• Title/Summary/Keyword: Rod shaped

Search Result 382, Processing Time 0.026 seconds

The Characteristic of Selective Attachment and Bioleaching for Pyrite Using Indigenous Acidophilic Bacteria at $42^{\circ}C$ ($42^{\circ}C$에서 토착호산성박테리아의 황철석 표면에 대한 선택적 부착과 용출 특성)

  • Park, Cheon-Young;Kim, Soon-Oh;Kim, Bong-Ju
    • Economic and Environmental Geology
    • /
    • v.43 no.2
    • /
    • pp.109-121
    • /
    • 2010
  • The bioleaching experiment under $42^{\circ}C$ was effectively carried out to leach the more valuable element ions from the pyrite in the Gangyang mine waste. Bacteria can survive at this temperature, as indigenous acidophilic bacteria were collected in the Hatchobaru acidic hot spring, in Japan. To enhance the bacterial activity, yeast extract was added to the pyrite-leaching medium. The indigenous acidophilic bacteria appeared to be rod-shaped in the growth-medium which contained elemental sulfur and yeast extract. The rod-shaped bacteria ($0.7\times2.6\;{\mu}m$, $0.6\times7\;{\mu}m$, $0.8\times5\;{\mu}m$ and $0.7\times8.4\;{\mu}m$) were attached to the pyrite surface. The colonies of the rod-shaped bacteria were selectively attached to the surroundings of a hexagonal cavity and the inner wall of the hexagonal cavity, which developed on a pyrite surface. Filament-shaped bacteria ranging from $4.92\;{\mu}m$ to $10.0\;{\mu}m$ in length were subsequently attached to the surrounding cracks and inner wall of the cracks on the pyrite surface. In the XRD analysis, the intensity of (111), (311), (222) and (320) plane on the bacteria pyrite sample relatively decreased in plane on the control pyrite sample, whereas the intensity of (200), (210) and (211) increased in these samples. The microbiological leaching content of Fe ions was found to be 3.4 times higher than that of the chemical leaching content. As for the Zn, microbiological leaching content, it was 2 times higher than the chemical leaching content. The results of XRD analysis for the bioleaching of pyrite indicated that the indigenous acidophilic bacteria are selectively attacked on the pyrite specific plane. It is expected that the more valuable element ions can be leached out from the mine waste, if the temperature is increased in future bioleaching experiments.

Isolation of Actinomycetes Producing Extracellular Adenosin Deaminase (세포외 Adenosine Deaminase를 생산하는 방선균의 분리)

  • 전홍기;김태숙
    • Korean Journal of Microbiology
    • /
    • v.28 no.1
    • /
    • pp.83-89
    • /
    • 1990
  • Two strains of actinomycetes producing extracellular adenosine deaminase, strain J-845S and strain J-326TK, were isolated from soil. Strain J-845S was gram-positive and non-acid-fast. This strain formed whitish, rod-shaped, smooth and non-motile spores on the aerial mycelium, and the spore chain was spiral. The hyphae of the mycelium branched abundantly. Cell wall chemotypes of the strain were of type I containing LL-diaminopimelic acids, and of phospholipid type II, and then strain J-845S was designated as Streptomyces sp.. Strain J-326TK was gram-positive and non-acid-fast. The hyphae of primary and aerial mycelium fragmented into irregular rod of coccus-like elements. The aerial mycelium either did not branch or sparsely branched. Cell wall composition was of type I and phospholipid type I. Thus, strain J-326TK was identified as Nocardioides sp.

  • PDF

The Preparation and Growth Mechanism of the Recovered Bi2Te3 Particles with Respect to Surfactants (회수된 Bi2Te3의 계면활성제에 따른 합성 및 성장 거동)

  • So, Hyeongsub;Song, Eunpil;Choa, Yong-Ho;Lee, Kun-Jae
    • Journal of Powder Materials
    • /
    • v.24 no.2
    • /
    • pp.141-146
    • /
    • 2017
  • $Bi_2Te_3$ powders are recovered by wet chemical reduction for waste n-type thermoelectric chips, and the recovered particles with different morphologies are prepared using various surfactants such as cetyltrimethylammonium bromide (CTAB), sodium dodecylbenzenesulfonate (SDBS), and ethylenediaminetetraacetic acid (EDTA). When citric acid is added as the surfactant, the shape of the aggregated particles shows no distinctive features. On the other hand, rod-shaped particles are formed in the sample with CTAB, and sheet-like particles are synthesized with the addition of SDBS. Further, particles with a tripod shape are observed when EDTA is added as the surfactant. The growth mechanism of the particle shapes depending on the surfactant is investigated, with a focus on the nucleation and growth phenomena. These results help to elucidate the intrinsic formation mechanism of the rod, plate, and tripod structures of the $Bi_2Te_3$ recovered by the wet reduction process.

Synthesis of CdS Nanocrystals with Different Shapes via a Colloidal Method

  • Bai, Jie;Liu, Changsong;Niu, Jinzhong;Wang, Hongzhe;Xu, Shasha;Shen, Huaibin;Li, Lin Song
    • Bulletin of the Korean Chemical Society
    • /
    • v.35 no.2
    • /
    • pp.397-400
    • /
    • 2014
  • Size- and shape-controlled monodisperse wurtzite structured CdS nanorods have been successfully synthesized using a facile solution-based colloidal method. Depending on the control of injection/growth temperatures and the variation of Cd-to-S molar ratios, the morphology of the CdS nanocrystals (NCs) can be adjusted into bullet-like, rod-like, and dot-like shapes. X-ray diffraction (XRD), transition electron microscopy (TEM), and absorption spectroscopy were used to characterize the structure, morphology, and optical properties of as-synthesized CdS NCs. It was found that uniform CdS nanorods could be successfully synthesized when the injection and growth temperatures were very high (> $360^{\circ}C$). The aspect ratios of different shaped (bullet-like or rod-like) CdS NCs could be controlled by simply adjusting the molar ratios between Cd and S.

Effect of Synthetic Temperature and Time on the Morphology of ZnO Crystals Fabricated by Thermal Evaporation of Al-Zn Mixture (Al-Zn 혼합물의 열 증발을 이용한 ZnO 결정의 합성에서 결정의 형상에 미치는 합성 온도와 시간의 영향)

  • Kim, Min-Sung
    • Korean Journal of Materials Research
    • /
    • v.25 no.6
    • /
    • pp.265-268
    • /
    • 2015
  • ZnO micro/nanocrystals at large scale were synthesized through the thermal evaporation of Al-Zn mixtures under air atmosphere. The effect of synthetic temperature and time on the morphology of the micro/nanocrystals was examined. It was found that the temperature and time affected the morphology of the ZnO crystals. At temperatures below $900^{\circ}C$, no crystals were synthesized. At a temperature of $1000^{\circ}C$, ZnO crystals with a rod shape were synthesized. With an increase in temperature from $1000^{\circ}C$ to $1100^{\circ}C$, the morphology of the crystals changed from rod shape to wire and granular shapes. As the time increased from 2 h to 3 h at $1000^{\circ}C$, tetrapod-shaped ZnO crystals started to form. XRD patterns showed that the ZnO crystals had a hexagonal wurtzite structure. EDX analysis revealed that the ZnO crystals had high purity. It is believed that the ZnO nanowires were grown via a vapor-solid mechanism because no catalyst particles were observed at the tips of the micro/nanocrystals in the SEM images.

Preparation of Zirconia Nanocrystalline Powder by the Hydrothemal Treatment at low Temperature (수열법에 의한 저온 결정형 지르코니아 나노 분말의 제조)

  • Noh, Hee-Jin;Lee, Jong-Kook;Seo, Dong-Seok;Hwang, Kyu-Hong
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.3
    • /
    • pp.308-314
    • /
    • 2002
  • The nanocrystalline zirconia powder was synthesized from the zirconium hydroxide precipitate by hydrothermal process with the reaction temperature range 100∼250$^{\circ}$C, reaction time 1∼48 hours and additive concentration 1, 5 N NaOH solutions. The lower hydrothermal treatment temperature, the inner spherical tetragonal zirconia was synthesized. The fraction of monoclinic phase zirconia with rod shape increased with increasing the hydrothermal treatment temperature. As the concentration of the NaOH solution increases, the synthesized particle in breadth and length increased; breadth and length ratio decreased. In the case of the low concentration of NaOH solution, however, the particle length became relatively larger than its breadth resulting in the rod-shaped particles with bigger aspect ratio.

A Study on the Mechanization of the Grounding Rod Earth Construction Method to Improve the Grounding Resistance Characteristics (봉형접지극 접지저항 향상을 위한 기계화 시공 연구)

  • Park, Jung-Shin;Cho, Sung-Jae;An, In-Suk
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.23 no.10
    • /
    • pp.143-150
    • /
    • 2009
  • The bar-shaped electrode is very popular in earth construction for its easy obtainments of the regulative grounding resistance values on power distribution systems in many countries. For these reason, a lots of researches are being proceeded on its deformation and materials. But the grounding construction has limit for improvement the grounding resistance characteristics not only by the improvement of the driven electrode, because that the grounding characteristics are very sensitive to soils(hard, soft). This study is about the construction methods on which the driven electrode can be serially or parallely connected using by hollow screw rod for obtaining the regulative grounding resistance values. The experimental results show that the grounding resistance values are reduced more than 30[%] comparing with the other construction methods under the same conditions(earth resistance, numbers of driven electrode, construction method of serial and parallel, chemicals for reducing grounding resistance, water).

Germanium-based pinning dopants for MgB2 bulk superconductors

  • Chung, K.C.;Ranot, M.;Shinde, K.P.;Oh, Y.S.;Kang, S.H.;Jang, S.H.;Hwang, D.Y.
    • Progress in Superconductivity and Cryogenics
    • /
    • v.21 no.2
    • /
    • pp.36-39
    • /
    • 2019
  • Effects of the spherically shaped Ge and the rod-like carbon-coated Ge on the superconducting properties of $MgB_2$ were investigated. Pure Ge and carbon-coated Ge nano-powders were synthesized under the different amount of $CH_4$ (0 to 5 kPa) by using DC thermal plasma method. When the $CH_4$ was added ~100 nm sized Ge with a spherical shape changed to rod-like morphology with a diameter of ~30-70 nm and a length of ~400-500 nm. Also it was confirmed that thin carbon layers of a few nanometers were formed along the rod length and the agglomerated carbons were found on the edges of rods. Pure spherical Ge and Ge/C rods were mixed and milled with Mg & B precursor to form the doped $MgB_2$ bulk samples by the solid-state reaction method. Almost no change of $T_c$ was noticed for the pure Ge-added $MgB_2$, whereas $T_c$ was found to decrease with the Ge/C-added $MgB_2$ samples. It was found that the pure spherical Ge showed to have a negative effect on the flux pinning of $MgB_2$. However, Ge/C rods can enhance the flux pinning property of $J_c$ due to the coated carbon on Ge rods.

Preliminary Study on Rapid Measurement of Gross Alpha/Beta and 90Sr Activities in Surface Soil by Mobile ZnS(Ag)/PTV Array and Handheld PVT Rod with Gated Energy Channels

  • Lee, Chanki;Kim, Hee Reyoung
    • Journal of Radiation Protection and Research
    • /
    • v.46 no.4
    • /
    • pp.194-203
    • /
    • 2021
  • Background: Surface soil radiation monitoring around nuclear facilities is important to classify and characterize the contaminated areas. A scanning and direct measurement technique can survey the sites rapidly before starting sampling analysis. Materials and Methods: Regarding this, we test and suggest a measurement technique for gross alpha/beta and 90Sr activities in surface soil based on a mobile ZnS(Ag)/PVT (polyvinyltoluene) array and a handheld PVT rod, respectively. To detect 90Sr selectively in soil mixed with naturally occurring radioactive materials, chosen energy channel counts from the multichannel analyzers were used instead of whole channel counts. Soil samples contaminated with exempt liquid 90Sr with 1 Bq·g-1, 3 Bq·g-1, and 10 Bq·g-1 were prepared and hardened by flocculation. Results and Discussion: The mobile ZnS(Ag)/PVT array could discriminate gross alpha, gross beta, and gamma radiation by the different pulse-shaped signal features of each sensor material. If the array is deployed on a vehicle, the scan minimum detectable concentration (MDC) range will be about 0.11-0.17 Bq·g-1 at 18 km·h-1 speed, highly sensitive to actual sites. The handheld PVT rod with 12 mm (Φ) × 20 mm (H) size can directly measure 90Sr selectively if channels on which energies are from 1,470 and 2,279 keV are gated, minimizing crossdetection of other radionuclides. These methods were verified by measuring soil samples fabricated with homogeneous 90Sr concentrations, showing static MDC of 2.16 Bq·g-1 at a measurement time of 300 seconds. Conclusion: Based on the results, comprehensive procedures using these detectors are suggested to optimize soil sites survey.

Effect of Morphology on Electron Transport in Dye-Sensitized Nanostructured $TiO_2$ Films

  • Park, Nam-Gyu;Jao van de Lagemaat;Arthur J. Frank
    • Journal of Photoscience
    • /
    • v.10 no.2
    • /
    • pp.199-202
    • /
    • 2003
  • The relationship between the morphology of nanostructured TiO$_2$ films and the photo-injected electron transport has been investigated using intensity-modulated photocurrent spectroscopy (IMPS). For this purpose, three different TiO$_2$ films with 5 ${\mu}{\textrm}{m}$ thickness are prepared: The rutile TiO$_2$ film with 500 nm-sized cluster-like spherical bundles composed of the individual needles (Tl), the rutile TiO$_2$ film made up of non-oriented, homogeneously distributed rod-shaped particles having a dimension of approximately 20${\times}$80 nm (T2), and the anatase TiO$_2$ film with 20 nm-sized spherically shaped particles (T3). Cross sectional scanning electron micrographs show that all of the TiO$_2$films have a quite different particle packing density: poorly packed Tl film, loosely packed T2 film and densely packed T3 film. The electron transport is found to be significantly influenced by film morphology. The effective electron diffusion coefficient D$_{eff}$ derived from the IMPS time constant is an order of magnitude lower for T2 than for T3, but the D$_{eff}$ for the Tl sample is much lower than T2. These differences in the rate of electron transport are ascribed to differences in the extent of interparticle connectivity associated with the particle packing density.ity.

  • PDF