• 제목/요약/키워드: Shear strain

검색결과 1,848건 처리시간 0.029초

Study of shear and elongational flow of solidifying polypropylene melt for low deformation rates

  • Tanner, R.I.;Kitoko, V.;Keentok, M.
    • Korea-Australia Rheology Journal
    • /
    • 제15권2호
    • /
    • pp.63-73
    • /
    • 2003
  • An experimental technique was developed to determine the strain-rate in a tensile specimen. Then one can calculate the transient isothermal elongational viscosity. Both shear and elongational viscosities were measured to study the effect of shear and elongational fields on the flow properties. The comparison between these viscosities shows that the onset of rapid viscosity growth as crystallization solidification proceeds occurs at about the same value of time at very small deformation rates (0.0028 and 0.0047 $s^{-1}$). The comparison of these measured viscosities as functions of shear and elongational Hencky strains also reveals that the onset of rapid viscosity growths starts at critical Hencky strain values. The behaviour of steady shear viscosity as function of temperature sweep was also explored at three different low shear rates. Finally, the influence of changing oscillatory frequencies and strain rates was also investigated.

비대칭 압연한 AA1100 판재에서 잔류전단변형에 미치는 롤과 재료간의 마찰의 영향 (Effect of friction between roll and sample on residual shear strains in AA1050 sheet during asymmetrical rolling)

  • 지영규;정효태;허무영
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 추계학술대회논문집
    • /
    • pp.156-158
    • /
    • 2003
  • Sheets of aluminum alloy 1050 were asymmetrically cold rolled in a rolling mill with different roll speeds. In order to promote the shear deformation during asymmetrical rolling, cold rolling without lubrication was performed. The variation of the shear strain state during asymmetrical rolling was tackled by means of FEM calculations. Asymmetrical rolling gave rise to the development of pronounced residual shear strain gradients throughout the thickness layers.

  • PDF

안티푸라민-에스® 로션의 레올로지 특성 연구 (Rheological Properties of Antiphlamine-S® Lotion)

  • 국화윤;송기원
    • Journal of Pharmaceutical Investigation
    • /
    • 제39권3호
    • /
    • pp.185-199
    • /
    • 2009
  • Using a strain-controlled rheometer [Advanced Rheometric Expansion System (ARES)], the steady shear flow properties and the dynamic viscoelastic properties of $Antiphlamine-S^{(R)}$ lotion have been measured at $20^{\circ}C$ (storage temperature) and $37^{\circ}C$ (body temperature). In this article, the temperature dependence of the linear viscoelastic behavior was firstly reported from the experimental data obtained from a temperature-sweep test. The steady shear flow behavior was secondly reported and then the effect of shear rate on this behavior was discussed in detail. In addition, several inelastic-viscoplastic flow models including a yield stress parameter were employed to make a quantitative evaluation of the steady shear flow behavior, and then the applicability of these models was examined by calculating the various material parameters. The angular frequency dependence of the linear viscoelastic behavior was nextly explained and quantitatively predicted using a fractional derivative model. Finally, the strain amplitude dependence of the dynamic viscoelastic behavior was discussed in full to elucidate a nonlinear rheological behavior in large amplitude oscillatory shear flow fields. Main findings obtained from this study can be summarized as follows : (1) The linear viscoelastic behavior is almostly independent of temperature over a temperature range of $15{\sim}40^{circ}C$. (2) The steady shear viscosity is sharply decreased as an increase in shear rate, demonstrating a pronounced Non-Newtonian shear-thinning flow behavior. (3) The shear stress tends to approach a limiting constant value as a decrease in shear rate, exhibiting an existence of a yield stress. (4) The Herschel-Bulkley, Mizrahi-Berk and Heinz-Casson models are all applicable and have an equivalent validity to quantitatively describe the steady shear flow behavior of $Antiphlamine-S^{(R)}$ lotion whereas both the Bingham and Casson models do not give a good applicability. (5) In small amplitude oscillatory shear flow fields, the storage modulus is always greater than the loss modulus over an entire range of angular frequencies tested and both moduli show a slight dependence on angular frequency. This means that the linear viscoelastic behavior of $Antiphlamine-S^{(R)}$ lotion is dominated by an elastic nature rather than a viscous feature and that a gel-like structure is present in this system. (6) In large amplitude oscillatory shear flow fields, the storage modulus shows a nonlinear strain-thinning behavior at strain amplitude range larger than 10 % while the loss modulus exhibits a weak strain-overshoot behavior up to a strain amplitude of 50 % beyond which followed by a decrease in loss modulus with an increase in strain amplitude. (7) At sufficiently large strain amplitude range (${\gamma}_0$>100 %), the loss modulus is found to be greater than the storage modulus, indicating that a viscous property becomes superior to an elastic character in large shear deformations.

Dynamic characteristics of combined isolation systems using rubber and wire isolators

  • Lee, Seung-Jae;Truong, Gia Toai;Lee, Ji-Eon;Park, Sang-Hyun;Choi, Kyoung-Kyu
    • Nuclear Engineering and Technology
    • /
    • 제54권3호
    • /
    • pp.1071-1084
    • /
    • 2022
  • The present study aims to investigate the dynamic properties of a novel isolation system composed of separate rubber and wire isolators. The testing program comprised pure compressive, pure-shear, compressive-stress dependence, and shear-strain dependence tests that used full-scale test specimens according to ISO 22762-1. A total of 22 test specimens were fabricated and investigated. Among the tests, the pure compressive test was a destructive test that reached up to the failure stage, whereas the others were nondestructive tests before the failure stage. Similar to the pure-shear test, at each compressive-stress level in the compressive dependence test or at each shear-strain level in the shear-strain dependence test, the cyclic loading was conducted for three cycles. In the nondestructive tests, examination of the dynamic shear properties in the X-direction was independent of the Y-direction. The test results revealed that the increase in the shear strain increased the energy dissipation but decreased the damping ratio, whereas the increase in the compressive stress increased the damping ratio. In addition, a macro model was developed to simulate the load-displacement response of the isolation systems, and the prediction results were consistent with the experimental results.

횡하중을 받는 말뚝의 Beam-Column 해석 (A Beam-Column Analysis of Laterally Loaded Piles)

  • 백원진;이강일;이진수;김주현;송병관
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2008년도 추계 학술발표회
    • /
    • pp.1212-1217
    • /
    • 2008
  • In this study, in order to clarify the effect of the direction of cyclic shear on the post-earthquake settlement the multi-directional shear tests were carried out for Toyoura Japan standard sand, Genkai natural sand and the Granulated Blast Furnace Slag (GBFS). In a series of tests, number of strain cycles was changed as n=5-200 and the shear strain amplitude varied from 0.1% to 1.0%. The relative density was also changed as Dr=50, 60 and 70%. From the test results for Toyoura sand and GBFS, it is clarified that the post cyclic settlement is relatively large at the small relative density and becomes large with the shear strain amplitude. When the influence of the direction of cyclic shear is decreases, the post cyclic settlement strain for Toyoura sand is converged to a constant value, but the GBFS is increased with the number of strain cycles.

  • PDF

Energy-based evaluation of liquefaction potential of uniform sands

  • Sonmezer, Yetis Bulent
    • Geomechanics and Engineering
    • /
    • 제17권2호
    • /
    • pp.145-156
    • /
    • 2019
  • Since behaviors of loose, dense, silty sands vary under seismic loading, understanding the liquefaction mechanism of sandy soils continues to be an important challenges of geotechnical earthquake engineering. In this study, 36 deformation controlled cyclic simple shear tests were performed and the liquefaction potential of the sands was investigated using three different relative densities (40, 55, 70%), four different effective stresses (25, 50, 100, 150 kPa) and three different shear strain amplitudes (2, 3.5, 5%) by using energy based approach. Experiments revealed the relationship between per unit volume dissipated energy with effective stress, relative density and shear strain. The dissipate energy per unit volume was much less affected by shear strain than effective stress and relative density. In other words, the dissipated energy is strongly dependent on relative density and effective stress. These results show that the dissipated energy per unit volume is very useful and may contain the non-uniform loading conditions of the earthquake spectrum. When multiple regression analysis is performed on experiment results, a relationship is proposed that gives liquefaction energy of sandy soils depending on relative density and effective stress parameters.

초소형 무연 단일 솔더볼 연결부의 전단강도 평가 (Evaluation of Shear Strength of a Miniature Lead-free Single Solder Ball Joint)

  • 주세민;김호경
    • 한국안전학회지
    • /
    • 제25권6호
    • /
    • pp.14-21
    • /
    • 2010
  • A miniature single solder ball joint is designed to mimic the actual solder joints used in the micro-electric industries. Shear tests were conducted to evaluate the mechanical behavior of miniature single solder joints at intermediate strain rates from $0.019\;s^{-1}$ to $2.16\;s^{-1}$ at room temperature. The shear fracture strength of the present solder ball joints generally increased with increasing shear strain rate, ranging from 32 to 51MPa. This behavior is affected by the sensitivity of bulk solder strength to strain rate. Shear fracture mode changed from brittle to partial ductile (failure inside the bulk solder) with an increase of shear speed. The unloading shear fracture toughness is generally consistent with the measure of the amount of bulk solder on the fractured surface.

미소변형 전단강성에 시간효과가 미치는 영향 (The Shear Stiffness of Small Strain with Time Effect)

  • 김수삼;신현영;김병일
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2001년도 춘계학술대회 논문집
    • /
    • pp.249-256
    • /
    • 2001
  • This study investigated the shear stiffness of level of small strain with time effect. Time effect consists of rest time, loading rate of recent and current stress path. In addition, for the measurement of small strain, overconsolidated state was represented in a triaxial cell, and drained stress path tests were carried out. Test results show that the loading rate of recent stress path has no effects on the stiffness of very small strain, but the shear stiffness of level of small strain increases with it. Finally, the rest time and the loading rate of current stress path have the effects on the shear stiffness of initial and small strain.

  • PDF

Strain Gauge를 이용한 핀형 로드셀 개발 (Development of the Pin Type Load-cell Using Strain Gauge)

  • 이동욱;박민혁;이계광;김인환;이석순
    • 한국기계가공학회지
    • /
    • 제13권4호
    • /
    • pp.75-82
    • /
    • 2014
  • A pin-type load-cell which uses shear-type strain gauges was developed to measure the tension of a wire in a winch. A finite element analysis was performed to determine the locations of the strain gauges. All of the shear-type strain gauges were attached onto parts that undergo regularly shear stress distributions. A Wheatstone bridge circuit was used to connect each of the gauges and to measure the strains. Linearity within the 5% error range was noted when testing the pin-type load-cell.

FCC 금속에서 압연 전단집합조직의 형성에 미치는 변형상태의 효과 (Effect of Strain Slates on the Formation of Shear Textures during Rolling in fcc Metals)

  • 강춘구;최웅규;허무영
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.483-486
    • /
    • 2005
  • In order to study the effect of strain states on the formation of shear textures during rolling in fcc metals, the evolution of textures was simulated by the full constrain model using various ideal strain states. Considering rolling as a two-dimensional problem, i.e., $\varepsilon_{22}\;=\;\varepsilon_{12}\;=\;\varepsilon_{23}\;=\;0$, the deviation from the plane-strain state manifest itself as nonzero contribution of $\varepsilon_{13}$. With increasing variations of $\varepsilon_{13}$, shear textures develop. The sign of ell hardly affects the evolution of textures. The texture simulation with various idealized strain states indicates that the ratio $\mid\varepsilon_{13}\mid/\mid\varepsilon_{11}\mid$ in each time interval in a roll gap plays a dominant role in the evolution of textures during rolling.

  • PDF