    • pp.541-549
    • /
    • 1998
  • Microstructural characteristics of hypereutectic Al-Si alloys during reheating at semi-solid temperature have been investigated. The size and morphology of primary Si particles in wedge-type mold-cast ingot has been compared with hot-rolled sheet and Si particulate reinforced Al composite. Effects of P and Sr addition on the morphological changes of primary Si particles have been also investigated. Observation of the solidification microstructures of the wedge-type mold-cast ingot at different cooling rates showed that alloying elements such as P and Sr affect the morphology of Si particles, especially in the area solidified at a slow cooling rate. Negligible change in the size of primary crystals was observed after reheating experiment, but ${\alpha}-halo$ formed around the Si particles and fine particles of Si precipitated in the surrounding area of the Si particles. In addition, there seemed to be no coarsening with increasing of holding time and the region of ${\alpha}-halo$ being decreased. Nucleation and recrystallization was accelerated with addition of alloying elements during hot rolling resulting in a decrease of primary Si particle size. In the case of extruded specimens, morphological change of primary Si particles was not observed after reheating. No ${\alpha}-halo$ formation was observed in Si reinforced Al composite because of the oxide film formed on the Si particles which acted as a diffusion barrier between substrate and the primary Si particles.

  • PDF

$Al_2O_3$/SiC Hybrid-Composite의 제조 (Fabrication of $Al_2O_3$/SiC Hybrid-Composite)

  • 이수영;임경호;전병세
    • 연구논문집
    • /
    • 통권26호
    • /
    • pp.103-112
    • /
    • 1996
  • $Al_2O_3/SiC$ Hybrid-Composite이 일반적인 분말공정에 의하여 제조되었다. 소결시 $\gamma-Al_2O_3에서 $\alpha-Al_2O_3$로의 전이에 seed역할을 하는 $\alpha-Al_2O_3의 첨가는 균일한 미세구조를 발달시켜 강도의 증진을 가져왔다. nano size의 SiC의 첨가는 $Al_2O_3$의 소결성과 입성장에 영향을 미쳐 파괴강도의 증진을 가져왔다. $Al_2O_3/SiC$ nano-Composite에 SiC plates의 첨가는 파괴강도의 감소를 가져왔지만, 상대적으로 파괴인성은 증진되었다. SiC plates에 nitride (BN, $Si_3N_4$ 코팅을 할 경우 crack deflection을 더욱 유발하여 파괴인성이 증진되었다.

  • PDF

Si 함량에 따른 Ti-Al-Si-C-N 코팅막의 미세구조와 기계적 특성의 변화에 관한 연구 (Effect of Si on the Microstructure and Mechanical Properties of Ti-Al-Si-C-N Coatings)

  • 홍영수;권세훈;김광호
    • 한국표면공학회지
    • /
    • 제42권2호
    • /
    • pp.73-78
    • /
    • 2009
  • Quinary Ti-Al-Si-C-N films were successfully synthesized on SUS 304 substrates and Si wafers by a hybrid coating system combining an arc ion plating technique and a DC reactive magnetron sputtering technique. In this work, the effect of Si content on the microstructure and mechanical properties of Ti-Al-C-N films were systematically investigated. It was revealed that the microstructure of Ti-Al-Si-C-N coatings changed from a columnar to a nano-composite by the Si addition. Due to the nanocomposite microstructure of Ti-Al-Si-C-N coatings, the microhardness of The Ti-Al-Si-C-N coatings significantly increased up to 56 GPa. In addition the average friction coefficients of Ti-Al-Si-C-N coatings were remarkably decreased with Si addition. Therefore, Ti-Al-Si-C-N coatings can be applicable as next-generation hard-coating materials due to their improved hybrid mechanical properties.

$Al_2O_3/SiC$ Hybrid-Composite에서 SiC에 질화물 코팅의 영향 (The Effect of Nitride Coating on SiC Platelet in $Al_2O_3/SiC$ Hybrid-Composite)

  • 이수영;임경호;전병세
    • 한국세라믹학회지
    • /
    • 제34권4호
    • /
    • pp.406-412
    • /
    • 1997
  • Al2O3/SiC hybrid-composite has been fabricated by the conventional powder process. The addition of $\alpha$-Al2O3 as seed particles in the transformation of ${\gamma}$-Al2O3 to $\alpha$-Al2O3 provided a homogeneity of the microstructure. The grain growth of Al2O3 are significantly surpressed by the addition of nano-size SiC particles. Dislocation were produced due to the difference of thermal expansion coefficient between Al2O3 and SiC and piled up on SiC particles in Al2O3 matrix, resulting in transgranular fracture. The high fracture strength of the composite was contributed to the grain refinement and the transgranular fracture mode. The addition of SiC platelets to Al2O3/SiC nano-composite decreased the fracture strength, but increased the fracture toughness. Coated SiC platelets with nitrides such as BN and Si3N4 enhanced fracture toughness much more than non-coated SiC platelets by enhancing crack deflection.

  • PDF

과공정 Al- Si 합금의 반응고 교반시 초정 Si 형상에 미치는 교반조건 및 개량원소 첨가 영향 (Effects of Stirring Condition and Refining Element Addition on the Primary Si Particle Morphology of Hypereutectic Al-Si Alloys Semi-Solid State Processing)

  • 김인준;김도향
    • 한국주조공학회지
    • /
    • 제18권5호
    • /
    • pp.474-480
    • /
    • 1998
  • Microstructural characteristics of semi-solid state processed hypereutectic Al-Si alloys have been investigated. Main concern of the present study is to investigate the effects of P and Sr addition on the size and morphology change of the primary Si particles. Refinement of the primary Si particles was observed with the addition of P and Sr at the early stage of semi-solid state processing, but such a refining effects became negligible resulting in Si particles with a near-spherical morphology with continuous stirring. This implies that the microstructural transformation mechanism became more dependent to stirring effects than to the alloying effects during semi-solid state processing. Brittle fracture and agglomeration were proposed as the mechanisms for microstructural alterations during semi-solid state processing.

  • PDF