The color of a natural diamond that contains nitrogen impurities can be enhanced by a high pressure high temperature (HPHT) treatment. Type IaAB diamond samples containing nitrogen impurities were executed by HPHT process of 5.6 Gpa, 10 min by varying the annealing temperature at 1600, 1650, and $1700^{\circ}C$. Property characterization was carried out using an optical microscope, FT-IR spectrometer, low-temperature PL spectrometer, and micro Raman spectrometer. By observing optical micrographs, it can be seen that diamond sample began to alter its color to vivid yellow at $1700^{\circ}C$. In the FT-IR spectrum, there were no Type changes of the diamond samples. However, amber centers leading to brown colors lessened after $1700^{\circ}C$ annealing. In the PL spectrum, all the H4 centers became extinct, while there were no changes of yellow color center H3 before or after treatment. In the Raman spectrum, no graphite spots were detected. Consequently, diamond color enhancement can be done by higher than $1700^{\circ}C$ HPHT annealing at 5.6 GPa-10 min.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.17
no.9
/
pp.988-993
/
2004
Luminescence characteristics of Ag-doped ZnO as the quantum dot materials to increasing the efficiency on dye-sensitized solar cells (DSC) have been studied. Ag doped ZnO powder was produced by the self-sustaining combustion process using ultrasonic spraying heating method. Luminescence wavelength region of the ZnO by Ag doping was shifted to longer wavelength. Tn the case of the Ag doped ZnO powder, broad luminescence spectrum centered on 600nm was observed. On the other hand, we compared PL data of RTA treated ZnO:Ag film at various temperatures because the front electrode of solar cell was in need of the sintering process. In XRD and PL data for RTA treated film at the 500$^{\circ}C$ showed good property. And, it was found that the grain size wasn't growing but only optical property was changed. According to the result of XRD, PL, absorption, emission spectrum and DV-X${\alpha}$ used in theoretical calculation, it is considered to be possible to use Ag doped ZnO as quantum dot material for improving DSC efficiency.
Photoluminescence(PL), XRD, TEM results $5\times1016/\textrm{cm}^2, 1\times10^{17}/\textrm{cm}^2, 3\times10^{17}/\textrm{cm}^2$ Si-implanted $SiO_2$ films on crystalline silicon are reported. At low dose implantation and low annealing temperature, visible PL are observed. The PL spectrum has 7400$\AA$ and 8360$\AA$ peaks. As annealing time increased, the PL intensity are increased and peak positions are changed. The PL spectrum are not observed at high dose implantation and high annealing temperature. For the samples of low dose and high annealing temperature, visible PL are observed at short annealing time (30 minutes) and disappear for more than 1 hour annealing. From XRD and TEM results, silicon cluster are related to nonradiative defects. It is concluded that the origin of visible PL in Si implanted SiO2 films are not nanocrystal but two kinds of radiative defects. The Si-O-O bonding related defects (O rich defects) and Si-Si-O bonding related defects (Si rich defects) are related to the PL spectrum and depend on concentraion of Si implantation, annealing temperature and time.
The 1R(Infra-Red) spectrum and PL(Photoluminescence) of the antiferromagnetic pure $MnF_2$ and the single crystal $MnF_2(1.5%\;EuF_3)$ with the rutile structures were measured. The detailed analysis of the measured PL data showed the differences of the optical property between the single crystal $MnF_2(1.5%\;EuF_3)$ and the pure $MnF_2$. It was found that the additional PL peak by the doping of the $EuF_3$ in $MnF_2$ is originated from the f-d transition of $Eu^{3+}$ from the temperature dependent intensity measurement.
Seo, Han Wook;Jeong, Da-Woon;Kim, Min Young;Hyun, Seoung Kyun;On, Ji Sun;Kim, Bum Sung
Journal of Powder Materials
/
v.24
no.4
/
pp.321-325
/
2017
In this study, we investigate the optical properties of InP/ZnS core/shell quantum dots (QDs) by controlling the synthesis temperature of InP. The size of InP determined by the empirical formula tends to increase with temperature: the size of InP synthesized at $140^{\circ}C$ and $220^{\circ}C$ is 2.46 nm and 4.52 nm, respectively. However, the photoluminescence (PL) spectrum of InP is not observed because of the formation of defects on the InP surface. The growth of InP is observed during the deposition of the shell (ZnS) on the synthesized InP, which is ended up with green-red PL spectrum. We can adjust the PL spectrum and absorption spectrum of InP/ZnS by simply adjusting the core temperature. Thus, we conclude that there exists an optimum shell thickness for the QDs according to the size.
The dependence of photoluminescence (PL) and photoluminescence itation (PLE) on preparation condi-tions and the aging of porous silicon carbide (PSC) have been investigatted. The fiber size of the material pre-pared under dark-current mode, labele d DCM, was larger than that of the photoassisted (PA)process.The intensity of the PL spectrum for the PA condition was higher than that of the DCM condition. The PA condition giving small fiber size exhibited amore prominent high-energy component but the emission bands of both con-ditionsobserved were rather similar. The origin of the PL may have played an importantrole in the surface defect center introduced by the reaction conditions ofHFatthe surface of the silicon carbide. Selective excita-tion of the PL bandsusingdifferent excitation wavelengths has been used to identify distinct componentswith-in the PL bandwidth. Two main PL bands with peak wavelength of494 and534 nm were clearly resolved. On the other hand, selectivc emission of the PLEbands using different emission wavelengths has been used to identify distinct components within the PLE bandwidth. The higher energy band with peak wavelength of 338 nm and the lower energy bands involving 390,451 and 500 nm were clearly resolved. According to the pro-ionged aging in air, PL spectra appearedasone band, This emission probably originated from states localized to the band-to-band recombination due to the oxidation on the crystallite surface.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.14
no.2
/
pp.145-151
/
2001
In this study, blue light emiting, soluble PPV copolymers were synthesized by Witting reaction and characterized. ITO/copolymer/Ca and ITO/copolymer/A1 structured light emitting diodes(LED) were fabricated and their I-V characteristics were examined. Copolymers showed $\pi$-$\pi$ transition in UV-Vis./NIR spectra. The PL and abosorption spectrum showed the symmetric vibration modes with mirror images which means that copolymers are highly aligned. By introducing aliphatic hydrocarbon group on polymer main chain, the solubility of copolymers was improved and no significant effects of substituent were observed. The band offset of copolymers are well suited as light emitting material for LED application than monomer or oligomer does. THe band offset of copolymers is ∼3eV in PL spectrum and the threshold voltages of ITO/copolymer/Ca and ITO/copolymer/Al structured LED 3V, 12V respectively. In the case of ITO/copolymer/Ca LED, it is believed that the amount of electrons and holes is well balanced and the recombination of opposite charges occurs easily because the work functions of Ca and Al electrodes are 2.9 and 4.3eV respectively and the difference in barrier height between polymer and electrode was small.
Journal of the Korean institute of surface engineering
/
v.35
no.5
/
pp.305-311
/
2002
Optical measurements have been used to study the biaxial tensile strain in heteroeptaxial ZnTe epilayers on the (100) GaAs substrate by hot wall epitaxy (HWE) with Zn reservoir. It is effect on the low-temperature photoluminescence spectrum of the material. Optimum growth condition has been determined by a four-crystal rocking curve (FCRC) and a low temperature photoluminescence measurement (PL). It was found that Zn partial pressure from Zn reservoir has a strong influence on the quality of grown films. Under the determined optimum growth condition, ZnTe epitaxial films with thickness of 0.72~24.8$\mu\textrm{m}$ were grown for studying the effect of the thickness on crystalline quality. The PL and FCRC results indicated that the quality of ZnTe films becomes higher rapidly with increase of thickness up to 6$\mu\textrm{m}$. The best value of the FWHM of the four crystal rocking curve, 66 arcsec, was obtained on the film with 12$\mu\textrm{m}$ in thickness. The PL spectrum shows the splitted strong free exciton emissions and very weak deep band emissions. These results show the high quality of films.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.13
no.1
/
pp.31-35
/
2003
The PL data bases reveal the fact that a part of lattice of HPHT treated diamond is reconfigured by the reduction, elimination, generation, and movement of vacancies and interstitials as well as of impurity elements. In particular, this very sensitive method clearly illustrated that minute amount of nitrogen impurities is present in all of these type IIa diamonds, and reveal the presence of a considerable number of point defects dispersed throughout the crystal lattice.
The belt source evaporation is for the large size AMOLED devices to re-sublimate the organic film deposited on the metal plate. Using the plane source, the PL spectrum of the doped organic film has been studied for the first time. The PL peak of the pure Alq3 film was 512nm and that of the pure Rubrene was 557nm. The PL peak of the 2% Rubrene doped Alq3 film was shifted to $536{\pm}2nm$. The PL peak wavelength measured at the front surface of the film and at the back surface of the film was measured as nearly same as that the doping ratio maintains uniform within the film thickness. In conclusion, the doping control of the organic film becomes real using the belt type plate sublimation deposition.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.