Purpose : The purpose of this study was aimed to compare the shear bond strength on dentin of three dentin bonding agents and two resin cements used in conjunction with self-cured composite resin core material. Material and method : Control group and six experimental groups were divided for this study. Control group was designated as specimens bonded with Tenure$ A&B^{(R)}$. Experimental groups were as follows : PB-BL group : specimens bonded with Prime&Bond $NT^{(R)}$, $BondLink^{(R)}$ SB-BL group : specimens bonded with $^{(R)}$, BondLink$SingleBond^{(R)}$ PB group : specimens bonded with Prime&Bond $NT^{(R)}$ SB group : specimens bonded with $SingleBond^{(R)}$ PF group : specimens bonded with $Panavia-F^{(R)}$ BI group specimens bonded with Bistite $II^{(R)}$ All specimens were stored in $37^{\circ}C$ distilled water for 24 hours, followed by the shear bond strength was tested by universal testing machine. The data was analysed statistically by Mann-Whitney test. Results : 1. For Prime&Bond $NT^{(R)}$ and $SingleBonde^{(R)}$, the shear bond strength was 0.24 MPa and 7.19 MPa each by each, while Tenure $A&B^{(R)}$ group control was measured at 13.93 MPa (p<0.05). Especially for Prime&Bond $NT^{(R)}$ it did not get conjunction with dentin. 2. For Prime&Bond $NT^{(R)}$ and $SingleBond^{(R)}$ using $BondLink^{(R)}$, there was no significant difference as a result of 11.73 MPa and 14.00 MPa each by each (p<0.05). 3. For $Panavia-F^{(R)}$ and Bistite $II^{(R)}$, they showed the highest shear bond strength as measured by 18.24 MPa and 16.09 MPa each (p<0.05).
연구목적: 본 연구의 목적은 자가중합 또는 이중중합을 위한 활성제가 포함된 상아질 접착제에서 활성제의 사용 유무가 자가중합 복합레진과 상아질 접착제간의 전단결합강도에 미치는 영향을 평가하는 것이다. 연구 재료 및 방법: 실험을 위하여 우식 및 충전물이 없는 건전한 대구치 50개를 주문제작한 아크릴릭 레진블록에 포매한 후, 모델 트리머로 연마하여 평활한 상아질면을 만든 후, 600grit 실리콘 카바이드 페이퍼로 연마하고 증류수에 보관하였다. 50개의 시편을 10개씩 5개 군으로 나눈 후, 상아질 접착제를 제조사의 지시대로 도포한 후, 플라스틱 주형을 이용하여 자가중합 복합레진 (Luxacore)을 접착시켰다. 상아질 접착제는 One-Step (OS군), Prime&Bond NT, AdheSE를 이용하였는데 Prime&Bond NT와 AdheSE는 단독으로 사용한 군 (PB군, AS군)과 활성제를 같이 사용한 군 (PBA군, ASA군)으로 다시 나누었다. 증류수에 24시간 보관 후, 인스트론 만능시험기를 사용하여 시편에 1 mm/min의 전단속도로 하중을 가하여 시편이 분리되는 최대 하중을 측정한 뒤, 단위 면적 당 결합강도 (MPa)로 환산하여 One-way ANOVA를 이용하여 비교, 분석하고 5% 유의수준에서 Tukey HSD 검정을 이용하여 분석하였다. 결과: 각 군의 전단결합강도의 평균을 보면, OS군이 18.6 MPa로 가장 높았고 그 다음이 PBA군 (10.3 MPa)과 ASA군 (10.2 MPa)이었고, PB군과 AS군이 각각 5.9 MPa, 6.0 MPa로 가장 낮은 전단결합강도를 나타내었다. 결론: 본 실험을 통해 Prime&Bond NT와 AdheSE에서 활성제를 같이 사용한 경우, 활성제를 사용하지 않은 경우보다 전단결합강도가 높아짐을 알 수 있었지만, 활성제가 포함되어 있지 않은 One-Step보다는 낮은 수치였다.
본 연구는 친수성 용매가 함유되어 있는 3종의 단일병 접착제의 적용 시간을 증가시켰을 때, 건조 상아질에 대한 재습윤의 효과가 있는지를 미세인장 결합강도의 측정을 통해 알아보고자 시행하였다. 실험대상은 최근에 발거한 상하악의 대구치로, 교합면 1/3부위의 치질을 치아 장축에 수직으로 절단하여 상아질을 노출시킨 후, $32\%$인산 (Unietch, Bisco Inc., Schaumburg, IL, USA)으로 15초간 산부식 하고 수세하였다. 치아는 무작위로 S군 (Single Bond), O군 (One-Step), P군 (Prime & Bond NT)으로 분류하였고, 각 군은 다시 3군 (W: 상아질 표면의 남아있는 과잉의 물을 수분에 적신 거즈를 이용하여 제거한 후, 즉시 단일병 접착제를 적용하고 광중합, D : 30초간 건조 한 후 즉시 단일병 접착제를 적용하고 광중합, 30: 30초간 건조 한 후 단일병 접착제를 30초간 적용하고 광중합)으로 소 분류하였다. 접착제 도포 후, 복합레진을 축조하고 접착계면이 $1mm^2$가 되도록 절단하여 각 군당 20개의 표본을 사용하여 미세인장 결합강도를 측정하였다. 5군,0군의 30초 적용군 (S-30, O-30)은 건조군 (S-D, O-D)보다 높은 미세인장 결합강도를 보였으며, S-30군의 경우 S-D군보다 통계학적으로 유의성 있게 높았다 (P<0.05). 하지만, P군의 30초 적용군 (P-30)은 건조군 (P-D)에 비해 미세인장 결합강도가 통계학적으로 유의성 있게 감소하였다 (P<0.05).
치아 교환시기에 발거된 치관이 건전한 유구치 상아질 표면을 One-Bottle 상아질 결합제인 Primer & Bond NT(DeTrey/Dentsply, Konstanz, Germany)와 Single Bond(3M Co. U.S.A.) 그리고 대조군으로 Scotchbond Multipurpose System(3M Co. U.S.A.)를 이용하여 각 제조자의 지침에 따라 처리하여 레진을 충전하고 광중합하였다. 1. 전단 결합 강도의 측정결과 Primer & Bond NT군인 1군, Single Bond군인 2군, 그리고 대조군으로 사용된Scotchbond Multipurpose System군인 3군의 순서로 1군에서 다소 높은 전단 결합 강도를 보였으나, 모든 군들간에는 통계적 유의차가 없었다(p>.05). 2. 주사 전자현미경 소견에서 1군 2군에서 서로 유사한 양상의 잘 형성된 혼화층이 관찰되었으며, 레진 테그와 측방 가지 또한 다수 관찰되었다. 반면 3군에서는 혼화층이나 측방가지의 형성이 1, 2군에 비해 다소 미약한 양상을 보였다.
법랑질과 상아질에 대한 접착시스템의 결합력은 타액이나 혈액에 의하여 저하될 수 있다. 제 5세대 상아질 결합제 적용시에 산부식된 치면이 타액에 오염될 경우, 보다 효율적인 치면 처리 방법을 알아보기 위해 여러 가지 치면 처리 방법과 조건을 설정한 다음 수복물의 유지력을 전단결합강도 측정으로 서로 비교 분석하고, 치아와 수복물 사이의 계면을 주사전자 현미경을 이용해 관찰하였다. 그 결과 우치상아질의 산부식후 타액오염된 경우, 물로 10초간 세척한 후 공기로 가볍게 건조하여 수복하면 전단결합강도의 감소가 일어나지 않았으나, Prime & Bond NT의 광중합후에 타액오염된 경우에는 물로 10초간 세척한 후 공기로 완전히 건조를 하여도 레진과의 결합력이 매우 약해지며 Prime & Bond NT를 재적용하더라도 전단결합강도의 상당한 감소를 보였으며, 주사전자 현미경 관찰결과 모든 군에서 유사한 혼화층과 레진태그의 형성을 보였으며 특이할만한 각 군간의 차이를 관찰할 수 없었다.
The purposes of this study were to evaluate the effect of adhesive property on microtensile bond strength and to determine the failure mode. Flat occlusal dentin surfaces were prepared using low-speed diamond saw. The dentin was etched with 37% phosphoric acid. The following adhesives were applied to the etched dentin to manufacturer's directions: Scotchbond Multi-Purpose in group SM, Prime&Bond NT in group NT, Scotchbond Multi-Purpose followed by Tetric-flow in group TR. After adhesive application, a cylinder of resin-based composite was built up on the occlusal surface. Each tooth was sectioned vertically to obtain the $1{\;}{\times}{\;}1\textrm{mm}^2$ "sticks". Microtensile bond strength were determined. Each specimen was observed under stereomicroscope and scanning electron microscope (SEM) to examine the failure mode. Data were analyzed using one way ANOVA. The results of this study were as follows:1. The microtensile bond strength value were:group SM ($18.98{\pm}3.01MPa$). group NT ($16.01{\pm}4.82MPa$) and group TR ($17.56{\pm}3.22MPa$). No significant statistical differences were observed among the groups (P>0.05). 2. Most of specimens showed mixed failure. In group TR, there was a higher number of specimens showing areas of cohesive failure in resin.
Nur, Metin;Uysal, Tancan;Yesilyurt, Cemal;Bayram, Mehmet
대한치과교정학회지
/
제40권4호
/
pp.267-275
/
2010
이번 연구의 목적은 맹출 또는 미맹출된 치아에 교정용 버튼을 부착 후 자가부식 접착제(self-etching adhesive)의 사용 유무에 대한 전단결합강도(shear bond strength)와 탈락모드를 비교하고자 함이다. 각각 84개의 맹출 또는 미맹출된 제3대구치를 사용하였다. 각각 치아의 협측면을 다음의 부착시스템 그룹으로 할당하였다. A, 기존방식: 1, Transbond XT (3M Unitek); 2, Prime & Bond NT (Dentsply/Caulk); 3, Single Bond (3M ESPE); B, 자가부식 접착제; 4, Clearfil SE Bond (Kuraray); 5, Transbond Plus (3M Unitek); 6, Clearfil S3 (Kuraray); 7, G Bond (GC). 부착물의 전단강도와 접착제 잔류지수를 측정하였으며 결과값은 ANOVA와 independent t-test 및 chi-square 검증을 통해 분석되었다. 맹출 또는 미맹출된 치아의 전단결합강도를 비교하였을 때 Clearfil SE와 G Bond에서 유의한 차이가 관찰되었다. Single Bond를 제외한 모든 접착시스템에서 맹출보다는 미맹출 치아면에서 높은 접착강도가 관찰되었다. 기존 접착제를 사용하는 경우 맹출 또는 미맹출 치아에 대한 접착강도에는 차이가 없을 수 있다. 그러나 임상의사는 사용 전에 self-etching system의 종류를 고려할 필요가 있다.
The purpose of this study was to compare the microhardness and the fluoride content of enamel and dentin around fluoride- or non fluoride-containing restorations. Forty extracted human teeth were used and prepared cervical cavities on proximal surface. Experimental teeth were divided into five groups . Group 1 : Prime & Bond NT and Z100, Group 2 Prime & Bond NT and F2000, Group 3 : Scotchbond Multi-purpose and Z100, Group 4 : Scothcbond Multi-purpose and F2000, Group 5 : Fuji II LC. The cavities were filled with dentin adhesives and restorative materials. After each tooth was bisected, one half was tested microharaness and the other half was analyzed the fluoride at the enamel and dentin by an EPMA-WDX device. The results were as follows; 1. There was no statistical difference among the microhardness of enamel surface in all group. 2. The microhardness at dentin of $100{\;}\mu\textrm{m}$ point in Group 2 and $20{\;}\mu\textrm{m}$ point in Grocup 4 was lower than that of normal dentin (p>0.05). 3. There was no statistical difference among the fluoride content of enamel surface in all group. 4. The fluoride content at the dentin of $30{\;}\mu\textrm{m}$ point in Group 2 and 5 were higher than those at $100{\;}\mu\textrm{m}{\;}and{\;}200{\;}\mu\textrm{m}$ point in Group 2 and normal dentin (p<0.05). 5. At the dentin of $30{\;}\mu\textrm{m}$ point, Group 2 showed higher fluoride content than Group 1 and 3, and Group 5 showed higher fluoride content than other groups.
The objective of this study was to evaluate the effect of configuration of cavity on the mechanical properties such as flexural strength and elastic modulus of resin composites. The materials used were $Clearfil^{TM}$ AP-X(Kuraray, Japan) and $Esthet-X^{TM}$(Dentsply, USA) as resin composite. Dentin-bonding systems used in the study were $Clearfil^{TM}$ SE Bond(Kuraray, Japan) and Prime & Bond $NT^{TM}$(Dentsply, USA). The specimens were prepared as 6 groups with 2 control groups and 4 experimental groups.(omitted)
The purpose of this study was to compare and to evaluate the combination use of 5 kinds of dentin adhesive systems and 5 kinds of composite resins using micro-shear bond test. Five adhesive systems (Prime & Bond NT (PBN). Onecoat bond (OC), Excite (EX), Syntac (SY), Clearfil SE bond (CS)) and five composite resins (Spectrum (SP), Synergy Compact (SC), Tetric Ceram (TC), Clearfil AP-X (CA), Z100 (Z1)) were used for this study ($5{\;}{\times}{\;}5{\;}={\;}25group$, n =14/group). The slices of horizontally sectioned human tooth were bonded with each bonding system and each composite resin, and tested by a micro-shear bond strength test. These results were analyzed statistically. The mean micro-shear bond strength of dentin adhesive systems were in order of CS (22.642 MPa), SY (18.368 MPa), EX (14.599 MPa). OC (13.702 MPa). PBN (12.762 MPa). The mean bond strength of self-etching primer system group (CS, SY) in dentin was higher than that of self-priming adhesive system groups (PBN, EX, OC) significantly (P<0.05). The mean bond strength of composite resins was in order of SP (19.008 MPa), CA (17.532 MPa). SC (15.787 MPa), TC (15.068 MPa). Z1 (14.678 MPa). Micro-shear bond strength of SP was stronger than those of other composite resins significantly (P < 0.05). And those of TC and Z1 were weaker than other composite resins significantly (P < 0.05). No difference was found in micro-shear bond strength of composite resin in self-etching primer adhesive system groups (CS, SY) statistically. However, there was significant difference of micro-shear bond strength of composite resin groups in self-priming adhesive systems group (PBN, EX, OC). The combination of composite resin and dentin adhesive system recommended by manufacturer did not represent positive correlation. It didn't seem to be a significant factor.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.