Fe-34.4Cr-14.5Ni-2.5Mo-0.4W-0.4Mn-0.5Si 합금의 고온 산화에 미치는 S의 영향 (Effect of Sulfur on the High-temperature Oxidation of Fe-34.4Cr-14.5Ni-2.5Mo-0.4W-0.4Mn-0.5Si Alloys)

  • 이동복;이경환;배근수;조규철;정재옥;김민정
    • 한국표면공학회지
    • /
    • 제50권5호
    • /
    • pp.386-391
    • /
    • 2017
  • Two kinds of steels whose compositions were Fe-34.4Cr-14.5Ni-2.5Mo-0.4W-0.4Mn-0.5Si-(0.009 or 0.35)S (wt.%) were centrifugally cast, and oxidized at $900^{\circ}C$ for 50-350 h in order to find the effect of sulfur on the high-temperature oxidation of Fe-34.4Cr-14.5Ni-2.5Mo-0.4W-0.4Mn-0.5Si-(0.009 or 0.35)S (wt.%) alloys. These alloys formed oxide scales that consisted primarily of $Cr_2O_3$ as the major oxide and $Cr_2MnO_4$ as the minor one through preferential oxidation of Cr and Mn. They additionally formed $SiO_2$ particles around the scale/alloy interface as well as inside the matrices. The high affinity of Mn with S led to the formation of scattered MnS inclusions particularly in the 0.35S-containing cast alloy. Sulfur was harmful to the oxidation resistance, because it deteriorated the scale/alloy adherence so as to accerelate the adherence and compactness of the formed scales.

Effect of Crystallization Treatment on the Magnetic Properties of Amorphous Strips Based on Co-Fe-Ni-B-Si-Cr Containing Nitrogen

  • Cho H.J.;Kwon H.T.;Ryu H.H.;Sohn K.Y.;You B.S.;Park W.W.
    • 한국분말재료학회지
    • /
    • 제13권4호
    • /
    • pp.285-289
    • /
    • 2006
  • Co-Fe-Ni-B-Si-Cr based amorphous strips containing nitrogen were manufactured via melt spinning, and then devitrified by crystallization treatment at the various annealing temperatures of $300^{\circ}C{\sim}540^{\circ}C$ for up to 30 minutes in an inert gas $(N_2)$ atmosphere. The microstructures were examined by using XRD and TEM and the magnetic properties were measured by using VSM and B-H meter. Among the alloys, the amorphous ribbons of $Co_{72.6}Fe_{9.8}Ni_{5.5}B_{2.4}Si_{7.1}Cr_{2.6}$ containing 121 ppm of nitrogen showed relatively high saturation magnetization. The alloy ribbons crystallized at $540^{\circ}C$ showed that the grain size of $Co_{72.6}Fe_{9.8}Ni_{5.5}B_{2.4}Si_{7.1}Cr_{2.6}$ alloy containing 121 ppm of nitrogen was about f nm, which exhibited paramagnetic behavior. The formation of nano-grain structure was attributed to the finely dispersed Fe4N particles and the solid-solutionized nitrogen atoms in the matrix. Accordingly, it can be concluded that the nano-grain structure of 5nm in size could reduce the core loss within the normally applied magnetic field of 300A/m at 10kHz.

Electrochemical Performance of M2GeO4 (M = Co, Fe and Ni) as Anode Materials with High Capacity for Lithium-Ion Batteries

  • Yuvaraj, Subramanian;Park, Myung-Soo;Kumar, Veerasubramani Ganesh;Lee, Yun Sung;Kim, Dong-Won
    • Journal of Electrochemical Science and Technology
    • /
    • 제8권4호
    • /
    • pp.323-330
    • /
    • 2017
  • $M_2GeO_4$ (M = Co, Fe and Ni) was synthesized as an anode material for lithium-ion batteries and its electrochemical characteristics were investigated. The $Fe_2GeO_4$ electrode exhibited an initial discharge capacity of $1127.8mAh\;g^{-1}$ and better capacity retention than $Co_2GeO_4$ and $Ni_2GeO_4$. A diffusion coefficient of lithium ion in the $Fe_2GeO_4$ electrode was measured to be $12.7{\times}10^{-8}cm^2s^{-1}$, which was higher than those of the other two electrodes. The electrochemical performance of the $Fe_2GeO_4$ electrode was improved by coating carbon onto the surface of $Fe_2GeO_4$ particles. The carbon-coated $Fe_2GeO_4$ electrode delivered a high initial discharge capacity of $1144.9mAh\;g^{-1}$ with good capacity retention. The enhanced cycling performance was mainly attributed to the carbon-coated layer that accommodates the volume change of the active materials and improves the electronic conductivity. Our results demonstrate that the carbon-coated $Fe_2GeO_4$ can be a promising anode material for achieving high energy density lithium-ion batteries.

공침법으로 제조한 Ni-Cu-Zn Ferrite의 Ni 첨가량과 온도에 따른 주파수 및 물리적 특성 연구 (A Study on Frequency and the Physical Properties of Ni-Cu-Zn Ferrites with the Variation of Ni Addition and Temperature Prepared by Co-Precipitation Method)

  • 김문석;고재귀
    • 한국자기학회지
    • /
    • 제15권5호
    • /
    • pp.282-286
    • /
    • 2005
  • 공침법으로 제조한 Ni-Cu-Zn ferrite를 사용하여 전파흡수체로 사용할 저온소결용 ferrite를 연구하였다. Ni 첨가량에 따른 조성비 및 가소온도와 소결온도 변화를 시켜 전파흡수특성 및 물리적 특성을 고찰하였다. XRD pattern을 통하여 spinel구조를 가짐을 확인하였고, 공침법으로 제조된 Ni-Cu-Zn ferrite 미분말이 나노입자 크기를 보였다 소결온도가 $1100^{\circ}C$이고 Ni 함량이 많을 수록 투자율이 낮고 손실계수도 높게 측정되어 흡수 능력도 좋아짐을 알 수 있고, MHz 영역에서 사용할 수 있다고 사료된다. 그리고 소결온도 $1100^{\circ}C$이고 $(Ni_{0.7}Cu_{0.2}Zn_{0.1}O)_{1.02}(Fe_{2}O_3)_{0.98}$ 조성일 때가 가장 손실이 크므로 전파흡수체로 사용할 조성임을 확인 할 수 있었다.

Crystallographic and Magnetic Properties of Nano-sized Nickel Substituted Cobalt Ferrites Synthesized by the Sol-gel Method

  • Choi, Won-Ok;Lee, Jae-Gwang;Kang, Byung-Sub;Chae, Kwang Pyo
    • Journal of Magnetics
    • /
    • 제19권1호
    • /
    • pp.59-63
    • /
    • 2014
  • Nano-sized nickel substituted cobalt ferrite powders, $Ni_xCo_{1-x}Fe_2O_4$ ($0.0{\leq}x{\leq}1.0$), were fabricated by the sol-gel method, and their crystallographic and magnetic properties were studied. All the ferrite powders showed a single spinel structure, and behaved ferrimagnetically. When the nickel substitution was increased, the lattice constants and the sizes of particles of the ferrite powders decreased. The M$\ddot{o}$ssbauer absorption spectra of $Ni_xCo_{1-x}Fe_2O_4$ ferrite powders could be fitted with two six-line subspectra, which were assigned to a tetrahedral A-site and octahedral B-sites of a typical spinel crystal structure. The increase in values of the magnetic hyperfine fields indicated that the superexchange interaction was stronger, with the increased nickel concentration in $Ni_xCo_{1-x}Fe_2O_4$. This could be explained using the cation distribution, which can be written as, $(Co_{0.28-0.28x}Fe_{0.72+0.28x})[Ni_xCo_{0.72-0.72x}Fe_{1.28-0.28x}]O_4$. The two values of the saturation magnetization and the coercivity decreased, as the rate of nickel substitution was increased. These decreases could be explained using the cation distribution, the magnetic moment, and the magneto crystalline anisotropy constant of the substituted ions.

CO$_2$ 분해 반응에서 금속 산화물이 첨가된 $Fe_2O_4$의 영향 (Effects of Magnetite added with Metallic Oxide on the Decomposition Reaction of Carbon Dioxide)

  • Kim, Seung-Ho;Park, Young-Goo
    • 한국환경보건학회지
    • /
    • 제24권1호
    • /
    • pp.32-37
    • /
    • 1998
  • The Carbon Dioxide is the gas, which causes green house effects, unusual changes in the weather, destruction of the life. Almost every nation in the world is trying to search the countermeasure to this poisonous gas. I synthesized $Fe_3O_4$ and NaOH, in order to decompose the Carbon Dioxide. Among the particles synthesizing $Fe_3O_4$, I chose the equivalent ratio 1.00 which can decompose the Carbon Dioxide best, and fixed that equivalent ratio and added the 0.005-3.00 mole percentage of NiCl$_2$ and synthesized $Fe_3O_4$. I studied the decomposition of the Carbon Dioxide and methanized reaction, by measuring its crystal structure, thermochemistrical character and specific surface area. In decomposing the Carbon Dioxide, I used oxygen-deficit Magnetite which I produced by injecting the hydrogen gas into the synthesized sample. I observed the methanization reaction by raising the temperature of sample up to 650$\circ$C and having it reacted with the hydrogen gas. The decomposition of the Carbon Dioxide was added 0.005, 0.03, 0.05 mole percentage of NiCl$_2$ was more effective than pure $Fe_3O_4$. All sample in which the decomposition of the Carbon Dioxide took place produced the methane gas.

  • PDF

액중 전기선 폭발법에 의한 Ni-free Fe계 나노 합금분말의 제조: 2. 용매의 영향 및 제조 방법에 따른 분말입자의 비교 (Fabrication of Ni-free Fe-based Alloy Nano Powder by Pulsed Wire Evaporation in Liquid: Part 2. Effect of Solvent and Comparison of Fabricated Powder owing to Fabrication Method)

  • 류호진;이용희;손광욱;공영민;김진천;김병기;윤중열
    • 한국분말재료학회지
    • /
    • 제18권2호
    • /
    • pp.112-121
    • /
    • 2011
  • This study investigated the effect of solvent on the fabrication of Ni-free Fe-based alloy nano powders by employing the PWE (pulsed wire evaporation) in liquid and compared the alloy particles fabricated by three different methods (PWE in liquid, PWE in Ar, plasma arc discharge), for high temperature oxidation-resistant metallic porous body for high temperature soot filter system. Three different solvents (ethanol, acetone, distilled water) of liquid were adapted in PWE in liquid process, while X-ray diffraction (XRD), field emission scanning microscope (FE-SEM), and transmission electron microscope (TEM) were used to investigate the characteristics of the Fe-Cr-Al nano powders. The alloy powder synthesized by PWE in ethanol has good particle size and no surface oxidation compared to that of distilled water. Since the Fe-based alloy powders, which were fabricated by PWE in Ar and PAD process, showed surface oxidation by TEM analysis, the PWE in ethanol is the best way to fabricate Fe-based alloy nano powder.

서남해안 연근해저 퇴적물의 중금속 함량 및 분포 (Some heavy metal concentration of surface sediments from the southwestern coast of Korea)

  • 전수경;조영길
    • 한국환경과학회지
    • /
    • 제11권12호
    • /
    • pp.1299-1305
    • /
    • 2002
  • Thirty sediment samples of the <63${\mu}{\textrm}{m}$ fraction collected from the southwestern coast of Korea were analysed for their heavy metal (Fe, Mn, Cr, Co, Cu, Ni, Zn and Pb) concentration. The results show that sediment texture plays a controlling role on the total metal concentrations and their spatial distribution. A single lM HCl extraction procedure was used in order to assess the environmental risk of heavy metals in bottom sediments. The non-residual fraction was the most abundant pool for Mn and Pb in most samples, which means that this metals are highly avaliable in these sediments. Cr, Ni, Fe, Co, Zn and Cu were mainly associated with the residual fraction, suggesting that their concentrations are controlled significantly by transport processes with the fine particles as carriers from diffuse pollution source. Concentration enrichment ratios(CER) were calculated from the non-residual contents and their values allowed us to classify the sediments according to their environmental risk.