• Title/Summary/Keyword: Reaction layer

Search Result 1,560, Processing Time 0.03 seconds

Non-Destructive Scientific Analysis of the Gold Fabric Excavated of Cheongsong Shim's Grave (청송심씨 묘에서 출토된 금직물의 비파괴 과학적 분석)

  • Lee, Hwang-Jo;Wi, Koang-Chul
    • Journal of Conservation Science
    • /
    • v.38 no.3
    • /
    • pp.243-253
    • /
    • 2022
  • Using non-destructive analytical methods, we identified the material characteristics of two gold fabric artifacts excavated from the Cheongsong Sim clan (Bugeum Wonsam, Jikgeum Chima), including the artifact condition, fiber type, surface contamination, and metallic threads. We found that the artifacts were buried and had turned brown; thus, we were unable to determine their original color. The fiber type was determined to be silk from cocoons, based on scanning electron microscopy, Fourier transform infrared (FT-IR) analyses of Amide I, II, III, and IV peaks, and color reactions Further, the FT-IR and X-ray fluorescence (XRF) analyses identified the white and black stains as natural resin hydrolyzed substances, such as lipids and proteins, that occurred as microbial decomposition due to body decay. Finally, the XRF analyses identified the thin gold layer of the metallic yarn as gold (Au). According to the FT-IR data and the color reaction to the metallic yarn medium, the adhesive component of the medium was a product of-Amides I, II, III, and 3000 cm-1 within Amides A and B (an animal type), respectively. Thus, the medium was identified as Hanji (Korean paper), which is made from domestically produced Broussonetia kazinoki fibers.

Development of surface functional coating thin film utilizing combined processes of plasma activation surface treatment and nanoclay dispersion: In applications for transparent water vapor and oxygen barrier packaging films (플라즈마 활성화 표면처리 공정과 나노클레이 분산 적층 코팅을 이용한 표면 기능성 코팅 박막 개발: 수분 및 산소 차단성이 우수한 투명 포장재)

  • Nam Il Kim;Geug Tae Kim
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.33 no.3
    • /
    • pp.97-103
    • /
    • 2023
  • Barrier films for transparent packaging materials with excellent moisture barrier properties are prepared, utilizing a nanoclay dispersion coating layer formed after a pretreatment process of plasma activation surface treatment process under vacuum at room temperature. Attention is paid on optimizing the coupling additive through the appropriate crosslinking process and optimal dispersion process of the coating process to enhance adhesion. Analysis of the functional coating thin film shows that the water vapor transmission rate is less than 10 g/m2/24 hrs (ASTM F-1249) and the oxygen transmission rate is less than 30 cc/m2/24 hrs (ASTM D3985). It is shown that water barrier properties of coating thin film prepared in this study are greater than conventional untreated films by 10 times or more. The thickness of the transparent gas barrier film is within 0.1 mm, and the transparent gas barrier complex is implemented in two layers. In the study of PET thin film interface characteristics, FT-IR experimental analysis shows the reaction activity was optimized at RDS 1.125 %.

Strength Development Characteristics of Clay Stabilized with Electric Furnace Steel Slag (전기로 제강슬래그로 안정화된 연약점토의 강도 발현 특성)

  • Hyeongjoo Kim;Taegew Ham;Taewoong Park;Taeeon Kim
    • Journal of the Korean GEO-environmental Society
    • /
    • v.25 no.5
    • /
    • pp.29-37
    • /
    • 2024
  • This study aimed to investigate the changes in chemical components that occur when weak clay is mixed with steel slag modified with calcium oxide, and to understand the expression characteristics of compressive strength according to hydrophilicity and curing time. XRF testing, SEM imaging, vane shear strength and uniaxial compressive strength testing were conducted. Calcium (Ca) released from the steel slag increases the Ca content in clay by increasing the number of crystal particles and forming a coating layer known as calcium silicate hydrate (CaO-SiO2-H2O) through chemical reactions with SiO2 and Al2O3 components. The weak clay stabilized with steel slag is classified into an initial inactive zone where strength relatively does not increase and an activation zone where strength increases over curing time. The vane shear strength of the initial inactive area was found to be 4.4 to 18.4 kN/m2 in the state of the weight mixing ratio Rss 30% (steel slag 30% + clay 70%). In the case of the active area, the maximum uniaxial compressive strength increased to 431.8 kN/m2 after 480 hours of curing time, which increased due to the apparent adhesion strength of clay through pozzolanic reaction. Therefore, considering the strength expression characteristics of stabilized mixed clay based on the mixing ratio (Rss) during the recycling of steel slag can enhance its practicality in civil engineering sites.

Surface Analysis Study on ZIRLO Cladding Hulls Oxidized at Low Temperatures (저온 산화된 ZIRLO 피복관의 표면분석 연구)

  • Jeon, Min Ku;Choi, Yong Taek;Lee, Chang Hwa;Kang, Kweon Ho;Park, Geun Il
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.12 no.3
    • /
    • pp.235-243
    • /
    • 2014
  • Surface oxidation behavior of ZIRLO (ZIRconium Low Oxidation) hulls was investigated using an X-ray photoelectron spectroscopy (XPS) technique. The effects of oxidation time (10-336 h at $500^{\circ}C$) and temperature ($400-700^{\circ}C$ for 10 h) were studied. Deconvolution results of the hulls oxidized at $500^{\circ}C$ revealed that a $ZrO_2$ phase appeared after 24 h (11.86%), and an increase in the $ZrO_2$ ratio was observed when the hulls were oxidized for 336 h (17.93%). On the other hand, the ZrO phase which employed 5.68% in the 10 h oxidized sample disappeared when the oxidation time increased to 24 h. The XPS results also showed that an increase in the oxidation temperature resulted in an increase in the ratio of ZrO, which increased from 0 to 5.68, 8.31, and 9.16% when the oxidation temperature increased from 400 to 500, 600, and $700^{\circ}C$, respectively. $ZrO_2$ phase was observed only in the sample that was oxidized at $700^{\circ}C$. The mechanism of ZrO formation was not conclusive, but it was suggested that a formation of hydroxide might have been accelerated at elevated temperatures leading to a formation of a $Zr(OH)_4$ phase. The relationship between the surface oxidation status of the hulls oxidized at $500^{\circ}C$ and their chlorination reaction feasibility was discussed, and it was suggested that the thickness of the oxide layer is an important parameter that determines the chlorination reaction feasibility.

Upregulation of Connexin43 Expression in Mitral Valves in a Rabbit Model of Hypercholesterolemia (고콜레스테롤혈증을 유발한 토끼의 승모판막에서 Connexin43 발현의 증가)

  • Kwon, Jong-Bum;Park, Chan-Beom;Sa, Young-Jo;Kim, Young-Du;Moon, Seok-Whan;Kim, Chi-Kyung
    • Journal of Chest Surgery
    • /
    • v.43 no.4
    • /
    • pp.356-363
    • /
    • 2010
  • Background: Connexin 43-mediated gap junctional communication plays an important role in atherosclerosis. Numerous studies have demonstrated a correlation between mitral valve annular calcification and atherosclerotic disease. However, the relevance of connexin 43 to mitral valve disease remains unclear. We hypothesized that the mechanism contributing to mitral valve disease is associated with alterations in cell-to-cell communication mediated by changes in Connexin 43 expression. Material and Method: Twenty male New Zealand rabbits were divided into two groups: animals in group 1 (n=10) were fed a normal chow diet, whilst those in group 2 (n=10) received a diet containing 1% cholesterol for 12 weeks. After sacrificing the animals, the mitral valves were excised and analyzed with immunohistochemical staining and Real-time Reverse Transcriptase polymerase chain reaction (real time RT-PCR). Result: Myofibroblasts and macrophages were found concentrated within the endothelial layer on the ventricular side of the leaflet in the cholesterol diet group. Immunohistochemial staining showed elevated expression of connexin43 in the cholesterol diet group. Real-time RT-PCR revealed increased connexin43 mRNA levels in mitral valves from hypercholesterolemic animals. Conclusion: Our finding that connexin43 expression is increased in mitral valves of hypercholesterolemic rabbits suggests that alterations in cell-to-cell communication via connexin43 containing gap junctions play a role in the development of mitral valve disease in hypercholesterolemia.

Characterization of SEI layer for Surface Modified Cathode of Lithium Secondary Battery Depending on Electrolyte Additives (전해질 첨가제에 따른 graphite 음극의 SEI분석 및 전기 화학적 특성 고찰)

  • Lee, Sung Jin;Cha, Eun Hee;Lim, Soo A
    • Journal of the Korean Electrochemical Society
    • /
    • v.19 no.3
    • /
    • pp.69-79
    • /
    • 2016
  • Lithium ion battery with high energy density is expanding its application area to electric automobile and electricity storage field beyond existing portable electric devices. Such expansion of an application field is demanding higher characteristic and stable long life characteristic of an anode material, the natural graphite that became commercialized in lithium ion battery. This thesis produced cathode by using natural graphite anode material, analyzed creation of the cathode SEI film created due to initial reaction by using electrolyte additives, VC (vinylene carbonate), VEC (vinyl ethylene carbonate), and FEC (fluoroethylene carbonate), and considered correlation with the accompanying electrochemical transformation. This study compared and analyzed the SEI film variation of natural graphite cathode according to the electrolyte additive with SEI that is formed at the time of initial filling and cathode of $60^{\circ}C$ life characteristic. At the time of initial filling, the profile showed changes due to the SEI formation, and SEI was formed in No-Additive in approximately 0.9 V through EVS, but for VC, VEC, and FEC, the formation reaction was created above 1 V. In $60^{\circ}C$ lifespan characteristic evaluation, the initial efficiency was highest in No-Additive and showed high contents percentage, but when cycle was progressed, the capacity maintenance rate decreased more than VC and FEC as the capacity and efficiency at the time of filling decreased, and VEC showed lowest performance in efficiency and capacity maintenance rate. Changes of SEI could not be verified through SEM, but it was identified that as the cycle of SEI ingredients was progressed through FT-IR, ingredients of Alkyl carbonate ($RCO_2Li$) affiliation of the $2850-2900cm^{-1}$ was maintained more solidly and the resistance increased as cycle was progressed through EIS, and specially, it was identified that the resistance due to No-Additive and SEI of VEC became very significant. Continuous loss of additives was verified through GC-MS, and the loss of additives from partial decomposition and remodeling of SEI formed the non-uniform surface of SEI and is judged to be the increase of resistance.

Electrochemical properties of $Gd_{0.8}Ca_{0.2}Co_{1-x}Fe_xO_3$ cathodes for medium-temperature SOFC (중간온도형 고체산화물 연료전지의 양극재료로서 $Gd_{0.8}Ca_{0.2}Co_{1-x}Fe_xO_3$의 전기화학특성)

  • Ryu Ji-H.;Jang Jong-H.;Lee Hee-Y.;Oh Seung-M.
    • Journal of the Korean Electrochemical Society
    • /
    • v.1 no.1
    • /
    • pp.1-7
    • /
    • 1998
  • For the purpose of finding new cathode materials for medium-temperature $(700\~800^{\circ}C)$ solid oxide fuel cells, $Gd_{0.8}Ca_{0.2}Co_{1-x}Fe_xO_3,\;(x=0.0\~0.5)$ are prepared, and their thermal stability and conductivity characteristics are investigated. Also, the cathodic activities are measured after the cathode layer being attached on CGO (cerium-gadolinium oxide) electrolyte disk. The X-ray analyses indicate that the materials prepared by calcining the citrate-gels at $800^{\circ}C$ have the orthorhombic perovskite structure without discernible impurities. The thermal stability of the undoped Co perovskite is so poor that it is decomposed to the individual binary oxide even at $1300^{\circ}C$. But the partially Fe-doped cobaltates exhibit a better thermal stability to retain their structural integrity up to $1400^{\circ}C$. The observation whereby both the undoped and Fe-doped cobaltates melt at ca. $1300^{\circ}C$ leads us to perform the electrode adhesion at <$1300^{\circ}C$. The cathodic activity of $Gd_{0.8}Ca_{0.2}Co_{1-x}Fe_xO_3,\;(x=0.0\~0.5)$, electrodes is superior to $La_{0.9}Sr_{0.1}MnO_3$, among the samples of $x=0.0\~0.5$, the x=0.2 cathode shows the best activity for the oxygen reduction reaction. It is likely that the Fe-doping provides a better thermal stability to the materials but in turn imparts an inferior cathodic activity, such that the optimum trade-off is made at x=0.2 between the two factors. The total electrical conductivity and ion conductivity of $Gd_{0.8}Ca_{0.2}Co_{1-x}Fe_xO_3$, are measured to be 51 S/cm and $6.0\times10^{-4}S/cm\;at\;800^{\circ}C$, respectively. The conductivity values illustrate that the materials are a mixed conductor and the reaction sites can be expanded to the overall electrode surface, thereby providing a better cathodic activity than $La_{0.9}Sr_{0.1}MnO_3$.

Comparative Study of Interfacial Reaction and Drop Reliability of the Sn-3.0Ag-0.5Cu Solder Joints on Electroless Nickel Autocatalytic Gold (ENAG) (Electroless Nickel Autocatalytic Gold (ENAG) 표면처리와 Sn-Ag-Cu솔더 간 접합부의 계면반응 및 취성파괴 신뢰성 비교 연구)

  • Jun, So-Yeon;Kwon, Sang-Hyun;Lee, Tae-Young;Han, Deog-Gon;Kim, Min-Su;Bang, Jung-Hwan;Yoo, Sehoon
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.29 no.3
    • /
    • pp.63-71
    • /
    • 2022
  • In this study, the interfacial reaction and drop impact reliability of Sn-Ag-Cu (SAC) solder and electroless nickel autocatalytic gold (ENAG) were studied. In addition, the solder joint properties with the ENAG surface finish was compared with electroless nickel immersion gold (ENIG) and electroless nickel electroless palladium immersion gold (ENEPIG). The IMC thickness of SAC/ENAG and SAC/ENEPIG were 1.15 and 1.12 ㎛, respectively, which were similar each other. The IMC thickness of the SAC/ENIG was 2.99 ㎛, which was about two times higher than that of SAC/ENAG. Moreover, it was found that the IMC thickness of the solder joint was affected by the metal turnover (MTO) condition of the electroless Ni(P) plating solution, and it was found that the IMC thickness increased when the MTO increased from 0 to 3. The shear strength of SAC/ENEPIG was the highest, followed by SAC/ENAG and SAC/ENIG. It was found that when the MTO increased, the shear strength was lowered. In terms of brittle fracture, SAC/ENEPIG was the lowest among the three joints, followed by SAC/ENAG and SAC/ENIG. Likewise, it was found that as MTO increased, brittle fracture increased. In the drop impact test, it was confirmed that the 0 MTO condition had a higher average number of failures than the 3 MTO condition, and the average number of failures was also higher in the order of SAC/ENEIG, SAC/ENAG, and SAC/ENIG. As a result of observing the fracture surface after the drop impact, it was found that the fracture was between the IMC and the Ni(P) layer.

Immunohistochemical Localization and the Characteristics of Antigenic Compnent Inducing IgE and IgG Antibodies in Spirometra erinacei (Spirometra erinacei에서 IgE와 IgG 항체를 유도하는 항원성분의 면역조직화학적 위치와 특성)

  • Chang-Hwan Kim;Sook-Jae Seo;Hong-Ja Kim;Kee-Hoon Kwak
    • Biomedical Science Letters
    • /
    • v.2 no.1
    • /
    • pp.1-12
    • /
    • 1996
  • Antigenic components reacting with IgE and IgG antibodies were localized in muscular layer of adult and of larva, sparganum. But the antigenic components inducing IgG were localized at tegument and parenchyma in addition to muscular layer in adult and sparganum. Also in sparganum, the surface of calcareous corpuscles of parenchyma showed immunoreactivity to IgG antibody. However antigenic components inducing IgE antibody were not localized in tegument and parenchyma, but in adult worm, we observed the immunopositive reaction at the lining of vitelline follicles in mature proglottis and on surface of egg shell within uterus of graved proglottis. By the method of immunogold-labelling, we observed the location of antigenic particles in tegument of sparganum. The density of antigenic particles inducing IgG was higher than that of antigen particles inducing IgE in syncytial tegument, tegument cells. A total of 43 and 36 protein bands were resolved from crude extracts of adult and sparganum, respectively, by SDS-PAGE. 34 bands from crude extracts of adult and larva were migrated to same positions. By EITB, 21 bands of 44 bands in adult were recognized with IgG antibody, and also 21 bands of 36 bands in sparganum. 13 bands of them were common antigenic components both in the adult worm and sparganum. Because 19 bands of 44 bands in adult worm were reacted with IgE antibody, they were IgE antigenic component. In sparganum, 13 bands were IgE antigenic components. 9 bands of them were common antigenic component inducing IgE antibody in both a-dult and sparganum. 3 bands of antigenic component recognized by IgE and IgG antibody were nonspecific antigen in both adult and sparganum of Spirometra erinacei.

  • PDF

Research of Diffusion Bonding of Tungsten/Copper and Their Properties under High Heat Flux

  • Li, Jun;Yang, Jianfeng
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.05a
    • /
    • pp.14-14
    • /
    • 2011
  • W (tungsten)-alloys will be the most promising plasma facing armor materials in highly loaded plasma interactive components of the next step fusion reactors due to its high melting point, high sputtering resistance and low deuterium/tritium retention. The bonding technology of tungsten to Cu alloy was one of the key issues. In this paper, W/CuCrZr diffusion bonding has been performed successfully by inserting pure metal interlay. The joint microstructure, interfacial elements migration and phase composition were analyzed by SEM, EDS, XRD, and the joint shear strength and micro-hardness were investigated. The mock-ups were fabricated successfully with diffusion bonding and the cladding technology respectively, and the high heat flux test and thermal fatigue test were carried out under actively cooling condition. When Ni foil was used for the bonding of tungsten to CuCrZr, two reaction layers, Ni4W and Ni(W) layer, appeared between the tungsten and Ni interlayer with the optimized condition. Even though Ni4W is hard and brittle, and the strength of the joint was oppositely increased (217 MPa) due primarily to extremely small thicknesses (2~3 ${\mu}m$). When Ti foil was selected as the interlayer, the Ti foil diffused quickly with Cu and was transformed into liquid phase at $1,000^{\circ}C$. Almost all of the liquid was extruded out of the interface zone under bonding pressure, and an extremely thin residual layer (1~2 ${\mu}m$) of the liquid phase was retained between the tungsten and CuCrZr, which shear strength exceeded 160 MPa. When Ni/Ti/Ni multiple interlayers were used for bonding of tungsten to CuCrZr, a large number of intermetallic compound ($Ni_4W/NiTi_2/NiTi/Ni_3T$) were formed for the interdiffusion among W, Ni and Ti. Therefore, the shear strength of the joint was low and just about 85 MPa. The residual stresses in the clad samples with flat, arc, rectangle and trapezoid interface were estimated by Finite Element Analysis. The simulation results show that the flat clad sample was subjected maximum residual stress at the edge of the interface, which could be cracked at the edge and propagated along the interface. As for the rectangle and trapezoid interface, the residual stresses of the interface were lower than that of the flat interface, and the interface of the arc clad sample have lowest residual stress and all of the residual stress with arc interface were divided into different grooved zones, so the probabilities of cracking and propagation were lower than other interfaces. The residual stresses of the mock-ups under high heat flux of 10 $MW/m^2$ were estimated by Finite Element Analysis. The tungsten of the flat interfaces was subjected to tensile stresses (positive $S_x$), and the CuCrZr was subjected to compressive stresses (negative $S_x$). If the interface have a little microcrack, the tungsten of joint was more liable to propagate than the CuCrZr due to the brittle of the tungsten. However, when the flat interface was substituted by arc interfaces, the periodical residual stresses in the joining region were either released or formed a stress field prohibiting the growth or nucleation of the interfacial cracks. Thermal fatigue tests were performed on the mock-ups of flat and arc interface under the heat flux of 10 $MW/m^2$ with the cooling water velocity of 10 m/s. After thermal cycle experiments, a large number of microcracks appeared at the tungsten substrate due to large radial tensile stress on the flat mock-up. The defects would largely affect the heat transfer capability and the structure reliability of the mock-up. As for the arc mock-up, even though some microcracks were found at the interface of the regions, all microcracks with arc interface were divided into different arc-grooved zones, so the propagation of microcracks is difficult.

  • PDF