Precast concrete structure has many advantages, but the assembled seam will affect potentially the overall seismic performance of structure. Based on the sidewall joint located in the bottom of assembled monolithic subway station, the main objectives of this study are, on one hand to present an experimental campaign on the seismic behavior of precast sidewall joint (PWJ) and cast-in-place sidewall joint (CWJ) subjected to low-cycle repeated loading, and on the other hand to explore the effect of shape and position of assembled seam on load carrying capacity and crack width of precast sidewall joint. Two full-scale specimens were designed and tested. The important index of failure pattern, loading carrying capacity, deformation performance and crack width were evaluated and compared. Based on the test results, a series of different height and variably-shape of assembled seam of precast sidewall joint were considered. The test and numerical investigations indicate that, (1) the carrying capacity and deformation capacity of precast sidewall and cast-in-place sidewall were very similar, but the crack failure pattern, bending deformation and shearing deformation in the plastic hinge zone were different obviously; (2) the influence of the assembled seam should be considered when precast underground structures located in the aquifer water-bearing stratum; (3) the optimal assembled seam shape and position can be suggested for the design of precast underground concrete structures according to the analysis results.
신구콘크리트 계면(접합부)의 전단강도 측정을 목적으로 보시험체를 사용한 정하중 및 피로하중의 재하실험이 수행되었다. 총 13개의 시험체중에서 정적재하실험을 통하여 5개 시험체의 전단강도를 측정하였고, 8개의 시험체는 2,000,000회 또는 3,000,000회의 반복하중을 가력한 후 전단강도를 측정하였다. 실험변수는 접합부거칠기, 전단보강철근 및 시구콘크리트간 부착력의 유무이었다. 정적재하실험에서, 접합부가 거칠면서 콘크리트간 부착력이 존재한 시험체의 경우, 평균전단강도는 $61kgf/cm^2$이었다. 유사한 조건의 시험체의 3,000,000회의 전단하중을 가력한 피로하중실험에서 접착부의 열화현상은 나타나지 않았다. 이 때 반복가력된 최대전단응력은 $20kgf/cm^2$으로 전단강도의 약 1/3수준이었다. 접합부가 거칠게 처리되지 않은 시험체와 접합부는 거칠지만 콘크리트간 부착력이 인위적으로 제거된 시험체의 경우에는 전단보강철근을 사용하여도 피로하중에 의한 접합부의 열화현상이 나타났다.
The dynaamic fatigue behavior of alumina ceramics was observed at room temperature using four-point bending method. Dynamic fatigue fracture strength was observed as function of down speed and notch length. The crack growth exponent of the specimens was calculated from the fracture strength and lifetime in dynamic fatigue test. After loading the stresses in the range of 0% to 105% compared with the average in-ert strength the value of residual fracture strength was measured for unnotched and 0.5mm notched speci-mens at the 0.001 and 0.0005 mm/min down speed respectively. After the 95% stress of the average inert strength was applied repeatedly the value of rsidual fracture strength was measured for 0.5mm notched specimens at the 0.001 and 0.0005 mm/min down speed respectively. The material constant A was found to be almost the same and not to depend on the loading mode or the down speed for unnotched and notched specimen. The value of fracture strength with time calculated from the constants n and A was in good agreement with the measured value.
보강토 옹벽은 기존 콘크리트 옹벽에 비하여 많은 장점을 지니고 있으나 장기적으로 지속하중 혹은 반복하중 등에 의한 잔류변형의 우려로 영구 구조물로서의 적극적인 적용에 장애가 되고 있다. 이 문제를 해결하기 위해서는 보강토 구조물의 시간 의존적 잔류변형 메카니즘의 규명과 아울러 잔류변형을 예측하고 제어하는 기술이 확보되어야 한다. 본 연구에서는 이러한 연구의 필요성에 근거하여 보강토 옹벽에 발생할 수 있는 장기변형 특성 고찰에 주안점을 두고 지오그리드와 표준사로 뒤채움된 모형 보강토 옹벽에 대한 지속하중 혹은 반복하중 등 다양한 하중이력에 대한 보강토 구조물의 장기변형 특성 메카니즘을 축소모형실험을 통해 고찰하였다. 그 결과 보강토 옹벽의 시간의존적 변형은 작용하는 하중특성 뿐만 아니라 뒤채움흙 및 보강재의 역학적 특성에도 많은 영향을 받는 것으로 나타났으며, 선행하중을 작용함으로써 시간 의존적 잔류변형을 제어할 수 있는 것으로 파악되었다.
본 연구에서는 두 종류의 전단지간 대 유효깊이의 비(a/d)를 가진 전단에 취약한 보 네 개에 대한 반복하중 실험을 수행하였다. 실험군에는 $6d_b$의 정착 길이의 $90^{\circ}$ 절곡된 갈고리를 가진 두 개의 스터럽을 묶은 하나의 다발 스터럽(bundled stirrups)을 배근하였으며 대조군에는 직경 50mm의 원형 헤드를 가진 헤디드 바를 배근하였다. 하나의 헤디드 바의 철근 직경은 하나의 다발 스터럽의 철근 직경과 같기 때문에 효과적인 실험 비교가 가능하였다. 실험 결과는 헤디드 바를 배근한 보가 일반 스터럽을 가진 보보다 연성, 에너지 흡수량, 최대하중 이후의 거동에 있어서 뛰어난 구조 성능을 보여 주었다. 반복하중에 의한 콘크리트 피복과 부분 압축파괴에 의해 스터럽의 갈고리는 바깥 방향으로의 변형과 함께 정착 성능을 상실하였다. 반면에, 헤디드 바는 헤드의 정착손실 방생 없이 변형률경화 시점을 지나서도 변형이 발생하였으며 압축 철근의 좌굴 발생을 지연하는 데에도 기여하는 것으로 나타났다. 반복하중에 의한 감소된 인장경화를 고려한 하중-변위 예측은 뛰어난 정확도를 보여 주었다.
PURPOSE. The purpose of this study was to compare computer-aided design/computer-aided manufacturing (CAD/CAM) abutment and prefabricated abutment in Morse taper internal connection type implants after cyclic loading. MATERIALS AND METHODS. The study was conducted with internal type implants of two different manufacturers (Group Os, De). Fourteen assemblies were prepared for each manufacturer group and divided into 2 groups (n=7): prefabricated abutments (Os-P, De-P) and CAD/CAM abutments (Os-C, De-C). The amount of axial displacement and the removal torque values (RTVs) were measured before and after cyclic loading (106 cycles, 3 Hz with 150 N), and the tensile removal force to dislodge the abutments was measured after cyclic loading. A repeated measures ANOVA and a pattern analysis based on the logarithmic regression model were conducted to evaluate the effect of cyclic loading on the axial displacement. The Wilcoxon signed-rank test and the Mann-Whitney test was conducted for comparison of RTV reduction% and tensile removal forces. RESULTS. There was no significant difference between CAD/CAM abutments and prefabricated abutments in axial displacement and tensile removal force; however, significantly greater RTV reduction% after cyclic loading was observed in CAD/CAM abutments. The correlation among the axial displacement, the RTV, and the tensile removal force was not significant. CONCLUSION. The use of CAD/CAM abutment did not significantly affect the amount of axial displacement and tensile removal force, but presented a significantly greater removal torque reduction% than prefabricated abutments. The connection stability due to the friction at the abutment-implant interface of CAD/CAM abutments may not be different from prefabricated abutment.
Recently, a theoretically-sound design approach, using an elastic multilayer model, is attempted in trackbed designs for the construction of high speed railways and new lines of conventional railways. In the elastic multilayer model, the stress-dependent resilient modulus($E_R$) is an important input parameter, that is, reflects substructure performance under repeated traffic loading. However, the evaluation method for resilient modulus using repeated loading triaxial test is not fully developed for practical purpose, because of costly equipment and the significantly fluctuated values depending on the testing equipment and laboratory personnel. In this study, the paper will present an indirect method to estimate the resilient modulus using dynamic properties. The resilient modulus of crushed stone, which is the typical material of sub-ballast, was calculated with the measured dynamic properties and the range of stress level of the sub-ballast, and approximated with the power model combined with bulk and deviatoric stresses. The resilient modulus of coarse grained material decreases with increasing deviatoric stress at a confining pressure, and increases with increasing bulk stress. Sandy soil(SM classified from Unified Soil Classification System) of subgrade was also evaluated and best fitted with the power model of deviatoric stress only.
반복회수에 대한 하중-변형률 선도로부터 구산 잔류변형률의 비교 결과에서 피로하중하의 GFRP관의 강성은 GFRP관의 유리섬유의 적층수가 클수록 크게 나타났으며, 이러한 현상은 피로파괴 직전까지 나타났다. 아울러 본 피로실험 결과를 회귀분석하여 구한 S-N선도에 의하면 정적극한강도 백분율에 대한 피로강도는 GFRP관의 유리섬유 적층수가 증가할수록 증가하였으며, 유리섬유의 적층수가 15, 25, 35층인 GFRP관의 반복회수 200만회에 대한 피로강도는 정적극한강도는 각각 약 75.2%, 79.5%, 84.2%로 나타났다.
반복적인 교통하중은 아스팔트 포장에 손상을 누적시키는 반면, 휴식기 동안 아스팔트 혼합물에는 축적된 손상의 회복현상이 지속적으로 일어난다. 이러한 손상회복 현상은 아스팔트 포장의 피로수명을 증가시킨다. 본 연구에서는 간접인장시험을 이용하여 아스팔트 혼합물의 손상회복특성을 측정할 수 있는 시험방법을 개발하고, 이를 통해 일단 아스팔트와 개질 아스팔트를 포함하는 총 네 가지 아스팔트 혼합물의 손상회복특성을 평가하였다. 본 연구에서 개발한 손상회복시험은 반복재하시험과 일련의 $M_R$시험으로 구성된다. 반복재하시험과 $M_R$ 시험 동안 회복변형 (resilient deformation)을 측정하고 응력과 변형률을 이용하여 DCSE (Dissipated Creep Strain Energy)를 구하고 이를 통해 아스팔트 혼합물의 손상회복특성을 평가할 수 있는 파라메터로서 $DCSE/DCSE_{applied}$를 이용한 정규화된 손상회복속도 (normalized healing rate)를 제안하였다. 실험결과, 아스팔트 혼합물의 손상회복속도는 온도가 증가함에 따라 지수 함수적으로 증가함을 알 수 있었으며, 아스팔트 혼합물의 손상회복특성은 폴리머 개질과 같은 아스팔트 바인더의 특성보다는 아스팔트 함량과 같은 혼합물의 구조적인 특성에 더 많은 영향을 받음을 알 수 있었다.
포장 공용성 모델은 역학적-경험적 포장설계법에서 포장의 수명을 결정하기 위한 가장 중요한 인자이다. 한국 포장연구 프로그램의 일환으로 한국형 포장설계법이 역학적-경험적 방법에 근거하여 현재 개발중에 있다. 본 연구에서는 포장 공용성모델중 아스팔트 혼합물의 영구변형 예측모델을 삼축압축 반복재하시험을 이용하여 개발하였다. 본 시험은 다양한 아스팔트 혼합물에 대하여 온도와 공극률을 변화시켜 하중재하 횟수에 따른 혼합물의 영구변형 특성을 조사하였으며, 본 시험결과를 이용하여 예측모델의 계수값을 결정하였다. 영구변형 예측모델의 계수값은 포장가속시험결과를 토대로 다양한 혼합물에 대한 시험결과를 이용하여 깊이에 따른 전단응력의 변화를 고려한 통합적인 소성변형 모델계수값을 정하는 것보다 혼합물의 종류에 따른 모델계수를 산정하는 것이 보다 정확한 결과를 예측할 것으로 판단된다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.