• 제목/요약/키워드: Plastic Viscosity

검색결과 188건 처리시간 0.021초

폐플라스틱 필름의 액상 열분해 특성에 관한 연구 (Liquid-phase Thermal Degradation Properties of Waste Plastic Film)

  • 황택성;김영수;강태원;황의환
    • 한국자원리싸이클링학회:학술대회논문집
    • /
    • 한국자원리싸이클링학회 2003년도 추계정기총회 및 국제심포지엄
    • /
    • pp.116-121
    • /
    • 2003
  • In this study, the thermal degradation process has been investigated at various reaction temperature$(350{\sim}400^{\circ}C)$ and times$(30{\sim}120\;min)$ in order to recycle waste plastic films as solid state wax. Waste plastic films were easily melted by adding a small amount of waxes. The effects of wax addition and nitrogen flow rate on their thermal degradation properties were investigated. FT-IR, GPC and viscometer were used to analyze properties of the solid wax including the structure, molicular weight distribution and melt viscosity. The average molecular weight of solid wax was decreased with increasing the reaction time, temperature and amount of wax added, Also, the viscosity of solid wax decreased with increasing the stirring speed at a constant reaction temperature and time, and its viscosity got close to zero above $390^{\circ}C$.

  • PDF

혼화재료를 치환한 시멘트 계열 재료에 대한 저점도형 고성능 감수제의 유동 성능 평가 (Fluidity Performance Evaluation of Low Viscosity Typed Superplasticizer for Cement-Based Materials Incorporating Supplementary Cementitious Materials)

  • 손배근;이향선;이유정;한동엽
    • 한국건축시공학회지
    • /
    • 제19권3호
    • /
    • pp.219-228
    • /
    • 2019
  • 본 연구의 목적은 저점도형 고성능 감수제가 혼화재료를 포함하는 시멘트 계열 재료의 유동성 및 레올로지 특성에 미치는 영향을 분석하여 기초적인 정보를 제공하는 것이다. 이에 플라이애시, 고로슬래그, 실리카흄을 치환한 시멘트 페이스트와 모르타르에 대하여 일반적인 고성능 감수제와 저점도형 고성능 감수제를 사용하여 실험을 실시하였다. 실험 결과 저점도형 고성능 감수제는 소성점도에 있어서 일반형 고성능 감수제보다 크게 저감시키는 것으로 나타났다. 이러한 결과를 바탕으로 본 연구가 향후 저점도형 고성능 감수제를 사용하는 데에 기초적인 데이터를 제공할 것으로 기대한다.

배합요인이 자기충전 콘크리트의 워커빌리티 및 레올로지 파라미터에 미치는 영향 분석 (Effect Analysis of Mix Designing Factors on Workability and Rheological Parameters of Self-Compacting Concrete)

  • 윤섭;한민철
    • 한국건축시공학회지
    • /
    • 제18권3호
    • /
    • pp.235-242
    • /
    • 2018
  • 본 연구에서는 SCC의 높은 민감성으로 인한 품질관리에 어려움을 극복하고자 굵은 골재의 부피, 잔골재의 종류, 단위수량, 공기량, 증점제 사용량 변화 등과 같은 다양한 배합요인이 SCC 특성에 미치는 영향을 분석하여 SCC의 초기물성을 정량적으로 판단할 수 있는 기초자료를 제공하고자 하였다. 실험결과, 항복응력은 굵은 골재 용적율이 증가할수록 낮아졌고 증점제 사용량이 증가할수록 증가하는 것으로 나타났다. 그러나 단위수량, 잔골재 종류 변화, 공기량 증감에 따른 항복응력값의 변화는 없는 것으로 나타났다. 배합요인에 따른 소성 점도는 항복응력과 비슷한 경향을 나타냈다. 또한 항복응력과 슬럼프 플로, $T_{50}$, V-lot와의 상관성 분석결과, 상관관계가 없었고 소성 점도와 $T_{50}$, V-lot와의 상관성은 매우 밀접한 관계가 있는 것으로 나타났는데, 특히, $T_{50}$ 및 V-lot 시간이 줄어들수록 소성 점도도 낮아지는 것을 알 수 있었다.

제산제 알루미나수화물의 콜로이드성과 제산능 (Collodial Properties and Acid Consuming Capacity of Hydrous Aluminum Oxide Suspension)

  • 이계주;이기명
    • 약학회지
    • /
    • 제35권4호
    • /
    • pp.277-282
    • /
    • 1991
  • Rheological, colloidal and micromeritical properties were followed to investigate aging mechanisms of hydrous aluminum oxide suspension using Zeta-meter systems, BET adsorption apparatus, Master sizer and electronmicroscope. The results indicate that hydrous aluminum oxide suspension revealed plastic flow with thixotropy. The viscosity, thixotropy and yield value were increased with increasing concentration. During aging process, the viscosity and thixotropic index were increased by an addition of glycerin, however, sorbitol stabilized aging process of the suspension being accompanied with growth of particle size and reduction in specific surface area, pore area and pore volume, and consistency. Diminution of adsorptive power of the particles was also protected by addition of sorbitol to hydrous aluminum oxide suspension. From these results, one of aging mechanism of hydrous aluminum oxide suspension assumed growth and/or crystallization of colloidal particles in aqueous suspension.

  • PDF

토석류 이동의 레올로지적 특성 (Rheological Characteristics of Debris Flows)

  • 김상규;서홍석
    • 한국지반공학회지:지반
    • /
    • 제13권5호
    • /
    • pp.125-132
    • /
    • 1997
  • 토석류는 다양한 크기의 흙 입자와 물이 고루 섞여 점성을 가진 유체처럼 하방향으로 이동한다는 사실이 관찰되었다. 이 관찰로부터 토석류를 비선행적인 점도를 가진 비뉴톤 유체처럼 거동하는 것으로 간주할 수 있다. 이 논문에서는 토석류의 레올로지적 특성을 규명하기 위해 산사태 현장에서 채취한 시료를 가지고 점도계를 사용하여 일련의 점도시험을 수행하였다. 그 결과, 토석류는 비뉴톤 유체 중 빙함 소성 모델로 거동한다는 사실이 밝혀졌다. 이 모델을 이용하면 토 석류의 이동을 예측할 수 있다.

  • PDF

고로슬래그 미분말을 함유한 고유동 모르터의 유동성상에 미치는 영향 요인에 관한 연구 (A Study on the Factors Affecting the High Fluid Mortar Containing Ground Granulated Blast-furnace Slag)

  • 김재훈;윤상천;지남용
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2002년도 학술.기술논문발표회
    • /
    • pp.29-36
    • /
    • 2002
  • High fluid concrete unlike OPC concrete is made with various material, and the phase of fresh concrete is considerably different. In order to understand fluidity phase and mix properties of high fluid concrete, concrete is required to access as suspension structure which consists of aggregate and paste. The focus of this paper is to analyze the test results and quantify the effect of mix proportions of molar and fineness modulus of ,and on the properties of fresh mortar. The effect of water-binder ratio, sand-binder ration, content; of ggbs (by mass of total cementitious materials), and various contents of water reducing agent on the yield stress and plastic viscosity of the mix is studied. Based on the experimental results, the following conclusion; can be drawn: (1) The mixing time needed (or high fluid mortar was approximately two times more than that of ordinary portland mortar. (2) The fluidity phase of mortar could be explained by yield stress of mix and the fluidity of mortar. (3) As the content of ggbs increased, yield stress of mortar was decreased and plastic viscosity of it was increased. (4) For the high fluid mortar, it was appeared that sand-binder ratio should be below 1.5.

  • PDF

초미분말 고로슬래그를 혼합한 시멘트 페이스트의 유동특성 (Rheological Properties of Cement Paste Containing Ultrafine Blastfurnace Slag)

  • 유창달;변승호;송종택
    • 한국세라믹학회지
    • /
    • 제44권8호
    • /
    • pp.430-436
    • /
    • 2007
  • Rheological properties of cement paste containing ultrafine blastfurnace slag (UBS, $9600cm^2/g$) were investigated by mini-slump test, pH meter, conduction calorimeter and coaxial cylinder viscometer. In order to improve rheological properties of the cement paste, granulated blastfurnace slag (GBS, $3500cm^2/g$) and polycarboxylate type superplasticizer (PC) were also used in this experiment. The fluidity of cement paste containing UBS was decreased. The yield stress and plastic viscosity of cement paste was increased with increasing UBS. But the rheological properties were improved when GBS and PC were added to UBS blended cement paste. In the relationship between the yield stress and the plastic viscosity or the mini-slump value, the yield stress of the cement paste was proportional to the plastic viscosity of it. However the cement paste mini-slump value was in inverse proportional to the yield stress.

점성을 고려한 PBD 타설 연약점토지반의 3차원 압밀해석 (3-Dimensional Consolidation Analysis Considering Viscosity on Soft Clay Ground improved by Plastic Board Drain)

  • 유승경;한중근;조성민;김지용
    • 한국지반신소재학회논문집
    • /
    • 제4권4호
    • /
    • pp.39-46
    • /
    • 2005
  • 점성을 고려한 연약점토지반의 압밀거동을 파악하기 위해 플라스틱보드드레인(PBD)에 의해 개량된 연약점토지반의 압밀거동에 대한 탄점소성 3차원 수치해석을 실시하였다. 본 연구에서 사용한 수치해석기법의 적용성은 기존에 실시한 모형실험의 결과와 수치해석의 결과를 비교함으로써 검증하였다. 수치해석 결과로부터 연약점토지반의 침하 및 과잉간극수압의 소산거동, 유효응력증분의 변화 특성을 파악할 수 있었으며, 기존의 일차원 압밀해석 결과와의 비교를 통해 개량지반에서 발생하는 이차압밀특성을 평가하였다.

  • PDF

고로슬래그 및 플라이 애시 분말을 혼합한 시멘트 페이스트의 유동특성 (Rheological Properties of Cement Paste Blended Blast Furnace Slag or Fly Ash Powder)

  • 송종택;박효상;변승호;유동우
    • 한국세라믹학회지
    • /
    • 제45권6호
    • /
    • pp.336-344
    • /
    • 2008
  • Rheological properties of cement pastes containing blast furnace slag (BFS: 3,900, $7,910\;cm^2/g$) or fly ash powder (FA: 4,120, $8,100\;cm^2/g$) according to the ratio of water/binder (W/B) and the dosage of polycarboxylate type superplasticizer (PC) were investigated by a mini slump and a coaxial cylinder viscometer. In this experiment, the ratio of replacing OPC with BFS or FA was 30 wt%, the W/B was from 30 to 70 wt%. As a result, the fluidity of cement paste containing BFS or FA was improved with increasing W/B and the dosage of PC. BFS or FA replaced cement paste with W/B 70% and PC 0.3% showed the highest fluidity. The segregation range of cement paste was occurred below $10\;d/cm^2$ of the yield stress and below 50 cPs of the plastic viscosity by the coaxial cylinder viscometer. And also it was formed that the plastic viscosity and the yield stress of FA replaced cement paste were higher than them of BFS replaced cement paste.

저점도형 감수제의 성능 분석 (Performance Analysis of Low-viscosity type Superplasticizer)

  • 한동엽
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 추계 학술논문 발표대회
    • /
    • pp.35-36
    • /
    • 2016
  • Recently, with the increasing demand of high performance of concrete, the mix design of concrete mixture has became low water-to-binder ratio with high binder content. To compensate these trend of mix design, high range water reducer, or superplascizier has been invented to achieve high flowable concrete. Although this superplasticizer provides favorable workability based on its dispersing action on the components of concrete mixture, it has an limitation of decreasing viscosity of the mixture, and thus it is difficult to secure sufficient workability for high performance concrete mixtures with high binder content. To improve the workability of concrete with high viscosity, recently, low-viscosity type superplasticizer was introduced, and in this research, a fundamental properties of low-viscosity type superplasticizer is evaluated.

  • PDF