• Title/Summary/Keyword: SEM $T_g

Search Result 161, Processing Time 0.029 seconds

Separation of $H_2$/$N_2$ Gas Mixture by PTMSP-PEI and PDMS-PEI Composite Membranes (PTMSP-PEI와 PDMS-PEI 복합막에 의한 수소/질소 혼합기체 분리)

  • 강태범;조성혜;이현경
    • Membrane Journal
    • /
    • v.13 no.4
    • /
    • pp.291-299
    • /
    • 2003
  • Polymer membranes such as poly(1-trimethylsilyl-1-propyne)-polyetherimide (PTMSP-PEI) and poly(dimethylsiloxane)- polyetherimide (PDMS-PEI) composite membrane were prepared by solution casting method. To investigate the characteristics of these membranes, the analytical methods such as FT-IR, $^1H-NMR,$ DSC, TGA, GPC, and SEM have been utilized. The number-average (equation omitted) and weight-average (equation omitted) molecular weight of PTMSP were 477,920 and 673,329 respectively. The glass transition temperature ($T_g$) of PTMSP was $224^{\circ}C.$ The separation of the gas mixture ($H_2/N_2$) through the composite membranes were studied as a function of pressure. The separation factor (${\alpha}, {\beta},$ quation omitted) of the composite membranes used in this work increased as the pressure of permeation cell increased. The real separation factor (${\alpha}$), head separation factor (${\beta}$), and tail separation factor (equation omitted) of PTMSP-PEI composite membrane were 2.28, 1.17, and 1.96 respectively at ${\Delta}P$ 30psi and $25^{\circ}C.$ (${\alpha}, {\beta}$ and equation omitted of PDMS-PEI composite membrane were 3.70, 1.53, and 2.42 respectively at ${\Delta}P$ 30psi and $25^{\circ}C$.

Synthesis and Crystal Chemistry of New Actinide Pyrochlores (새로운 파이로클로어의 합성 및 결정화학적 특징)

  • ;;;Sergey V. Yudintsev
    • Journal of the Mineralogical Society of Korea
    • /
    • v.15 no.1
    • /
    • pp.78-84
    • /
    • 2002
  • New pyrochlore-type phases($A_2$$B_2$$O_{7}$) were synthesized in the systems: CaO-C$eO_2$-T$iO_2$, CaO-$UO_2$(T$hO_2$)-Z$rO_2$, CaO-$UO_2$(T$hO_2$)-$Gd_2$$O_3$-T$iO_2$-Z$rO_2$, 및 CaO-T$hO_2$-S$nO_2$. The starting materials were pressed with the pressure of 200~400 MPa and sintered at 1500~ 155$0^{\circ}C$ for 4~8 hours in air and at 1300~ 135$0^{\circ}C$ for 5 ~50 hours under oxygen atmosphere. The products were characterized using XRD, SEM/EDS and TEM. In the bulk compositions of CaCe$Ti_2$$O_{7}$, CaTh$Zr_2$$O_{7}$,($Ca_{0.5}$ Gd$Th_{0.5}$)(ZrTi)$O_{7}$) ($Ca_{0.5}$Gd$Th_{0.5}$)(ZrTi)$O_{7}$, ($Ca_{0.5}$G$dU_{0.5}$)(ZrTi)$O_{7}$ and CaTh$Sn_2$$O_{7}$ , pyrochlore was the major phase, together with other oxide phase $of_2$$O_{7}$ fluorite structure. In the samples with target compositions CaU$Zr_2$$O_2$$Ca_{0.5}$ G$dU_{0.5}$)$Zr_2$T$iO_{7}$ pyrochlore was not identified, but a fluorite-structured phase was detected. The formation factor as the stable phase depended on crystal chemical characteristics of the actinide and lanthanide elements of the system concerned.

Study on the Antitumor Substance Isolated from Oldenlandiae diffusae Herba (백화사활초(白花蛇活草)로부터 분리(分離)된 항암성물질(抗癌性物質)에 관(關)한 연구(硏究))

  • kim, Sung-Hoon
    • Journal of Haehwa Medicine
    • /
    • v.4 no.2
    • /
    • pp.273-297
    • /
    • 1996
  • Hexane fraction of Oldenlandiae diffusae Herba(ODH) which was being used for the treatment of caner in oriental medicine showed the best cytotoxicity against L1210 and A549 in the solvent fractions. Antitumor substance isolated from hexane fraction of ODH was identified as ursolic acid(UA) by photometric analysis. IC50 of UA against cancer cells as SNU-1, HCT15, XF498, SK-MEL2 and A549 was $13{\mu}g/m{\ell}$, $15{\mu}g/m{\ell}$, $12{\mu}g/m{\ell}$, $9{\mu}g/m{\ell}$ and $11{\mu}g/m{\ell}$ respectively. It significantly inhibited the metastasis to lungs and kidneys from pulmonary colonization assay and study on histological changes of organs and showed the enhancing effect on B cell dosage-dependently by FACS analysis. T/C % of UA against S-180 cells was 171 % and its cytotoxicity against SNU-1 iant was confirmed from the morphological changes by elctronic microscopes such as SEM and TEM that it induced undulated membrane 4 hr after UA treatment, and the breakdown of cell membrane and nucleus 24 hr after UA treatment.

  • PDF

Recycling Natural Rubber Vulcanizates through Mechanochemical Devulcanization

  • Jang G. K.;Das C. K.
    • Macromolecular Research
    • /
    • v.13 no.1
    • /
    • pp.30-38
    • /
    • 2005
  • Sulfur-cured gum natural rubber vulcanizates were devulcanized using two different concentrations of diallyl disulfide. The devulcanization process was performed at $110^{\circ}C$ min in an open two-roll cracker-cum-mixing mill. Natural rubber vulcanizates having various sulfur/accelerator ratios were used to study the cleavage of monosulfide, disulfide, and polysulfide bonds. The properties of devulcanized natural rubber increased upon increasing the disulfide concentration and the mechanical properties of the revulcanized natural rubber increased upon decreasing the sulfur content in the original rubber vulcanizates. The scorch time and the maximum state of cure both increased when the ground vulcanizates were treated with higher amounts of disulfide. TGA and DMA were conducted to study the effects of the devulcanization on the thermal stability and the $T_g$ behavior of the vulcanizates. SEM analysis was conducted to study how the failure mechanism was affected by the devulcanization process. It was possible to recover $70-80\%$ of the original gum rubber properties by using this process. From IR spectroscopic analysis, we observed that the oxidation of the main chains did not occur during high-temperature milling.

A Synthesis of Spherical MCM-48 with the Molar Ratio of Surfactant and Silica (계면활성제와 실리카 몰비의 조절에 따른 구형 MCM-48의 합성)

  • Lee, Ha-Young;Park, Sang-Won
    • Journal of Environmental Science International
    • /
    • v.19 no.6
    • /
    • pp.681-687
    • /
    • 2010
  • Mesoporous silica was prepared from hydrothermal synthesis using gel mixture of tetraethylorthosilcate (TEOS) as silica source and cetyltrimethylammonium bromide (CTMABr) as a surfactant. In the optimum synthesis cause, molar ratio of template and silica changed. The surface and structure properties of mesoporous silica were determined by XRD, SEM, TEM and BET. Also, surface potential of mesoporous silica was measured using zeta potential. $N_2$ adsorption isotherm characteristics, including the specific surface area ($S_{BET}$), total pore volume $V_T$), and average pore diameter ($D_{BJH}$), were determined by BET. As a result, SBET of $100m^2/g{\sim}1500m^2/g$ was determined from the $N_2$ adsorption isotherm. Also, the average pore diameter was 2 nm∼4 nm. Mesoporous silica's surface potential of minus charge was determined from zeta potential.

Highly Economic and High Quality Zinc-flake Manufacturing by High Kinetic Processing

  • Ren, H.;Benz, H.U.;Chimal V., O.;Corral G., M.S.;Zhang, Y.;Jaramillo V., D.;Zoz, H.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.975-976
    • /
    • 2006
  • The present paper is a parameter study of zinc flake production using a Simoloyer CM01 horizontal high energy rotary ball mill. The manufactured flakes have a dimension in thickness (t) < $1{\mu}m$ and diameters (d) 5-100 ${\mu}m$, consequently a ratio d/t up to 200. The flake geometry is mainly controlled by the variation of process parameters such as rotary speed of the rotor, ratio of powder/ball charge, load ratio of the system, process temperature, operating model and the quantity of process control agent (PCA). The Zn flakes were characterized by SEM, tap densitometry, laser diffraction and water coverage measurement.

  • PDF

Carbon Material from Natural Sources as an Anode in Lithium Secondary Battery

  • Bhardwaj, Sunil;Sharon, Maheshwar;Ishihara, T.;Jayabhaye, Sandesh;Afre, Rakesh;Soga, T.;Sharon, Madhuri
    • Carbon letters
    • /
    • v.8 no.4
    • /
    • pp.285-291
    • /
    • 2007
  • Carbon materials of various morphologies were synthesized by pyrolysis of Soap-nut seeds (Sapindus mukorossi), Jack Fruit seeds (Artocarpus heterophyllus), Date-seeds (Phoenix dactylifera), Neem seeds (Azadirachta indica), Tea leaves (Ehretia microphylla), Bamboo stem (Bambusa bambus) and Coconut fiber (Cocos nucifera), without using any catalyst. Carbon materials thus formed were characterized by SEM XRD and Raman. Carbon thus synthesized varied in size (in ${\mu}m$) but all showed highly porous morphology. These carbon materials were utilized as the anode in Lithium secondary battery. Amongst the various precursors, carbon fibers obtained from Soap-nut seeds (Sapindus mukorossi) and Bamboo stem (Bambusa bambus), even after $100^{th}$ cycles, showed the highest capacity of 130.29 mAh/g and 92.74 mAh/g respectively. Morphology, surface areas and porosity of carbon materials obtained from these precursors were analyzed to provide interpretation for their capacity to intercalate lithium. From the Raman studies it is concluded that graphitic nature of carbon materials assist in the intercalation of lithium. Size of cavity (or pore size of channels type structure) present in carbon materials were found to facilitate the intercalation of lithium.

The Variation in Optical Constants of Te-doped G $e_{15}Sb_{85}$ Thin Films with Diode-Laser Exposing Time (다이오드 레이저 노출시간에 따른 Te-doped G $e_{15}Sb_{85}$ 박막의 광학 상수 변화)

  • 김홍석;정진만;이현용;정홍배
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1997.11a
    • /
    • pp.30-33
    • /
    • 1997
  • In this paper, we studied the variation in optical constants of Te-doped G $e_{15}$ /$Sb_{85}$ thin films with 7800$\AA$ diode-laser exposing time and power. The reflectances were increased with the increase of laser exposure time and the laser power in all films. Also, the refractive indices of the films after exposing were higher than those of the as-deposited films. Thus, the fast crystallization was caused by addition to the more Te content at the lower lacer power. It was observed that the surface morphologies of the exposed films are higher than those of the as-deposited films by SEM analysis. Therefore, it is considered that the T $e_{0.5}$(G $e_{15}$ /$Sb_{85}$)$_{99.5}$ thin films will show the high contrast ratio and high SNR and have fast erasing time due to crystallization when these films is applied to optical recording materials.terials.s.

  • PDF

Synthesis and Physical Properties of Sm Doped Pb Free 3 Phase-Glasses (Sm 농도에 따른 무연 3상 유리계의 합성과 물리적 성질)

  • Park, Jong-Ho
    • Korean Journal of Materials Research
    • /
    • v.22 no.7
    • /
    • pp.368-373
    • /
    • 2012
  • Glasses were prepared with compositions of $(13-x)BaO-80B2_O_3-7Li_2O{\cdot}xSm_2O_3$, BBLSx(x=0.5, 0.4, 0.3) by melting the starting materials of boron oxide(99.9%), lithium oxide(99.9%), barium carbon oxide(99.9%), and samarium oxide(99.9%) and then quenching the melt at $1350^{\circ}C$. This led to good-quality BBLSx(x=0.4, 0.3) and poor-quality BBLSx(x=0.5) glasses. The physical and structural properties of the BBLSx glasses were studied by means x-ray diffraction, scanning electron microscopy(SEM), differential scanning calorimetry(DSC), and dielectric spectroscopy. From the x-ray diffraction and SEM results, the quality of the BBLSx glasses significantly depends on the $Sm_2O_3$ concentration. The x-ray diffraction pattern showed that the crystallites in the BBLSx glasses after heat treatment at $700^{\circ}C$ may be $LiBaB_9O_{15}$. From the DSC results, the glass transition temperatures($T_g$), crystallization temperatures($T_c$), and the maximum temperatures of the crystallized($T_p$) BBLSx glasses all changed with the $Sm_2O_3$ concentration. According to the dielectric spectroscopy results, the values of the real dielectric constant and Tan ${\delta}$ of the BBLSx glasses depended on the $Sm_2O_3$ concentration. The values of the real dielectric constant and Tan ${\delta}$ were also shown to depend on the measuring temperature, possibly due to the ion migration in the bulk of the BBLSx glasses.

Mössbauer Study of Al0.2CoFe1.8O4 Ferrite Powders (Mössbauer 분광법에 의한 Al0.2CoFe1.8O4분말의 자기적 특성 연구)

  • Chae, Kwang-Pyo;Lee, Jae-Gwang;Kweon, Hyuck-Su;Lee, Young-Bae
    • Journal of the Korean Magnetics Society
    • /
    • v.13 no.6
    • /
    • pp.231-236
    • /
    • 2003
  • The $Al_{0.2}$CoF $e_{1.8}$ $O_4$ferrite powders have been prepared by the sol-gel method. The crystallographic and magnetic properties of the sample depending on annealing temperature have been investigated by means of x-ray diffraction, FE SEM, Mossbauer spetroscopy and vibrating sample magnetometry. The x-ray diffractions of all samples annealing temperature above 873 K clearly indicate the presence of spinel structure, the lattice constant decrease from 8.425 $\AA$ at 873 K to 8.321 $\AA$ at 1073 K, whereas the particle size rapidly increase from about 39 nm at 673 K to about 108 nm at 1073 K. The Mossbauer spectra annealed above 873 K could be fitted as the superposition of two sextets due to F $e^{3+}$ at A-site and B-site. The isomer shift (IS) and quadruple splitting (QS) values nearly constant with annealing temperature, whereas magnetic hyperfine field ( $H_{hf}$) of A-site slowly in crease and that of B-site fastly increases with increasing annealing temperature. The magnetic behaviour of powders shows that the saturation magnetization increase from 0.7 emu/g at 473 K to 72.1 emu/g at 1073 K while the coercivity decrease from 0.951 kOe at 673 K to 0.374 kOe at 1073 K with increasing annealing temperature.