The Examination of Strength Properties of Mortar with Variation of Fine Particle Size Distribution of Oyster Shell (굴 패각의 잔골재 입도분포 변화에 따른 모르타르의 강도특성)

  • Choi, In-Kwon;Hong, Sang-Hun;Jung, Ui-In;Kim, Bong-Joo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2017.11a
    • /
    • pp.43-44
    • /
    • 2017
  • In this study, mortar strength was measured by grinding oyster shell and changing the particle size distribution. For the experiment, the oyster shells were processed to a fine aggregate size of 10mm or less. In this experiment, seven particle size distribution conditions were selected and tested. Because oyster shells are different in density from sand, their volume ratios were calculated and converted to mass ratios of 1: 3. The strength test was carried out one day after the steam curing.

  • PDF

Fabrication of Core-Shell Structured Ni-Based Alloy Nanopowder by Electrical Wire Explosion Method

  • Lee, A-Young;Lee, Gwang-Yeob;Oh, Hye-Ryeong;Kim, Hyeon-Ah;Kim, Song-Yi;Lee, Min-Ha
    • Journal of Powder Materials
    • /
    • v.23 no.6
    • /
    • pp.409-413
    • /
    • 2016
  • Electrical wire explosion in liquid media is a promising method for producing metallic nanopowders. It is possible to obtain high-purity metallic nanoparticles and uniform-sized nanopowder with excellent dispersion stability using this electrical wire explosion method. In this study, Ni-Fe alloy nanopowders with core-shell structures are fabricated via the electrical explosion of Ni-Fe alloy wires 0.1 mm in diameter and 20 mm in length in de-ionized water. The size and shape of the powders are investigated by field-emission scanning electron microscopy, transmission electron microscopy, and laser particle size analysis. Phase analysis and grain size determination are conducted by X-ray diffraction. The result indicate that a core-shell structured Ni-Fe nanopowder is synthesized with an average particle size of approximately 28 nm, and nanosized Ni core particles are encapsulated by an Fe nanolayer.

Preparation of Methyl Methacrylate-Styrene System Core-Shell Latex by Emulsion Polymerization (유화중합에 의한 Methyl Methacrylate-Styrene계 Core-Shell 라텍스 입자 제조에 관한 연구)

  • Kim, Nam-Seok;Kim, Duck-Sool;Lee, Seok-Hee;Park, Keun-Ho
    • Journal of the Korean Applied Science and Technology
    • /
    • v.22 no.2
    • /
    • pp.96-105
    • /
    • 2005
  • Core-shell polymers of methyl methacrylate-styrene system were prepared by sequential emulsion polymerization in the presence of sodium dodecyl benzene sulfonate(SDBS) as an emulsifier using ammonium persulfate(APS) in an initiator and the characteristics of these core-shell polymers were evaluated. Core-shell composite latex has the both properties of core and shell components in a particle, whereas polymer blends or copolymers show a combined physical properties of two homopolymers. This unique behavior of core-shell composite latex can be used in various industrial fields. However, in preparation of core-shell composite latex, several unexpected matters are observed, for examples, particle coagulation, low degree of polymerization, and formation of new particles during shell polymerization. To solve this matters, we study the effects of surfactant concentrations, initiator concentrations, and reaction temperature on the core-shell structure of PMMA-PSt and PSt-PMMA. Particle size and particles distribution were measured by using particle size analyzer, and the morphology of the core-shell composite latex was observed by using transmission electron microscope. Glass temperature was also measured by using differential scanning calorimeter. To identify the core-shell structure, pH of the composite latex solutions was measured.

Buckling and Optimum Reinforcement of Axially Stiffened Cylindrical Shells (보강(補剛) 원통 Shell의 좌굴(挫屈) 및 최적보강(最適補强))

  • Jang, Chang-Doo;Nho, Wan
    • Bulletin of the Society of Naval Architects of Korea
    • /
    • v.24 no.1
    • /
    • pp.42-50
    • /
    • 1987
  • The energy expressions are formulated for the axially stiffened shell treating the stiffeners as discrete elements. The principle of minimum potential energy is employed to formulate the buckling equations for a simply supported, axially stiffened shell under uniform axial compression. The displacement functions are expended into double trigonometric series. The mode assuming method employed in this paper makes it possible to reduce the matrix size of the eigenvalue problem considerably. Effects are made to investigate the transition from overall buckling to local buckling and to verify the existence of the minimum stiffness ratio of stiffener as in the case of stiffened plate. The results of the calculation show that the critical stiffener size increase linearly as the length of the shell increases. The results also show that the overall buckling load decreases and the local buckling load has a nearly constant value as the length of the shell increases. The results show very good agreements with other computational available.

  • PDF

A study on Calcination Characteristics of Powdered Oyster Shell (굴패각 재활용 방안에 관한 기초연구 -굴패각 소성가공특성-)

  • Kim, Jong-Oh;Lee, Sang Eun;Lee, Chang-Ho
    • Journal of the Korea Organic Resources Recycling Association
    • /
    • v.15 no.1
    • /
    • pp.143-148
    • /
    • 2007
  • The objective of this study was to investigate the proper conditions of calcination and calcium extraction from powdered oyster shell. The physical characteristics such as particle size distribution, surface morphology, and thermal gravity were examined. The following result were obtained. As the powdered oyster shell was ignited in high temperature of $650^{\circ}C$ to $950^{\circ}C$, the calcination reactions was effectively progressed. The amount of weight loss during calcination would be matched with the generation of carbon dioxide gas. In the calcination of powdered oyster shell, the amount of weight loss increased according to the increased of calcination temperature and the decrease of mean particle size. It was founded that the proper temperature and retention time of calcination was $850^{\circ}C$ and 40 minute. In the extraction of calcium into liquid form using acid addition, the calcination oyster shell was more effective than the non-calcinated shell. The liquid calcium extraction technique using the calcinated oyster shell needed more researches considering cost evaluation.

  • PDF

Preparation of Polystyrene-Polyetherimide Core-Shell Particles by Dispersion Polymerization (분산중합에 의한 폴리스티렌-폴리에테르이미드 코어-셀 입자의 합성)

  • Ahn, Byung Hyun
    • Applied Chemistry for Engineering
    • /
    • v.25 no.5
    • /
    • pp.526-530
    • /
    • 2014
  • Polystyrene-poly(etheramic acid) core-shell particles were prepared by dispersion polymerization of styrene using poly(etheramic acid) obtained by the reaction of 2,2'-bis[4-(3,4-dicarboxyphenoxy) phenyl]propane dianhydride and 3,5-diamniobenzoic acid as a stabilizer. 4-Vinylbenzyltrimethylammonium chloride was used as a comonomer to increase the binding efficiency of poly(etheramic acid). When the ethanol-water mixture (7 : 3) was used as a reaction medium, particles were stabilized well and the size distribution of particles was fairly narrow. The particle size increased with the amount of styrene. The particles polymerized in the dimethylformamide-water mixture had a broad size range. Polystyrene-poly(etheramic acid) core-shell particles were transformed to polystyrene-polyetherimide core-shell particles by the chemical imidization of shells.

The Examination Fire Resistance of Mortar According to Particle Size Distrivution as Oyster Shell Fine Aggregate (굴 패각의 잔골재 입도분포 변화에 따른 모르타르의 내화성 검토)

  • Choi, In-Kwon;Jung, Ui-In;Kim, Bong-Joo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2017.05a
    • /
    • pp.71-72
    • /
    • 2017
  • The oyster shell is lightweight and exhibits strength characteristics similar to sand. In this study, mortar specimens were fabricated by crushing them and processed to 5mm or less of the fine aggregate standard, and examined the fire resistance of the mortar according to changes in particle size distribution. In this experiment, seven particle size distribution conditions were tested. In addition, the mixing ratio was fixed at 1: 3, and the experiment was conducted in terms of the volume ratio because the densities of sand and oyster shells were different.

  • PDF

Preparation of Core-shell Type Nanoparticles of Poly($\varepsilon$-caprolactone) /Poly(ethylene glycol)/Poly( $\varepsilon$-caprolactone) Triblock Copolymers

  • Ryu, Jae Gon;Jeong, Yeong Il;Kim, Yeong Hun;Kim, In Suk;Kim, Do Hun;Kim, Seong Ho
    • Bulletin of the Korean Chemical Society
    • /
    • v.22 no.5
    • /
    • pp.467-475
    • /
    • 2001
  • A triblock copolymer based on $poly(\varepsilon-caprolactone)$ (PCL) as the hydrophobic part and poly(ethylene glycol) (PEG) as the hydrophilic portion was synthesized by a ring-opening mechanism of ${\varepsilon}-caprolactone$ with PEG containing a hydroxyl group at bot h ends as an initiator. The synthesized block copolymers of PCL/PEG/PCL (CEC) were confirmed and characterized using various analysis equipment such as 1H NMR, DSC, FT-IR, and WAXD. Core-shell type nanoparticles of CEC triblock copolymers were prepared using a dialysis technique to estimate their potential as a colloidal drug carrier using a hydrophobic drug. From the results of particle size analysis and transmission electron microscopy, the particle size of CEC core-shell type nanoparticles was determined to be about 20-60 nm with a spherical shape. Since CEC block copolymer nanoparticles have a core-shell type micellar structure and small particle size similar to polymeric micelles, CEC block copolymer can self-associate at certain concentrations and the critical association concentration (CAC) was able to be determined by fluorescence probe techniques. The CAC values of the CEC block copolymers were dependent on the PCL block length. In addition, drug loading contents were dependent on the PCL block length: the larger the PCL block length, the higher the drug loading content. Drug release from CEC core-shell type nanoparticles showed an initial burst release for the first 12 hrs followed by pseudo-zero order release kinetics for 2 or 3 days. CEC-2 block copolymer core-shell type nanoparticles were degraded very slowly, suggesting that the drug release kinetics were governed by a diffusion mechanism rather than a degradation mechanism irrelevant to the CEC block copolymer composition.

Evaluation of Methods Used in the Calculation of Condition Index Using the Mussel, Mytilus coruscus (Gould, 1861) Collected from Chuja Island, Cheju, Korea (추자도산 홍합, Mytilus coruscus (Gould, 1861) 의 Condition Index 산정에 대한 연구)

  • 강도형;최광식
    • The Korean Journal of Malacology
    • /
    • v.15 no.1
    • /
    • pp.57-62
    • /
    • 1999
  • Condition indices (Cl) are considered to be useful measurements of the nutritive and health status of bivalves although studies on Cl of bivalves are limited due to the lack of a standard formula for calculating Cl. This study attempts to generate Cl of the mussel, Mytilus coruscus inhabiting along the coastal area of Chuja Island in Cheju using three primary formulas. the formulas used in this study: (1) Cl-vol= [tissue dry weight (g) 1000] /shell cavity volume (ml). (2) Cl-wt= [tissue dry weight (g) 1000] / internal shell cavity capacity (g). (3) Cl-size= tissue wet weight (g)/[shell length (mm)]$\^$3/. Monthly condition indices calculated with the three formulas are compared using ANOVA, Duncan's multiple range test and Pearson correlation coefficient. In Chuja Island M. coruscus collected ranged from 50 to 180 mm in shell length. Monthly ranges of Cl-values were 67.48 to 140.61 (Cl-vol), 74.67 to 118.02 (Cl-wt) and 1.4 10$\^$-5) to 1.6 10$\^$-5/ (Cl-size). Cl-vol values in August were higher than two Cl-values in the other months. Monthly Cl-vol was significantly different from Cl-wt and Cl-size. (p<0.05). The results of this study suggest that volumetric condition index (Cl-vol) used in this study is acceptable as a standard measure to evaluate conditions of M. coruscus.

  • PDF

Correlation Coefficient Studies on Certain Quantitative Traits in the Silkworm, Bombyx mori L.

  • Begum, A.Naseema;Yamamoto, T.
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.5 no.1
    • /
    • pp.44-52
    • /
    • 2002
  • To understand the relationship among different quantitative traits, correlation studies were performed by utilizing eighty-eight inbred strains of silkworm, Bombyx mori L. on twelve economic characters. Analysis resulted in correlation of 5th instar period with total larval period (r = 0.7882), cocoon weight with shell weight (r = 0.8326), shell weight with shell ratio (r = 0.5067), shell ratio with raw silk % (r = 0.7570), raw silk % with filament length (r = 0.3490), filament size (denier) with reelability (r = 0.3193) and boil-off loss % (r = 0.2792). Negative correlation was observed among filament length with filament size (r = 0.7582) and reelability with boil-off loss % (r = -0.3236). Correlation of different quantitative characters for quality silk production is discussed.