There are certain types of construction that produces many defects during the construction of apartment buildings. It may be due to construction errors in the type itself, but more often, it is due to defects derived from other types of construction. Thus, to reduce such secondary defects and prevent fundamental defects in particular types of construction, academic research on the types of construction causing secondary defects should be actively conducted. In addition, as claimed in this study, the industries should work harder to improve the quality of the type of construction that causes secondary defects, rather than just trying to improve the ostensible problems. If the efforts of each sector are backed up, the disputes over defect repair in apartment building construction will reduce in general, which in turn will lead to a reduction in national loss within the construction industry.
Intrinsic gettering is usually used to improve wafer quality which is an important factor for reliable ULSI devices. The two-step annealing method was adopted in order to investigate interactions between oxygens and secondary defects during oxygen precipitation process in lightly and heavily boron doped silicon wafers with high energy $^{11}B^+$ ion implantation. Secondary defects were inspected nearby the projected range by high resolution transmission electron microscopy. Oxygen pileup was measured in the vicinity of the projected range by secondary ion mass spectrometry for heavily boron doped silicon wafers.
Kim, Ju Hyun;Yoo, Kwae Hwan;Na, Man Gyun;Kim, Jin Weon;Kim, Kyeong Suk
Nuclear Engineering and Technology
/
제46권2호
/
pp.225-234
/
2014
Wall-thinned defects caused by accelerated corrosion due to fluid flow in the inner pipe appear in many structures of the secondary systems in nuclear power plants (NPPs) and are a major factor in degrading the integrity of pipes. Wall-thinned defects need to be managed not only when the NPP is under maintenance but also when the NPP is in normal operation. To this end, a test technique was developed in this study to detect such wall-thinned defects based on the temperature difference on the surface of a hot pipe using infrared (IR) thermography and a cooling device. Finite element analysis (FEA) was conducted to examine the tendency and experimental conditions for the cooling experiment. Based on the FEA results, the equipment was configured before the cooling experiment was conducted. The IR camera was then used to detect defects in the inner pipe of the pipe specimen that had artificially induced defects. The IR thermography developed in this study is expected to help resolve the issues related to the limitations of non-destructive inspection techniques that are currently conducted for NPP secondary systems and is expected to be very useful on the NPPs site.
A high-resolution transmission electron microscopy study on the lattice defects formed in the high energy P ion implanted silicon was carried out on an atomic level. Results show that Lomer dislocations, 60$^{\circ}$perfect dislocations, 60$^{\circ}$ dislocation dipole and extrinsic stacking fault formed in the near Rp of as-implanted specimen. In the annelaed specimens, interstitial Frank loops, 60$^{\circ}$perfect disolations, 60$^{\circ}$dislocation dipoles, stacking faults, precipitates, perfect dislocation loops and <112> rodlike defects existed exclusively near in the Rp with various annealing temperature and time. From these results, it is concluded that extended secondary defects as well as the point defect clusters could be formed without annealing. Even at low temperature annealing such as 55$0^{\circ}C$, small interstitial Frank loops could be formed and precipitates were also formed by $700^{\circ}C$ annealing. The defect band annealed at 100$0^{\circ}C$ for 1 hr could be divided into two regions depending on the distribution of the secondary defects.
The interrelation of secondary defects, intermediate S' phase and aging condition in Al-2.0 wt% Cu-1.1 wt% Mg alloy is studied by transmission electron microscope. The results obtained in this study are as follows. 1. High density of dislocation loops, helices and stacking faults are observed in this specimen with aging treatment. 2. The number of dislocation loops and the width of loop free zone (LFZ) are increased with aging time. 3. The intermediate S' phase precipitates and grows on the dislocations and secondary defects. 4. The misfit dislocations are formed around intermediate S' phase. 5. It is thought that the helices appear to be produced by the climb of screw dislocations, while the dislocation loops appear to be formed both by condensation of vacancies into collapsed discs and by interaction of helices with screw of opposite sign.
Journal of the Korean Association of Oral and Maxillofacial Surgeons
/
제46권5호
/
pp.361-366
/
2020
Guided bone regeneration (GBR) is a surgical procedure that utilizes bone grafts with barrier membranes to reconstruct small defects around dental implants. This procedure is commonly deployed on dehiscence or fenestration defects ≥2 mm, and mixing with autogenous bone is recommended on larger defects. Tension-free primary closure is a critical factor to prevent wound dehiscence, which is critical cause of GBR failure. A barrier membrane should be rigidly fixed without mobility. If the barrier is exposed, closed monitoring should be utilized to prevent secondary infection.
The effects of risering design and alloying element on the formation of defects such as external depression, primary and secondary shrinkage cavities in ductile cast iron were investigated. Two types of risering design for the cylindrically step-wise specimen, No. 1(progressive solidification) and No. 2(directional solidification) risering designs, were prepared and six different alloy compositions were casted. In the No. 1 risering design, external depression or primary shrinkage cavities due to liquid contraction were observed in all the specimens from SG 10 to SG 60. The defects caused by liquid contraction seemed to be more affected by risering design than alloying elements. The secondary shrinkage cavities were also observed in all the specimens but a swollen surface was not observed in all the castings. The primary shrinkage cavities were located right under the top surface or connected to the top surface, and were characterized by smooth surfaces. On the other hand, the secondary shrinkage cavities were positioned in the thermal center of the specimen steps 3 and 4, and characterized by rough surfaces. In the No. 2 risering design, no external depression or primary shrinkage cavities due to liquid contraction were observed in all the specimens from SG 10 to SG 60. However, the secondary shrinkage cavities were formed in the thermal center of specimens SG 40, 50 and 60. Like the No. 1 risering design, a swollen surface was not observed in all the castings.
Journal of the Korean Association of Oral and Maxillofacial Surgeons
/
제26권6호
/
pp.666-671
/
2000
Objectives: This study evaluated the availability of mandibular symphysis corticocancellous block grafts in patients treated for reconstruction of intraoral jaw defects. Materials & Methods: 8 patients with mandibular and maxillary bony defects were treated with corticocancellous block of symphysis. The types of defects included 4 pathologic jaw defects and 4 vertical and/or horizontal alveolar deficiencies. The age ranged from 13 to 45 years. Additional treatments such as plate fixation, alloplastic bony substitutes, and/or barrier membrane application were perfomred. They were evaluated for complications and healing of defects. Follow-up period ranged from 6 to 15 months. Results: 2 patients experienced complications such as wound dehiscence and mild resorption of exposed bone. None of the patients needed secondary operation. Paresthesia of lip, chin, and teeth were recovered completely by 6 months postoperatively. Reconstructed wound showed favorable healing and bony consolidation. Conclusion: Corticocancellous block of mandibular symphysis can be used for the reconstruction of a variety of intraoral local jaw defects selectively. Advantages were easy fixation of graft, possibility of restoration of original alveolar contour, and decreased donor site morbidity.
Intrinsic and proximity gettering are popular processes to get higher cumulative production yield and usually adopt multi-step annealing and high energy ion implantation, respectively. In order to test the combined processed of these, high energy \ulcornerAs\ulcorner ion implantation and 2-step annealing process were adopted. After the ion implantation followed by 2-step annealing, the wafers were cleaved and etched with Wright etchant. The morphology of cross section on samples was inspected by FESEM. The concentration profile of As was measured by SRP. The location and type of secondary defects inspected by HRTEM were dependent on the 1st annealing temperatures. That is, a line of dislocation located at $1.5mutextrm{m}$ apart from the surface at $600^{\circ}C$ lst annealing was changed to some dislocation lines or loops nearby the surface at 100$0^{\circ}C$. The density of dislocation line was reduced but the size of the defects was enlarged as the temperature increased.
The eccentric extrusion and bending process for the forming of the curved rectangular hollow tube is newly developed. Generally the bending process of hollow tube is the secondary process followed by the extrusion process of the hollow tube from the round billet. So many defects such as wrinkling and the difference of wall thickness can be happened during the secondary bending process. In order to avoid the defects the new process named as "the eccentric extrusion and bending process" is suggested and applied to the U-bending of rectangular hollow tube. In this paper the kinematically admissible velocity field between the dies surface and the internal plug boundary surface s developed for the curving velocity. By the using of this curving velocity field the curvature of extruded products can be calculated with the parameters such as eccentricity dies length friction constant aspect ratio.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.