Bond strength of orthodontic brackets bonded to enamel with a self-etching primer after bleaching and desensitizer application (미백과 탈감작제 도포 후 셀프 에칭 프라이머를 이용한 브라켓 접착 시 법랑질과 브라켓 간의 결합 강도)

  • Attar, Nuray;Korkmaz, Yonca;Kilical, Yasemin;Saglam-Aydinatay, Banu;Bicer, Ceren Ozge
    • The korean journal of orthodontics
    • /
    • v.40 no.5
    • /
    • pp.342-348
    • /
    • 2010
  • Objective: The aim of this study was to compare the shear bond strengths (SBS) of orthodontic brackets bonded to enamel with a self-etching primer after bleaching, desensitizer application and combined treatment. Methods: Forty-eight premolars were randomly divided into four groups, each with n = 12 premolar samples. The four groups were; Group1: 15% hydrogen-peroxide office bleaching agent (Illumin$\acute{e}$ Office-IO), Group 2: IO + BisBlock Oxalate Dentin-Desensitizer, Group 3: Bis Block Oxalate Dentin-Desensitizer, Group 4: No treatment (control). Twenty-four hours after bonding, the specimens were tested in SBS at a crosshead speed of 5 mm/min until the brackets debonded. The failure mode of the brackets was determined by a modified adhesive remnant index. Results: Bleaching, bleaching and desensitizer treatment, and desensitizer treatment alone all significantly reduced SBS of the orthodontic brackets ($p$ = 0.001). No statistically significant difference was found between Group 1, Group 2 and Group 3 (Group 1-Group 2, $p$ = 0.564; Group 1-Group 3, $p$ = 0.371; Group 2-Group 3, $p$ = 0.133). The predominant mode of failure for the treatment groups (Group1, Group 2 and Group 3) was at the enamel-adhesive interface leaving 100% of the adhesive on the bracket base. Conclusions: Bleaching and desensitizer treatment should be delayed until the completion of orthodontic treatment.

Studies on the Frost Heave Revelation and Deformation Behaviour due to Thawing of Weathered Granite Soils (화강암 풍화토의 동상 발현 및 융해에 따른 변형 거동에 관한 연구)

  • 류능환;최중대;류영선
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.37 no.3_4
    • /
    • pp.61-71
    • /
    • 1995
  • Natural ground is a composite consisted of the three phases of water, air and soil paircies. Among the three components, water as a material is weU understood but soil particles are not in foundation engineering. Especially, weathered granite soil generally shows a large volumetric expansion when they freeze. And, the stability and durability of the soil have shown decreased with repetitive freezing and thawing processes. These unique charcteristics may cause various construction and management problems if the soil is used as a construction material and foundation layers. This project was initiated to investigate the soil's physical and engineering characteristics resulting from freezing and freezing-thawing processes. Research results may be used as a basic data in solving various problems related to the soil's unique characteristics. The following conclusions were obtained: The degree of decomposition of weathered granite soil in Kangwon-do was very different between the West and East sides of the divide of the Dae-Kwan Ryung. Soil particles distributed wide from very coarse to fine particles. Consistency could be predicted with a function of P200 as LL=0.8 P200+20. Permeability ranged from 10-2 to 10-4cm/sec, moisture content from 15 to 20% and maximum dry density from 1.55 to 1.73 g /cmΥ$^3$ By compaction, soil particles easily crushed, D50 of soil particles decreased and specific surface significantly increased. Shear characteristics varied wide depending on the disturbance of soil. Strain characteristics influenced the soil's dynamic behviour. Elastic failure mode was observed if strain was less than 1O-4/s and plastic failure mode was observed if strain was more than 10-2/s. The elastic wave velocity in the soil rapidly increased if dry density became larger than 1.5 g /cm$^3$ and these values were Vp=250, Vg= 150, respectively. Frost heave ratio was the highest around 0 $^{\circ}C$ and the maximum frost heave pressure was observed when deformation ratio was less than 10% which was the stability state of soil freezing. The state had no relation with frost depth. Over freezing process was observed when drainage or suction freezing process was undergone. Drainage freezing process was observed if freezing velocity was high under confined pressure and suction frost process was occurred if the velocity was low under the same confined process.

  • PDF

A numerical study on the 3-Dimensional shape characteristics of small underground cavities (소규모 지하공동 3차원 형상 특성을 반영한 수치해석에 관한 연구)

  • An, Joon-Sang;Kang, Kyung-Nam;Son, Ki-Il;Kim, Woo-Seok;Kim, Byung-Chan
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.20 no.5
    • /
    • pp.787-807
    • /
    • 2018
  • When conducting the underground safety impact assessment under the special law in Korea, it is essential to investigate the occurrence of underground cavities. When underground cavities were discovered, the underground safety was assessed through numerical analysis. The previous study has suggested the stability evaluation based on the factor of safety by changing the 2D shape of the small underground cavity. In this study, the effects of small underground cavities considering 3D shapes were examined using a continuum analysis program and compared with the 2D results presented in previous study. If the 3-Dimensional shape of the underground cavity is found close to the sphere type, it would be reasonable to evaluate the factor of safety by the shear strength reduction method regardless of the size and position of the cavity. If a high-aspect ratio underground cavity with a depth of 2 m or more from the ground surface and an aspect ratio (a/b) of 2.0 or more is in the vertical direction, not only the factor of safety but the failure mode shape should be cautions in the stability evaluation using the shear strength reduction method. The results of this study are expected to be basic data on underground safety impact assessment.

Comparison on the Behavior according to Shapes of Tension Web member in gap K-joints in Cold-formed Square Hollow Sections (인장웨브재 형태에 따른 각형강관 갭K형 접합부의 거동 비교)

  • Jeong, Sang Min;Bae, Kyu Woong;Moon, Tae Sup
    • Journal of Korean Society of Steel Construction
    • /
    • v.17 no.5 s.78
    • /
    • pp.561-568
    • /
    • 2005
  • The object of this paper is to determine appropriateness for use of high-strength tensile bar as a tension web member. The gap K-joint of tensile bar types were compared with gap K-joint of square hollow section (SHS) types. For the same width-to-thickness ratio ($2{\gamma}=33.3$ ), tests were performed on four specimens of the SHS type and eight specimens of the tensile bar type. The comparison of capacity with the experimental results showed a capacity of the SHS type joint to be higher than that of the tensile bartype joint for the same brace-to-chord width ratio. Moreover, the capacity of the SHS type joints increased proportionally to the width ratio ${\beta}$), while tensile bar type joints increased as the tension width ratio (${\beta}2$). In failure mode, SHS-type specimens showed local buckling of the compression brace and plastic failure was observed between the tension brace and chord face, and with the tensile bar type specimens there appeared punching shear failure of the chord face at the toe of the connection plate. It is, therefore, concluded that width-to-thickness ratio should be lower than that of the hollow-section type and the relation between tension and compression width ratio should be considered.

An effect of Dentin Bonding Procedure on the Shear Bond Strength of Resin Cement to Porcelain Restoration (도재 수복물 합착시 상아질 접착 술식이 레진 시멘트의 전단결합강도에 미치는 영향)

  • Kang, Hae-Jin;Shin, Soo-Yeon
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.28 no.1
    • /
    • pp.67-78
    • /
    • 2012
  • The purpose of this study was to determine whether there were differences in shear bond strength to human dentin using IDS technique compared with DDS. Forty freshly extracted human molars were and devided into 4 groups. The control group specimens were, on the morrow of tooth preparation, light-cured after application of dentin bonding agent and cemented with resin cement. The IDS/SE(immediate dentin sealing, Clearfil$^{TM}$ SE Bond) and IDS/SB (immediate dentin sealing, Adapter$^{TM}$ Single Bond 2) specimens were, on the morrow of tooth preparation, light-cured after application of dentin bonding agent(Clearfil$^{TM}$ SE Bond and Adapter$^{TM}$ Sing Bond 2, respectively), whereas DDS specimens were not treated with any dentin bonding agent. IDS/SE, IDS/SB and DDS specimens were thermocycled. Following that delay, specimens were cemented with resin cement. The dentin bonding agent was left unpolymerized until the application of porcelain restoration. Shear bond strengths were measured using a universal testing machine. Specimens also were evaluated for mode of fracture using an optical microscope. The mean shear bond strengths of control group and IDS/SE groups were not statistically different from one another. The bond strength of IDS/SE group had a significantly higher mean than that of DDS group. There was no significant difference in the mean shear bond strength between IDS/SB(4.11MPa) and DDS group. The evaluation of failure modes indicates that most failures in the control group and IDS/SE groups were mixed, whereas failures in the DDS group were interfacial. When preparing teeth for indirect ceramic restoration, IDS with Clearfil$^{TM}$ SE Bond results in improved shear bond strength compared with DDS.

Lateral Strength of Double-Bolt Joints to the Larix Glulam according to Bolt Spacing (볼트 간격에 따른 낙엽송 집성재 이중 볼트접합부의 전단강도)

  • Kim, Keon-Ho;Hong, Soon-Il
    • Journal of the Korean Wood Science and Technology
    • /
    • v.36 no.3
    • /
    • pp.1-8
    • /
    • 2008
  • The lateral strength test of bending type was done to investigate the lateral capacity of the double bolt connection of domestic larix glulam according to bolt spacing. In the shear specimen, which is bolted connection in the inserted plate type, the hole of bolt was made, changing the diameter of bolt (12 mm and 16 mm), the number of bolt (single bolt : control and double bolt), the direction of bolt row (in parallel to grain : Type-A and in perpendicular to grain : Type-B) and the bolt spacing (Type-A : 4 d and 7 d and Type-B : 3 d and 5 d). Lateral capacity and failure mode of bolt connection were compared according to conditions. In prototype design (KBCS, 2000), the reduction factor of the allowable shear resistance that the bolt spacing is reduced was calculated. The results were as follows. 1) Bearing stress per bolt in the single and double bolt connection of Type-A was directly proportional to bolt diameter and bolt spacing. Bearing stress of Type-B decreased as bolt diameter was increased, and decreased by 2~10% when bolt diameter was increased. 2) In the single bolt connection and the double bolt connection of Type-A, the splitted failure was formed in the edge direction. When the bolt spacing was 3 d in Type-B, bolt was yielded more in the part of tension than in the part of compression, and the splitted failure started at the bolt in the part of tension. In the 5 d spacing specimen, the bolt in the part of tension was yielded similarly to bolt in the part of compression, and the splitted failure started in the part of compression. 3) In the prototype design, the reduction factor was calculated by non-dimensionizing the yielding load in the standard of bolt spacing (Type A : 7 d and Type B : 5 d). In 12 mm bolt connection, the reduction factor of bolt spacing 4 d (type-A) and single bolt connection was 0.87 and 0.55, respectively, and the reduction factor of bolt spacing 3 d (Type-B) and single bolt connection was 0.91 and 0.55, respectively. In 16 mm bolt connection, the reduction factor of bolt spacing 4 d (type-A) and single bolt connection was 0.96 and 0.76, respectively, and the reduction factor of bolt spacing 3 d (Type-B) and single bolt connection was 0.91 and 0.77, respectively.

Flexural Strengthening of Reinforced Concrete Beams Using Carbon Fiber Mesh (탄소섬유 메쉬를 사용한 철근콘크리트 보의 휨보강)

  • Seo, Soo-Yeon;Yun, Hyun-Do;Choi, Chang-Sik;Choi, Ki-Bong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.9 no.2
    • /
    • pp.181-190
    • /
    • 2005
  • The objective of this work is to study the flexural strengthening effectiveness of Carbon Fiber Mesh (CFM) in reinforced concrete beams. Flexural strengthening for a simply supported reinforced concrete (RC) beam using CFM is developed by bonding CFM to the soffit of the beam. In this experimental program, five medium-sized reinforced concrete beams strengthened with CFM are tested in bending to evaluate reinforcing effects of the CFM. The beams are designed to have high shear capacity so that expected dominant failure mode of specimens is bending. The reinforcing effect of CFM is small at crack initiation, but is considerable in flexural rigidity of the beam after crack initiation. In comparing the behaviors of strengthened and virgin beams each other, it is shown that the strength of RC beams can be enhanced by attaching CFM. A fairly good agreement between the measured values and the calculated ones is obtained at both the cracking strength and yield strength of the strengthened beams.

Effect of geometrical configuration on seismic behavior of GFRP-RC beam-column joints

  • Ghomia, Shervin K.;El-Salakawy, Ehab
    • Advances in concrete construction
    • /
    • v.9 no.3
    • /
    • pp.313-326
    • /
    • 2020
  • Glass fiber-reinforced polymer (GFRP) bars have been introduced as an effective alternative for the conventional steel reinforcement in concrete structures to mitigate the costly consequences of steel corrosion. However, despite the superior performance of these composite materials in terms of corrosion, the effect of replacing steel reinforcement with GFRP on the seismic performance of concrete structures is not fully covered yet. To address some of the key parameters in the seismic behavior of GFRP-reinforced concrete (RC) structures, two full-scale beam-column joints reinforced with GFRP bars and stirrups were constructed and tested under two phases of loading, each simulating a severe ground motion. The objective was to investigate the effect of damage due to earthquakes on the service and ultimate behavior of GFRP-RC moment-resisting frames. The main parameters under investigation were geometrical configuration (interior or exterior beam-column joint) and joint shear stress. The performance of the specimens was measured in terms of lateral load-drift response, energy dissipation, mode of failure and stress distribution. Moreover, the effect of concrete damage due to earthquake loading on the performance of beam-column joints under service loading was investigated and a modified damage index was proposed to quantify the magnitude of damage in GFRP-RC beam-column joints under dynamic loading. Test results indicated that the geometrical configuration significantly affects the level of concrete damage and energy dissipation. Moreover, the level of residual damage in GFRP-RC beam-column joints after undergoing lateral displacements was related to reinforcement ratio of the main beams.

Experimental Study on Interfacial Bond Stress between Aramid FRP Strips and Steel Plates (아라미드 FRP 스트립과 강판 사이의 계면 부착응력에 관한 실험적 연구)

  • Park, Jai Woo;Ryoo, Jae Yong;Choi, Sung Mo
    • Journal of Korean Society of Steel Construction
    • /
    • v.27 no.4
    • /
    • pp.359-370
    • /
    • 2015
  • This paper presents the experimental results for the interfacial bond behaviour between AFRP strip and steel members. The objective of this paper is to examine the interfacial behavior and to evaluate the interfacial bond stress between Aramid FRP strips and steel plates. The test variables were bond length and AFRP thickness. 18 specimens were fabricated and one-face shear type bond tests were conducted in this study. There were two types of failure mode which were debonding and delamination between AFRP strip and steel plates. From the test, the load was increased with the increasing of bond length and AFRP thickness, which was observed that maximum increase of 63 and 86% were also achieved in load with the increasing of bond length and AFRP thickness, respectively. Finally, bond and slip characteristics had the elastic bond-slip model and it was observed that bond strength and fracture energy were not affected by bond length and AFRP thickness.

An Experimental Study on Seismic Capacity Improvement of Masonry Buildings by Glass Fiber Reinforced Methods (유리섬유보강에 의한 조적조 건축물의 내진 성능향상에 관한 실험 연구)

  • Cho, Sang-Min;Choi, Sung-Mo;Kwon, Ki-Hyuk;Lee, Su-Cheul
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.4 no.2 s.13
    • /
    • pp.47-52
    • /
    • 2004
  • Whereas The masonry buildings are safe under gravity loads, most of the masonry buildings in Korea have many structural defects under a lateral load due to an earthquake acceleration. But there is no earthquake resistant design code for the Masonry in Korea. Therefore it may be necessary to be set up an seismic code and be suggested for reinforcing methods for existing masonry buildings. The purpose of this paper is to investigate seismic capacity of reinforced masonry buildings subjected to earthquake load. The typical two models of the masonry building in Korea are selected through a site investigation. On the basis of test results, the fiber reinforcing effect of the two models was considerable. The maximum base shear force and deformation capacity for RM were remarkably increased. It was found that the pier rocking failure was a dominant mode for the RM buildings during a seismic excitation.