This study tried to analyze about the investment effects on the spent capital and possessed tangible assets of some hospitals during their hospital management. For this analysis purpose, this study used the financial data of 100 hospitals which presented their financial statements to an finance-information company from 2004 to 2006. The analysis was done with PEFR(Percentage of External Funds Required) and Tangible Asset. The FEPR considered the retained interior fund relating to the investment types in the hospital industry. And the Tangible Asset was related to the possession condition of facilities and equipment. The EBIT rate(Earnings before interest and tax to sales) meaning the management performance and tangible asset turnover were used as the measured variables of investment effect. As the result of data analysis, it was identified that the tangible asset like the hospitals's facilities and equipment was not an agent significantly to influence on the management performance(EBIT rate), the eventual goal of hospital management. But, it was identified that there was some differences tangible asset turnover according to each hospital's main characteristics. And at targeting the all sample hospitals, it was found that the management performance(EBIT rate) had some significant effect on the retained earnings rate, a part of source of PEFR.
Microstructure and mechanical properties of Fe-Si-Mn-P high strength steel sheet have been investigated by controlling the cooling rate. Bainite and ferrite were obtatined by annealing in the ferrite pluse austenite region, and ferrite and austenite were obtatined after annealing in the fully austenite region. Ferrite and pearlite were obtained when the cooling rate was controlled from the annealing temperature above $760^{\circ}C$ and bainite showed with increasing cooling rate, however below $760^{\circ}C$ ferrite and bainite were obtained. Tensile strengths and hardness nearly unchanged with increasing cooling rate after control the cooling rate from the temperature above $760^{\circ}C$, while tensile strengths increased and elongation decreased with increasing cooling rate when the cooling rate was controlled from the tempeature below $760^{\circ}C$. Without regard to annealing temperature, tensile strength increased and elongation decreased with increasing cooling rate. Tensile strengths and elongation values heat treated in the ferrite plus austenite region were higher than those in the fully austenite region. Retained austenite and strength-elongation balance showed the maximum value at $780^{\circ}C$ and decreased with increasing annealing temperature. Strength-elongation balance value was controlled by the retained austenite.
The effects of cooling rate on the microstructures, precipitation of Cu-cluster, .epsilon.-Cu and impact toughness of high strength low alloy(HSLA) steel were studied using hardness tester, impact tester, DSC(differential scanning calorimetry), AES(auger electron spectroscopy) and TEM(transmission electron microscopy). Not only the Cu-precipitates but also the segregation of Cu, As, Sb, P, S, N, Sn along grain boundary were not observed at the specimens heat treated from 800.deg. C to 300.deg. C with the cooling time of 12-125 sec. The Cu-cluster, .epsilon.-Cu are formed by introducing ageing after cooling and the effect of precipitates on hardening increase after cooling was the same in all cooling rate. The peak hardness was obtained at an ageing of 500.deg. C in all cooling conditions. The impact energy become higher as the cooling time increases. This fact can be explained to be due to the tempering effect applied on the cooling stage since the present alloy has a relatively high Ms temperature and the local high concentration of the retained austenite.
본 연구는 후산정체 젖소에 있어서 Lipopolysaccharide(LPS)의 처리가 번식 성적에 미치는 영향을 구명하기 위하여 분만 후 12시간이 경과하여도 후산이 배출되지 않은 홀스타인 개체 33두 및 대조구 12두에 대하여 분만후 20일째에 LPS 100 ${\mu}g$을 자궁 내에 주입한 다음 7일후에 발정이 발현되었을 때 인공수정을 실시하여 다음과 같은 결과를 얻었다. 후산정체 젖소에 있어서 첫 수정에 의한 수태율은 대조구의 경우 공시한 12두가 모두 첫 수정에 의해 수태가 되지 않았고 처리구는 33두중 11두가 수태되어 33.3%의 수태율을 나타내었다. 후산정체 젖소에 있어서 대조구 및 처리구의 분만후 수태까지의 일수는 각각 $149.6{\pm}34.3$일 및 $53.0{\pm}12.5$일로 처리구가 대조구에 비하여 유의적(p<0.01)으로 단축되는 경향을 나타내었다. 후산정체 젖소에 있어서 대조구 및 처리구의 수태당 종부 횟수는 각각 $3.6{\pm}0.8$회 및 $2.1{\pm}0.3$회로 처리구가 대조구에 비하여 유의적(p<0.05)으로 낮은 경향을 나타내었다.
White cast iron of 3%C-10%Cr-5%Mo-5%W was casted, and then heat treated with three different methods such as homogenizing, austenitizing and tempering to observe its effects on the microstructure, hardness and abrasive wear resistance. In uni-directional soldification, bamboo tree-like $M_7C_3$ carbide grew along with the heat flow direction, and fishbone-like $M_6C$ carbide was dispersed randomly among $M_7C_3$ carbides. While almost pearlitic structures were observed in the as-cast specimen, those of the heat treated specimens consisted of secondary carbide, retained austenite and tempered martensite. In austenitized specimen, the amounts of retained austenite were 60.88% due to the higher cooling rate encountered in forced air cooling. On the other hand, the amounts of retained austenite were reduced from 60.88% to 23.85% in tempered specimen due to the transformation of austenite into tempered martensite. The hardness of tempered specimen showed the highest value, and then decreased in the order of austenitized, as-cast and homogenized specimens. But, the abrasive wear resistance of austenitized specimen was the highest, and then decreased in the order of tempered, as-cast and homogenized specimens.
The objective of this study was to evaluate the duration of retained placenta (RP) on postpartum diseases and culling in dairy cows. Data were collected from 456 Holstein cows between 2008 and 2010. RP (${\geq}$ 24 h after parturition) and postpartum diseases were diagnosed by farm managers and a veterinarian according to standardized definitions. The overall incidence rate of RP was 14.0%, and the incidence rate of RP with fourth and higher parity was two times that of cows having offspring for the first time. The duration of RP was 2 to 15 days with a mean of 6.8 days, except for cases of fourth and higher parity which had a mean of 10.5 days. A total of 63% of cows with RP had postpartum diseases. Among the cows diagnosed with RP, 23.4% developed metritis, and of those, 35.3% developed endometritis or pyometra. A total of 25% (n = 16) cows with RP were culled within 60 days in milk (DIM) and of those culled, 75% (n = 12) had postpartum diseases. These results suggest that RP increases the risk of postpartum diseases such as metritis and mastitis and is a culling hazard up to 60 DIM.
The variation of the mechanical properties and the formation of retained austenite with heat treatment conditions in austempered Si bearing carbon steels has been investigated. In the case of a steel containing 0.35C-1.48Si-0.95Mn, it has been found that a feather shape bainite structure of lath are obtained under a isothermal treated condition at just below the Ms temperature, and the martensite, bainitic ferrite and retained austenite of second phase particles on the ferrite matrix for a isothermal treated steels after intercritical annealing are precipitated in a linked shape. The retained austenite with $2{\mu}m$ size induced as TRIP is found to increase with increasing the formation rate of retained austenite for the intercritical annealing and high Si containing steels. The tensile strength is increased as austempering temperature increases in all isothermal treatment temperature, whereas the elongation is shown to roughly decrease as the tensile strength increases. The values of tensile strength-elongation balance have showed a marked dependence upon the elongation rather than the tensile stregth, and their values are increased for high Si containing steels and intercritical annealing condition. The most optimum result has been shown to be the tensile stregth-elongation balance of $2882.4kgf/mm^2.%$ and the elongation of 33.3% for a "B" steel in the heat treating temperature range of $780{\sim}370^{\circ}C$.
PURPOSE. This retrospective study aims at the evaluation of implant-supported overdentures (IODs) supported by ceramo-galvanic double crowns (CGDCs: zirconia primary crowns + galvano-formed secondary crown). MATERIALS AND METHODS. In a private practice, 14 patients were restored with 18 IODs (mandible: 11, maxilla: 7) retained by CGDCs on 4 - 8 implants and annually evaluated for technical and/or biological failures/complications. RESULTS. One of the 86 inserted implants failed during the healing period (cumulative survival rate (CSR) implants: 98.8%). During the prosthetic functional period (mean: $5.9{\pm}2.2years$), 1 implant demonstrated an abutment fracture (CSR-abutments: 98.2%), and one case of peri-implantitis was detected. All IODs remained in function (CSR-denture: 100%). A total of 15 technical complications required interventions to maintain function (technical complication rate: 0.178 treatments/patients/year). CONCLUSION. Considering the small sample size, the use of CGDCs for the attachment of IODs is possible without an increased risk of technical complications. However, for a final evaluation, results from a larger cohort are required.
In order to compare mechanical properties of ausformed martensite with those of marformed martemsite in Fe-30%Ni-0.1%C alloy and to investigate their strengthening mechanisms, ausformed martensite and marformed martensite were prepared by ausforming treatment and marforming treatment respectively. The microstructures were observed and the quantities of retained austenite, hardness, yield strength, ultimate tensile strength and elongation were examined. The strength of ausformed martensite was mainly increased because of the lattice defects inherited from austenite. The ductility of ausformed martensite was constant at the rate of 7-8% by ductile matrix formation of the retained austenite in spite of the increase in strength. The strength of marformed martensite was increased by the increment in dislocation density, the crossing of transformation twin with deformation twin and the mutual crossing of deformation twin. The ductility of mar formed martensite was slightly lower than that of ausformed martensite, but the strength of mar formed martensite was prominently higher.
Ichinohe, T.;Tamura, T.;Ueda, K.;Okubo, M.;Asahida, Y.
Asian-Australasian Journal of Animal Sciences
/
제8권3호
/
pp.267-273
/
1995
The differences in rumen particle pool size, passage rate and rumen degradability in sheep receiving three varieties of orchardgrass hay harvested at pre-heading (H1), early-bloom (H2) and late-bloom (H3) were investigated using four ruminal-cannulated wethers (68 kg) fed 1,300 g of the hay once a day. Representative samples of whole rumen contents were collected at different times after feeding and the quantities of rumen particle pools [large particle pool (LPP), retained on a $1,180{\mu}m$ sieve; small particle pool (SPP), retained on a 47 but passed a $1,180{\mu}m$ sieve; and soluble fraction (SOL), passed a $47{\mu}m$ sieve (SOL)] were determined by a wet-sieving technique. The fullowing results were obtained: 1) The dry weight of whole rumen contents were significantly lower (p < 0.05) for HI than for H2 or H3. The reduction rate of whole rumen contents was slightly but significantly greater for HI that, the other hay varieties. 2) The LPP disappearance rates were 26.2, 25.3 and 21.7 g DM/h for H1, H2 and H3, respectively, and no statistical differences were found among the hay varieties. Appreciable changes were not observed with SPP and SOL throughout measurements for all hay varieties; however the SPP was markedly greater (p <0.05) for H2 and ill than for HI, while SOL did not differ among hay varieties. 3) The SPP passage rate (g DM/h) and effective rumen degradability (%) for HI, H2 and ill were, respectively, 9.7, 56.6; 16.9, 42.3; and 18.0, 28.9. The ruminal tum-over rate for SPP appeared to be higher for HI than for the other hay varieties.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.