  • As high temperature superconductor applications became a reality due to increase in coated conductor performance, it is important to understand their stability behavior to design safe electrical power systems. Coated conductors can be stabilized with different metals and alloys for different types of application, to yield excellent electrical, thermal and mechanical performance. We have experimentally studied the dependence of quench and recovery characteristics of stainless steel stabilized coated conductors on the amplitude of current and duration time. Stability test of 3cm long sample were performed in a liquid nitrogen bath cooling condition by applying a short period over current pulses for 50 and 100ms, with amplitude up to ~6 times the critical current. The transport current that flows before and after the current pulse was fixed at about ~80-85% critical current. We analyzed the quench and recovery phenomena of the test sample using the current voltage characteristic.

Stability characteristics of DyBCO coated conductor stabilized with stainless steel

  • Dixit, Manglesh;Kim, Tae-Hyung;Oh, Sang-Soo;Song, Kyu-Jeong;Kim, Ho-Min;Park, Kwon-Bae
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.288-289
    • /
    • 2005
  • As high temperature superconductor applications became a reality due to increase in coated conductor performance, it is important to understand their stability behavior to design safe electrical power systems. We have experimentally studied the dependence of quench and recovery characteristics of coated conductors on the amplitude of current and duration time. The sample used in the present study is stabilized with stainless steel. Stability tests of 3 cm long sample were performed in a liquid nitrogen bath cooling condition by applying a short period over current pulses for 50 and 100 ms, with amplitude up to ~ 6 times of the critical current. The transport current that follows before and after the current pulse was fixed about ~85% the critical current. We analyzed the quench recovery using the current voltage characteristic.

  • PDF

초전도 병렬 무유도권선의 온도 해석 (The Analysis of Temperature on Superconducting Parallel Bifilar Winding)

  • 오윤상;이상진;배준한;고태국
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1995년도 하계학술대회 논문집 A
    • /
    • pp.134-136
    • /
    • 1995
  • A superconducting parallel bifilar winding shows the phenomenon which is known as 'fast quench'. We analyzed the temperature characteristics on the winding by computer simulation, and confirmed theses by experiment. The temperature of the quenched point rose gradually as the source voltage was increased. The temperature changed radically as first, but had a gentle slope after a few milliseconds. As the source voltage was large, the initial quenched length also increased. The points in this quenched length showed almost the same temperature. but the points where initial quench had not occurred showed radical temperature gradient. We could observe that the temperature of the whole wire increased simultaneously as the fast quench occurred on the superconducting parallel bifilar winding, because a number of quenched points in that wire appeared at the same time.

  • PDF

초전도 퓨즈의 전압별 특성 (Characteristics of a superconductive fuse according to applied voltages)

  • 최효상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 춘계학술대회 논문집 방전 플라즈마 유기절연재료 초전도 자성체연구회
    • /
    • pp.169-172
    • /
    • 2004
  • We present the basic properties of a superconducting current limiting fuse (SCLF) based on YBCO/Au films. The SCLFs consists of YBCO stripes covered with Au layers for current shunt. Under the source voltage of 100 $V_{rms}$, the longer the duration time of fault current was, the shorter its discharge time was. The duration time of fault current and its discharge time were reduced by increased voltages in the range of 200 - 300 $V_{rms}$. We thought that this was because the quench propagation was limited by local melting generated with higher voltage.

  • PDF

코일 형태로 제작한 박막형 고온초전도 전류제한기의 특성 해석 (Characteristics of a Coil type Fault Curent Limiters using a High-Tc Superconducting Thin Film)

  • 정동철;최효상;박종광;임성훈;고건문;한병성
    • 대한전기학회논문지:전력기술부문A
    • /
    • 제49권8호
    • /
    • pp.418-423
    • /
    • 2000
  • In this paper, we reported the current limiting properties of superconducting fault current limiters (SFCL). Our SFCL was patterned in a coil-type on a YBCO film deposited using rf sputtering techniques and was coated with a gold shunt layer in order to disperse the heat generated at hot spots in the YBCO film. Current increased up to 13.5 Apeak at 60 Hz for the voltage of 11.5 Vpeak, which is the minimum quench point, and increased up to 17.6 Apeak at 60 Hz for the voltage of 80 Vpeak. The quench completion time was 5 msec at 11.5 Vpeak and 4 msec at 80 Vpeak respectively. We think that this architecture using coil-type SFCL can be useful for the protection of the power delivery systems from fault currents.

  • PDF

Simultaneous Quench Characteristic of Resistive Superconducting Fault Current Limiting Modules by using BSCCO Tape

  • Yang Seong-Eun;Ahn Min-Cheol;Park Dong-Keun;Youn Il-Goo;Jang Dae-Hee;Ko Tae-Kuk
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제8권2호
    • /
    • pp.43-45
    • /
    • 2006
  • Recently, the resistive Fault Current Limiter (SFCL) made with Coated Conductor (CC) has been researched with an advanced capability in CC. Current limiting elements must be connected in series in order to fabricate the resistive SFCL having large capacity. By the way, unless the applied voltage in the SFCL is distributed to the elements when the fault occurred, those elements will be critically damaged. Thus simultaneous quench of the elements is an important factor to design the resistive SFCL. In this paper, simultaneous quench characteristics of current limiting module by using BSCCO 2223 were researched before manufacturing the resistive SFCL by using CC. At the first fault stage, the elements generated the resistance at the same time. However, the unequal voltage is applied to the each element in process of time. The method is suggested to solve the problem of the unequal distribution. These experimental results will play an important part in developing for the resistive SFCL by using CC.

Current and voltage loading tests off resistive SFCL

  • 최효상;현옥배;김혜림;황시돌;박권배
    • Progress in Superconductivity
    • /
    • 제3권2호
    • /
    • pp.241-246
    • /
    • 2002
  • We have performed the current and voltage loading tests of resistive superconducting fault current limiters (SFCLS) based on $YBa_2$$Cu_3$$O_{7}$(YBCO) films with the diameter of 2 inch. The SFCL consists of meander-type YBCO stripes covered with 200 nm Au layer grown in situ for current shunt and heat dispersion at hot spots. The minimum quench current of an SFCL unit was about 25 Apeak. Seven SFCL units were connected in parallel fur the current load ing tests at power source of 100 $V_{rms}$ $/2,000A_{rms}$. This SFCL units had maximum limiting current of 170 Apeak during the fault instant and then successfully controlled the fault current below 100 Apeak within 1~2 msec after short circuit. Increased short current also reduced the quench completion time with little change of current limiting characterization. We connected six SFCL units in series fur the voltage loading tests at power source of $1,200 V_{rms}$/170 $A_{rms}$ at this time. The shunt resistors were inserted into each SFCL unit to eliminate power imbalance originated from serial connection of SFCL units. Each SFCL unit was quenched simultaneously during the fault condition. The current increased up to 40 $A_{peak}$ and decreased to 14 $A_{peak}$ after 3 cycles. Quench was completed within 1 msec after the fault. We confirmed operating characteristics of 140 kVA($120 A_{rms}$ $\times$ 1,200 $V_{rms}$) SFCL and presented the manufacturing possibility of 3.3 kV SFCL using 4 inch YBCO films.BCO films.lms.

  • PDF

Current limiting characteristics of transformer type SFCL with coupled secondary windings according to its winding direction

  • Han, Tae Hee;Lim, Sung Hun
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제19권2호
    • /
    • pp.44-47
    • /
    • 2017
  • In this paper, the current limiting characteristics of the transformer type superconducting fault current limiter (SFCL) with the two coupled secondary windings due to its winding direction were analyzed. To analyze the dependence of transient fault current limiting characteristics on the winding direction of the additional secondary winding, the fault current limiting tests of the SFCL with an additional secondary winding, wound as subtractive polarity winding and additive polarity winding, were carried out. The time interval of quench occurrence between two superconducting elements comprising the transformer type SFCL with the additional secondary winding was confirmed to be affected by the winding direction of the additional secondary winding. In case of the subtractive polarity winding of the additional secondary winding, the time interval of the quench occurrence in two superconducting elements was shorter than the case of the additive polarity winding.

THERMALLY INDUCED PHASE SEPARATION IN TERNARY POLYMER SOLUTION

  • Jung, Bum-Suk;Kang, Yong-Soo;Jones, Richard-A.L.
    • 한국막학회:학술대회논문집
    • /
    • 한국막학회 1999년도 The 7th Summer Workshop of the Membrane Society of Korea
    • /
    • pp.79-82
    • /
    • 1999
  • Using Small Angle Light Scattering (SALS), the effect of quench depth on the kinetics of phase separation for ternary solution blends was investigated. The system was composed of two polymers (polystyrene and polybutadiene) and a solvent (toluene). The analyses of the early stage of phase separation were based of the Cahn-Hilliard theory [1,5]. Apparent diffusion coefficients and the fastest mode of fluctuations were evaluated, when quench depth of the system were varied near the critical composition of polymer. In the late stage of phase separation, the domain growth showed a power law with the 1/3 exponent, i.e. $q_m(t)~t^{-1/3}$. For comparison between real images and scattering profiles with time, the image of phase domains with time were obtained by using Laser Confocal Scanning Microscopy (LSCM).

  • PDF

Investigation of a best oxidation model and thermal margin analysis at high temperature under design extension conditions using SPACE

  • Lee, Dongkyu;No, Hee Cheon;Kim, Bokyung
    • Nuclear Engineering and Technology
    • /
    • 제52권4호
    • /
    • pp.742-754
    • /
    • 2020
  • Zircaloy cladding oxidation is an important phenomenon for both design basis accident and severe accidents, because it results in cladding embrittlement and rapid fuel temperature escalation. For this reason during the last decade, many experts have been conducting experiments to identify the oxidation phenomena that occur under design basis accidents and to develop mathematical analysis models. However, since the study of design extension conditions (DEC) is relatively insufficient, it is essential to develop and validate a physical and mathematical model simulating the oxidation of the cladding material at high temperatures. In this study, the QUENCH-05 and -06 experiments were utilized to develop the best-fitted oxidation model and to validate the SPACE code modified with it under the design extension condition. It is found out that the cladding temperature and oxidation thickness predicted by the Cathcart-Pawel oxidation model at low temperature (T < 1853 K) and Urbanic-Heidrick at high temperature (T > 1853 K) were in excellent agreement with the data of the QUENCH experiments. For 'LOCA without SI' (Safety Injection) accidents, which should be considered in design extension conditions, it has been performed the evaluation of the operator action time to prevent core melting for the APR1400 plant using the modified SPACE. For the 'LBLOCA without SI' and 'SBLOCA without SI' accidents, it has been performed that sensitivity analysis for the operator action time in terms of the number of SIT (Safety Injection Tank), the recovery number of the SIP (Safety Injection Pump), and the break sizes for the SBLOCA. Also, with the extended acceptance criteria, it has been evaluated the available operator action time margin and the power margin. It is confirmed that the power can be enabled to uprate about 12% through best-estimate calculations.