비정질강섬유 보강 고강도 콘크리트의 온도별 잔존 역학적 특성 평가 (The residual mechanical properties evaluation according to temperature of the amorphous metallic fiber reinforced high strength concrete)

  • 서동균;김규용;이상규;황의철;유하민;남정수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2020년도 가을 학술논문 발표대회
    • /
    • pp.98-99
    • /
    • 2020
  • This study is aim to assess mechanical properties which is highly related to structural safe and durability of 100MPa high strength concrete mixed with amorphous metallic fiber. All specimens were heated with low velocity heating rate(1℃/min.), residual compressive strength and residual flexural strength was evaluated. The specimens were cooled down to room temperature after heating. As a result, in the case of 100MPa high-strength concrete, the residual compressive strength enhancing effect of amorphous metallic fiber has showed with the mix proportion of fiber. In addition, residual flexural strength showed more regular pattern before 300℃ then residual compressive strength, but simillar decreasing behavior was shown after 300℃ like residual compressive strength. Further study about fiber pull-out behavior and fiber mechanical, chemical property change due to temperature is needed.

  • PDF

A comparative experimental study on the mechanical properties of cast-in-place and precast concrete-frozen soil interfaces

  • Guo Zheng;Ke Xue;Jian Hu;Mingli Zhang;Desheng Li;Ping Yang;Jun Xie
    • Geomechanics and Engineering
    • /
    • 제36권2호
    • /
    • pp.145-156
    • /
    • 2024
  • The mechanical properties of the concrete-frozen soil interface play a significant role in the stability and service performance of construction projects in cold regions. Current research mainly focuses on the precast concrete-frozen soil interface, with limited consideration for the more realistic cast-in-place concrete-frozen soil interface. The two construction methods result in completely different contact surface morphologies and exhibit significant differences in mechanical properties. Therefore, this study selects silty clay as the research object and conducts direct shear tests on the concrete-frozen soil interface under conditions of initial water content ranging from 12% to 24%, normal stress from 50 kPa to 300 kPa, and freezing temperature of -3℃. The results indicate that (1) both interface shear stress-displacement curves can be divided into three stages: rapid growth of shear stress, softening of shear stress after peak, and residual stability; (2) the peak strength of both interfaces increases initially and then decreases with an increase in water content, while residual strength is relatively less affected by water content; (3) peak strength and residual strength are linearly positively correlated with normal stress, and the strength of ice bonding is less affected by normal stress; (4) the mechanical properties of the cast-in-place concrete-frozen soil interface are significantly better than those of the precast concrete-frozen soil interface. However, when the water content is high, the former's mechanical performance deteriorates much more than the latter, leading to severe strength loss. Therefore, in practical engineering, cast-in-place concrete construction is preferred in cases of higher negative temperatures and lower water content, while precast concrete construction is considered in cases of lower negative temperatures and higher water content. This study provides reference for the construction of frozen soil-structure interface in cold regions and basic data support for improving the stability and service performance of cold region engineering.

표면특수가공에 따른 재료의 피로균열에 관한 연구 (A Study on the Fatigue Crack of Material by Surface Non-Traditional Machining)

  • 이태연;이승호;강진식
    • 소성∙가공
    • /
    • 제10권3호
    • /
    • pp.179-184
    • /
    • 2001
  • The influence of the fatigue crack propagation by shot peening was studied in this paper. Fatigue tests were carried out on the unpeened and shot peened CT specimens. The changes of mechanical properties, residual stress, fatigue fracture surface etc. by shot peening were investigated. The mechanical properties, residual stress, fatigue surface etc. by shot peening were investigated. The mechanical peened specimen improved in fatigue life up to 14% by shot peening. The reason of increase in the fatigue life was closely related with the compressive residual stress, which was 519.7MPa on surface. Another reason was the constraint on crack opening on surface region, it is due to the decrease in slope of crack propagation direction.

  • PDF

횡방향 등방성을 고려한 단섬유 인장 실험 모델링 (Modeling of Single Fiber Pull-Out Experiment Considering the Effects of Transverse Isotropy)

  • 설일찬;이춘열;채영석
    • 대한기계학회논문집A
    • /
    • 제26권7호
    • /
    • pp.1384-1392
    • /
    • 2002
  • Single fiber pull-out technique has been commonly used to characterize the mechanical behavior of interface in fiber reinforced composite materials. An improved analysis considering the effects of transversely isotropic properties of fiber and the effects of thermal residual stresses in both radial and axial directions along the fiber/matrix interface is developed for the single fiber pull-out test. Although the stress transfer properties across the interface is not much affected by considering the transversely isotropic properties of fiber, interfacial debonding is notably encouraged by the effect. The interfacial shear stress that plays an important role in interfacial debonding is very much affected by the component of axial thermal residual stress in the bonded region, which can induce a two-way debonding mechanism.

2단쇼트피닝에 의한 피로특성의 향상 (The Improvement of Fatigue Properties by 2-step Shot Peening)

  • 이승호;심동석
    • 한국표면공학회지
    • /
    • 제36권6호
    • /
    • pp.475-479
    • /
    • 2003
  • In this study, to investigate the effects of 2-step shot peening at the surface of spring steel, tests are conducted on spring steel and shot peened specimens. Various tests are accomplished to evaluate mechanical properties influenced by shot peening process, and fatigue tests are also performed to evaluate the improvement of fatigue strength. And then the residual stresses are examined. The mechanical properties of material did not change so much by shot peening. However, the fatigue strength of notched specimen remarkably increased. In the case of 1-step shot peening, fatigue strength increased by about 20% than unpeened specimen. Especially, in the case of 2-step shot peening, fatigue strength increased by about 40%, because the residual compressive stress at surface was higher than that of 1-step shot peened specimen. The fatigue strength and life are closely related to the value and position of maximum compressive residual stress by shot peening.

수직벽으로 연속 충돌하는 액적들의 비산/잔류 동적 거동 가시화 및 분석 연구 (Visualization and Analysis of the Dynamic Behavior of Splashes and Residuals of Droplets Continuously Colliding with a Vertical Wall)

  • 노재현;이훈석;박태영;김승호
    • 한국가시화정보학회지
    • /
    • 제22권2호
    • /
    • pp.82-89
    • /
    • 2024
  • In this study, experiments were conducted to visualize and analyze the dynamic characteristics of splash and residual liquid film formation during and after the injection of water droplets onto vertically situated solid substrates with varying surface wettability, elasticity, and microtexture. As wettability decreased (higher contact angle), more splash droplets formed, and the residual liquid film decreased. Low contact angles resulted in thin residual films and less splash. Surface elasticity absorbed the impact forces of droplets, thereby decreasing splash phenomena and significantly reducing the formation of residual liquid films due to surface vibration. Surfaces with microtextures demonstrated control over droplet splash direction, guiding the liquid along desired pathways. High-speed imaging provided detailed insights, showing that surface properties critically influence splash dynamics and residual liquid film formation.

계장화 압입시험법을 이용한 구조물 용접부의 잔류응력 평가 (Residual stress evaluation of weldment in structures using instrumented indentation technique)

  • 이정석;최열;김광호;유근봉;권동일
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 춘계학술발표대회 개요집
    • /
    • pp.288-290
    • /
    • 2005
  • Apparent mechanical properties in structural components can be different from the initially designed values due to the formation of the residual stress in metal forming and welding. Therefore, the evaluation of residual stress has great importance in the reliability diagnosis of structural components. A nondestructive continuous indentation technique has been proposed to evaluate various strength concerning mechanical properties from the analysis of load-depth curve. In this study, quantitative residual stress estimation on API X65 welded joints for natural gas pipeline was performed by analyzing the variation of indentation loading curve by residual stress through a new proposed theoretical model.

  • PDF

Ni-Fe 합금 도금층의 기계적 물성에 영향을 미치는 도금인자 (The Effects of Electroplating Parameters on the Mechanical Properties of Nickel-Iron Alloy Electrodeposits)

  • 고영권;임태홍;이재호
    • 마이크로전자및패키징학회지
    • /
    • 제15권4호
    • /
    • pp.71-76
    • /
    • 2008
  • 전기도금법에 의한 니켈-철 합금 도금층은 전류인가방식, 전류밀도, 첨가제, 도금 욕에서 철과 니켈에 농도비 등과 같은 공정 변수에 따라 그 조성이 민감하게 변화하고 특히 전류인가방식에 따라 도금 층의 조성과 기계적인 특성이 달라지는 경향을 보이고 있다. 본 연구에서는 전류의 인가방식과 전류밀도 변화에 따른 경도, 내마모성, 인성,표면 거칠기 및 잔류응력 등의 기계적인 물성의 변화를 연구하였다. 전류인가방식을 직류에서 펄스전류로 변환시킴에 따라 인장강도가 15% 증가하였으며, 잔류음력이 10% 감소하였고, 내마모성이 30% 향상되었다.

  • PDF

Fire Resistance Studies on High Strength Steel Structures

  • Wang, Wei-Yong;Xia, Yue;Li, Guo-Qiang
    • 국제초고층학회논문집
    • /
    • 제7권4호
    • /
    • pp.287-298
    • /
    • 2018
  • High strength steels have been widely applied in recent years due to high strength and good working performance. When subjected to fire conditions, the strength and elastic modulus of high strength steels deteriorate significantly and hence the load bearing capacity of structures reduces at elevated temperatures. The reduction factors of mechanical properties of high strength steels are quite different from mild steels. Therefore, the fire design methods deduced from mild steel structures are not applicable to high strength steel structures. In recent ten years, the first author of this paper has carried out a lot of fundamental research on fire behavior of high strength steels and structures. Summary of these research is presented in this paper, including mechanical properties of high strength steels at elevated temperature and after fire exposure, creep response of high strength steels at elevated temperature, residual stresses of welded high strength steel member after fire exposure, fire resistance of high strength steel columns, fire resistance of high strength steel beams, local buckling of high strength steel members, and residual strength of high strength steel columns after fire exposure. The results show that the mechanical properties of high strength steel in fire condition and the corresponding fire resistance of high strength steel structures are different from those of mild steel and structures, and the fire design methods recommended in current design codes are not applicable to high strength steel structures.

An experimental and numerical analysis of concrete walls exposed to fire

  • Baghdadi, Mohamed;Dimia, Mohamed S.;Guenfoud, Mohamed;Bouchair, Abdelhamid
    • Structural Engineering and Mechanics
    • /
    • 제77권6호
    • /
    • pp.819-830
    • /
    • 2021
  • To evaluate the performance of concrete load bearing walls in a structure under horizontal loads after being exposed to real fire, two steps were followed. In the first step, an experimental study was performed on the thermo-mechanical properties of concrete after heating to temperatures of 200-1000℃ with the purpose of determining the residual mechanical properties after cooling. The temperature was increased in line with natural fire curve in an electric furnace. The peak temperature was maintained for a period of 1.5 hour and then allowed to cool gradually in air at room temperature. All specimens were made from calcareous aggregate to be used for determining the residual properties: compressive strength, static and dynamic elasticity modulus by means of UPV test, including the mass loss. The concrete residual compressive strength and elastic modulus values were compared with those calculated from Eurocode and other analytical models from other studies, and were found to be satisfactory. In the second step, experimental analysis results were then implemented into structural numerical analysis to predict the post-fire load-bearing capacity response of the walls under vertical and horizontal loads. The parameters considered in this analysis were the effective height, the thickness of the wall, various support conditions and the residual strength of concrete. The results indicate that fire damage does not significantly affect the lateral capacity and stiffness of reinforced walls for temperature fires up to 400℃.