비휘발성 메모리 소자응용을 위한 과잉 Bi 첨가에 따른 BLT 박막의 강유전 특성 (Ferroelectric Properties of Bi3.25La0.75 Ti3O12 Thin Films with Excess Bi Contents for Non-Volatile Memory Device Application)

  • 김경태;김창일;강동희;심일운
    • 한국전기전자재료학회논문지
    • /
    • 제15권9호
    • /
    • pp.764-769
    • /
    • 2002
  • The effect of excess Bi contents on the ferroelectric properties of B $i_{3.25}$ L $a_{0.75}$ $Ti_3$ $O_{12}$ (BLT) thin films has been investigated. Bismuth lanthanum titanate thin films with excess Bi contents were prepared onto Pt/Ti/ $SiO_2$/Si substrate by metalorganic decomposition (MOD) technique. The structure and morphology of the films were analyzed using X-ray diffraction (XRD) and atomic force microscopy (AFM), respectively. From the XRD analysis, BLT thin films show polycrystalline structure and the layered-perovskite phase was obtained over 10% excess of Bi contents. As a result of ferroelectric characteristics related to the Bi content of the BLT thin film, the remanent polarization and dielectric constant decreased with increasing over Bi content of 10% excess. The BLT film with Bi content of 10% excess was measured to have a dielectric constant of 326 and dielectric loss of 0.024. The BLT thin films showed little polarization fatigue test up to 3.5$\times$10$^{9}$ bipolar switching cycling.

Sol-gel법으로 제조된 Tb-doped PZT(60/40) 박막의 강유전 특성 (Ferroelectric properties of sol-gel derived Tb-doped PZT thin films)

  • 손영훈;김경태;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 추계학술대회 논문집 Vol.16
    • /
    • pp.51-54
    • /
    • 2003
  • Tb-doped lead zirconate titanate($Pb_{1.1}(Zr_{0.6}Ti_{0.4})O_3$; PZT) thin films on $Pt(111)/Ti/SiO_2/Si(100)$ substrates prepared by a sol-gel method. Films have a Zr/Ti ratio of 60:40 and perovskite phase structure. The effect on the structural and electrical properties of films measured according to Tb content. Dielectric and ferroelectric properties of PZT thin films were altered significantly by Tb-doping. The PZT thin film with higher dielectric constant and improved leakage current characteristic was obtained by adding 0.3 mol% Tb. At 100 kHz, the dielectric constant and the dielectric loss of the 0.3 mol% Tb-doped PZT thin film were 1611 and 0.24, respectively The remanent polarization(2Pr) of the 0.3 mol% Tb-doped PZT thin film was $61.4\;{\mu}C/cm^2$ and the coercive field was 61.9 kV/cm. Tb-doped PZT thin films showed improved fatigue characteristics comparing to the undoped PZT thin film.

  • PDF

코팅 조건에 따른 BST 박막의 표면 이미지 특성 (The Surface Image Properties of BST Thin Film by Depositing Conditions)

  • 홍경진;기현철;오수홍;조재철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 센서 박막재료 반도체재료 기술교육
    • /
    • pp.107-110
    • /
    • 2002
  • The optical memory devices of BST thin films to composite $(Ba_{0.7}\;Sr_{0.3})TiO_{3}$ using sol-gel method were fabricated by changing of the depositing layer number on $Pt/Ti/SiO_{2}/Si$ substrate. The structural properties of optical memory devices to be ferroelectric was investigated by fractal analysis and 3-dimension image processing. The thickness of BST thin films at each coating numbers 3, 4 and 5 times was $2500[\AA]$, $3500[\AA]$ and $3800[\AA]$. BST thin films exhibited the most pronounced grain growth. The surface morphology image was roughness with coating numbers. The thin films increasing with coating numbers shows a more textured and complex configuration.

  • PDF

BST 박막 소자의 유전특성 (The Dielectric Characteristics of BST Thin Film Devices)

  • 홍경진;민용기;신훈규;조재철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.660-663
    • /
    • 2001
  • The devices of BST thin films to composite (Ba$\_$0.7/ Sr$\_$0.3/)TiO$_3$using sol-gel method were fabricated by changing of the depositing layer number on Pt/Ti/SiO$_2$/Si substrate. The thin film capacitor to be ferroelectric devices was investigated by structural and electrical properties. The thickness of BST thin films at each coating numbers 3, 4 and 5 times was 2500[${\AA}$], 3500[${\AA}$], 3800[${\AA}$]. The dielectric factor of thin film when the coating numbers were 3, 4 and 5 times was 190, 400 and 460 on frequency 1[MHz]. The dielectric loss of BST thin film was linearly increased by increasing of the specimen area.

  • PDF

Dielectric properties of ZrTiO4 thin films deposited by DC magnetron reactive sputtering

  • Kim, Taeseok;Park, Byungwoo;Hong, Kug-Sun
    • Journal of Korean Vacuum Science & Technology
    • /
    • 제3권2호
    • /
    • pp.130-133
    • /
    • 1999
  • Paraelectric ZrTiO4 thin films were synthesized on a Si(100) substrate using DC magnetron reactive sputtering. Films deposited above-400$^{\circ}C$ exhibited crystalline characteristics. The dielectric constants ($\varepsilon$) and dielectric losses (tan$\delta$) of as-deposited and annealed films were measured in the 1 MHz range using a Pt upper electrode and a phosphorous-doped si bottom electrode. Preliminary data showed that as the deposition temperature increased, the dielectric losses decreased while the dielectric constants did not change significantly. similar trends for dielectric losses were observed when the as-deposited samples were annealed at 800$^{\circ}C$. The reduction of dielectric losses at high-deposition temperatures and post annealing correlated well with the x-ray diffraction peak widths.

  • PDF

Chemical Solution Deposition of PZT/Oxide Electrode Thin Film Capacitors and Their Micro-patterning by using SAM

  • Suzuki, Hisao
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.II
    • /
    • pp.907-912
    • /
    • 2005
  • Micro-patterns of $Pb(Zr_{0.53}Ti_{0.47})O_3$, PZT, thin films with a MPB composition were deposited on $Pt/Ti/SiO_2/Si$ substrate from molecular-designed PZT precursor solution by using self-assembledmonolayer(SAM) as a template. This method includes deposition of SAM followed by the optical etching by exposing the SAM to the UV-light, leading to the patterned SAM as a selective deposition template. The pattern of SAM was formed by irradiating UV-light to the SAM on a substrate and/or patterned PZT thin film through a metal mask for the selective deposition of patterned PZT or lanthanum nickel oxide (LNO) precursor films from alkoxide-based precursor solutions. As a result, patterned ferroelectric PZT and PZT/LNO thin film capacitors with good electrical properties in micrometer size could be successfully deposited.

  • PDF

Bi 첨가량에 따른 BLT 박막의 유전특성 (Dielectric properties of $Bi_{3.25}La_{0.75}Ti_3O_{12}$ thin films with Bi contents)

  • 김경태;김창일;강동희;심일운
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.371-374
    • /
    • 2002
  • Bismuth lanthanum titanate thin films with excess Bi contents were prepared onto Pt/Ti/$SiO_2$/Si substrate by metalorganic decomposition (MOD) technique. The structure and morphology of the films were analyzed using X-ray diffraction (XRD) and atomic force microscopy (AFM), respectively. From the XRD analysis, BLT thin films show polycrystalline structure and the layered-perovskite phase was obtained over 10% excess of Bi contents. As a result of ferroelectric characteristics related to the Bi content of the BLT thin film, the remanent polarization and dielectric constant decreased with increasing over Bi content of 10 % excess. The BLT film with Bi content of 10% excess was measured to have a dielectric constant of n9 and dielectric loss of 1.85[%]. The BLT thin films showed little polarization fatigue test up to 3.5 x $10^{9}$ bipolar switching cycling.

  • PDF

Preparation and Properties of Sol-Gel Processed Lead Lanthanum Titanate Thin

  • Kim, Hyun-Hoo;Lee, Jung-Geun
    • Transactions on Electrical and Electronic Materials
    • /
    • 제1권1호
    • /
    • pp.17-21
    • /
    • 2000
  • In order to investigate the dependence of a content in lead lanthanum titanate (PLT) films and heat treatment, sol-gel process has been used. Four types of PLT thin films with the chemical formula, Pb$\_$1-x/ La$\_$x/Ti$\_$1-x/4/O$_3$(X=18, 21, 24 and 28 mole %) have been fabricated on Pt/Ti/SiO$_2$/Si multi-layers and ITO/glass substrates, The post-annealing temperature in the range of 400~700 $\^{C}$ is applied for the formation of perovskite structure in PLT films. The structureal, electrical and optical properties of PLT film with the addition of La content are estimated. The films orientation and surface structure of films are studied by XRD (X-ray diffraction) and SEM(scanning electron microscopy). The P-E hysteresis loop become narrower with increasing La content. The average transmittance of the films is about 80%.

  • PDF

Eu 첨가에 따른 PZT 박막의 유전 특성 (Dielectric properties of Eu-doped PZT thin films)

  • 손영훈;김경태;김창일;장의구;이병기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.155-158
    • /
    • 2002
  • Eu-doped lead zirconium titanate $Pb_{1.1}(Zr_{0.3}Ti_{0.7})O_{3}$ thin films on the Pt/Ti/$SiO_2$/Si substrates prepared by a metalorganic decomposition (MOD) method. The effect on the structural and electrical properties of the films measured according to Eu content. Eu-doping altered significantly the dielectric and ferroelectric properties. The remanent polarization and coercive field decreased with increasing the concentration of Eu content. The dielectric constant and dielectric loss of the film decreased with increasing Eu contents. The 3 mol% of Eu-doped PZT thin film showed large remanent polarization and the fatigue characteristic of the film did not change up to $10^9$ switching cycles.

  • PDF

Eu 첨가에 따른 PZT 박막의 강유전 특성 (Ferroelectirc Properties of Eu-doped PZT Thin Films)

  • 김창일;손영훈;김경태;김동표;이병기
    • 한국전기전자재료학회논문지
    • /
    • 제16권7호
    • /
    • pp.611-615
    • /
    • 2003
  • Eu-doped lead zirconate titanate(Pb$\sub$1.1/(Zr$\sub$0.6/Ti$\sub$0.4/)O$_3$; PZT) thin films on the Pt/Ti/SiO$_2$/Si substrates prepared by a sol-gel method. The effect on structural and electrical properties of PZT thin films measured according to the Eu content. Eu-doping altered significantly dielectric and ferroelectric properties. The remanent polarization and the coercive field decreased with the increasing Eu content. The dielectric constant and the dielectric loss of PZT thin films decreased with the increasing Eu content. The 0.5 mol% of Eu-doped PZT thin film showed improved fatigue characteristic comparing to the undoped PZT thin film.