• 제목/요약/키워드: Rupture strength

Search Result 460, Processing Time 0.028 seconds

An Experimental Study on the Engineering Properties of HPFRCC According to Kinds, Shapes and Volume Fraction of Fibers (섬유의 종류, 형상 및 치환율에 따른 HPFRCC의 공학적 특성에 관한 실험적 연구)

  • Kim, Young-Duck;Cho, Bong-Suk;Kim, Jae-Hwan;Kim, Gyu-Yong;Choi, Kyung-Yuel;Kim, Moo-Han
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2003.11a
    • /
    • pp.59-62
    • /
    • 2003
  • Kinds, shapes and fraction ratios of fibers have influence on properties of HPFRCC(High-Performance Fiver Reinforced Cementitious Concrete) like bending strength, strain capacity and fracture toughness. For example, hydrophilic fibers have different chemical bond strength from hydrophobic fibers, fiber shapes influence on fiber pull-out and rupture, and fiber volume fraction influence on bending strength. In this study, to estimate influences of kinds, shapes and fraction ratios of fibers, we make HFRCC with 3 kind of fiber in various volume fraction of fiber and compare cracking, bending strength and fracture toughness. As the results, bending strength of HPFRCC was increased as fiber volume fraction was increase and fiber tensile strength was increase, and strain capacity and fracture toughness of HFRCC was higher in fiber pull-out fracture than in fiber rupture fracture. And HFRCC showing pseudo strain hardening has higher fiber reinforce efficiency than others.

  • PDF

Experimental Study of Bending and Bearing Strength of Parallel Strand Lumber (PSL) from Japanese Larch Veneer Strand

  • OH, Seichang
    • Journal of the Korean Wood Science and Technology
    • /
    • v.50 no.4
    • /
    • pp.237-245
    • /
    • 2022
  • This study examined the structural performance of experimental parallel strand lumber (PSL) from a Larch veneer strand. The prototype of PSL from a Larch veneer strand was manufactured in the experimental laboratory and tested. The bending and dowel bearing strength were determined from the modulus of elasticity (MOE), modulus of rupture (MOR), and dowel bearing strength based on a 5% offset yield load. The test results indicated that the average MOR of PSL was higher than that of 2 × 4 dimension lumber, and the average MOE of PSL was lower than that of 2 × 4 dimension lumber. A linear relationship was observed between the MOR and MOE. The allowable bending stress of PSL was derived as specified in ASTM D2915 and compared with other research. The dowel bearing strength of PSL in parallel to the grain was approximately double that perpendicular to the grain of PSL. A comparison of several theoretical calculations based on each national code for the dowel bearing strength was conducted, and some theoretical equations produced results closer to the experimental results when it was parallel to the grain, but the difference was higher in the case perpendicular to the grain. The test results showed that PSL made with Japanese larch veneer strands appeared to be suitable for a raw material of structural composite lumber (SCL) appeared to be used as a raw material for SCL.

Static Creep Behaviour of Super-Duralumin(Al 2024) (초 두랄루민(Al 2024)의 정적인 크리프 거동)

  • 황경충;윤종호
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 2004.10a
    • /
    • pp.22-27
    • /
    • 2004
  • Super-duralumin has widely been used as the part materials of aerospace and automobile industry because it has high specific strength and also is light. But, we have little design data about the creep behaviors of the alloy. Therefore, in this study, every creep test under four constant stress conditions have been conducted for four temperature conditions. A series of creep tests had been performed to get the basic design data and life prediction of super-duralurnin products and we have gotten the following results. First, the stress exponents showed the descending trend as the test temperatures increase. Secondly, the creep activation energy gradually decreased as the stresses become bigger. Thirdly, the constant of Larson-Miller parameters on this alloy was estimated about 6. And last, the fractographs at the creep rupture showed both the brittle fracture due to the transgranular rupture.

  • PDF

Tensile Properties and Creep Rupture Characteristics of Cu-1Cr-0.5Zr/STS316L Friction Welded Joints at Elevated Temperature (Cu-1Cr-0.5Zr 합금과 STS316L강의 마찰용접재의 고온 인장 성질과 크리프 파단 특성)

  • Yoo, I.J.;Kong, Y.S.;Kim, S.J.
    • Journal of Power System Engineering
    • /
    • v.6 no.4
    • /
    • pp.49-55
    • /
    • 2002
  • In this paper, the elevated temperature tensile properties and short-time creep rupture characteristics were investigated for the friction welded joints of dissimilar materials, Cu-1%Cr-0.5%Zr and STS316L. The joining tests on Cu-1%Cr-0.5%Zr/STS316L by friction welding were performed, and optimum joining conditions of the friction welded joints were determined. The characteristics of the elevated temperature tensile strength, hardness, fractographs were examined, and the creep rupture characteristics for the optimum welded joints were investigated under uniaxal static load at 300, 400 and $500^{\circ}C$.

  • PDF

Numerical Simulation of the Effect of Finite Diaphragm Rupture Process on Micro Shock Tube Flows

  • Arun Kumar, R.;Kim, Heuy-Dong
    • Proceedings of the Korean Society of Propulsion Engineers Conference
    • /
    • 2012.05a
    • /
    • pp.309-317
    • /
    • 2012
  • Recent years have witnessed the use of micro shock tube in various engineering applications like micro combustion, micro propulsion, particle delivery systems etc. The flow characteristics occurring in the micro shock tube shows a considerable deviation from that of well established conventional macro shock tube due to very low Reynolds number and high Knudsen number effects. Also the diaphragm rupture process, which is considered to be instantaneous process in many of the conventional shock tubes, will be crucial for micro shock tubes in determining the near diaphragm flow field and shock formation. In the present study, an axi-symmetric CFD method has been applied to simulate the micro shock tube, with Maxwell's slip velocity and temperature jump boundary conditions. The effects of finite diaphragm rupture process on the flow field and the shock formation was investigated, in detail. The results show that the shock strength attenuates rapidly as it propagates through micro shock tubes.

  • PDF

The Effect of Curvature Radius and Material of Diaphragm on the Valve Opening Time in Diaphragm Type S/R Valve (S/R 밸브에서 격막의 곡률반경과 재료가 밸브 개구시간에 미치는 영향)

  • Cheon, Heung-Kyun;Hwang, Jae-Gun;Cho, Tae-Seok;Kwon, Young-Doo;Kwon, Soon-Bum
    • Proceedings of the KSME Conference
    • /
    • 2007.05b
    • /
    • pp.2961-2966
    • /
    • 2007
  • When the pressure at the weak spot established at a certain part of a high pressure vessel or piping system exceeds a design pressure, this weak spot is burst, and the pressurized gas emitted through the weak spot will cause a compression wave system. In this connection, in the present study, an experimental study by using a conventional shock tube facility is performed to estimate the effects of the material of diaphragm, curvature radius and thickness of materials on the valve opening time in diaphragm. Pressure sensor having 500kHz in natural frequency is installed at 35mm downstream of the rupture diaphragm to measure the static pressure history of propagating and being accumulated compression wave. 4 kinds of materials are used as diaphragm that is aluminium, copper, stainless steel and zinc. The diaphragm radii of curvature R are ${\infty}$, 120mm and 60, respectively. And the depth for $90^{\circ}$ groove is 0.04mm. It is found that the smaller the tensile strength and elongation of the rupture diaphragm is, the smaller the radius of curvature of the rupture diaphragm is, and for the same conditions the thinner the thickness of the rupture diaphragm is, the shorter the valve opening time becomes. Also, the tensile strength, elongation and the radius of curvature of the rupture diaphragm for the same conditions are smaller, the maximum pressure rise caused by the coalescences of the compression wave is smaller. Finally the pressure ratio is higher, the valve opening time is shortened and gradient of pressure increment is more steepen.

  • PDF

Effect of Combining Wood Particles and Plastic(Polypropylene) Screen on the Physical and Mechanical Properties of Board (목재(木材)파이티클과 플라스틱(폴리프로필렌) 망(網)의 결체(結締) 보오드의 물리(物理) 및 기술적(機械的) 성질(性質)에 미치는 영향(影響))

  • Lee, Phil-Woo;Park, Heon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.16 no.1
    • /
    • pp.21-44
    • /
    • 1988
  • As a way for the effective utilization of pallman chips and sawdusts, these furnish materials were combined with non-woody material of plastic (polypropylene) screen in board manufacturing to improve their weak physical and mechanical properties. The conventional boards were made with conditions of specific gravity 0.40, 0.55, 0.70, and 0.85, resin content 8, 10, 12 and 14%, and number of polypropylene screen 1, 2, 3 and 4, and press-lam boards were also manufactured. The physical and mechanical properties were measured and discussed on thickness swelling, bending modulus of rupture and elasticity, tensile strength, internal bond strength, and screw holding strength. The results obtained at this study were summarized as follows: 1. In thinckness swelling both of pallman chip board and sawdust board were improved by the increase of resin content, and press-lam boards showed lower thickness swelling than conventional boards. 2. Both the modulus of rupture and elasticity were increased with the increase of specific gravity, and press-lam boards showed higher modulus of rupture and elasticity than conventional boards. On the other hand, modulus of rupture was increased with the increase of number of polypropylene screen and resin content whereas these effects in modulus of elasticity was not recognized. 3. Tensile strength was increased with the increase of specific gravity, and the boards combined with polypropylene screen showed higher tensile strength than control boards. Also tensile strength was increased with the increase of number of polypropylene screen, and press-lam boards revealed higher tensile strength than conventional boards. 4. Internal bond strength was increased with the increase of specific gravity, and the boards combined with polypropylene screen were lower in internal bond strength than control boards. Also, the boards combined with odd number of polypropylene screen showed lower internal bond strength than those combined with even number of polypropylene screen. 5. Screw holding strength was increased with the increase of resin content and specific gravity but significant difference was not approved between boards combined with polypropylene screen and control boards. In press-lam boards, pallman chip boards of higher specific gravity but sawdust boards of lower specific gravity showed better screw holding strength than control boards.

  • PDF

Performance of self-compacting concrete at room and after elevated temperature incorporating Silica fume

  • Ahmad, Subhan;Umar, Arshad;Masood, Amjad;Nayeem, Mohammad
    • Advances in concrete construction
    • /
    • v.7 no.1
    • /
    • pp.31-37
    • /
    • 2019
  • This paper evaluates the workability and hardened properties of self-compacting concrete (SCC) containing silica fume as the partial replacement of cement. SCC mixtures with 0, 2, 4, 6, 8 and 10% silica fume were tested for fresh and hardened properties. Slump flow with $T_{500}$ time, L-box and V-funnel tests were performed for evaluating the workability properties of SCC mixtures. Compressive strength, splitting tensile strength and modulus of rupture were performed on hardened SCC mixtures. Experiments revealed that replacement of cement by silica fume equal to and more than 4% reduced the slump flow diameter and increased the $T_{500}$ and V-funnel time linearly. Compressive strength, splitting tensile strength and modulus of rupture increased with increasing the replacement level of cement by silica fume and were found to be maximum for SCC mixture with 10% silica fume. Further, residual hardened properties of SCC mixture yielding maximum strengths (i.e., SCC with 10% silica fume) were determined experimentally after heating the concrete samples up to 200, 400, 600 and $800^{\circ}C$. Reductions in hardened properties up to $200^{\circ}C$ were found to be very close to normal vibrated concrete (NVC). For 400 and $600^{\circ}C$ reductions in hardened properties of SCC were found to be more than NVC of the same strength. Explosive spalling occurred in concrete specimens before reaching $800^{\circ}C$.

Biomechanical Analysis of Walking and Running after a Surgically Repaired Achilles Tendon Rupture (아킬레스건 파열 수술 후 걷기 및 달리기 운동역학적 분석)

  • Heo, Jeong;Park, Sang-Kyoon
    • Korean Journal of Applied Biomechanics
    • /
    • v.31 no.4
    • /
    • pp.241-248
    • /
    • 2021
  • Objective: The purpose of this study was to investigate the difference in muscle strength, kinematics, and kinetics between injured and non-injured sides of the leg after Achilles Tendon Rupture surgery during walking and running. Method: The subjects (n=11; age = 30.63 ± 5.69 yrs; height = 172.00 ± 4.47 cm; mass = 77.00 ± 11.34 kg; time lapse from surgery = 29.81 ± 10.27 months) who experienced Achilles Tendon Rupture (ATR) surgery participated in this study. The walking and running trials were collected using infrared cameras (Oqus 300, Qualisys, Sweden, 100 Hz) on instrumented treadmill (Bertec, U.S.A., 1,000 Hz) and analyzed by using QTM (Qualisys Track Manager Ver. 2.15; Qualisys, U.S.A). The measured data were processed using Visual 3D (C-motion Inc., U.S.A.). The cutoff frequencies were set as 6 Hz and 12 Hz for walking and running kinematics respectively, while 100 Hz was used for force plate data. Results: In ATR group, muscle strength there were no difference between affected and unaffected sides (p> .05). In kinematic analysis, subjects showed greater ROM of knee joint flexion-extension in affected side compared to that of unaffected side during walking while smaller ROM of ankle dorsi-plantar and peak knee flexion were observed during running (p< .05). In kinetic analysis, subjects showed lower knee extension moment (running at 2.2 m/s) and positive ankle plantar-flexion power (running at 2.2 m/s, 3.3 m/s) in affected side compared to that of unaffected side (p< .05). This lower positive ankle joint power during a propulsive phase of running is related to slower ankle joint velocity in affected side of the subjects (p< .05). Conclusion: This study aimed to investigate the functional evaluation of the individuals after Achilles tendon rupture surgery through biomechanical analysis during walking and running trials. Based on the findings, greater reduction in dynamic joint function (i.e. lower positive ankle joint power) was found in the affected side of the leg compared to the unaffected side during running while there were no meaningful differences in ankle muscle strength and walking biomechanics. Therefore, before returning to daily life and sports activities, biomechanical analysis using more dynamic movements such as running and jumping trials followed by current clinical evaluations would be helpful in preventing Achilles tendon re-rupture or secondary injury.