• Title/Summary/Keyword: NbTi alloy

Search Result 159, Processing Time 0.022 seconds

Oxidation Properties and Biocompatibility of Ti-8wt.%Ta-8wt.%Nb Alloy (Ti-8wt.%Ta-3wt.%Nb합금의 산화특성 및 생체안정성)

  • Lee Doh-Jae;Lee Kyung-Ku;Park Bum-Su;Lee Kwang-Min;Park Sang-Won
    • Journal of the Korean institute of surface engineering
    • /
    • v.39 no.1
    • /
    • pp.43-48
    • /
    • 2006
  • The oxidation behavior and Biocompatibility of pure Ti and Ti-8Ta-3Nb alloy were studied in dry air atmosphere. The specimens showed that Ti-8Ta-3Nb alloy had higher oxidation resistance than pure Ti at $650^{\circ}C$. Cytotoxicity test also revealed that moderate oxidation treatment lower cell toxicity and Ti-8Ta-3Nb alloy showed better results compared with pure Ti. The weight gains during the oxidation increase rapidly at temperature above $600^{\circ}C$.

Investigation on the Effects of Hydrogen Charging on Oxidation Behavior of Ultrahigh-Strength Automotive Steels (초고강도 자동차용 강의 환원정전류인가에 따른 산화 거동 변화 연구)

  • Ha, Heon-Young;Kim, Hye-Jin;Moon, Joonoh;Lee, Tae-Ho;Jo, Hyo-Haeng;Lee, Chang-Geun;Yoo, Byung-Kil;Yang, Won-Seog
    • Corrosion Science and Technology
    • /
    • v.16 no.6
    • /
    • pp.317-327
    • /
    • 2017
  • The change in the oxidation behavior of three types of B-added ultrahigh strength martensitic steels containing Ti and Nb induced by applying constant cathodic current was investigated. In a 3% NaCl+0.3% $NH_4SCN$ solution, the overall polarization behavior of the three alloys was similar, and degradation of the oxide film was observed in the three alloys after applying constant cathodic current. A significant increase in the anodic current density was observed in the Nb-added alloy, while it was diminished in the Ti-added alloy. Both Ti and Nb alloying decreased the hydrogen overpotential by forming NbC and TiC particles. In addition, the thickest oxide film was formed on the Ti-added alloy, but the addition of Nb decreased the film thickness. Therefore, it was concluded that the remarkable increase in the anodic current density of Nb-added alloy induced by applying constant cathodic current density was attributed to the formation of the thinnest oxide film less protective to hydrogen absorption, and the addition of Ti effectively blocked the hydrogen absorption by forming TiC particles and a relatively thick oxide film.

Study for Fatigue Crack Propagation Behavior of Ti-alloy (Ti 합금의 피로 특성 고찰)

  • 정화일;조규종
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1997.10a
    • /
    • pp.786-789
    • /
    • 1997
  • Ti-6Al-4V has been used widely in biomedical field. But because of its toxicity, the ${\beta}$ stabilizing element, V, in Ti-6Al-4V has been replaced by Nb, Ta. Ti-10Ta-10Nb has been developed for biomedical applications. The fatigue crack propagation behavior of Ti-alloy(Ti-10Ta-10Nb) was investigated, in comparison with that of pure Ti. In order to better understand the fundamental fatigue behavior of Ti-10Ta-10Nb, rotating bending fatigue tests have been carried out. Ti-10Ta-10Nb has a better fatigue strength than pure Ti. In this paper, fatigue life has been predicted with Nisitani's equation of the fatigue crack propagation that can be established by measuring fatigue crack growth rates.

  • PDF

Effects of Melting and Rolling Condition of Ti-10wt.%Ta-10wt.%Nb Alloy on Microstructure Variation (용해 및 가공조건 변화가 Ti-10wt.%Ta-10wt.%Nb합금의 미세조직에 미치는 영향)

  • Lee, Doh-Jae;Lee, Kwang-Min;Kim, Min-Ki;Lee, Kyung-Ku
    • Journal of Korea Foundry Society
    • /
    • v.22 no.3
    • /
    • pp.114-120
    • /
    • 2002
  • A new titanium based alloy, Ti-10Ta-10Nb, has designed to examine the improved mechanical properties and biocompatibility. A specimen of titanium alloy was melted in a consumable vacuum arc furnace and homogenized at $1050^{\circ}C$ for 24 h. The effect of hot rolling on microstructure was estimated after rolling at $400^{\circ}C$ and $800^{\circ}C$ respectively. Surface of melted alloy by consumable vacuum arc melting was consisted of rough surface and it was changed to sound surface by coating of $ZrO_2$ slurry on copper mold surface. The hardness of Ti-10Ta-10Nb alloy increased with the amount of${\alpha}+{\beta}$ phase. Ti-10Ta-10Nb alloy showed $Widmanst{\"{a}}ten$ structure by hot rolling at $800^{\circ}C$ and in the rolling ${\beta}-region$ was negligible effects on microstructure refining.

Effect of Oxygen Content on Aging Properties of Ti-39Nb-6Zr alloy (Ti-39Nb-6Zr 합금의 산소함량에 따른 시효특성 변화)

  • Han, Chan Byeol;Lee, Dong-Geun
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.35 no.2
    • /
    • pp.88-95
    • /
    • 2022
  • Titanium alloy for bio-medical applications have been developed to reduce the toxicity of alloying elements and avoid the stress-shielding effect which is caused by relatively high elastic modulus compared to bone. Ti-39Nb-6Zr (TNZ40) alloy of elastic modulus exhibits around 40 GPa in the case of beta single phase. However, the strength of this alloy is lower than the other types of titanium alloys. Many research found that adding oxygen to beta-titanium alloys is beneficial for improving the strength through solid solution strengthening. In this study, TNZ40 ingots with addition of O were prepared by an arc remelting process (Ti-39Nb-6Zr-0.16O (wt.%), Ti-39Nb-6Zr-0.26O (wt.%)). Thermo-mechanical processing (i.e., heat treatment, cold swaging and aging heat treatment) has been performed under various conditions. Therefore, the aim of this study is to investigate the effect of oxygen content and ω phase formation on microstructure and mechanical properties.

A Study on Corrosion Resistance and Mechanical Properties of Ti-15Sn System Alloys for Medical Implants (생체용 Ti-15Sn계 합금의 내식성 및 기계적 성질에 관한 연구)

  • Lee, Doh-Jae;Kim, Dae-Hwan;Park, Hyo-Byeong;Lee, Kyung-Ku
    • Journal of Korea Foundry Society
    • /
    • v.20 no.3
    • /
    • pp.208-215
    • /
    • 2000
  • The mechanical properties and corrosion resistance of Ti alloys for medical implants have been investigated. Ti, Ti-15Sn-4Nb and Ti-15Sn-4Nb-2Zr alloys were melted in arc furnace and the corrosion resistance of Ti alloys was evaluated by anodic polarization test. The microstructure and mechanical properties of Ti alloys were analysed by optical microscope, hardness and tensile tester. The tensile strength of the pure-Ti improved by addition of Sn and Nb and Ti-15Sn-4Nb alloy showed better Rockwell hardness compared with pure Ti. However, there was no significant difference in corrosion resistance between thoseTi-alloys made of Pure-Ti and Ti-15Sn-4Nb alloy. The passive films on the Ti-15Sn-4Nb alloy in air atmosphere consisted of $TiO_2$, SnO and NbO as demonstrated by X-ray photoelectron spectroscopy(XPS)

  • PDF

Interfacial reactions in Cu/NbTi multilayer thin films and superconducting wires (임게전류밀도 향상을 위한 Cu/NbTi다층박막과 초전도 선재에서의 계면반응)

  • 심재엽;백홍구;하동우;오상수;류강식
    • Electrical & Electronic Materials
    • /
    • v.8 no.4
    • /
    • pp.478-486
    • /
    • 1995
  • Cu/NbTi multilayer thin films and superconducting wires were fabricated and heat treated with conventional annealing and analyzed by differential scanning calorimetry (DSC) as a basic study for the enhancement of Jc. Interfacial reactions of Cu/NbTi multilayer thin films and superconducting wires were investigated with optical microscope, SEM, and XRD. According to the effective heat of formation (EHF) model, CU$\_$3/Ti was predicted as a first phase. However, considering the crystalline structure and thermodynamics, CuTi was predicted as a first phase. According to the results of DSC and XRD, CU$\_$2/Ti was found to be the first phase, followed by the formation Of CU$\_$4/Ti. The difference in first crystalline phase between the experimental result and the predicted one was discussed. In case of Cu/NbTi superconducting wires, the compounds formed at the Cu/NbTi interface grew with annealing time and the amount of compounds formed in Nb-47wt%Ti alloy was larger than that in Nb-50wt%Ti alloy. It seemed that the incubation time for the formation of compounds in Nb-50wt%Ti alloy was longer than that formed in Nb-47wt%Ti alloy. Also, the diffusion was the rate controlling step for the growth of compounds in all specimens. These compounds were formed at 500-600.deg. C for I hour annealing and, thus, the drawing time below I hour must be required to minimize the growth of compounds for the enhancement of Jc.

  • PDF

Microstructure and Mechanical Properties of $Ti_3Al-Nb$ Alloys and TiB(Ti-25Al-11Nb) Metal Matrix Composite Fabricated by Spark Plasma Sintering Process (방전플라즈마 소결법으로 제작된 $Ti_3Al-Nb$ 합금 및 TiB/(Ti-25Al-11Nb) 금속기 복합재료의 미세조직과 기계적 성질)

  • 이성열
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.27 no.1
    • /
    • pp.124-133
    • /
    • 2003
  • Ti-25Al-xNb (x=0, 3, 7, 11, 13 at. %) alloys and 18 vol. % TiB/(Ti-25Al-11Nb) metal matrix composite were fabricated by spark plasma sintering process at 900-120$0^{\circ}C$. Microstructural characteristics of the sintered bodies were identified by SEM, EDX analysis, X-ray diffraction, and differential scanning calorimeterric method. $Ti_3Al$ alloy was consisted of equiaxed $\alpha_2$ phase. $Ti_3Al-Nb$ alloys and the matix of TiB/(Ti-25Al-11Nb) metal matrix composite had the morphology that O phase was precipitated at the grain boundary of $\alpha_2$phase. Volume fraction of O phase and hardness were depended on the concentration of Nb in $Ti_3Al-Nb$ alloy, Rule of mixing could be applied to hardness and Young's modulus of 18 vol. % TiB/(Ti-25Al-11Nb) metal matrix composite.

Fabrication and Biomaterial Characteristics of HA added Ti-Nb-HA Composite Fabricated by Rapid Sintering (급속소결에 의한 HA가 첨가된 Ti-Nb-HA 복합재료의 제조 및 생체재료 특성)

  • Woo, Kee Do;Kim, Sang Hyck;Kim, Ji Young;Park, Sang Hoon
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.1
    • /
    • pp.86-91
    • /
    • 2012
  • Ti-6Al-4V extra low interstitial (ELI) alloy has been widely used as an orthopedic implant material because of its excellent biocompatibility, corrosion resistance and mechanical properties. However, V-free titanium alloys such as Ti-6%Al-7%Nb and Ti-5%Al-2.5%Fe have recently been developed because of the toxicity of V. Hydroxyapatite (HA) is used as a coating material on Ti or Ti biomaterials due to its good biocompatibility. However, HA coated on Ti alloy causes a problem for tissue by peeling off during usage. Therefore, such peeling off during long time usage can be suppressed by adding HA in Ti or Ti alloy composites. The aim of this study was to manufacture an ultra fine grained (UFG) Ti-Nb-HA bulk alloy, which is usually difficult to fabricate using melting and casting technology, by rapid sintering process using high energy mechanical milled (HEMM) powder.

A Study on Microstructure and Mechanical Properties of Hf, Ta Added Ti-l5Sn-4Nb system Alloys for Biomaterial (Hf, Ta가 첨가된 Ti-l5Sn-4Nb계 생체용 합금의 미세조직 및 기계적 성질에 관한 연구)

  • 김대환;이경구;박효병;이도재
    • Journal of the Korean institute of surface engineering
    • /
    • v.33 no.4
    • /
    • pp.251-260
    • /
    • 2000
  • Ta and Hf added Ti-l5Sn-4Nb alloys without V and Al elements for biomaterial were melted by arc furnace in response to recent concerns about the long term safety of Ti-6Al-4V alloy. All specimens were homogenized at $1000^{\circ}C$ and solution treatment was performed at $812^{\circ}C$ and aging treatment at $500^{\circ}C$. The microstructure and mechanical properties were analysed by optical micrograph, hardness tester and instron. Ti-l5Sn-4Nb system alloys showed widmanstatten microstructure which is typical microstructure in $\alpha$$\beta$ type Ti alloys. The Ti-l5Sn-4Nb-2Hf and Ti-l5Sn-4Nb-2Ta alloys showed better hardness and tensile strength compared with Ti-6Al-4V. The result of XPS analysis, Ti-l5Sn-4Nb alloy in air atmosphere consisted of $TiO_2$, SnO and NbO.

  • PDF