무가압 소결법에 의한 SiC-$TiB_2$계 도전성 복합체의 특성 (Properties of Pressureless Sintered SiC-$TiB_2$ Electroconductive Composites)

  • 박미림;주진영;신용덕;소병문
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 춘계학술대회 논문집 유기절연재료 전자세라믹 방전플라즈마 연구회
    • /
    • pp.118-122
    • /
    • 2001
  • The ${\beta}-SiC+TiB_2$ ceramic electroconductive composites were pressureless-sintered and annealed by adding 12wt% $Al_2O_3+Y_2O_3$(6 : 4wt%) powder as a function of sintering temperature. The relative density is over 78.83% of the theoretical density and increased with increasing sintering temperature. The phase analysis of the composites by XRD revealed of $\alpha$-SiC(6H), $TiB_2$, $Al_5Y_2O_{12}$ and $\beta$-SiC(15R). Flexural strength showed the highest of 140 MPa for composites sintered at $1900^{\circ}C$. The vicker's hardness increased with increasing sintering temperature and showed the highest of 4.07 GPa at $1900^{\circ}C$. Owing to YAG, the fracture toughness showed the highest of 4.07 $MPa{\cdot}m^{1/2}$ for composites at $1900^{\circ}C$. The electrical resistivity was measured by the Pauw method from $25^{\circ}C$ to $700^{\circ}C$. The electrical resistivity of the composites showed the PTCR(Positive Temperature Coefficient Resistivity).

  • PDF

High $T_c$ Pb-free (1-x)$BaTiO_3-x(Bi_{1/2}Na_{1/2})TiO_3$ 세라믹의 미세구조와 PTCR 특성 (Microstructure and PTCR characteristic of high $T_c$ lead-free ((1-x)$BaTiO_3-x(Bi_{1/2}Na_{1/2})TiO_3$ characteristic)

  • 김철민;조용수;정영훈;이영진;이미재;백종후;이우영;김대준
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.32-32
    • /
    • 2008
  • Microstructure and positive temperature coefficient of resistivity (PTCR) characteristics of $0.9BaTiO_3-0.1(Bi_{0.5}Na_{0.5})TiO_3$ [BaBiNT] ceramics doped with $Nb_2O_5$ were investigated in order to develop the Pb-free high Curie temperature ($T_c$)(>$160^{\circ}C$) PTC thermistor. The BaBiNT ceramics showed a tetragonal perovskite structure, irrespective of the added amount of $Nb_2O_5$. They also have a homogeneous microstructure. The resistivity of BaBiNT ceramics was gradually decreased by doping $Nb_2O_5$, which might be due to $Nb^{+5}$ ions substituting for $Ti^{+4}$ sites. The PTCR characteristics of BaBiNT ceramics appeared when the amount of doped $Nb_2O_5$ exceeded 0.0025mol%. Moreover, the abrupt grain growth was observed for the 0.03mol% $Nb_2O_5$added BaBiNT ceramics. It showed an especially high $T_c$ of approximately $172^{\circ}C$ and good PTCR characteristics of a high $\rho_{max}/\rho_{min}$ ratio ($2.96\times10^3$), a high resistivity temperature factor (11.40/$^{\circ}C$) along with a relatively low resistivity ($3.5\times10^4\Omega{\cdot}cm$).

  • PDF

상압소결(常壓燒結)한 $SiC-ZrB_2$ 전도성(電導性) 복합체(複合體)의 미세구조(微細構造)와 특성(特性)에 미치는 Annealing 온도(溫度)의 영향(影響) (Effect of Annealing Temperature on Microstructure and Properties of the Pressureless-Sintered $SiC-ZrB_2$ Electroconductive Ceramic Composites)

  • 신용덕;주진영
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제55권9호
    • /
    • pp.434-441
    • /
    • 2006
  • The effect of pressureless-sintered temperature on the densification behavior, mechanical and electrical properties of the $SiC-ZrB_2$ electroconductive ceramic composites was investigated. The $SiC-ZrB_2$ electroconductive ceramic composites were pressureless-sintered for 2 hours at temperatures in the range of $1,750{\sim}1,900[^{\circ}C]$, with an addition of 12[wt%] of $Al_2O_3+Y_2O_3$(6:4 mixture of $Al_2O_3\;and\;Y_2O_3$) as a sintering aid. The relative density and mechanical properties are increased markedly at temperatures in the range of $1,850{\sim}1,900[{^\circ}C]$. The relative density, flexural strength, vicker's hardness and fracture toughness showed the highest value of 81.1[%], 230[MPa], 9.88[GPa] and $6.05[MPa\;m^{1/2}]$ for $SiC-ZrB_2$ composites of $1,900[{^\circ}C]$ sintering temperature at room temperature respectively. The electrical resistivity was measured by the Pauw method in the temperature ranges from $25[{^\circ}C]\;to\;700[{^\circ}C]$, The electrical resistivity showed the value of $1.36{\times}10^{-4},\;3.83{\times}10^{-4},\;3.51{\times}10^{-4}\;and\; 3.2{\times}10^{-4}[{\Omega}{\cdot}cm]$ for SZ1750, SZ1800, SZ1850 and SZ1900 respectively at room temperature. The electrical resistivity of the composites was all PTCR(Positive Temperature Coefficient Resistivity). The resistance temperature coefficient showed the value of $4.194{\times}10^{-3},\;3,740{\times}10^{-3},\;2,993{\times}10^{-3},\;3,472{\times}10^{-3}/[^{\circ}C}$ for SZ1750, SZ1800, SZ1850 and SZ1900 respectively in the temperature ranges from $25[{\circ}C]\;to\;700[{\circ}C]$, It is assumed that because polycrystallines such as recrystallized $SiC-ZrB_2$ electroconductive ceramic composites, contain of porosity and In Situ $YAG(Al_5Y_3O_{12})$ crystal grain boundaries, their electrical conduction mechanism are complicated. In addition, because the condition of such grain boundaries due to $Al_2O_3+Y_2O_3$ additives widely varies with sintering temperature, electrical resistivity of the $SiC-ZrB_2$ electroconductive ceramic composites with sintering temperature also varies with sintering condition. It is convinced that ${\beta}-SiC$ based electroconductive ceramic composites for heaters or ignitors can be manufactured by pressureless sintering.

상압소결(常壓燒結)한 $SiC-TiB_2$ 전도성(電導性) 복합체(複合體)의 미세구조(微細構造)와 특성(特性)에 미치는 Annealing 온도(溫度)의 영향(影響) (Effect of Annealing Temperature on Microstructure and Properties of the Pressureless-Sintered $SiC-TiB_2$ Electroconductive Ceramic Composites)

  • 신용덕;주진영
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제55권10호
    • /
    • pp.467-474
    • /
    • 2006
  • The effect of pressureless-sintered temperature on the densification behavior, mechanical and electrical properties of the $SiC-TiB_2$ electroconductive ceramic composites was investigated. The $SiC-TiB_2$ electroconductive ceramic composites were pressureless-sintered for 2 hours at temperatures in the range of $1,750{\sim}1,900[^{\circ}C]$, with an addition of 12[wt%] $Al_2O_3+Y_2O_3(6:4\;mixture\;of\;Al_2O_3\;and\;Y_2O_3)$ as a sintering aid. The relative density, flexural strength, vicker's hardness and fracture toughness showed the highest value of 84.92[%], 140[MPa], 4.07[GPa] and $3.13[MPa{\cdot}m^{1/2}]$ for $SiC-TiB_2$ composites of $1,900[^{\circ}C]$ sintering temperature at room temperature respectively. The electrical resistivity was measured by the Pauw method in the temperature ranges from $25[^{\circ}C]\;to\;700[^{\circ}C]$. The electrical resistivity showed the value of $5.51{\times}10^{-4},\;2.11{\times}10^{-3},\;7.91{\times}10^{-4}\;and\;6.91{\times}10^{-4}[\Omega{\cdot}cm]$ for ST1750, ST1800, ST1850 and ST1900 respectively at room temperature. The electrical resistivity of the composites was all PTCR(Positive Temperature Coefficient Resistivity). The resistance temperature coefficient showed the value of $3.116{\times}10^{-3},\;2.717{\times}10^{-3},\;2.939{\times}10^{-3},\;3.342{\times}10^{-3}/[^{\circ}C]$ for ST1750, ST1800, ST1850 and ST1900 respectively in the temperature ranges from $25[^{\circ}C]\;to\;700[^{\circ}C]$. It is assumed that because polycrystallines, such as recrystallized $SiC-TiB_2$ electroconductive ceramic composites, contain of porosity and In Situ $YAG(Al_5Y_3O_{12})$ crystal grain boundaries, their electrical conduction mechanism are complicated. In addition, because the condition of such grain boundaries due to $Al_2O_3+Y_2O_3$ additives widely varies with sintering temperature, electrical resistivity of the $SiC-TiB_2$ electroconductive ceramic composites with sintering temperature also varies with sintering condition. It is convinced that ${\beta}-SiC$ based electroconductive ceramic composites for heaters or ignitors can be manufactured by pressureless sintering.

Nb+5첨가된 반도성 BaTiO3세라믹스에서 MoO3의 영향과 주파수 특성 (Effect of MoO3 Addition and Their Frequency Characteristics in Nb+5 doped Semiconductive BaTiO3 Ceramics)

  • 윤상옥;정형진;윤기현
    • 한국세라믹학회지
    • /
    • 제24권1호
    • /
    • pp.63-69
    • /
    • 1987
  • Effect of MoO3 additiion on the semiconductive BaTiO3 ceramics doped with 0.2 mole% Nb2O5 and their frequency characteristics have been investigated on the view of intergranular barrier layer model through the observation of changes in their electrical properties. The resistivity increases with the increase of MoO3 addition, but the capacitance, the frequency dependence of capacitance and the effect of positive temperature coefficient of resistivity (PTCR) decrease. It is explained by the possible increase in the thickness of potential barrier due to the formation of insulating layer and thus decrease in the degree of energy band bending. Both the PTCR effect and resistivity decrease with the increase of frequency due to the possible elimination of barrier layer at the grain boundary.

  • PDF

밀폐유도용해로 제조된 2원계 Skutterudite CoSb3의 열전특성 (Thermoelectric Properties of Binary Skutterudite CoSb3 Prepared by Encapsulated Induction Melting)

  • 유신욱;정재용;어순철;김일호
    • 한국재료학회지
    • /
    • 제16권5호
    • /
    • pp.312-317
    • /
    • 2006
  • Binary skutterudite $CoSb_3$ compounds were prepared by the encapsulated induction melting (EIM) process, and their thermoelectric, microstructural and mechanical properties were examined. Single-phase ${\delta}-CoSb_3$ was successfully produced by the EIM and subsequent heat treatment at 773 K-873 K for 24 hours in vacuum. Seebeck coefficient increased with increasing heat treatment temperature up to 673 K, showing the positive signs in the range of measuring temperature. However, the samples heat-treated at 773 K-873 K showed negative Seebeck coefficient from room temperature to 400 K, while it showed positive signs above 400 K. Electrical resistivity decreased with increasing temperature, showing typical semiconducting conductivity. Thermal conductivity decreased drastically with increasing heat-treatment temperature. This is closely related with the phase transition to ${\delta}-CoSb_3$.

$Al_2O_3+Y_2O_3 첨가량에 따른 {\beta}-SiC-ZrB_2$계 전도성 복합체의 특성 (The Properties of $\beta-SiC-ZrB_2$ Electroconductive Ceramic Composites with $Al_2O_3+Y_2O_3$Contents)

  • 신용덕;주진영;황철
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제49권9호
    • /
    • pp.516-522
    • /
    • 2000
  • The mechanical and electrical properties of the hot-pressed and annealed $\beta-SiC-ZrB_2$ electroconductive ceramic composites were investigated as a function of the liquid forming additives of$Al_2O_3+Y_2O_3$ Phase analysis of composites by XRD revealed $\alpha-SiC(6H) ZrB_2\; and YAG(Al_5Y_3O_{12})$ The relative density of composites were increased with increased Al2O3+Y2O3 contents. The Flexural strength showed the highest value of 390.6MPa for composites added with 20wt% Al2O3+Y2O3 additives at room temperature. Owing to crack deflection crack bridging phase transition and YAG of fracture toughness mechanism the fracture toughness showed the highest value of 6.3MPa.m1/2 for composites added with 24wt% Al2O3+Y2O3 additives at room temperature. The resistance temperature coefficient showed the value of$ 2.46\times10^{-3}\;, 2.47\times10^{-3},\; 2.52\times10^{-3}/^{\circ}C$ for composite added with 16, 20, 24wt% Al2O3+Y2O3 additives respectively. The electrical resistivity of the composites was all positive temperature coefficient resistance(PTCR) in the temperature range of $256{\circ}C\; to\; 900^{\circ}C$.

  • PDF

Thickness Dependence of the Electrical Properties in NiCr Thin Film Resistors Annealed in a Vacuum Ambient for π - type Attenuator Applications

  • Phuong Nguyen Mai;Lee Won-Jae;Yoon Soon-Gil
    • 한국전기전자재료학회논문지
    • /
    • 제19권8호
    • /
    • pp.712-716
    • /
    • 2006
  • NiCr thin films prepared on $SiO_2/Si$ substrates at room temperature by magnetron co-sputtering technique and then annealed in a vacuum ambient $(3{\times}10^{-6}\;Torr)\;at\;400^{\circ}C$. The grain size and crystallinity of the films increased with film thickness. The resistivity of the films slightly decreases as the film thickness increases, Temperature coefficient resistance (TCR) exhibits positive values irrespective of film thickness and TCR in the range of 50 to 400 nm thickness shows suitable values for the application of 10 dB in ${\pi}-type$ attenuators.

SiC-$TiB_2$ 전도성(電導性) 복합체(複合體)의 특성(特性)에 미치는 가압(加壓)의 영향(影響) (Effect of Pressure on Properties of the SiC-$TiB_2$ Electroconductive Ceramic Composites)

  • 신용덕;서재호;주진영;고태헌;이정훈
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2008년도 제39회 하계학술대회
    • /
    • pp.1228-1229
    • /
    • 2008
  • The composites were fabricated 61[vol.%] ${\beta}$-SiC and 39[vol.%] $TiB_2$ powders with the liquid forming additives of 12[wt%] $Al_2O_3+Y_2O_3$ as a sintering aid by pressure or pressureless annealing at 1,650[$^{\circ}C$] for 4 hours. Reactions between SiC and transition metal $TiB_2$ were not observed in the microstructure and the phase analysis of the SiC-$TiB_2$ electroconductive ceramic composites. Phase analysis of SiC-$TiB_2$ composites by XRD revealed mostly of ${\alpha}$-SiC(6H), $TiB_2$, and In Situ $YAG(Al_5Y_3O_{12})$. The relative density, the flexural strength and the Young's modulus showed the highest value of 88.32[%], 136.43[MPa] and 52.82[GPa] for pressure annealed SiC-$TiB_2$ composites at room temperature. The electrical resistivity showed the lowest value of 0.0162[${\Omega}{\cdot}cm$] for pressure annealed SiC-$TiB_2$ composite at 25[$^{\circ}C$]. The electrical resistivity of the pressure annealed SiC-$TiB_2$ composite was positive temperature coefficient resistance (PTCR) but the electrical resistivity of the pressureless annealed SiC-$TiB_2$ composites was negative temperature coefficient resistance(NTCR) in the temperature ranges from 25[$^{\circ}C$] to 700[$^{\circ}C$].

  • PDF

$\beta-SIC-ZrB_{2}$복합체의 파괴인성과 전기전도도에 미치는 YAG의 영향 (Effect of YAG on the Fracture Toughness and Electrical Conductivity of $\beta-SIC-ZrB_{2}$ Composites)

  • 신용덕;주진영;윤세원;황철;박미림
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.839-842
    • /
    • 2000
  • The mechanical and electrical properties of the hot-pressed and annealed $\beta$-SiC-ZrB$_2$ electroconductive ceramic composites were investigated as function of the liquid forming additives of $Al_2$O$_3$+Y$_2$O$_3$. Phase analysis of composites by XRD revelled $\alpha$ -SiC(6H), ZrB$_2$, and YAG(Al$_{5}$ Y$_3$O$_{12}$ ). Owing to crack deflection, crack bridging, phase transition and YAG of fracture toughness mechanism, the fracture toughness showed the highest value of 6.3MPa.m$^{1}$2/ for composites added with 24wt% $Al_2$O$_3$+Y$_2$O$_3$additives at room temperature. The resistance temperature coefficient respectively showed the value of 2.46$\times$10$^{-3}$ , 2.47$\times$10$^{-3}$ , 2.52$\times$ 10$^{-3}$ $^{\circ}C$ for composite added with 16, 20, 24wt% A1$_2$O$_3$+Y$_2$O$_3$additives. The electircal resistivity of the composites was all positive temperature coefficient resistance(PTCR) in the temperature range of $25^{\circ}C$ to 90$0^{\circ}C$.