A numerical method for estimating the elastic modulus of recycled concrete

  • Zhou, Xinzhu;Zheng, Jianjun;Chen, Ting;Zhang, Jian;Wang, Chuanyang;Wu, Jiefeng
    • Computers and Concrete
    • /
    • v.23 no.3
    • /
    • pp.161-170
    • /
    • 2019
  • This paper aims at presenting a numerical method for estimating the elastic modulus of recycled concrete with crushed aggregates. In the method, polygonal aggregates following a given sieve curve are generated, and placed into a square simulation element with the aid of the periodic boundary condition and the overlap criterion of two polygonal aggregates. The mesostructure of recycled concrete is reconstructed by embedding an old interfacial transition zone (ITZ) layer inside each recycled aggregate and by coating all the aggregates with a new ITZ layer. The square simulation element is discretized into a regular grid and a representative point is selected from each sub-element. The iterative method is combined with the fast Fourier transform to evaluate the elastic modulus of recycled concrete. After the validity of the numerical method is verified with experimental results, a sensitivity analysis is conducted to evaluate the effects of key factors on the elastic modulus of recycled concrete. Numerical results show that the elastic modulus of recycled concrete increases with the increase of the total aggregate content and the elastic moduli of old and new ITZ but decreases with increasing the replacement ratio of recycled aggregate and the thicknesses of old and new ITZ. It is also shown that, for a replacement ratio of recycled aggregate smaller than 0.3, the elastic modulus of recycled concrete is reduced by no more than 10%.

Durability of Mortar Matrix Replaced with Recycled Fine Aggregates (순환골재(循環骨材)를 혼입(混入)한 모르타르 경화체(硬化體)의 내구(耐久) 특성(特性))

  • Kim, Jong-Pil;Lee, Seung-Tae;Jung, Ho-Seop;Park, Kwang-Pil;Kim, Seong-Soo
    • Resources Recycling
    • /
    • v.16 no.6
    • /
    • pp.20-27
    • /
    • 2007
  • This paper presents a detailed experimental study on the durability properties of mortar matrix made with two kind of recycled fine aggregates(RAA, RAB) and five replacement levels (0, 25, 40, 75 and 100) of the recycled fine aggregates as a partial replacement of natural fine aggregate (NA). The durability properties of mortar matrix was evaluated using compressive strength, chloride ion ingress, sulfate attack and carbonation. The test results indicated that the water absorption and Adhered mortar of the recycled fine aggregate was a major factor controlling durability properties. Hereafter, when using built recycled fine aggregate is expected, appropriate removal Adhered mortar and reasonable replacement ratio of recycled fine aggregates was 25% weight of cement are advised to apply to the concrete materials.

Engineering Properties of the Non-Cement Mortar using the Fly ash from Combined Heat Power Plant and Recycled Fine Aggregate (열병합발전소 플라이애시와 순환잔골재를 사용한 무시멘트 모르타르의 공학적 특성)

  • Nam, Han-Kook;Lim, Jeong-Geun;Lee, Sang-Soo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.15 no.6
    • /
    • pp.553-559
    • /
    • 2015
  • In this study, to suggest the application method of recycled fine aggregate, the non-cement mortar was prepared and studied with the binders of blast furnace slag, fly ash, and fly ash from combined heat power plant. As a basic experiment, a series of tests was conducted to determine the potions of the binders and types of activator. When the binder was consisted with 20% of fly ash and 40% of fly ash from combined heat power plant, the highest strength of the mortar was obtained, and as an activator, the combination of sodium hydroxide 2.5%, and calcium hydroxide 7.5% showed the highest strength of the mortar. Therefore, this study focuses on engineering properties of mortar contains fly ash from combined heat power plant and recycled fine aggregate according to replacement ratio of recycled fine aggregate based on the optimum mix from the basic experiment. As a result, the best replacement ratio of recycled fine aggregate is 75%.

Effect of Replacing Fine Aggregate by Cathode-Ray Tube(CRT) Waste Glass on Gamma-ray Shielding Properties of Cement Mortar Specimen (폐 브라운관(CRT) 유리의 잔골재 대체가 모르타르 시험체의 감마선 차폐에 미치는 영향)

  • Choi, Yoon-Suk;Lee, Seon-Min;Kim, Tae-Sang;Kim, Il-Sun;Yang, Eun-Ik
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.7
    • /
    • pp.172-180
    • /
    • 2019
  • In this study, the microstructure and gamma-ray shielding efficiency of CRT glass mortar specimen were evaluated with replacement ratio and material properties. The results show that as the replacement ratio of CRT waste glass increases, the volume of pores with diameters below 50 nm and above 400 nm is increased. Also, the half-value layer of CRT glass mortar decreased with the increasing of linear attenuation coefficient. In addition, compressive and flexural strength were reduced when CRT waste glass was replaced as the fine aggregate, but the mechanical performance of CRT mortar specimen could be obtained by substitution of the mineral admixture.

The Strength and Length Change Properties of Recycled Aggregate Concrete(RAC) by Compressive Strength Levels (압축강도 수준별 순환골재 콘크리트의 강도와 길이변화 특성)

  • Lee, Bong-Chun;Lee, Jun;Cho, Young-Keun;Jung, Sang-Hwa
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.4
    • /
    • pp.307-312
    • /
    • 2015
  • This paper addresses mechanical properties and length change performance of the recycled aggregate concretes(RAC) in which natural coarse was replaced by recycled coarse aggregate(RCA) by compressive strength levels(20, 35, 50 MPa). A total of 9 RAC were produced and classified into three series, each of which included three mixes designed with three compressive strength levels of 20 MPa, 35 MPa and 50 MPa and three RCA replacement ratios of 0, 50 and 100%. Physical/Mechanical properties of RAC were tested for slump test, compressive strength, and length change. The test results indicated that the workability of RC could be improved or same by RCA replacement ratios, when compared with that containing no RCA. This is probably because of the RCA shape improving the workability of RAC. Also, the test results showed that the compressive strength was decreased by 9~10% as the RCA replacement ratios increase. However, the length change ratio by the RCA replacement ratios increased regardless of compressive strength levels. At 20 MPa level, the length change ratio was 8~40% which was much higher than that of 4~17% at both 35 and 50 MPa levels. Therefore, it was considered that such admixture addition preventing dry shrinkage is required in order to improve the properties of the RAC at 20 MPa level.

Mix Design Procedure of Structural Concrete Using Artificial Lightweight Aggregates Produced from Bottom Ash and Dredged Soils (바텀애시 및 준설토 기반의 인공 경량골재를 활용한 구조용 콘크리트의 배합설계 절차)

  • Lee, Kyung-Ho;Yang, Keun-Hyeok
    • Journal of the Korea Institute of Building Construction
    • /
    • v.18 no.2
    • /
    • pp.133-140
    • /
    • 2018
  • The objective of this study is to propose a reliable mixing design procedure of concrete using artificial lightweight aggregate produced from expanded bottom ash and dredged soil. Based on test results obtained from 25 mixes, empirical equations to determine water-to-cement ratio, unit cement content, and replacement level of lightweight fine aggregates were formulated with regard to the targeted performance (compressive strength, dry density, initial slump, and air content) of lightweight aggregate concrete. From the proposed equations and absolute volume mixing concept, unit weight of each ingredient was calculated. The proposed mix design procedure limits the fine aggregate-to-total aggregate ratio by considering the replacement level of lightweight fine aggregates, different to previous approach for expanded fly ash and clay-based lightweight aggregate concrete. Thus, it is expected that the proposed procedure is effectively applied for determining the first trial mixing proportions for the designed requirements of concrete.

An Experimental Study on the Replacement Proportion of Recycled Aggregate Effecting in the Engineering Properties of Recycled Concrete (Part 1, Experimental Program and Fluidity Performance of Fresh Concrete (재생골재콘크리트의 공학적 특성에 미치는 재생골재 혼합조건의 영향에 관한 실험적 연구 (제 1보, 실험계획 및 아직 굳지 않은 유동화 특성을 중심으로 ))

  • 최진성;윤병수;임정수;심진만;남상일;김무한
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1993.04a
    • /
    • pp.16-21
    • /
    • 1993
  • The study of recycled aggregate concrete in which demolition waste is utilized to produce aggregate for new concrete, can contribute to the solution of two problems. The first is the shortage of aggregate from river, and the second is the waste disposal problem. In comparison with natural aggregate concrete, recycled aggregate concrete shows reductions in compressive strength, tensile strength , vending strength, shear strength and increases in drying shrinkage and creep. Recycled aggregate concrete may also be less durable due to increase in porosity and permeability. Therefore, the purpose of this study is to analyze the applicability of recycled concrete in the influence of a substitute ratio of recycled sand gravel.

  • PDF

A Study on the Optimal Concrete Mix-proportion Selection of PHC-pile by Using of Air-cooled Blast Furnace Slag Coarse Aggregate (괴재 고로슬래그 굵은 골재 사용에 따른 PHC-Pile용 콘크리트 최적 배합 도출에 관한 연구)

  • Jeon, In Ki;Lee, Joo Hun;Park, Yong Kyu;Kim, Hyun Woo;Yoon, Ki Won
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2014.05a
    • /
    • pp.270-271
    • /
    • 2014
  • In this study, a replacement ratio of blast furnace slag coarse aggregate and a water binder ratio by an optimum combination of PHC file was investigated. As a results, the target strength 78.5MPa was altogether satisfied in a mix proportion 28-G100-SG0 and W/B ratio 26 %. The surface rupture was generated in 28-G0-SG100 combination after curing with the autoclave. According to the result of measuring the ingredient, the majority were the MgOH2 hydrate.

  • PDF

Bond Behavior of Recycled Coarse Aggregate Concrete Deteriorated by Freezing and Thawing (동결융해를 받은 순환 굵은골재 콘크리트의 부착성능)

  • Choi, Ki-Sun;Lee, Min-Jung;Yun, Hyun-Do;Kang, Ki-Woong;You, Young-Chan;Kim, Keung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.1097-1100
    • /
    • 2008
  • The purpose of this study to investigate the bond strength of recycled coarse aggregate concrete deteriorated by freezing and thawing. Concrete specimens with recycled coarse aggregate representing lower limit of the quality standard (water absorption : 3.0%, specific gravity : $2.5g.cm^3$) were manufactured and tested. The replacement ratio (0, 30, 60 and 100%) of recycled coarse aggregate and freezing-thawing cycles were considered in this test. From the test results, it was found that the bond strength of normal strength concrete is not affected by the replacement ratio of recycled coarse aggregate under freezing and thawing conditions. Also, the bond strength of the natural and recycled coarse aggregate concrete using AE admixtures was not decreased by frost action.

  • PDF

Fresh and hardened properties of rubberized concrete using fine rubber and silpozz

  • Padhi, S.;Panda, K.C.
    • Advances in concrete construction
    • /
    • v.4 no.1
    • /
    • pp.49-69
    • /
    • 2016
  • This work investigates the mechanical properties of conventional concrete (CC) and self compacting concrete (SCC) using fine rubber and silpozz were accompanied by a comparative study between conventional rubberized concrete (CRC) and self compacting rubberized concrete (SCRC). Fine rubber (FR) from scrap tires has replaced the fine aggregate (FA) and Silpozz has been used as a replacement of cement at the proportions of 5, 10 and 15%. Silpozz as a partial replacement of cement in addition of superplasticiser (SP) increases the strength of concrete. Fresh concrete properties such as slump test, compaction factor test for CRC, whereas for SCRC slump flow, $T_{500}$, V-funnel, L-box, U-box, J-ring tests were conducted along with the hardened properties tests like compressive, split tensile and flexural strength test at 7, 28 and 90 days of curing. The durability and microstructural behavior for both CRC and SCRC were investigated. FR used in the present study is 4.75 mm passing with fineness modulus 4.74.M30 grade concrete is used with a mix proportion of 1:1.44:2.91 and w/c ratio as 0.43. The results indicate that as FR quantity increases, workability of both CRC and SCRC decreases. The results also show that the replacement of natural fine aggregate (NFA) with FR particles decreases the compressive strength with the increase of flexural strength observed upto 5% replacement of FR. Also replacement of cement with silpozz resulted enhancement of strength in SCRC.