• Title/Summary/Keyword: PZI

Search Result 13, Processing Time 0.027 seconds

Dynamic Analysis of Tip-actuators for Controlling Tip-media Gap in Cantilever Type Optical Data Storage (캔틸레버형 광 정보저장에서의 빠른 팁/매체 간극제어를 위한 팁/구동기의 동역학적 분석)

  • 이성규;송기봉;김준호;김은경;박강호;남효진;이선영;김영식
    • Proceedings of the Korean Society for Noise and Vibration Engineering Conference
    • /
    • 2003.05a
    • /
    • pp.1004-1008
    • /
    • 2003
  • Near-filed optical storage using cantilever aperture tip is a promising way fer next generation optical data storage. To enhance the speed of reading and writing data, gap between tip and media should be controlled fast and precisely within near field region. In this paper, several PZT actuators are analyzed far constructing dual servo control algorithm: coarse actuators(stact. PZT, bimorph PZI) for media surface inclination and One actuator(film PZT) for media surface roughness. Dynamic analysis of stack PZT, bimorph PZT, and film PZT are performed through the frequency response. Based on the frequency response and mathematical model, fast analog controller is designed.

  • PDF

Piezoelectric and Acoustic Properties of PZI-Polymer 1 -3-0 Type Composite (PZT-고분자 1-3-0형 복합압전체의 압전 및 음향특성)

  • 양윤석;유영준;최헌일;손무헌;사공건
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.317-320
    • /
    • 1999
  • In this study, the piezoelectric ceramics PZT powder was synthesized by Wet-Dry combination method. And the flexible 1-3-0 type composites were fabricated with piezoceramic PZT and Eccogel polymer matrix embedded 3rd phase. Dielectric constant of 1-3-0 type composites was lower than that of single phase PZT ceramics. Thickness mode coupling factor k/sub t/ which was comparable with single phase PZT ceramics and mechanical quality factor Qm were about 0.65 and 6, respectively. These composites are considered as a good candidates for broad-band type transducer applications. The acoustic impedance of 1-3-0 type composites was lower than that of single phase PZT ceramics. Therefore, these composites would be better used for hydrophone applications.

  • PDF

Preparation of PZI Tapes by Solvent Washing Dry Method (용매세척건조법에 의한 PZT 테입 제조)

  • 신효순;윤석진;김현재
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.300-303
    • /
    • 1999
  • For the fast dry of the aqueous tape, the process which water was replaced by organic solvent was proposed. So-called, it was the solvent washing dry, Three organic solvents (methanol, ethanol, and acetone) were selected for the washing solvent. The weight loss of the washed tapes was measured to evaluate the dry rate of the tapes and dried tapes were examined the generation of the cracks with the variations of the organic solvent and the washing time. Methanol, ethanol, and acetone were all available organic solvents for this method. The tapes washed in methanol, ethanol, and acetone were dried rapidly for twenty minutes. After thirty minutes, the weight losses were not any more. The solvent of the lower surface tension can decreases the crack of dried tape. If solvent substitutes water completely, though it was fast dried, crack can be eliminated. The tape casting system was designed for the solvent washing dry and prepared. An homogeneous tape was established by continuous tape casting process.

  • PDF

Piezoelectric and dielectric properties of PMN-PZI ceramics will PNN substitution (PNN 치환에 따른 PMN-PZT 세라믹스의 유전 및 압전 특성)

  • 황상모;이정선;윤광희;류주현;정회승
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.434-437
    • /
    • 2001
  • In this study piezoelectric and dielectric properties of Pb(Mn$\sub$1/3/Nb$\sub$2/3/)O$_3$-Pb(Zr,Ti)O$_3$ ceramics were investigated with Pb(Ni$\sub$1/3/Nb$\sub$2/3/)O$_3$ substitution. As the Pb(Ni$\sub$1/3/Nb$\sub$2/3/)O$_3$) substitution was increased, dielectric constant and electromechanical coupling factor (kp) were increased while mechanical quality factor decreased.

  • PDF

Characteristics of PAN-PZI Ceramics with $BaCO_3$Addition ($BaCO_3$ 첨가량에 따른 PAN-PZT계 세라믹스의 특성)

  • 박타리;이동균;최지원;김현재;윤석진;조봉희;고태국
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.981-984
    • /
    • 2001
  • The piezoelectric properties of 0.05pb(A $l_{0.5}$N $b_{0.5}$) $O_3$-0.95Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$+0.7wt%N $b_2$ $O_{5}$ +0.5wt%Mn $O_2$ceramics with the additives of BaC $O_3$were investigated. For the additions of BaC $O_3$, the dielectric constant ($\varepsilon$$^{T}$ $_{33}$ ), the piezoelectric constant ( $d_{33}$ ), the electromechanical coupling factor ( $k_{p}$ ), and . the mechanical quality factor ( $Q_{m}$ ) were increased, but dielectric loss (tan$\delta$) was decreased. The highest piezoelectric properties and dielectric properties were observed at the sintered temperature of 120$0^{\circ}C$ and 0.4 wt% of BaC $O_3$, and the properties of $d_{33}$ , $k_{p}$ , and $Q_{m}$ were 339(x10$^{-12}$ C/N), 59% and 1754, respectively.vely.y.y.

  • PDF

A Study on Dielectric Properties of PMN-PSS-PZI ceramics with Ni, Mn (Ni, Mn가 첨가된 PMN-PSS-PZT 세라믹스의 유전 특성에 관한 연구)

  • Shin, Hyea-Kyoung;Kim, Hyun-Chul;Soung, Nak-Jin;Bae, Seon-Gi
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.764-767
    • /
    • 2004
  • This study was to measure the minuteness structure, dielectric properties of (0.3-x)PMN - XPSS-0.7PZT+0.5wt%NiO+0.5wt%$MnO_2$(x=0.05, 0.10, 0.15, 0.20, 0.25)ceramics according to sintering temperature and PSS moi percentage after manufacturing the specimens with a general method. the results of this study were gotten such as follows. The crystal structure of ceramic has the rombohedral structure in XRD. it appeared that addition of Ni, Mn additive was helpful to the formation of stable structure. Dielectric constant at $20^{\circ}C$ showed its maximum value 890.001 in specimens sintered at $1000^{\circ}C$, x=0.15mol. and dielectric loss showed its minimum value 6.95[%] in specimens sintered at $1000^{\circ}$, x=0.05mol. The variation rate of dielectric constant according to the change of frequency was decreased by increasing frequency, The variation rate of dielectric constant according to the change of temperature was increased by increasing temperature.

  • PDF

Properties of PZI Thin film on the Ru/RuO2 Electrode (Ru/RuO2전극에 성장한 PZT 박막의 특성에 관한 연구)

  • Kang, Hyun-Il;Choi, Jang-Hyun;Park, Young;Song, Joon-Tae
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.10
    • /
    • pp.865-869
    • /
    • 2002
  • The structural and electrical properties of PZT (lead zirconate titante) thin films grown on Pt (platinum) and Ru/Ru $O_2$(ruthenium/ruthenium oxide) electrodes were investigated. Thin films of PZT were deposited on a variety of electrodes using the rf-magnetron sputtering process. PZT films exhibited polycrystalline structure with strong PZT (100) plane and weak (211) plane for an optimizied Pt electrode and (100), (101), (111), (200), (210), (211) planes for Ru/Ru $O_2$. Switching polarization versus fatigue characteristic of Pt/Ti electrodes showed 20% degradation up to 1 $\times$ 10$_{9}$ cycles. No significant fatigue was observed in the films on Ru/Ru $O_2$ electrodes up to Ix109 test cycles. The results show that the new Ru/Ru $O_2$ bottom electrodes are expected to reduce the degradation of ferroelectric fatigue.

Dielectric and Piezoelectric Properties of Low Temperature Sintering PSN-PZI Ceramics with BiFe3 Substitution (BiFe3첨가에 따른 저온소결 PSN-PZT세라믹스의 유전 및 압전 특성)

  • 류주현;정광현;정영호
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.5
    • /
    • pp.492-496
    • /
    • 2004
  • In this study, (0.96 -x)(PSN-PZT)-xBF-0.04 PNW+0.3wt%MnO$_2$+0.6wt%CuO ceramics were fabricated with the variations of the amount of BiFeO$_3$substitution and sintering temperature for the development of modified ceramics which can be sintered in the low temperature($\leq$100$0^{\circ}C$ ), and their microstructural, dielectric and piezoelectric characteristics were investigated. As the amount of BiFeO$_3$ substitution was increased, the density, mechanical quality factor(Q$_{m}$) and electromechanical coupling factor(k$_{p}$) showed the maximum value at each of sintering temperature. At sintering temperature of 98$0^{\circ}C$ and BiFeO$_3$substitution of 2 mol%, the density, dielectric constant and electromechanical coupling factor(k$_{p}$) showed the maximum value of 7.84 g/㎤, 1415 and 0.49, respectively. And at sintering temperature of 95$0^{\circ}C$ and BiFeO$_3$substitution of 3mol%, mechanical quality factor showed the maximum value of 1062. 1062.

Ferroelectric Properties of PZT Thin Films by RF-Magnetron sputtering (RF 마그네트론 스퍼터링 법을 이용한 PZT 박막의 강유전 특성)

  • Park, Young;Joo, Pil-Yeoun;Yi, Ju-Sin;Song, Jun-Tae
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.341-344
    • /
    • 1999
  • The effects of post annealing treatments of ferroelectrlclty in PZT(P $b_{1.05}$(Z $r_{0.52}$, $Ti_{0.48}$) $O_3$ thin film deposited on Pt/ $SiO_2$/Si substrate by RF-Magnetron sputtering methode was Investigated. Analyses by RTA(Rapid Thermal Annealing) treatments reveled that the crystallization process strongly depend on the healing temperature. The Perovskite structure with strong PZT (101) plan was obtained by RTA treatments at 75$0^{\circ}C$ With increasing RTA temperature of PZI thin films, the coercive field and remanent Polarization decreased, while saturation polarization( $P_{r}$) was decreased. P-E curves of Pt/PZT/Pt capacitor structures demonstrate typical hysteresiss loops. The measure values of $P_{r}$,. $E_{c}$ and dielectric constants by post annealed at 75$0^{\circ}C$ were 38 $\mu$C/$\textrm{cm}^2$ 35KV/cm and 974, respectively. Switching polarization versus fatigue characteristic showed 12% degradation up to 10$^{7}$ cycles.s.s.s.s.s.s.

  • PDF

A Study on the Electrical properties of PSN-PMN-PZI system ceramics modified With $Y_2O_3$and $Fe_2O_3$ ($Y_2O_3$$Fe_2O_3$ 첨가에 따른 PSN-PMN-PZT 세라믹스의 전기적 특성에 따른 연구)

  • 민석규;황상모;이용우;류주현;김종선
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.269-272
    • /
    • 1999
  • In this study, electrical properties and TCFr of Pb(Sb$_{1}$2/Nb$_{1}$2/)O$_3$-Pb(Mn $_{1}$3/Nb$_{2}$3/)O$_3$-Pb(zr, Ti)O$_3$ composition ceramics were investigated wish the Zr/Ti ratio and the additions of Y2O3. and Fe$_2$O$_3$ Electromechanical coupling factor(Kp) showed the highest value of 0.555 in the Zr/Ti=0.50/0.50 ratio ,however, dielectric constant showed the highest value of 1,217 in the Zr/Ti = 0.49/0.51 ratio. Excellent TCFr vague of 421ppm/$^{\circ}C$] at-30~9O$^{\circ}C$ was appeared in the Zr/Ti=0.50/0.50 ratio and electro-mechanical coupling factor(Kp) , mechanical quility factor(Qm) and dielectric constant was 0.496, 1,286 and 1,085 ,respectively ,in the composition ceramics of lwt%Y$_2$O$_3$ and 0.3wt%Fe$_2$O$_3$.

  • PDF