Effect of Al on Structural and Magnetic Characteristics of CoCrFeNiMnAlx High Entropy Alloys

  • Majid Tavoosi;Ali Ghasemi;Gholam Reza Gordani;Mohammad Reza Loghman Estarki
    • 한국재료학회지
    • /
    • 제33권3호
    • /
    • pp.95-100
    • /
    • 2023
  • This research examines the effect of adding aluminum on the structural, phasic, and magnetic properties of CoCrFe NiMnAlx high-entropy alloys. To this aim, the arc-melt process was used under an argon atmosphere for preparing cast samples. The phasic, structural, and magnetic properties of the samples were characterized by x-ray diffraction (XRD), scanning electron microscopy (SEM), and vibrational magnetometry (VSM) analyses. Based on the results, the addition of aluminum to the compound caused changes in the crystalline structure, from FCC solid solution in the CoCrFeNiMn sample to CoCrFeNiMnAl BBC solid solution. It was associated with changes in the magnetic property of CoCrFeNiMnAlx high-entropy alloys, from paramagnetic to ferromagnetic. The maximum saturation magnetization for the CoCrFeNiMnAl casting sample was estimated to be around 79 emu/g. Despite the phase stability of the FCC solid solution with temperature, the solid solution phase formed in the CrCrFeNiMnAl high-entropy compound was not stable, and changed into FCC solid solution with temperature elevation, causing a reduction in saturation magnetization to about 7 emu/g.

베릴륨이 함유되지 않은 니켈-크롬 합금 코어와 코발트-크롬 합금 코어의 적합도 비교평가 (Comparison of the marginal and internal fit of cores fabricated by Ni-Cr alloy(non-beryllium) and Co-Cr alloy)

  • 김기백;김재홍;김웅철;김지환
    • 대한치과기공학회지
    • /
    • 제34권4호
    • /
    • pp.353-359
    • /
    • 2012
  • Purpose: The aim of this study measured and compared the marginal and internal fit of metal cores with two base metal alloy (Ni-Cr alloy(non-beryllium), Co-Cr alloy). Methods: Maxillary right first molar abutment fabricated by titanium was prepared for this study. Impressions(10ea) were made from titanium model, and study models were poured with improved dental stone. Wax cores of twenty were prepared for burn-out and casting. Ten wax cores cast Ni-Cr alloy(non-Be), and finally ten cast Co-Cr alloy. Marginal and internal fit of cores was evaluated using silicone replica technique and digital microscope(x160). The data were statistically analyzed with the independent samples t-test (${\alpha}$ <.05). Results: Mean(standard deviation, SD) marginal and internal fit total size of Ni-Cr alloy(non-Be) group was $73.3(14.4){\mu}m$ and of Co-Cr alloy group $65.6(17.4){\mu}m$. The marginal and internal fit total size of Ni-Cr alloy group(non-Be) was statistically significantly greater than that of Co-Cr alloy group (P=.004). Conclusion: Co-Cr alloy cores in this study had a better marginal fit than Ni-Cr alloy(non-Be) cores.

DC 마그네트론 스퍼터링 NiCr 박막의 열처리 조건에 따른 미세구조 및 표면특성 (Micro Structure and Surface Characteristics of NiCr Thin films Prepared by DC Magnetron Sputter according to Annealing Conditions)

  • 권용;김남훈;최동유;이우선;서용진;박진성
    • 한국전기전자재료학회논문지
    • /
    • 제18권6호
    • /
    • pp.554-559
    • /
    • 2005
  • Ni/Cr thin film is very interesting material as thin film resistors, filaments, and humidity sensors because their relatively large resistivity, more resistant to oxidation and a low temperature coefficient of resistance (TCR). These interesting properties of Ni/Cr thin films are dependent upon the preparation conditions including the deposition environment and subsequent annealing treatments. Ni/Cr thin films of 250 nm were deposited by DC magnetron sputtering on $Al_2O_3/Si$ substrate with 2-inch Ni/Cr (80/20) alloy target at room temperature for 45 minutes. Annealing treatments were performed at $400^{\circ}C,\;500^{\circ}C,\;and\;600^{\circ}C$ for 6 hours in air or $H_2$ ambient, respectively. The clear crystal boundaries without crystal growth and the densification were accomplished when the pores were disappeared in air ambient. Most of surface was oxidic including NiO, $Ni_2O_3$ and $Cr_xO_y$(x=1,2, y=2,3) after annealing in air ambient. The crystal growth in $H_2$ ambient was formed and stabilized by combination with each other due to the suppression of oxidized substance on film surface. Most oxidic Ni was restored when the oxidic Cr was present due to its stability in high-temperature $H_2$ ambient.

$H_2/O_2$ 비에 따른 Hybrid HVOF 용사된 $Cr_3C_2$-7wt%(NiCr) 용사층의 특성 및 산화거동 (Characteristics and oxidation behavior of the hybrid-HVOF sprayed $Cr_3C_2$-7wt%(NiCr) coatings depending on $H_2/O_2$ ratio)

  • 김병희;서동수
    • Journal of Welding and Joining
    • /
    • 제15권4호
    • /
    • pp.126-135
    • /
    • 1997
  • $H_2/O_2$ 비에 따른 Hybrid HVOF 용사된 $Cr_3C_2$-7wt%(NiCr) 용사층의 특성 및 산화거동 This study was performed to investigate the influence of fuel/oxygen ratio (F/O=3.2, 3.0, 2.8) on the characteristics and the oxidation behavior of the hybrid-HVOF sprayed $Cr_3C_2$-7wt%NiCr coatings. Decomposition and the oxidation of the $Cr_3C_2$was occured during spraying. The degree of transformation from $Cr_3C_2$to $Cr_7C_3$ was increased with decreasing the F/O ratio. The microstructural differences of the as sprayed coating with F/O ratio can not be distinguished, However, large pores were diminished and then the coatings became dense by heat treatment. Microhardness of the as-sprayed specimen which sprayed with F/O=3.0 condition was hightest ($Hv_{300}$=1140) and the hardness was increased to 1500 after heat treatment at $600^{\circ}C$ for 50hrs in air. It was supposed that hardness was increased due to the formation of $Cr_2O_3$ within $Cr_3C_2$/$Cr_7C_3$matrix and the densification of coating layer during heat treatment. Apparent activation energy for oxidation was varied from 21.2 kcal$mol^{-1}K^{-1}$ to 23.8 kcal$mol^{-1}K^{-1}$ with respect to the F/O ratio. The surface morphology was changed to porous and oxide chusters were grown after oxidation $1000^{\circ}C$ for 50 hours by the aggressive evolution of gas phase ($CrO_3$ and$CO_2$). The oxide cluster was composed of Ni and Cr.

  • PDF

플라즈마 용사 및 EB-PVD에 의한 열벽코팅 수명에 대한 산화물 생성의 영향 (The Effect of Oxide Formation on the Lifetime of Plasma Sprayed or EB-PVD Thermal Barrier Coatings)

  • 이의열
    • 한국표면공학회지
    • /
    • 제27권2호
    • /
    • pp.91-98
    • /
    • 1994
  • For the plasma sprayed as well as the EB-PVD thermal barrier coatings, the fracture paths within the oxidation products developed at the interface between the partially stabilized zirconia ceramic coating and NiCoCrAlY bond coat during cyclic thermal oxidation has been investigated. It was observed that the fracture in the oxidation products primarily took place within the oxide such as $Ni_{1-x}Co_3(Al_,Cr)_2O_4$ or at the interface between the oxide and $Al_2O_3$. It was found that Al2O3 developed first, followed by the Ni/Co/Cr rich oxides such as ,,$Ni_{1-x}Co_x(Al_,Cr)_2O_4$ $Cr_2O_3$and NiO at the interface between the ceramic coating and the bond coat in a cyclic high temperature environment. It was therfore concluded that the formation of the oxide containing Ni, Cr and Co was a life-limiting event for thermal barrier coatings during cyclic thermal oxidation.

  • PDF

가스버너 열충격에 의한 NiCr/ZrO2계 경사기능재의 열적 파괴특성 (Fracture Characteristics of NiCr/ZrO2 Functionally Graded Material by Gas Burner Thermal Shock)

  • 송준희
    • 한국세라믹학회지
    • /
    • 제43권4호
    • /
    • pp.247-252
    • /
    • 2006
  • Joining Yittria Stabilized Zirconia (YSZ) to NiCr metal was fabricated using YSZ/NiCr Functionally Graded Materials (FGM) Interlayer by hot pressing process. Microscopic observations demonstrate that the composition and microstructure of YSZ/NiCr FGM distribute gradually in stepwise way, eliminating the macroscopic ceramic/metal interface such as that in traditional ceramic/metal joint. The thermal characteristics of this YSZ/FGM/NiCr joint were studied by thermal shock testing and therml barrier testing. Thermal shock test was conducted by gas burner rig. Acoustic Emission (AE) monitoring was performed to analyze the microfracture behavior during the thermal shock test. It could be confirmed that FGM was the excellent performance of thermal shock/barrier resistance at above $1000^{\circ}C$.

Corrosion of Fe-Cr Steels at 600-800℃ in NaCl Salts

  • Lee, Dong Bok;Kim, Min Jung;Yadav, Poonam;Xiao, Xiao
    • 한국표면공학회지
    • /
    • 제51권6호
    • /
    • pp.354-359
    • /
    • 2018
  • NaCl-induced hot corrosion behavior of ASTM T22 (Fe-2.25Cr-1Mo), T91 (Fe-9Cr-1Mo), T92 (Fe-9Cr-1.8W-0.5Mo), 347HFG (Fe-18-Cr-11Ni), and 310H (Fe-25Cr-19Ni) steels was studied after spraying NaCl on the surface. During corrosion at $600-800^{\circ}C$ for 50-100 h, thick, non-adherent, fragile, somewhat porous oxide scales formed. All the alloys corroded fast with large weight gains owing to fast scaling and destruction of protective oxide scales. Corrosion rates increased progressively as the corrosion temperature and time increased. Corrosion resistance increased in the order of T22, T91, T92, 347HFG, and 310H, suggesting that the alloying elements of Cr, Ni, and W beneficially improved the corrosion resistance of steels. Basically, Fe oxidized to $Fe_2O_3$, and Cr oxidized to $Cr_2O_3$, some of which further reacted with FeO to form $FeCr_2O_4$ or with NiO to form $NiCr_2O_4$.

Zn-Pr-Co-Er-M(M=Ni, Mg, Cr)산화물계 바리스터의 전기적, 유전적 특성 (Electrical and Dielectric Characteristics of Zn-Pr-Co-Er-M(M=Ni, Mg, Cr) Oxides-Based Varistors)

  • 남춘우;김명준
    • 한국세라믹학회지
    • /
    • 제41권8호
    • /
    • pp.605-609
    • /
    • 2004
  • 다양한 금속산화물(NiO, MgO, Cr$_2$O$_3$) 첨가에 따른 ZnO 바리스터의 미세구조, 전기적, 유전적 특성을 조사하였다. 평균 결정립 크기는 NiO 첨가로 증가한 반면 Cr$_2$O$_3$ 첨가로 감소하였다 이로 인해 바리스터 전압은Cr$_2$O$_3$ 첨가시 더 높게 나타났다. 바리스터 가운데서 Cr$_2$O$_3$가 첨가된 바리스터가 비직선 지수가 40.5, 누설전류가 2.7 $\mu$A로 가장 우수한 비직선성을 나타내었으며, 유전손실도 0.0589로 비교적 낮게 나타났다.