• 제목/요약/키워드: Normal Deformation

검색결과 555건 처리시간 0.029초

AZ31 Mg 합금의 쌍정 형성에 미치는 초기 집합조직의 영향 (Effect of Initial Texture on the Twinning Formation of AZ31 Mg Alloy)

  • 이병호;김용우;박성혁;이종수
    • 소성∙가공
    • /
    • 제16권6호
    • /
    • pp.467-472
    • /
    • 2007
  • In this study, the effects of initial texture on the twinning formation of AZ31 Mg rolled sheet was investigated. Uniaxial compression tests were carried out on samples cut along the normal direction(ND) and roiling direction(RD), respectively, of rolled AZ31 Mg alloy sheet at various temperatures (RT, 200, 250, 300, 350, $400^{\circ}C$) with the fixed strain rate($10^{-2}/s$). The results showed that deformation twining occurred actively only in the RD specimens, which promoted homogeneous deformation as compared to the ND specimens. The effect of temperature on the formation of deformation twins was also investigated, and the slip/twin transition temperature was found to be approximately $250^{\circ}C$.

인코넬 690의 변형 및 재결정 (Deformation and Recrystallization of INCONEL 690)

  • 표은종;허무영
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1995년도 추계학술대회논문집
    • /
    • pp.167-171
    • /
    • 1995
  • The formation of preferred orientations in cold rolled and recrystallized Inconel 690 sheets was studied by the x-ray texture measurements and TEM observations. The increasing{220} pole intensity in the plane normal at the higher reductions was related to the{110}<112> texture component. The rolling texture of the Inconel 690 was the pure metal type. THe dislocation cells were found in the near{110}<112> oriented grains. The onset of deformation twins in the {112}<111>oriented grains. The onset of deformation twins in the {112}<111> oriented grains. The onset of deformation twins in the {112}<111> oriented grains caused the weakening of {112}<111> and the development of {552}<115> in the rolling texture. The annealing texture of the Inconel 690 sheets was dependent on the annealing temperature. The annealing texture of 750$^{\circ}C$ annealed sheets was similar to the cold rolling texture. The major preferred orientations of the 950$^{\circ}C$ annealed specimens were {112}<110> and {001}<110>. The formation of fine and closely spaced annealing twins in the specimen annealed at 1150$^{\circ}C$ led to the randomization of the annealing texture.

  • PDF

변형유기 식각 힐록 현상을 이용한 기계화학적 극미세 Writing 기법에 대한 연구 (A Study of Mechanochemical Hyperfine-Writing Technique Using Deformation Induced Etch Hillock Phenomena)

  • 강충길;윤성원
    • 한국정밀공학회지
    • /
    • 제22권7호
    • /
    • pp.71-78
    • /
    • 2005
  • The purpose of this study is to suggest a hyperfine maskless writing technique by using the nanoindentation and HF wet etching technique. Indents were made on the surface of Pyrex7740 glass by the hyperfine indentation process with a Berkovich diamond indenter, and they were etched in $50\;wr\%$ HF solution. After etching process, convex structure was obtained due to the deformation-induced hillock phenomena. In this study, effects of indentation process parameters (etching time, normal load, loading .ate, hold-time at the maximum load) on the morphologies of the indented surfaces after isotopic etching were investigated from an angle of deformation energies. Finally, sample characters were written to show the possibility of the application.

Analysis of post-construction deformation characteristics of concrete faced rockfill dams

  • Kim, You-Seong;Won, Myoung-Soo;Song, Young-Chul;Yoon, Deok-Joong
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2007년 가을학술발표회
    • /
    • pp.528-541
    • /
    • 2007
  • To get the possible for management and maintenance, it was analyzed the deformation characteristics, such as crest of embankment and concrete face slab, and leakage of concrete faced rockfill dams (CFRD). There are trends that embankment deformation depends on intact strength used rockfills rather than dam height, deformation normal to concrete face slab during the first reservoir filling is occurred more than 80% of the total deformation in general, and the magnitude and trend of concrete face slab deformation is similar to post-construction crest settlement. The results showed that the range of post-construction crest settlement suggested by Sherard and Cooke (1987), and Clements (1984) had a good agreement in the cases using rockfill with very high intact strength, but it had a trend which underestimated crest settlement in the cases using rockfill with medium to high intact strength. The maximum leakage rate in general was observed during the first reservoir filling and long-term leakage rate was rapidly increased when the dam height exceeds approximately 120m.

  • PDF

힘평형법을 이용한 V-형다이 평면변형 자유형 단조공정의 초기변형 해석 (The Incipient Deformation Analysis for Plane Strain Open-Die Forging Processes with V-shaped Dies Using the Force Balance Method)

  • Lee, J.H.;Kim, B.M.
    • 한국정밀공학회지
    • /
    • 제10권4호
    • /
    • pp.109-117
    • /
    • 1993
  • Force balance method is employed to predict forging information such as forging load, tool pressure and normal stress at the surface of tangential velocity discontinuity. The incipient stages of deformation for the plane strain forging of rectangular billets in V-shaped dies of different semi-angles are analysed. To construct an approximate model for the analysis of deformation by the force balance method in the incipient deformation stages, slip-line field is used. When the deformation mode by slip-line method is the same as that by force balance method, the slip-line method and the force balance method give identical solutions. The effects of die angle, coefficient of friction, billet geometries and deforma- tion characteristics are also investigated. In order to verify the validity of force balance analysis, the rigid-plastic finite element simulation for the various forgig parameters are performed and performed and find to be in good agreement.

  • PDF

가스터빈 발전기의 계자권선 손상에 관한 역학적 분석 (Mechanical Analysis of Field Coil Deformation in Gas Turbine Generator)

  • 한석우;권영동;최규하
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 하계학술대회 논문집 A
    • /
    • pp.107-109
    • /
    • 1998
  • This paper presents mechanical analysis of gas turbine generator (113MVA, $3{\phi}$, 2P, 0.9PF, F class, 3600rpm, 60Hz, 13.8kV, 4.72kA, Air-Cooling) field coil deformation. Rotor end coil deformation is only appeared on turbine end but collector end coil is normal. Expansion direction of end coil is tangential not axial. Deformation appears more severe at top turn. Retaining ling is expanded by centrifugal force of coil and itself. In case friction coefficient between coil top surface and retaining ring insulation inner surface is small, coil end length ${\ell}$ does not change. However, in case friction coefficient big condition, coil end is expanded ${\Delta}{\ell}$ due to start and stop. Deformation is assumed about 30mm by watching photograph inner surface of retaining ring is coated by Teflon at manufacturing condition. Usually Teflon coating insulation surface is small friction coefficient. It's value 0.08${\sim}$0.15. However it's value exceeds more than 0.297. Since top turn deformation appears. The distortion and subsequent failure have occurred because of the lack of a sufficient slip-plane between the top field coil conductors and the inside surface of the retaining ring insulation on the turbine end of the field-winding.

  • PDF

절리면 거\ulcorner각의 손상을 고려한 개별체 절리 유한요소 (An Isoparmetric Kiscrete Joint Element with Joint Surface Degradation)

  • 이연규;이정인
    • 터널과지하공간
    • /
    • 제7권1호
    • /
    • pp.20-30
    • /
    • 1997
  • A discrete joint finite element with joint surface degradation was developed to investigate the shear behavior of rough rock joint. Isoparametric formulation was used for facilitating the implementation of the element in existing Finite Element Codes. The elasto-plastic joint deformation model with the discontinuity constitutive law proposed by Plesha was applied to the element. The reliability of the developed finite element code was successfully testified through numerical direct shear tests conducted under both constant normal stress and constant normal displacement conditions. The result of the numerical direct shear test showed that the code can capture characteristic deformation features envisaged in the direct shear test of rough rock joint.

  • PDF

DADS 및 MSC/NASTRAN을 이용한 다물체계 유연물체의 동역학 해석

  • 김창부;백윤기
    • 한국정밀공학회지
    • /
    • 제18권2호
    • /
    • pp.63-71
    • /
    • 2001
  • This paper introduces a method for calculation of dynamic stress occurring in flexible bodies of a moving multibody system by using commercial softwares DADS for dynamic analysis and MSC/NASTRAN for finite element analysis. Three methods for model transient response analysis of a flexible body are summarized. Elastic deformation of a flexible body can be described with normal modes and static modes composed of constraint modes and residual attachment modes. The deformation modes divided into fixed-interface modes and free-interface modes can be determined by using MSC/NASTRAN and selected for dynamic analysis. The dynamic results obtained from DADS are utilized to calculate dynamic stress by using mode-displacement method or mode-acceleration method of MSC/NASTRAN. As a numerical example of the analysis, we used a three dimensional slider-crank model with a flexible connecting rod.

  • PDF

TiN 박막의 탄소성 유한요소해석 (Elastic-Plastic Finite Element Analysis of TiN Thin Film)

  • 김정실;김석삼
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2001년도 제34회 추계학술대회 개최
    • /
    • pp.331-340
    • /
    • 2001
  • Elastic-Plasitc Finite element analysis is peformed about the TiN coated medium. The normal contact is simulated by a rigid asperity pressing the surface of an elastic-plastic half-surface. The case of a surface film stiffer than the substrate is considered, and general solutions for the subsurface stress and deformation fields are presented for several coating thickness. Additionally, the critical normal loads for deformation in the substrate and coating fracture are calculated when the yield of TiN film follows the Maximum Principal Stress Theory and Von Mises Theory. The results can be subsumed in failure maps for TiN thin film on steel.

  • PDF

일정 수직강성 조건하 화강암 인장절리의 전단거동 특성 (Shear Behavior of Rough Granite Joints Under CNS Conditions)

  • 박병기;이창수;전석원
    • 터널과지하공간
    • /
    • 제17권3호
    • /
    • pp.203-215
    • /
    • 2007
  • 암반의 역학적 변형거동과 안정성은 불연속면의 역학적 특성에 크게 좌우되기 때문에 터널이나 암반구조물의 안정성 해석 및 설계를 위해서는 반드시 암반 불연속면의 역학적 성질을 규명할 필요가 있다. 지하암반 절리면의 실제 거동을 실내에서 정확히 모사하기 위해 본 연구에서는 일련의 일정 수직강성 조건하 직접 전단시험을 수행하여 초기 수직응력, 전단속도 그리고 절리면의 거칠기가 거친 화강암 절리면의 전단거동특성에 미치는 영향을 살펴보았다. 일정 수직강성 조건에서 거친 암석절리에 대한 시험 결과 전단거동은 일반적으로 1차 정점 전단응력에서의 전단응력 감소 정도에 따라 크게 두 가지 형태의 전단거동을 보이는 것으로 구분되었다. 초기 수직응력이 증가함에 따라 정점 전단변위와 1차 정점 전단응력은 증가하지만 마찰각과 정점 마찰계수의 경우 감소하는 것으로 나타났으며, 전단강성과 평균마찰계수의 경우는 초기 수직응력에 영향을 받지 않는 것으로 나타났다. 거친 절리에 대한 전단속도의 영향은 초기 수직응력이 낮은 경우 일부 전단변수들에서 약간 관찰되었으나 수직응력이 증가함에 따라 대부분의 전단시험 결과변수들에서 전단속도의 영향은 미미하였다. 거칠기에 따른 전단거동의 변화를 분석하였으나 명확한 관련성이 나타나는 경우보다 시료간의 편차가 심한 경우가 많았다.