• Title/Summary/Keyword: Ni-20 Cr

Search Result 319, Processing Time 0.022 seconds

A Study on the Adaptability and Cytotoxicity of Porcelain Bonded Ni-Cr Alloy (도재소부용 Ni-Cr합금의 적합성과 세포독성에 관한 연구)

  • Choi, Boo-Byung;Shin, Myung-Chull
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.20 no.1
    • /
    • pp.7-17
    • /
    • 1982
  • In order to investigate the internal adaptability and cytotoxicity for porcelain fused to metal Ni-Cr alloy, two commercial alloys (Generic Gold-R alloy, Aalba Dent- Valloy)were employed and compared with new developed beryllium free Ni-Cr alloy (KIST-K alloy). After cementation of each crown to abutment die before and after ceramic bonding respectively, dies were mounted to epoxy resin and the internal space was measured between crown and die of each point on sagittal section. The results were as follows: 1) The results show that the space between the crown and the die was largest at the incisal edge, followed by the shoulder or the bevel and chamfer. The least was to be in the axial surface. 2) There were no significant difference in the adaptability of the compared alloys. 3) On day 2 of the experiment the cell multiplication was slightly inhibited by R and K alloys. However, observations taken at day 4 and 7 showed normal cell multiplication process compared to control group. 4) Alloy V exhibited the most severe cell toxicity among the alloys tested on day 2. By day 4 and 7 it showed a decrease level in toxicity, however it did not exhibit normal cell growth as compared to control group.

  • PDF

A study on the high temperature properties of CoNiCrAlY coating fabricated by HVOF and LPPS process (LPPS용사법과 HVOF 용사법으로 제조된 CoNiCrAlY 코팅의 고온물성에 관한 연구)

  • 강현욱;권현옥;송요승
    • Journal of the Korean institute of surface engineering
    • /
    • v.34 no.2
    • /
    • pp.161-168
    • /
    • 2001
  • A Thermal Barrier Coating (TBC) can play an important role in protecting parts from harmful environments at high temperatures such as oxidation, corrosion, and wear in order to improve the efficiency of aircraft engines by lowering the surface temperature of the turbine blade. The TBC can increase the life span of the product and improve the operating properties. Therefore, in this study the mechanical and thermal properties of the TBC such as oxidation, fatigue and shock at high temperatures were evaluated. A samples of a bond coat (CoNiCrAlY) produced by the High Velocity Oxygen Fuel (HVOF) and Low Pressure Plasma Spray (LPPS) method were used. The thickness of the HVOF coating layer was approximately $450\mu\textrm{m}$ to 500$\mu\textrm{m}$ and the hardness number of the coating layer was between 350Hv and 400Hv. The thickness of the LPPS coating was about 350$\mu\textrm{m}$ to 400$\mu\textrm{m}$ and the hardness number of the coating was about 370Hv to 420Hv. The X-ray diffraction analysis showed that CoNiCrAlY coating layer of the HVOF and LPPS was composed of the $\beta$and ${\gamma}$phase. After the high temperature oxidation test, the oxide scale with about l0$\mu\textrm{m}$ to 20$\mu\textrm{m}$ thickness appeared at the coating surface on the Al-depleted zone was observed under the oxide scale layer.

  • PDF

Evaluation of Elevated Temperature Strength of Al-Cr-Zr Alloys Strengthened by Nanostructured Crystallines and Intermetallic Compounds (I) (나노 결정립과 금속간화합물상에 의해 강화된 고온, 고강도 Al-Cr-Zr 합금개발 및 특성평가 (I))

  • 양상선
    • Journal of Powder Materials
    • /
    • v.6 no.1
    • /
    • pp.49-55
    • /
    • 1999
  • Al-Cr-Zr nanocomposite metal powders were prepared by mechnical alloying (MA) in order to develop aircraft structure materials with lighter weight and lower cost than the conventional Ti and Ni alloys. The morphological changes and microstrutural evolution of Al-6wt.%Cr-3wt.%Zr nanocomposite metal powders during MA were investigated by SEM, XRD and TEM. The approximately 50$\mu$m sized Al-Cr-Zr nanocomposite metal powders has been formed after 20 h of MA. The individual X-ray diffraction peaks of Al, Cr and Zr were broadened and peak intensitied were decreased as a function of MA time. The observed Al crystallite size by TEM was in the range of 20 nm, which is a simliar value calculated by Scherrer equation. The microhardness of Al-Cr-Zr nanocomposite metal powders increases alomost linearly with increase of the processing time, reaching a saturation hardness value of 127 kg/$mm^2$ after 20 h of processing. The intermetallic compound phase of $Al_3Zr_4$ in the matrix was identifed by XRD and TEM.

  • PDF

Relationship between Serum Levels of Microminerals and Lipids in Korean Adults on Self-Selected Diet (정상 성인의 혈중 미량무기질과 지질과의 관련성에 관한 연구-충남지역 일부 여대생의 혈중 As, Cr, Mn, Se, Ni을 중심으로-)

  • 최미경
    • Korean Journal of Community Nutrition
    • /
    • v.5 no.2
    • /
    • pp.289-296
    • /
    • 2000
  • The purpose of this study was to investigate the relationship and lipids in healthy adults on self-selected diets. These subjects consisted of 40 female college students residing in Chungnam. Anthropometric measure-ments, diet intake measurements, and blood collection were conducted. Serum concentrations of 5 microminerals(As, Cr, Mn, Se, Ni), lipids(triglyceride, total cholesterol, HDL-cholesterol), and glucose were measured by an ICP spectrometer and biochemical analyzer. The results were as follows. The mean age of the subjects was 22.34 years and the mean weight, height, and BMI were 52.89kg, 161.29cm and 20.34, respectively. The mean serum concentrations appeared to be 14.60ug/dl(As), 1.87ug/dl(Cr), 0.18ug/dl(Mn), 23.50ug/dl(Se), 0.21ug/dl(Ni), 60.73mg/dl(triglyceride), 138.49mg/dl(total cholesterol), 65.95mg/dl(HDL-cholesterol), 60.39mg/dl(LDL-cholesterol) and 88.82mg/dl(glucose). When analyzed by Pearson’s correlation coefficient, the serum concentration of Cr was negatively correlated with Ca and vitamin B12 intake(p〈0.05, p〈0.05) respectively, Mn was negatively correlated with Na intake(p〈0.05), Ni, however, was positively correlated with K intake(p〈0.05). The serum concentration of Se was positively correlated with LDL-cholesterol(p〈0.05), Ni, however, negatively correlated with total cholesterol, HDL-cholesterol, LDL-cholesterol, and glucose, respectively(p〈0.001, p〈0.01, p〈0.05). Further studies are needed to clarify the precise micromineral intakes, nutritional assessment of microminerals, and cause-effect relation of microminerals and serum lipids.

  • PDF

Wear Corrosion Behaviour of Nitrogen Ion Implanted Super Stainless Steel (질소이온주입된 초내식성 스테인리스강의 마모부식 특성)

  • Kang, Sun-Hwa;Kim, Cheol-Sang
    • Proceedings of the KOSOMBE Conference
    • /
    • v.1994 no.12
    • /
    • pp.175-177
    • /
    • 1994
  • The wear corrosion behaviour of a nitrogen ion implanted super stainless steel (S.S.S, 22Cr - 20Ni - 6Mo - 0.25N) was compared with those of S.S.S, 316L SS and TiN coated 316L SS. The Cr and Ni amounts won out from the materials were investigated using an electrothermal atomic absorption spectrometry. We observed that the Cr dissolution rate of the S.S.S was similar to that of 316L SS, however, the Ni release of the S.S.S was feater than 316L SS. The metal ions released from the nitrogen ion implanted S.S.S surface were significantly reduced. The wear corrosion behaviour of the stainless steels was not correlated with the results shown by a static metal ion release test.

  • PDF

Characteristics of ($AI_2$ $O_3$40%$YiO_2$)NiCr thermal sprayed composite coatings (($AI_2$ $O_3$40%$YiO_2$)NiCr 복합용사피막의 특성)

  • 김경호;박경채;김태형
    • Proceedings of the KWS Conference
    • /
    • 2003.05a
    • /
    • pp.114-116
    • /
    • 2003
  • The multi function sprayed coating is used for direct-heating, wear resistance and high bonding strength. The merits of surface direct-heating coatings are short warming time, low power consumption and better wear resistance that can be used in many organization parts. In this study, the surface direct-heating and wear resistance can be improved by spraying the proper materials on the surface $Al_2$O$_3$40%TiO$_2$ powder and Ni-20%Cr powder that had the properties of conduction and high wear resistivity are used in order to improve wear resistance, electrical properties and bonding strength.

  • PDF

Effect of RF Sputtering Conditions on Properties of Thin Film Resistor for Microwave Device (초고주파용 박막저항의 특성에 미치는 RF 스파터링 조건의 영향)

  • Ryu, Sung-Rok;Koo, Bon-Keup;Kang, Beong-Don;Ryu, Jei-Chun;Kim, Dong-Jin
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.07b
    • /
    • pp.913-917
    • /
    • 2003
  • In the electronic components and devices fabrication, thin film resistors with low TCR(temperature coefficient of resistance) and high precision have been used over 3 GHz microwave in recent years. Ni-Cr alloys thin films resistors is one of the most commonly used resistive materials because it has low TCR and highly stable resistance. In this work, we fabricated thin film resistors using Evanohm alloys target(72Ni-20Cr-3Al-4Mn-Si) of s-type with excellent resistors properties by RF-sputtering. Also we reported best deposited conditions of thin film resistors for microwave to observe microstructure and electronic properties of thin film according to deposited conditions(between target and substrate, power supply)

  • PDF

Sliding Wear and Corrosion Resistance of Copper-based Overhead Catenary for Traction Systems

  • Kwok, C.T.;Wong, P.K.;Man, H.C.;Cheng, F.T.
    • International Journal of Railway
    • /
    • v.3 no.1
    • /
    • pp.19-27
    • /
    • 2010
  • In the present study, the electrical sliding wear and corrosion resistance of pure copper (Cu) and six age-hardened copper alloys (CuCr, CuZr, CuCrZr, CuNiSiCr, CuBe and CuBeNi) were investigated by a pin-on-disc tribometer and electrochemical measurement. Various copper-based alloys in the form of cylindrical pin were forced to slide against a counterface stainless steel disc in air under unlubricated condition at a sliding velocity of 31 km/h under normal load up to 20 N with and without electric current. The worn surface of and wear debris from the specimens were studied by scanning electron microscopy. Both mechanical wear and electrical arc erosion were the wear mechanisms for the alloys worn at 50 A. Owing to its good electrical conductivity, high wear and corrosion resistance, CuCrZr is a promising candidate as the overhead catenary material for electric traction systems.

  • PDF

Heavy Metals in Surface Sediments from Doam Bay, Southwestern Coast of Korea (한국 남서해안 도암만 표층퇴적물의 중금속 함량 및 분포 특성)

  • CHO, HYEONG-CHAN;CHO, YEONG-GIL
    • The Sea:JOURNAL OF THE KOREAN SOCIETY OF OCEANOGRAPHY
    • /
    • v.20 no.4
    • /
    • pp.159-168
    • /
    • 2015
  • Forty-four surface sediments from Doam Bay were analyzed for total organic carbon (TOC), total nitrogen (TN), total metal (Al, Fe, Mn, Cr, Cu, Ni, Pb, Zn) and further chemical partitioning of metals were carried out in some samples. The TOC (0.32~3.10%) and TN (0.03~0.26%) values of the samples were similar to those of other coastal area. The C/N ratios ranged from 7.9 to 11.9 with an average 9.3 which revealed that contribution of terrestrial organic matters was relatively rare. Contents of analysed metals showed a level lower than threshold effects level (TEL) in sediment quality guidelines. Based on the chemical speciation of metals, the lattice fractions were found in the order Cr > Cu > Ni > Zn > Pb > Mn, while Mn and Pb are the ratio of the non-lattice fractions accounted for more than 50%. The average baseline values were obtained relative cumulative frequency curves and linear regression analysis. The respective baseline concentrations for Cu, Ni, Pb, Zn, Cr and Mn were 11.8, 23.1, 26.8, 76.6, 56.7, 585 mg/kg, respectively. Based on geoaccumulation index ($I_{geo}$) with a baseline values of Mn showed that face the contamination phase from estuarine stations. However, in case of Zn and Pb, although there is no sign of contamination, it could be release from sediment when there is a change in the environment, which is caused from the high ratio of non-lattice fractions.

Magnetoresistance of $[FeNi/Cu/CoFe(Co)/Cu]_N$ Spin-Valve Multilayers ($[FeNi/Cu/CoFe(Co)/Cu]_N$ Spin-Valve 다층박막의 자기저항 특성)

  • 김미양;이정미;최규리;오미영;이장로
    • Journal of the Korean Magnetics Society
    • /
    • v.9 no.1
    • /
    • pp.41-47
    • /
    • 1999
  • $Buffer/[NiFe/Cu/CoFe(Co)/Cu]_N$ spin valve multilayers prepared by dc magnetron sputtering on a corning glass substrate using NiFe and CoFe(Co) posses different coercivities. Dependence of magnetoresistance on the type and thickness of buffer layer, thickness of Cu, NiFe, stacking number of multilayer, substrate temperature and annealing temperature in the form $[NiFe/Cu/CoFe(Co)/Cu]_N$ spin-valve multilayers were investigated. To evaluate effect of magnetoresistance for this samples, X-ray diffraction analysis, vibrating sample magnetometer analysis, and magnetoresistance measurement (4-probe method) were performed the maximum magnetoresistance ratio and coercivity were 7.5 % and 140 Oe, respectively for $Cr-50{\AA}/[NiFe-20{\AA}/Cu-{\AA}/Co-20{\AA}/Cu-50{\AA}]_10$ at substrate temperature of 9$0^{\circ}C$. Magnetoresistance slope maintained 0.25%/Oe until 15$0^{\circ}C$ of annealing temperature, and then decreased to 0.03%/Oe at 20$0^{\circ}C$. It was confirmed that the main factor of thermal stability was deteriorating of soft magnetic properties in the NiFe layer.

  • PDF