Statement of problem. Use of the conventional dental impression procedure is problematic in patients who have difficulty opening their mouth, difficulty breathing through their nose or tendency to gag. Purpose. It is necessary to make individual trays more comfortable for patients during impression taking procedure. It was reported at the KAP Annual Meeting 2001 Seoul that an improved impression technique was suitable for this purpose. In this study, the accuracy of the improved dental impression method for implant was compared with the conventional dental impression method. Material and methods. An oral simulator was made from clear acrylic resin block which had similar form of edentulous ridge. For setting up the standard, five fixtures were installed on it. Study casts were made using two kinds of impression techniques. One was the conventional method that was taken using silicone impression material and an individual resin tray under connection of inter-fixture relation. The other was the improved method in which was the connection of the impression coping and the thermoformed polymethyl methacrylate tray. In addition, two different study casts were made from the improved impression body. The coordinates of the fixture on the study model were measured by three-dimensional coordinate measuring equipment. Then the distances between each fixture were calculated and compared with that of oral simulator. Accuracy of the each impression method was also assessed. Results. The differences of inter-fixture dimension between study casts and simulator in the improved impression technique showed $0.014{\pm}0.016mm$ and $0.017{\pm}0.022mm$, respectively and that of the conventional method was $0.017{\pm}0.014mm$. There was no significant difference between the improved impression technique and conventional method. Conclusion. The improved impression technique is useful for multiple support implants.
광 발광성 (photoluminescence, PL)과 광 반사성(reflectivity)의 두 가지 광학적 성질을 동시에 가지고 있는 새로운 다층 DBR(distributed Bragg reflector) 다공성 실리콘 composite 필름을 개발하였다. 발광 효율이 높은 실리콘 고분자 폴리실올을 PMMA(polymethylmethacrylate)에 첨가하여 다층 DBR 다공성 실리콘 표면에 코팅을 한 composite 필름을 제조하였다. 이 composite 필름은 510 nm에서의 발광스펙트럼과 565 nm에서의 반사스펙트럼을 동시에 나타낸다. 이러한 composite 필름은 광학적 정보가 저장되어있고 물리적인 힘을 가하여도 그 광학적 정보를 잃지 않는 장점을 갖는다. 또한 다층 DBR 다공성 실리콘 필름은 쉽게 부서지는 단점 때문에 다루기가 어려운 반면 composite 필름은 고분자로 고형화 되어있으므로 기계적인 안정도를 증가시킬 수 있었다.
PURPOSE. The aim of this study was to compare the flexural strength of polymethyl methacrylate (PMMA) and bis-acryl composite resin reinforced with polyethylene and glass fibers. MATERIALS AND METHODS. Three groups of rectangular test specimens (n = 15) of each of the two resin/fiber reinforcement were prepared for flexural strength test and unreinforced group served as the control. Specimens were loaded in a universal testing machine until fracture. The mean flexural strengths (MPa) was compared by one way ANOVA test, followed by Scheffe analysis, using a significance level of 0.05. Flexural strength between fiber-reinforced resin groups were compared by independent samples t-test. RESULTS. For control groups, the flexural strength for PMMA (215.53 MPa) was significantly lower than for bis-acryl composite resin (240.09 MPa). Glass fiber reinforcement produced significantly higher flexural strength for both PMMA (267.01 MPa) and bis-acryl composite resin (305.65 MPa), but the polyethylene fibers showed no significant difference (PMMA resin-218.55 MPa and bis-acryl composite resin-241.66 MPa). Among the reinforced groups, silane impregnated glass fibers showed highest flexural strength for bis-acryl composite resin (305.65 MPa). CONCLUSION. Of two fiber reinforcement methods evaluated, glass fiber reinforcement for the PMMA resin and bis-acryl composite resin materials produced highest flexural strength. Clinical implications. On the basis of this in-vitro study, the use of glass and polyethylene fibers may be an effective way to reinforce provisional restorative resins. When esthetics and space are of concern, glass fiber seems to be the most appropriate method for reinforcing provisional restorative resins.
Jang, Woo Young;Seo, Dong Nam;Park, Jung Gyu;Kim, Hyung Tae;Lee, Sung Min;Kim, Suk Young;Kim, Ik Jin
한국세라믹학회지
/
제53권6호
/
pp.604-609
/
2016
This study reports on wet-foam stability with respect to porous ceramics from a particle-stabilized colloidal suspension that is achieved through the addition of polymethyl methacrylate (PMMA) using a wet process. To stabilize the wet foam, an initial colloidal suspension of $Al_2O_3$ was partially hydrophobized by the surfactant propyl gallate (2 wt.%) and $SiO_2$ was added as a stabilizer. The influence of the PMMA content on the bubble size, pore size, and pore distribution in terms of the contact angle, surface tension, adsorption free energy, and Laplace pressure are described in this paper. The results show a wet-foam stability of more than 83%, which corresponds to a particle free energy of $2.7{\times}10^{-12}J$ and a pressure difference of 61.1 mPa for colloidal particles with 20 wt.% of PMMA beads. It was possible to control the uniform distribution of the open/closed pores by increasing the PMMA content and by adding thick struts, leading to the achievement of a higher-stability wet foam for use in porous ceramics.
연구 목적: 본 연구는 연마 술식에 따른 polymethyl methacrylate (PMMA)의 표면 거칠기의 차이를 비교하고, 광중합 광택제가 PMMA의 표면 거칠기에 주는 영향과 이후 칫솔질에 의한 거칠기의 변화를 알아보는데 그 목적이 있다. 연구 재료 및 방법: 총 60개의 $10{\times}10{\times}5\;mm$ 크기의PMMA 시편을 만들었다. 중합 방법 (압력 하 중합과 대기압 하 중합)과 표면 연마 방법 (기계적 연마와 화학적 연마)에 따라 대조군을 포함하여 각 10개씩 총 6군으로 나누었다. 기계적 연마는 카바이드 덴처버로 표면 마무리 한 후, 러버 포인트와 퍼미스를 이용하여 하였으며, 화학적 연마는 표면 마무리 후 광중합 광택제 ($Plaquit^{(R)}$; Dreve-Dentamid GMBH)를 도포하여 실시 하였다. 연마가 완료된 후 비 접촉식 3차원적 표면 형상 분석장치인 Accura $2000^{(R)}$으로 표면거칠기를 측정하였으며, 그 3차원적 영상을 얻었다. 그 후 칫솔질에 의한 마모의 영향을 평가하기 위해 초음파 전동 칫솔을 이용하여 각 시편당 칫솔질을 행하고 다시 Accura $2000^{(R)}$에 의한 표면 분석을 시행하였으며, 거칠기의 정도는 Ra 값으로 표시하였다. 연마 후와 칫솔질 후의 표면 거칠기를 비교하기 위한 통계적 분석은 Mann-Whitney test와 t-test를 이용하여 95% 유의수준에서 실시하였다. 결과: 화학적 연마군은 기계적 연마군에 비해 통계적으로 유의한 작은 평균 표면 거칠기 값을 보였으며 (P = .0045), 일반 대기압 하에서 중합시킨 군에서 그 차이가 더 크게 나타났다 (P = .0138). 초음파 전동 칫솔에 의한 모의 칫솔질 후 표면 거칠기는 기계적 연마군을 제외한 모든 군에서 크게 증가하였으며, 칫솔질 후의 표면 거칠기는 각 군에서 통계적으로 유의한 차이를 보이지 않았다. 결론: 비록 칫솔질에 의한 마모의 영향으로 표면 거칠기가 증가하기는 하지만, 화학적 연마가 기계적 연마에 비해 우수한 표면 거칠기를 보인다고 할 수 있다.
베이스메이크업 중의 하나인 프레스드 파우더는 주요 품질 속성으로 밀착성과 발림성이다. 일반적으로 메이크업 화장료에서 밀착성을 향상시키면 반대속성인 발림성이 저하되기 때문에 밀착성과 발림성을 동시에 충족시키는데 한계가 있었다. 본 연구에서는 두 가지 주요 속성을 만족시키기 위해서 air jet mill 공정을 시도하였고, lauroyl lysine (LL)과 sodium cocoyl glutamate (SCG)의 혼합물로 습식 코팅 처리한 sericite를 적용하여 밀착성을 향상시켰다. 또한, 분산성이 단분산성을 이루고 있는 polymethyl methacrylate (PMMA)와 diphenyl dimethicone/ vinyl diphenyl dimethicone/ silsesquioxane crosspolymer (DDVDDSC)를 적용하여 발림성을 향상시켜 서로 양립하기 어려운 두 가지 품질 속성을 모두 만족시켰다. air jet mill 공정은 제약, 식품 산업에서 주로 적용되고 있으며 화장품 분야에서는 파우더 소재 가공을 위해 사용되고 있는 공법이다. 본 연구에서는 air jet mill 공정을 제조 공정단계에서 접목시켜 최적의 입경인 $6.8{\mu}m$의 화장료를 완성할 수 있었다. 그리고, EDS 매핑으로 Ti 원소가 화장료에서 전체적으로 고르게 분포하고 있음을 확인하였고, SEM 분석을 통하여 판상 입자의 모서리 부분이 둥글게 가공처리 됨을 확인하였다. 이는 화장 도구를 이용하여 화장료를 취하여 피부에 도포할 때, 발림성이 향상되는 효과를 줄 수 있다고 판단된다. 피부 친화성이 우수한 LL과 저자극이면서 코코넛에서 유래한 SCG를 습식 코팅하여 sericite의 밀착성을 더욱 향상시켰다. 그리고, PMMA의 분산성과 형태가 발림성에 미치는 영향을 평가하기 위해서 SEM을 분석하였다. 유사한 형태를 갖는 구형 및 진구형에서도 분포도가 균일하고 단분산상일 때 발림성 효과가 더욱 증가하는 것으로 나타났다. PMMA의 단분산성과 입경에 따른 발림성을 동마찰계수 측정으로 확인하였고, 최적의 함량을 결정하였다. 그리고, 실리콘 러버 파우더 종류에 따른 발림성과 경도, 낙하안정성 등을 확인하여 DDVDDSC를 결정하였다. 최종적으로 PMMA의 단분산성과 실리콘 러버 파우더가 발림성에 영향을 끼치는 것을 알 수 있었다. 이와 같은 화장료는 적정한 경도를 갖으면서도 낙하안정성이 우수하며, 경시에 따른 안정성도 우수하였다. 본 연구 결과를 통해 본 논문에서 제시하는 프레스드 파우더의 밀착성과 발림성을 향상시킬 수 있는 한 가지 방법으로 활용될 수 있을 것이라 판단된다.
The ignition phenomena of a solid fuel plate of polymethyl-methacrylate(PMMA), which is vertically positioned and exposed to a thermal radiation source, is numerically studied here. A two-dimensional transient model includes such various aspects as thermal decomposition of PMMA, gas phase radiation absorption, gas phase chemical reaction and air entrainment by natural convection. Whereas the previous studies considers the problem approximately in a one-dimensional form by neglecting the natural convection, the present model takes account of the two-dimensional effect of radiation and air entrainment. The inert heating of the solid fuel is also taken into consideration. Radiative heat transfer is incorporated by th Discrete Ordinates Method(DOM) with the absorption coefficient evaluated using gas species concentration. The thermal history of the solid fuel plate shows a good agreement compared with experimental results. Despite of induced natural convective flow that induces heat loss from the fuel surface, the locally absorbed radiant energy, which is converted to the internal energy, is found to play an important role in the onset of gas phase ignition. The ignition is considered to occur when the rate of variation of gas phase reaction rate reaches its maximum value. Once the ignition takes place, the flame propagates downward.
A polymer-based multi-walled carbon nanotube (MWCNT) field emission device was fabricated from a composite dispersion of MWCNTs and waterborne polymethyl methacrylate (PMMA). The waterborne PMMA synthesized through the emulsion polymerization method was added to minimize the reagglomeration of dispersed MWCNTs with surfactants in water, and increase the adhesion between the and the substrate. The field emission properties of the fabricated device were optimized by adjusting the density of the emitter and the adhesion between the MWCNTs and the substrate. These were done by controlling the polymer concentration added to the MWCNT dispersion, as well as the amount of spray coating on the substrate. The results confirm the successful fabrication of a polymer-based MWCNT field emission device with a low field of 1.07 $V/{\mu}m$ and a good electric field enhancement factor of 2445. The device was fabricated by adding 0.8 mg/mL of polymer solution to the MWCNT dispersion and applying 20 cycles of spray coating. Application of this same MWCNT/polymer composite solution to a flexible polymer substrate also resulted in the successful fabrication of an electric field emission device with uniform emission and long time stability.
Purpose: This study is a mechanical strength supplementation of denture base resin Polymethyl methacrylate (PMMA) is in general use for denture base resin of the partial and full denture, however, The polymerization process of PMMA is not stabilized. Because of compatibility problems, preceding studies were performed, which were enhancing mechanical strength(Camilo Machado 2007),(Ana M. 2008), addition filler to materials property(Ayse Mese, 2008), self curing method(Hiroshi Shimizu, 2008). Methods: The carbon fiber and polyacetal filler, reinforced the mechanical strength for improving the stability of denture base resin were supplemented to the self cured resin. The Modulus of elasticity and the restoring force were calculated by tensile test. Results: The strengths of the heat and self cured resin were respectively decreased and increased, when the filler was supplemented to the denture base resin and the modulus of elasticity of both heat and self cured resin were not increased, when the filler was supplemented to the denture base resin. Conclusion: The restoring forces of self cured resin containing 10% filler were increased, when the filler was supplemented to the denture base resin.
한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.II
/
pp.1462-1465
/
2005
In this report, the FE characteristics of carbon nanotubes (CNTs) treated using both thermal annealing and mechanical coatings on the as-grown CNTs system atically studied. It was found that in the high temperature annealed samples, CNTs were attacked at its root during annealing due to a small amount of oxygen, and were pulled out of the substrate in places after FE measurements because of the contact resistance. However, for the mechanically coated samples both with spin on glass (SOG) and polymethyl methacrylate (PMMA), CNTs were found to be nearly intact after FE measurements and showed reliable FE characteristics over repeatable voltage scan. The reliability of CNTs during FE could be owing to the strong adhesion of CNTs to the substrate both by SOG and PMMA coatings.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.