• Title/Summary/Keyword: PC 그라우트

Search Result 10, Processing Time 0.022 seconds

Study on Material Segregation of Grout and Filling Characteristic of Grouting for Post-Tensioned Concrete Beam (PC 그라우트의 재료분리 및 PC 빔 그라우팅 충전성에 관한 연구)

  • Lee, Jun-Ki;Choi, Joon-Ho;Yoon, Jeong-Seob;Cho, In-Sung
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.3
    • /
    • pp.419-426
    • /
    • 2010
  • This paper discusses a series of experiments including material improvement in order to ensure quality of grouting for the post-tensioned structure. In presstressed concrete, grouting refers to the construction procedure of filling empty space of duct enclosing the prestress tendons using cementitious material, To date, adequate quality control of the grouting has not been established in Korea because the relationship between the grouting and durability of post-tensioned structure is not well-recognized. The Korean standard does not consider the important material characteristic, wick effect, which is caused by tendons in the ducts, and furthermore current standard testing method does not quantify reasonable material segregation. As a result, the grout material, which satisfies the current material standards, may well exhibit excessive bleeding of water or shrinkage during construction. In this study, international codes and standards related to grouting were surveyed. The mix proportions of the constituents and novel admixtures were suggested to meet equivalently with these standards. Performance of this enhanced grout was compared with common domestic grouts using the international standard testing method. A series of mock-up specimens considering geometry of PC beam was constructed and grout flow pattern was observed as the grout was injected. It was observed that the grouting performance was highly influenced by material properties and filling characteristic can be varied depending on geometry of ducts.

Investigation for Detecting the Poorly Grouting of a PC Girder Bridge (충격탄성파법을 이용한 PC형교의 그라우트 미충전부 탐사측정)

  • Lee, Sang-Hun;Sagara, Yuzo;Endo, Takao
    • 한국방재학회:학술대회논문집
    • /
    • 2010.02a
    • /
    • pp.40.2-40.2
    • /
    • 2010
  • PC형교에서는 거더의 복부와 하부에 PC강선을 수용하는 쉬이스가 배치되어 있어며, 그 내부에 그라우트를 충전함으로서 PC강선과 콘크리트를 간접적으로 부착시킨다. 그러나, 이 충전이 불충분하면, 쉬이스 내부에 물이 침투하여 PC강선이 부식하거나, 동결융해 작용에 의한 쉬이스 배치 위치에서의 횡방향 균열이 발생한다. 본 연구에서는, 충격탄성파법을 이용하여 실구조물에 대한 그라우트 미충전부 탐사측정을 실시하고, 미충전부로 보여지는 장소를 천공으로 확인함으로서 본 방법의 실용성에 대하여 보고한다.

  • PDF

Comparion of Korea-Japan Quality Standards for Grout Materials about PC Member assembly (PC부재 조립용 그라우트 재료 품질 기준의 한일 비교)

  • Kim, Yeon-Ho;Lee, Bum-Sik;Kim, Min-Jun;Kim, Ki-Ho;Jun, Myoung-Hoon
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.11a
    • /
    • pp.127-128
    • /
    • 2023
  • Recently, OSC (off-site construction) construction has been revitalized as a response to the decline in building quality and productivity due to lack of skilled manpower at construction sites, and PC (precast concrete) construction, a representative OSC construction, is insufficiently applied to public housing.This is the situation.In addition, in the case of general contents appearing in standard specifications, the construction standards for quality assurance remain in the 1990s and do not correspond to the current construction environment.In order to improve the quality of PC member joints, we compared and analyzed Korean and Japanese specifications to establish appropriate standards for PC construction quality control, focusing on the quality of grout used in joints.

  • PDF

Grouting Injection Effectiveness of a Permeable Compacting Grout using Permeable Compaction Type Packer (침투다짐형 팩커를 이용한 침투다짐 그라우트의 주입 효과)

  • Park, Sung-Yong;Shim, Houng-Gen;Kang, Hee-Jin;Lim, One-Bin;Kim, Yong-Seong
    • Journal of the Korean Geosynthetics Society
    • /
    • v.16 no.2
    • /
    • pp.149-158
    • /
    • 2017
  • Permeating injection is commonly known as an ideal type of injection in grouting reservoir embankment, yet often-combined permeating and fracturing injection grouting operation can disturb the original soil. A grouting method has been regarded as effective and developed to ameliorate the possible disturbance problem. It involves compaction grouting with low expansive pressure near the injection hole and repetitive injection and compaction with grout material that allows ideal permeating injection. This thesis develops Hybrid Grout (ie. HG grout) that allows various application in any ground condition combined together, has high fineness and low viscosity, and expands permeation injection to silty sand. It researches on the injection effect of permeable compaction grout which is done with PC packer and is a combination of HG grout and expansion agent to obtain permeation compaction effect on the area near grout injection spot by developing Permeable Compaction Type Packer(ie. PC packer). As the developed PC packer, HG grout, and and expansion agent (HI-E) are applied to reservoir embankment reinforcement grouting, possibile permeation compaction effect that satisfies reservoir embankment grouting standard is confirmed according to the research.

The Effect of PC-Based SP on Rheology and Strength of High Strength Grout (PC계 유동화제가 고강도 그라우트에 유동성 및 강도에 미치는 영향)

  • Kim, Beomhwi;Yi, Chongku
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2022.04a
    • /
    • pp.148-149
    • /
    • 2022
  • The use of high-strength grout applied for facility foundations and bridges has recently been expanding in offshore wind farm. Wind farm in offshore require bearing capacity for horizontal loads such as wind, waves, and earthquakes. In order to improve the bearing force of the base part, sufficient fluidity and a certain strength should be ensured so that the high-strength grout is densely charged in the narrow space of the connection part. Therefore, in this study, changes in fluidity and strength according to the ratio of PC-based superplasticizer mixed in high-strength grout were measured. As a result, as the ratio of the superplasticizer increased, fluidity increased and strength decreased. However, the strength did not decrease when the ratio of superplasticizer was above a 0.005. Therefore, it was confirmed that the fluidity change was remarkable when a 0.005 ratio of PC-based superplasticizer were added.

  • PDF

A study on ready-mixed-mortar for prestressed concrete grouting material (PC(Prestressed Concrete)그라우트용 레미탈에 관한 연구)

  • 박길수;전진호;김경덕;이학봉;노현승;이완경
    • Cement Symposium
    • /
    • no.27
    • /
    • pp.54-60
    • /
    • 2000
  • As conventional grouting materials for the sheath such as cement slurry or cement-mortar are mixed and pumped in site, those harden with bleeding or shrinkage and meets low compressive strength. Also the materials haven''t always same cements, sand size d

  • PDF

Experimental Studies on Bond and Splice Performance of Splice Sleeve for Connecting Rebar (철근연결용 스플라이스 슬리브의 이음 및 부착성능에 대한 실험적 연구)

  • Kang, Duk Man;Park, Yong Gul;Lee, Hyeon Gi;Moon, Do Young
    • Journal of the Korean Society for Railway
    • /
    • v.20 no.2
    • /
    • pp.257-264
    • /
    • 2017
  • The PC (Precast Concrete) construction method is a technique where concrete members that have been produced in a plant are constructed on site. Thus, continuity and secure integration of a structure that can be obtained by connecting rebars at splicing joint for PC members are the main areas of concern for this method. To evaluate the splicing and bonding performance according to application of a splice sleeve for connecting rebar in this research study, the diameter of rebar, development length, grouting strength etc. were set as variables. The performance and stiffness of splicing according to the development length of grout strength were measured and evaluated. In addition, by conducting comparative analysis on each of the variables, the factors that affected the splice sleeve for connecting rebar were discussed. The results confirmed that the strength and stiffness of the splice sleeve for connecting rebar were significantly affected by the development length while the increase in performance according to grout strength was not as significant.

A Study on Ready-Mixed-Mortar for Prestressed Concrete grouting material (PC (Prestressed Concrete) 그라우트용 레미탈에 관한 연구)

  • 박길수;김경덕;이학봉;노현승;이완경
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.04a
    • /
    • pp.888-895
    • /
    • 2000
  • As conventional grouting materials for the sheath such as cement slurry or cement-mortar are mixed and pumped in site, those harden with bleeding or shrinkage and meets low compressive strength. Also the materials haven't always same cements, sand size distributions, additives in site, so those materials have unstable quality properties. We have studies on ready-mixed-mortar for grouting pretensioned or post-tensioned cables and rods to encapsulate the steel so that we have developed a formulation of specially selected, flowable, shrinkage-compensating materials.

  • PDF

An Experimental Study on the Evaluation of Bearing Strength of the Vertical Joint in Precast Concrete Large Panel Structures (대형판 조립식 구조 수직접합부 지압강도 평가에 관한 연구)

  • Chung, Lan;Cho, Seung-Ho;Hwang, Min-Ha
    • Magazine of the Korea Concrete Institute
    • /
    • v.8 no.4
    • /
    • pp.181-189
    • /
    • 1996
  • It is well-known that the hearing strength in vertical joints of precast concrete large panel system is affected by grout compressive strength angle of shear key and bearing area. 21 vertical joint specimens were tested to investigate the effects of these parameters The analysis of test results shows that : 1. The higher be grout compressive strength, the higher will shear strength be. And the bearing strength does not so increase in proportion of bearing area. 2. The shear key with the angle of $20^{\circ}$shows the highest bearing strength among three angle variables of $20^{\circ}$, $25^{\circ}$, $30^{\circ}$.

Measurement of Verticality and Joint Gaps of a Near-surface Disposal Facility Vault Through a Mock-up Test for Fill-up Stages (표층처분시설 처분고의 목업테스트를 통한 채움단계별 수직도 및 이음부 벌어짐 측정)

  • Choi, Dong-Ho;Ann, Ki-Yong;Choi, In-Yong;Lee, Hyuk-Jin
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.4
    • /
    • pp.537-544
    • /
    • 2021
  • In order to describe the fill-up stages of a near-surface disposal facility vault, a mock-up test is performed, and its behavior during the fil l -up stages is investigated. On an in-site concrete foundation with a l ength of 6600mm, a width of 6600mm and a thickness of 400mm, a reinforced concrete disposal vaul t is manufactured with 4 precast (PC) corner wal l s and 8 PC side wal l s. 36 wasted drums are pl aced on the 1st fl oor in 6 by 6, and then the empty space is fil l ed with grout fil l er. These processes are repeated up to the 5th floor, and the verticality and the joint gaps are measured for each fill-up stage. The verticality is measured using a level at 6 positions on each side wall (3 positions on the left and right sides, respectivel y), i.e. a total of 24 positions on the 4 side wal l s. The joint gaps are measured at 9 positions on each side wal l (3 positions on the left, center and right sides, respectively), I.e. a total 36 positions on the 4 side walls. To measure the joint gaps, crack tips are installed on the left and right sides of every joint gap, and vernier calipers are used. The measured verticality obtained through the mock-up test was found to be ±0.1° based on the initial stage (ST0), and the result of the joint gap was up to 0.38mm. This appears to have a negligible effect on the structure.