• Title/Summary/Keyword: Photocatalytic film

Search Result 105, Processing Time 0.024 seconds

Synthesis and characterization Au doped TiO2 film for photocatalytic function

  • Son, Jeong-Hun;Bae, Byung-Seo;Bae, Dong-Sik
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.25 no.6
    • /
    • pp.280-284
    • /
    • 2015
  • Au doped $TiO_2$ nanoparticles have been synthesized using a reverse micelle technique combined with metal alkoxide hydrolysis and condensation. Au doped $TiO_2$ was coated with glass substrate. The size of the particles and thickness of the coating can be controlled by manipulating the relative rates of the hydrolysis and condensation reaction of TTIP within the micro-emulsion. The average size of synthesized Au doped $TiO_2$ nanoparticle was about in the size range of 15 to 25 nm and the Au particles formed mainly the range of 2 to 10 nm in diameter. The effect of synthesis parameters, such as the molar ratio of water to TTIP and the molar ratio of water to surfactant, are discussed. The synthesized nanopaticles were coated on glass substrate by a spin coating process. The thickness of thin film was about 80 nm. The degradation of MB on a $TiO_2$ thin film was enhanced over 20 % efficiency by the incorporation of Au.

A Study on the Photon Energy Characteristics of Photocatalytic $TiO_2$ Ferroelectrics Thin Film According to Coating Thickness (광촉매용 $TiO_2$ 강유전체 박막의 증착 두께에 따른 Photon Energy 특성에 관한 연구)

  • 김병인;전인주;이상일
    • Proceedings of the Korean Institute of IIIuminating and Electrical Installation Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.329-334
    • /
    • 2002
  • This study evaporates TiO$_2$ layer thickness differently with RF sputtering method on Si Wafer(n-100). Thin film is made with the structure of Si+TiO$_2$ and Si+TiO$_2$+Al by evaporating TiN which is used as Antireflection of superintegrated semiconductor integrated circuit with Photo Catalyst. The research is performed to increase the characteristics of photon energy according to TiO$_2$ thickness and the reliability and reproducibility of TiO$_2$ thin film. Reversal of electric Permittivity values is induced by dipole polarization shown in the dielectric of thin film. Complex electric constant ($\varepsilon$$_1$, $\varepsilon$$_2$) has larger peak values as it's thickness is thinner and then it is larger according to the increase of frequency. Electric Permittivity by photon energy has large value in imaginary number and is reduced exponentially by the increase of carrier density according to that of photon energy.

  • PDF

PHOTOCATALYTIC ANTIEUNGAL ACTIVITY AGAINST CANDIDA ALBICANS BY $TiO_2$ COATED ACRYLIC RESIN DENTURE BASE

  • Yang Ji-Yeon;Kim Hee-Jung;Chung Chae-Heon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.44 no.3
    • /
    • pp.284-294
    • /
    • 2006
  • Statement of problem. Proliferation of Candida albicans is primarily within the plaque on the fitting surface of the denture rather than on the inflamed mucosa. Consequently, the treatment of the denture is equally important as treatment of the tissue. Cleansing and disinfection should be efficiently carried-out as the organisms can penetrate into the voids of the acrylic resin and grow in them, from which they can continue to infect and reinfect bearing tissues. Purpose. The purpose of this study was to evaluate the applicability of photocatalytic reaction to eliminate Candida albicans from acrylic resin denture base, and to investigate the anti-fungal effect with various UVA illumination time. Materials and Methods. The specimens were cured by the conventional method following the manufacturer's instruction using thermal polymerized denture base resin (Vertex RS: Dentimex, Netherlands). $TiO_2$ photocatalyst sol(LT), which is able to be coated at normal temperature, was made from the Ti-alkoxide progenitor. The XRD patterns, TEM images and nitrogen absorption ability of the $TiO_2$ photocatalyst sol(LT) were compared with the commercial $TiO_2$ photocatalyst P-25. The experimental specimens were coated with the mixture of the $TiO_2$ photocatalyst sol(LT) and binder material (silane) using dip-coater, and uncoated resin plates were used as the control group. Crystallinity of $TiO_2$ of the specimen was tested by the XRD. Size, shape and chemical compositions were also analyzed using the FE-SEM/ EDS. The angle and methylene blue degradation efsciency were measured for evaluating the photocatalytic activity of the $TiO_2$ film. Finally, the antifungal activity of the specimen was tested. Candida albicans KCTC 7629(1 ml, initial concentration $10^5$ cells/ ml) were applied to the experiment and control group specimens and subsequently two UVA light source with 10W, 353 nm peak emission were illuminated to the specimens from 15cm above. The extracted $2{\mu}l$ of sample was plated on nutrient agar plate ($Bacto^{TM}$ Brain Heart Infusion; BD, USA) with 10 minute intervals for 120 minute, respectively. It was incubated for 24 hours at $37^{\circ}C$ and the colony forming units (CFUs) were then counted. Results. Compared the characteristics of LT photocatalyst with commercial P-25 photocatalyst, LT were shown higher activity than P-25. The LT coated experimental specimen surface had anatase crystal form, less than 20 nm of particle size and wide specific surface area. To evaluate the photocatalytic activity of specimens, methylene blue degradation reaction were used and about 5% of degradation rate were measured after 2 hours. The average contact angle was less than $20^{\circ}$ indicating that the LT photocatalyst had hydrophilicity. In the antifungal activity test for Candida albicans, 0% survival rate were measured within 30 minute after irradiation of UVA light. Conclusion. From the results reported above, it is concluded that the UVA-LT photocatalytic reaction have an antifungal effect on the denture surface Candida albicans, and so that could be applicable to the clinical use as a cleaning method.

Preparation of nanocrystalline $TiO_2$ photocatalyst films by using a titanium naphthenate (티타늄 나프테네이트를 이용한 나노결정질 $TiO_2$ 광촉매 박막의 제조)

  • 이선옥;김상복;윤연흠;강보안;황규석;오정선;양순호;김병훈
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.12 no.5
    • /
    • pp.240-246
    • /
    • 2002
  • $TiO_2$ films on soda-lime-silica glasses were prepared by spin coating-pyrolysis process using titanium naphthenate as a starting material. As-deposited films were pyrolyzed at $500^{\circ}C$ for 10 min in air and annealed at 500, 550 and $600^{\circ}C$ for 30 min in air. Crystallinity of the film was investigated by X-ray diffraction analysis. A field emission-scanning electron microscope and an atomic force microscope were used for characterizing the surface morphology and the surface roughness of the film. After annealing at 550 and $600^{\circ}C$, the X-ray diffraction patterns consist of only anatase peak. Films annealed at 500 and $550^{\circ}C$ exhibited flat surfaces. While with the increase in annealing temperature to $600^{\circ}C$, the $TiO_2$ film showed abnormal growth of three-dimensional needle-shaped grains. For all samples, high transmittance, above 90 % at 500 nm, was obtained at visible range. To investigate photocatalytic properties, IR absorbance associated with the C-H stretching vibrations of a thin solution-cast film of stearic acid under 365 nm (2.4 mW/$\textrm{cm}^2$) UV irradiation was estimated.

Fabrication of super hydrophilic TiO2 thin film by a liquid phase deposition (액상증착법에 의한 초친수 TiO2 박막 제조)

  • Jung, Hyun-Ho;Kim, Jin-Ho;Hwang, Jong-Hee;Lim, Tae-Young;Choi, Duk-Gun
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.20 no.5
    • /
    • pp.227-231
    • /
    • 2010
  • Super hydrophilic $TiO_2$ thin films with photocatalytic property were successfully fabricated on a glass substrate by liquid phase deposition (LPD). The $TiO_2$ thin film formed nano particles on a surface at $70^{\circ}C$. As an immersion time in $TiF_4$ solution increased, the thickness of thin films gradually increased. $TiO_2$ thin film showed a water contact angel of below ca. $5^{\circ}$ and the transmittance of ca. 75~90 % in visible range. In addition, $TiO_2$ thin film showed the photocatalytic property to decompose methyl orange solution by the illumination of UV light. The surface morphologies, optical properties and contact angel of prepared thin films with a different immersion time were measured by field emission scanning electron microscope (FE-SEM), atomic force microscope (AFM), UV-Vis spectrophotometer and contact angle meter.

Fabrication of Photocatalyst Glass Beads Coated with TiO2 Thin Film by a Layer-by-Layer Process (LBL법에 의해 TiO2막이 코팅된 광촉매 글라스 비드 제조)

  • Lee, Ji-Sun;Chae, Yoo-Jin;Lee, Mi-Jai;Kim, Sei-Ki;Hwang, Jong-Hee;Lim, Tae-Young;Hyun, Soong-Keun;Kim, Jin-Ho
    • Korean Journal of Materials Research
    • /
    • v.22 no.7
    • /
    • pp.379-383
    • /
    • 2012
  • $TiO_2$ thin films consisting of positively charged poly(diallyldimethylammonium chloride)(PDDA) and negatively charged titanium(IV) bis(ammonium lactato) dihydroxide(TALH) were successfully fabricated on glass beads by a layer-by-layer(LBL) self-assembly method. The glass beads used here showed a positive charge in an acid range and negative charge in an alkaline range. The glass beads coated with the coating sequence of(PDDA/TALH)n showed a change in the surface morphology as a function of the number of bilayers. When the number of bilayers(n) of the(PDDA/TALH) thin film was 20, Ti element was observed on the surface of the coated glass beads. The thin films coated onto the glass beads had a main peak of the (101) crystal face and were highly crystallized with XRD diffraction peaks of anatase-type $TiO_2$ according to an XRD analysis. In addition, the $TiO_2$ thin films showed photocatalytic properties such that they could decompose a methyl orange solution under illumination with UV light. As the number of bilayers of the(PDDA/TALH) thin film increased, the photocatalytic property of the $TiO_2$-coated glass beads increased with the increase in the thin film thickness. The surface morphologies and optical properties of glass beads coated with $TiO_2$ thin films with different coating numbers were measured by field emission scanning electron microscopy(FE-SEM), X-ray diffraction(XRD) and by UV-Vis spectrophotometry(UV-vis).

Thin Films for Environmental Application and Energy Devices

  • Kim, Young-Dok
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.91-91
    • /
    • 2012
  • We aim in synthesizing various functional thin films thinner than ~ 10 nm for environmental applications and photovoltaic devices. Atomic layer deposition is used for synthesizing inorganic thin films with a precise control of the film thickness. Several examples about application of our thin films for removing volatile organic compounds (VOC) will be highlighted, which are summarized in the below. 1) $TiO_2$ thin films prepared by ALD at low temperature ($<100^{\circ}C$) show high adsorption capacity for toluene. In combination with nanostructured templates, $TiO_2$ thin films can be used as building-block of high-performing VOC filter. 2) $TiO_2$ thin films on carbon fibers and nanodiamonds annealed at high temperatures are active for photocatalytic oxidation of VOCs, i.e. photocatalytic filter can be created by atomic layer deposition. 3) NiO can catalyze oxidation of toluene to $CO_2$ and $H_2O$ at $<300^{\circ}C$. $TiO_2$ thin films on NiO can reduce poisoning of NiO surfaces by reaction intermediates below $200^{\circ}C$. We also fabricated inverted organic solar cell based on ZnO electron collecting layers on ITO. $TiO_2$ thin films with a mean diameter less than 3 nm on ZnO can enhance photovoltaic performance by reducing electron-hole recombination on ZnO surfaces.

  • PDF

Research Trends on Chemical Mechanical Polishing Using Ultraviolet Light (자외선 광을 활용하는 화학기계적 연마에 관한 연구 동향)

  • Lee, Hyunseop
    • Tribology and Lubricants
    • /
    • v.38 no.6
    • /
    • pp.247-254
    • /
    • 2022
  • Chemical mechanical polishing (CMP) is a hybrid surface-polishing process that utilizes both mechanical and chemical energy. However, the recently emerging semiconductor substrate and thin film materials are challenging to process using the existing CMP. Therefore, previous researchers have conducted studies to increase the material removal rate (MRR) of CMP. Most materials studied to improve MRR have high hardness and chemical stability. Methods for enhancing the material removal efficiency of CMP include additional provision of electric, thermal, light, mechanical, and chemical energies. This study aims to introduce research trends on CMP using ultraviolet (UV) light to these methods to improve the material removal efficiency of CMP. This method, photocatalysis-assisted chemical mechanical polishing (PCMP), utilizes photocatalytic oxidation using UV light. In this study, the target materials of the PCMP application include SiC, GaN, GaAs, and Ru. This study explains the photocatalytic reaction, which is the basic principle of PCMP, and reviews studies on PCMP according to materials. Additionally, the researchers classified the PCMP system used in existing studies and presented the course for further investigation of PCMP. This study aims to aid in understanding PCMP and set the direction of future research. Lastly, since there have not been many studies on the tribology characteristics in PCMP, research on this is expected to be required.

Performance assessment of {tris (2-methyl-1-aziridinyl) phosphine oxide} photocatalytic mineralization in a falling film reactor, using response surface methodology

  • Saien, J.;Raeisi, A.;Soleymani, A.R.;Norouzi, M.
    • Advances in environmental research
    • /
    • v.1 no.4
    • /
    • pp.289-304
    • /
    • 2012
  • Tris (2-methyl-1-aziridinyl) phosphine oxide (MAPO) is extremely poisonous and persistent in aqueous media. An efficient UV/nano$TiO_2$ process was employed for its mineralization in a high duty falling film photo-reactor based on an experimental design scheme that considers interactions between the main variables. The influencing variables and their range were determined with preliminary studies. The results show substrate mineralization to some extent under mild conditions of: T = $30^{\circ}C$, pH = 8.5, $[MAPO]_0=60\;mg\;L^{-1}$ and $[TiO_2]=110\;mg\;L^{-1}$. The relative importance of the influencing parameters were initial pH > temperature > $[MAPO]_0$ > [$TiO_2$]; while the interdependence of all the parameters was significant. Accordingly, a reduced quadratic expression was developed. Meanwhile, mineralization kinetic studies, based on chemical oxygen demand, revealed a power law model with order of 2.6 during process time until 150 min.

Structural and Photocatalytic Properties of TiO2 Thin Film Coated Glass Beads (유리알에 코팅된 TiO2 박막의 구조 및 광촉매 특성)

  • Ji Eun, Jeong;Chang-Yong, Lee
    • Applied Chemistry for Engineering
    • /
    • v.34 no.1
    • /
    • pp.30-35
    • /
    • 2023
  • The glass bead surface was coated using a TiO2 sol, after which dry-treated (TB) and calcined (TBc) samples were prepared. Photocatalytic degradation of methylene blue and toluene, as well as characterization of the TiO2 thin films, were carried out. The TiO2 thin film of the TB sample had the same shape as the sponge foam, according to FE-SEM, XPS, and FTIR analyses, and contained both amorphous and crystalline TiO2. On the other hand, crystalline TiO2 was mainly present in the TiO2 thin film of the TBc sample, and needle-shaped particles and tiny ones were mixed. The adsorption capacity for methylene blue and the degradation rate of the TBc sample were less than 10 % compared with those of the TB sample, and the adsorption capacity and degradation rate of the TBc sample decreased similarly as the amount of TiO2 coating increased. The amount of toluene adsorption for the TBc sample (46 mg/g) was smaller than that of the TB sample with the same coating amount, but the degradation rate was similar. In the case of the TB sample, the degradation rate for toluene decreased less than the adsorption capacity as the amount of TiO2 coating increased. This result is considered to be because, in the non-calcined TB sample, the active site reduction of the crystalline particles occurred less and the specific surface area of the amorphous texture decreased as the amount of TiO2 coating increased.