An Experimental Study on Wafer Demounting by Water Jet in a Waxless Silicon Wafer Mounting System

  • Kim, Kyoung-Jin;Kwak, Ho-Sang;Park, Kyoung-Seok
    • 반도체디스플레이기술학회지
    • /
    • 제8권2호
    • /
    • pp.31-35
    • /
    • 2009
  • In the silicon wafer polishing process, the mounting stage of silicon wafer on the ceramic carrier block has been using the polishing template which utilizes the porous surface instead of traditional wax mounting method. Here in this article, the experimental study is carried out in order to study the wafer demounting by water jet and the effects of operating conditions such as the water jet flowrate and the number of water jet nozzles on the wafer demounting time. It is found that the measured wafer demounting time is inversely proportional to the water flowrate per nozzle, regardless of number of nozzles used; implying that the stagnation pressure by the water jet impingement is the dominant key factor. Additionally, by using the transparent disk instead of wafer, the air bubble formation and growth is observed under the disk, making the passage of water flow, and subsequently demounting the wafer from the porous pad.

  • PDF

시선추적을 이용한 카페 공간 마감재 차이의 시각주의력 특성 (Characteristics of Visual Attention for the Different Type of Material Finishing in Cafe Space Using by Eye-tracking)

  • 최진경;김주연
    • 한국실내디자인학회논문집
    • /
    • 제27권2호
    • /
    • pp.3-11
    • /
    • 2018
  • This study aims to investigate whether there is intensionally changing eye - gaze on the cafe space images with floor finishing materials. In the Yarbus' experiment, he argued that changing information that an observer is asked to obtain from an image changes pattern of eye movements. Based on the scan path evidence, this research have questions as (1) the difference of visual attention on finishing floor material stimulus, (2) visual attention of initial activity time and type of movement paths on AOIs, and (3) visual relation floor area with another AOIs. Eye movements were recorded with the SMI REDn Scientific, which sampled eye position at 30Hz and lasted 2 minutes(120s). Although viewing was binocular, only the right eye was tracked. Of the 66 observers(mean age 22 years, standard deviation: ${\pm}1.82$) who participated in the experiment done by the four point calibration and validation procedures at the beginning tasks. Analyzing qualitative data from the number of fixation and duration on AOIs divided into four parts (AOI I-Floor, AOI II-Wall, AOI III-Ceiling, and AOI IV-Counter) in the stimulus. The results from this experiment analyzed as follows. First, it was significant in the difference of the average number of AOIs fixation times observed for the spatial image using the wood tile flooring material and the polishing tile. The wood tile flooring of stimulus had higher fixation number on AOI-II, AOI-III, and AOI-IV than the polishing tile. On seeing AOI-I was higher attention in the polishing tile stimulus. Second, the observers examined AOI-II intensively in both stimuli. However, the visual intensity was also followed by on the AOI-IV and AOI-I in the wood tile flooring stimulus, and on AOI-I, AO-IV in the polishing tile. Third, visual attention data on each AOIs have divided into the time range of "5 sec" for both images. In the wood tile stimulus, the horizontal movement path followed by AOI-II, AOI-IV, and AOI-II. In the polished tile stimulus, the movement path followed by moving vertically to AOI-II, AOI-I, and AOI-II. This study approached meaningfully and found out the characteristics of visual attention, according to the different intentions of visual attention, the relationship pathways of visual mechanism appeared and also activated by eye-tracking experiments.

도정도별 쌀의 취반에 대한 역학적 연구 (Kinetic Studies on Cooking of Rice of Various Polishing Degrees)

  • 최홍식;김성곤;변유량;권태완
    • 한국식품과학회지
    • /
    • 제10권1호
    • /
    • pp.52-56
    • /
    • 1978
  • 쌀의 취반에 대한 기작을 아끼바레(도정도,50%,70% 및 90%)를 이용하여 연구하였다. 취반(취반온도 $90^{\circ}-120^{\circ}C$)후 밥알의 hardness는 Texturometer로 측정하였다. 취반속도는 1차 반응의 식으로 표시될 수 있었으며, 취반온도 $90^{\circ}-120^{\circ}C$사이의 온도 계수는 2 이었다. 취반의 활성화 에너지는 $100^{\circ}C$이하에서는 약 17,000cal/mole, $100^{\circ}C$ 이상에서는 약 9,000cal/mole이었다. 쌀의 도정도 및 쌀의 취반전 침지시간은 활성화 에너지에 영향을 주지 않았으나, 반응속도 상수는 도정도가 높아질수록 증가하였고 취반시간은 반대로 감소하였다. 쌀의 취반과정은 다음의 두 기작으로 설명할 수 있었다. 즉 취반온도는 $100^{\circ}C$이하에서는 쌀의 성분 및 물에 의한 화학반응이, 취반온도 $100^{\circ}C$이상에서는 취반된 부분으로부터 취반되지 않은 부분(즉 반응이 진행되고 있는 부분)으로의 물의 확산속도가 취반속도를 제한하였다.

  • PDF

주파수 변동에 따른 초음파방오장비의 파울링제거효과 (Antifouling Effect of an Ultrasonic System Operating at Different Frequencies)

  • 배진우;박관식;류명록;박권하
    • 해양환경안전학회지
    • /
    • 제25권5호
    • /
    • pp.609-616
    • /
    • 2019
  • 선박에 파울링이 발생되면 운항 중 선박의 저항이 증가하게 되고 이로 인해 연료 소모량도 높아지게 된다. 또한 파울링의 제거에 많은 시간이 필요하게 되어 전체적으로 선박의 유지보수 비용이 증대되는 문제점이 있다. 이러한 문제점을 해결하고 환경오염을 방지하기 위해 주석과 같은 독성 물질을 포함하지 않는 자기연마형 방오도료를 개발하고 있다. 이와 같은 종래기술은 해수와의 마찰이나 진동이 많이 발생하는 운항 중에는 연마기능이 촉진되어 방오성능이 증대되나, 정박 중과 같이 실제로 파울링이 심화되는 경우에는 해수의 흐름이 없어 연마기능이 저하되어 방오성능이 떨어지는 문제점이 있다. 이러한 문제점을 해결하기 위해 선체의 진동 및 해수의 흐름이 없어서 연마 기능이 저하되는 정박 중에도 진동을 부여하여 연마 기능의 저하를 방지하는 제품을 개발하였다. 개발된 초음파 방오장비의 성능의 신뢰성을 위해 파형발생기의 반복성을 확인하였고 장치의 파울링 제거효율의 정성적인 경향은 시편을 통해 파악하였다. 실험 결과 주파수와 진폭의 반복성의 변동계수 값은 평균 0.2 %, 4.0 %를 나타냈고 시편의 파울링 발생량은 No.5 시편에서 73.3 g으로 가장 많았고 파울링 제거효율은 장치를 설치하지 않은 시편과 비교하여 평균 93.2 % 값을 확인할 수 있었다.

표면 성상에 따른 수용성 발수제 혼입 시멘트 모르타르의 발수특성 (Water Repellent Characteristics According to the Surface Properties of Cement Mortar Mixed with Water-soluble Water Wepellent)

  • 강석표;강혜주;홍성욱;양승현
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제24권6호
    • /
    • pp.42-49
    • /
    • 2020
  • 본 논문은 시멘트계 재료의 표면 및 구체에 소수성을 부여하여 내구성을 향상시키기 위한 기초연구이다. 실란/실록산계 혼합형 발수제를 첨가한 시멘트 모르타르를 제조하고 초기 수화성능 및 유동성능, 재령별 압축강도를 측정하였다. 또한 표면연마 전후의 물접촉각 및 흡수율을 측정하였다. 실란/실록산계 혼합형 발수제를 첨가한 시멘트 모르타르의 플로우는 발수제 첨가량 1.5%까지는 감소하는 것으로 나타났으며 첨가량 3.0%에서는 증가하였다. 실란/실록산계 혼합형 발수제를 첨가할 경우 시멘트 페이스트의 응결시간은 초결 및 종결 모두 지연되는 것으로 나타났다. 압축강도는 발수제의 최대 첨가량 3.0%에서 최대 30%까지 감소하는 것으로 나타났다. 실란/실록산계 발수제를 시멘트 모르타르에 첨가할 경우 접촉각은 커지는 것으로 나타났으며, 표면연마 후 접촉각은 표면연마 전보다 커지는 것으로 나타났다. 실란/실록산계 혼합형 발수제의 첨가는 표면뿐만 아니라 연마로 인하여 손상된 표면과 단면에서도 소수성을 나타내었다. 실란/실록산계 혼합형 발수제를 시멘트 모르타르에 첨가할 경우 흡수율은 낮아지는 것으로 나타났으며, 표면연마 후 흡수율은 표면연마 전보다 커지는 것으로 나타났다.

도정수율별 보리의 수화공정(水和工程)에 관(關)한 속도론적(速度論的) 연구(硏究) (A Kinetic Study on the Hydration Process of Barley Kernels with Various Polishing Yields)

  • 목철균;이현유;남영중;민병용
    • 한국식품과학회지
    • /
    • 제15권2호
    • /
    • pp.136-140
    • /
    • 1983
  • 도정수율별 보리의 수화특성(水和特性)을 $20{\sim}60^{\circ}C$ 범위에서 조사하고 속도론적으로 해석하였다. 흡수량(吸水量)은 수화시간(水和時間)의 평방근에 비례하였으며 흡수양상(吸水樣相)은 흡수량(吸水量) $0.45{\sim}0.55g\;H_2O/g$ solid 이후에서 변화하였다. 수화속도(水和速度)는 도정수율 50>70>95>90%>무도정맥의 순서였으며 수화온도(水和溫度)가 높을수록 증가하였다. 이 때 곡립내부(穀粒內部)로의 물의 확산도(擴散度)는 Arrhenius방정식에 의거하여 변화하였으며 활성화에너지는 도정맥의 경우 $6.9{\sim}9.5Kcal/mole$, 무도정맥의 경우 11.6Kcal/mole이었다.

  • PDF

A comparative study on the accuracies of resin denture bases and metal denture bases

  • Park Hwee-Woong;Kim Chang-Whe;Kim Yung-Soo
    • 대한치과보철학회지
    • /
    • 제39권3호
    • /
    • pp.250-259
    • /
    • 2001
  • Since the late 1930s, acrylic resins have been the materials of choice for the fabrication of complete denture bases. It has excellent esthetic properties, adequate strength, low water sorption, and low solubility. But acrylic resin has disadvantage of processing shrinkage that reduces denture retention and accuracy of denture occlusion. Metals also have been used in denture base material. Metals used in denture bases display excellent strength and dimensional stability. The major disadvantages associated with metal denture bases include increased cost, difficulty in fabrication, compromised esthetic qualities, and inability to re-base. The purpose of this study is to compare the artificial tooth movements of complete dentures with resin bases and metal bases after curing, deflasking, polishing immersion in water for 1 week and 4 weeks. Twenty-four maxillary complete resin denture bases with artificial teeth were fabricated. Twelve of them were resin based and other twelve of them were metal based. Fine crosses were marked on the incisal edges of right central incisors and distobuccal cusps of be second molars. Measurements were done for the changes of distances of reference points at the time of wax denture, after deflasking after decasting after polishing after immersion in water for 1 week and 4 weeks Meaurements were done to the accuracy of 0.001mm with a measuring microscope. The results were as follows : 1. Metal base showed significantly less tooth movement than resin base after curing and decasting (p<0.01). 2. Metal base showed significantly less tooth movement than resin base after polishing (p<0.01). 3. After immersion in water for 1 week and 4 weeks, metal base showed less movement than resin base. Difference was significant for anterior-posterior distances (p<0.01), but not significant for molar-to-molar distance (p>0.01). 4. 1 week and 4 weeks of immersion failed to compensate the initial processing shrinkage of metal and resin bases (p>0.01).

  • PDF

전.구치 겸용 혼합형 복합레진의 두 가지 연마법에 따른 표면조도 (SURFACE ROUGHNESS OF UNIVERSAL COMPOSITES AFTER POLISHING PROCEDURES)

  • 이재용;신동훈
    • Restorative Dentistry and Endodontics
    • /
    • 제28권5호
    • /
    • pp.369-377
    • /
    • 2003
  • The aim of this study was to evaluate the effect of two polishing methods and chemical conditioning on the surface of hybrid composites. Ninety cylindrical specimens (diameter:8mm, depth:2mm) were made with three hybrid composites-Filtek Z250, Tetric Ceram. DenFil. Specimens for each composite were randomly divided into three treatment subgroups $^{\circled1}$ Mylar strip (no treatment). $^{\circled2}$ Sof-Lex XT system, $^{\circled3}$ PoGo system. Average surface roughness(Ra) was taken using a surface profilometer at the time of setting and after immersion into 0.02N lactic acid for 1 week and 1 month. Representative specimens were examined by scanning electron microscopy. The data were analyzed using ANOVA and Scheffe's tests at 0.05% significance level. The results were as follows:1. Mylar strip resulted in smoother surface than PoGo and Sof-Lex system (p<0.001). Sof-Lex system gave the worst results. 2. Tetric Ceram was smoother than DenFil and Z250 when cured under only mylar strip. However, it was significantly rougher than other materials when polished with PoGo system. 3. All materials showed rough surface after storage in 0.02N lactic acid, except groups polished with a PoGo system. The PoGo system gave a superior polish than Sof-Lex system for the three composites. However. the correlation to clinical practice may be limited, since there are several processes. such as abrasive, fatigue, and corrosive mechanisms. Thus. further studies are needed for polishing technique under in vivo conditions.

보리의 저장기간과 도정도에 따른 취급특성 변이 (Cooking Quality of Barley as Influenced by Storage Period and Polishing Degree)

  • 이은섭;박문웅;이호진
    • 한국작물학회지
    • /
    • 제36권3호
    • /
    • pp.236-240
    • /
    • 1991
  • 적정수율과 저장기간이 보리의 취급특성에 미치는 영향을 구명하고자 도정비율을 50-70%가 되게 5수준으로 하고 취급시간을 40-80분간 5수준으로 처리하여 급수율과 퍼짐성을 조사한 결과와 저장기간 1년-8년까지된 시료로 Amylogram과 Textur-ometer로 Texture 특성을 조사한 결과를 보면 다음과 같다. 1. 모든 도정비율에서 급수율은 취급시간 40분과 50분사이에서 급격한 증가를 나타냈고, 그 이후에는 증가폭이 둔화되었고 도정비율이 낮을수록 수분흡수율은 증가되었다. 2. 퍼짐성은 흡수율과 유사한 경향을 나타내 밀접한 관련을 보였다. 3. 저장기간에 따른 흡수율과 퍼짐쌀을 50분 취급에서는 저장기간이 길수록 낮아지는 경향을 보였고, 백도는 저장기간과는 관련을 보이지 않았다. 4 Amylogram특성과 Texture특성은 저장년도에 따라 일정한 경향을 보이지 않는데 이는 생산년도가 달라 재배환경이 품질에 영향을 미친 것으로 사료된다.

  • PDF

치과기공실(齒科技工室)의 작업공정별(作業工程別) 소음(騷音)에 관한 연구(硏究) (A Study on the Noise by working Process in Dental Laboratory)

  • 남상용
    • 대한치과기공학회지
    • /
    • 제15권1호
    • /
    • pp.27-41
    • /
    • 1993
  • Degree of noise by personal dental laboratory working process and degree of noise by complex dental laboratory working process were measured separtely. The time of exposure to noise greater than 70dB was analyzed. Then, the whole degree of noise in dental laboratory was estimated on the basis of afore-mentioned information. Questionaire were employed to investigate the mental, emotional and physiological effects of noise in dental technicians, The purpose of this study was to provide basic information on keeping dental techneicans who are exposed to noise pollution in good working condition and good health. Results obtained are as follows ; 1. Polishing process in each working part showed high degree of noise greater than 70dB in terms of degree of noise by personal working. 2. Degree of noise by complex working process in each working part was greater than that of personal working process. 3. Time of exposure to noise complex working process the part of porcelain 150min, partial denture 120 min, crown and bridge 100 min, full denture 80 min. 4. Degree of noise by time in dental laboratory was 80dB in general for polishing process and below 75dB for waxing process. 5. Effects of noise on mental and emotional state of dental technicians showed that they felt irritated every day(14%), irritated once in a while(29%) and easily ger mad(19%). 6. Effects of noise on heart and stomach were hyper-gastric acid(38%), gastric ulcer(11%), gastritis(5%), deuodenal ulcer(3%) and weak heart function(32%). 7. Effects of noise in the hearing ability were weak(39%), moderate(33%) and normal(14%) Data presented in this study demonstrated that noise in the dental laboratory exerts profound effect on dental technicians mentally, physiologically and emotionally, in light of the above results, therefore, it appears advisable to devots substantial on the management of working condition and put further(continuing) efforts in the investigation for reducing noise problem.

  • PDF