• 제목/요약/키워드: Nb-Si-B alloy

검색결과 65건 처리시간 0.03초

연자성 나노결정합금 분말의 열처리 온도에 의한 전자파 흡수 특성의 영향 (Effect of Annealing Temperature on the Electromagnetic Wave Absorbing Properties of Nanocrystalline Soft-magnetic Alloy Powder)

  • 홍순호;손근용;박원욱;문병기;송용설
    • 한국분말재료학회지
    • /
    • 제15권1호
    • /
    • pp.18-22
    • /
    • 2008
  • The electromagnetic (EM) wave absorption properties with a variation of crystallization annealing temperature have been investigated in a sheet-type absorber using the $Fe_{73}Si_{16}B_7Nb_3Cu_1$ alloy powder. With increasing the annealing temperature the complex permeability (${\mu}_r$), permittivity (${\varepsilon}_r$) and power absorption changed. The EM wave absorber shows the maximum permeability and permittivity after the annealing at $610^{\circ}C$ for 1 hour, and its calculated power absorption is above 80% of input power in the frequency range over 1.5 GHz.

Magnetic Properties of FeCuNbSiB Nanocrystalline Alloy Powder Cores Using Ball-milled Powder

  • Kim, G. H.;T. H. Noh;Park, G. B.;Kim, K. Y.
    • 한국자기학회:학술대회 개요집
    • /
    • 한국자기학회 2002년도 동계연구발표회 논문개요집
    • /
    • pp.202-203
    • /
    • 2002
  • Ribbon type nanocrystalline alloy cores have shown excellent soft magnetic properties in the high frequency range because of small crystalline anisotropy and nearly zero magnetostriction[1]. In present, however ribbon alloys gives some limit in applications such as a large inductor and reactors of PFC circuit, which are required good DC bias property and low loss in the high frequency. Powder alloys with ultra fine grain structure can be an important way to overcome this kind of disadvantage, and to improve the high frequency soft magnetic properties in conventional metallic powder cores[2]. (omitted)

  • PDF

Fe73.5Cu1Nb3Si15.5B7나노 결정립 합금 분말 코아의 자기적 특성 (The Magnetic Properties of Nanocrystalline Fe73.5Cu1Nb3Si15.5B7 Alloy Powder Cores)

  • 노태환;최혁열;안상재
    • 한국자기학회지
    • /
    • 제14권1호
    • /
    • pp.7-12
    • /
    • 2004
  • F $e_{73.5}$C $u_1$N $b_3$S $i_{15.5}$ $B_{7}$ 비정질 리본 합금을 490∼61$0^{\circ}C$의 온도 범위에서 열처리하고 이를 볼 밀링 하여 얻은 250∼850$\mu\textrm{m}$크기의 자성분말과 5wt%의 세라믹 절연체로 구성된 분말 코아의 자기적 특성에 열처리 온도가 미치는 영향을 조사하였다. 5$50^{\circ}C$에서 1 h동안 열처리하여 직경 11 nm의 $\alpha$-Fe상 나노 결정립 구조로 되었을 때(전기비저항은 110$\mu$$.$cm)가장 높은 실효투자율 및 품질계수를 나타내었으며 그 값은 각각 125와 53이었고, 실효투자율의 경우 약 500 KHz에 이르기까지 일정한 크기를 유지하였다. 그리고 이 열처리 조건에서 230 mW/㎤(f=50 KHz, $B_{m}$ =0.1 T)의 대단히 낮은 자심손실을 나타내었다. 그러나 이 합금의 분말 코아는 종래의 분말 코아 재료(MPP,센더스트 등)에 비해 그리 우수하지 못한 직류 바이어스 특성 특히 저 자장 하에서의 낮은 퍼센트 투자율을 나타내었는데, 이는 종래의 소재와 유사한 투자율을 얻는데 너무 큰 입도의 분말이 필요한 것에 그 원인이 있는 것으로 이해되었다.

Effect of Magnetic Field Annealing on Microstructure and Magnetic Properties of FeCuNbSiB Nanocrystalline Magnetic Core with High Inductance

  • Fan, Xingdu;Zhu, Fangliang;Wang, Qianqian;Jiang, Mufeng;Shen, Baolong
    • Applied Microscopy
    • /
    • 제47권1호
    • /
    • pp.29-35
    • /
    • 2017
  • Transverse magnetic field annealing (TFA) was carried out on $Fe_{73.5}Cu_1Nb_3Si_{15.5}B_7$ nano-crystalline magnetic core with the aim at decreasing coercivity ($H_c$) while keeping high inductance ($L_s$). The magnetic field generated by direct current (DC) was applied on the magnetic core during different selected annealing stages and it was proved that the nanocrystalline magnetic core achieved lowest $H_c$ when applying transverse field during the whole annealing process (TFA1). Although the microstructure and crystallization degree of the nanocrystalline magnetic core exhibited no obvious difference after TFA1 compared to no field annealing, the TFA1 sample showed a more uniform nanostructure with a smaller mean square deviation of grain size distribution. $H_c$ of the nanocrystalline magnetic core annealed under TFA1 decreased along with the increasing magnetic field. As a result, the certain size nanocrystalline magnetic core with low $H_c$ of 0.6 A/m, low core loss (W at 20 kHz) of 1.6 W/kg under flux density of 0.2 T and high $L_s$ of $13.8{\mu}H$ were obtained after TFA1 with the DC intensity of 140 A. The combination of high $L_s$ with excellent magnetic properties promised this nanocrystalline alloy an outstanding economical application in high frequency transformers.

Bulk Amorphous and/or Nanocrystalline Finemet Alloy Prepared by Super-high-pressure Consolidation

  • Lu, Wei;Yanb, Biao
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.788-789
    • /
    • 2006
  • Microstructure and soft magnetic properties of bulk amorphous and/or nanocrystalline $Fe_{73.5}Cu_1Nb_3Si_{13.5}B_9$ alloys prepared by consolidation at 5.5GPa were investigated. The relative density of the bulk sample 1 (from amorphous powders) was 98.5% and the grain sizes were about 10.6nm. While the relative density and grain sizes of bulk sample 2 (from nanocrystalline powders) are 98% and 20.1nm, respectively. Particularly, the bulk samples exhibited a good combined magnetic property: for Sample1, $M_s=125emu/g$ and $H_c=1.5Oe;$ for Sample2, $M_s=129emu/g$ and $H_c=3.3Oe$. The success of synthesizing the nanocrystalline Fe-based bulk alloys will be encouraging for the future development of bulk nanocrystalline soft magnetic alloys.

  • PDF

Microstructure and Magnetic Properties of Au-doped Finemet-type Alloy

  • Le, Anh-Tuan;Kim, Chong-Oh;Ha Nguyen Duy;Chau Nguyen;Tho Nguyen Duc;Lee, Hee-Bok
    • Journal of Magnetics
    • /
    • 제11권1호
    • /
    • pp.36-42
    • /
    • 2006
  • In this report, we demonstrate a comprehensive analysis of the effects of Au addition on the microstructure and magnetic properties of $Fe_{73.5}Si_{13.5}B_{9}Nb_{3}Au_1$ Finemet-type alloy. It was found that the as-quenched alloys were the amorphous state and turned into nanocrystalline state under heat treatments. The DSC analysis indicates that the sharply exothermal peak corresponding to the crystallization of the $\alpha-Fe(Si)$ was observed at $547-579^{\circ}C$ depending on the heating rates, which is little higher than that of original Finemet (542-$570{^{\circ}C}$, respectively). Besides, the thermomagnetic result confirmed that the full substitution of Cu by Au with the single phase structure in the M(T) curve along cooling cycle. Ultrasoft magnetic properties of the nanocrystallized samples were significantly enhanced by the proper annealing such as the increase of permeability and the decrease of the coercivity. The optimum annealing condition was found at the annealing temperature of $540^{\circ}C$ and the increase of the annealing time up to 90 min.

연자성 합금 분말의 입자크기에 따른 전자파 흡수 특성 비교 (Study of Electromagnetic Wave Absorption Properties with Particle Size in Soft Magnetic Alloy Powder)

  • 홍순호;손근용;박원욱;남정미;문병기;송용설
    • 한국분말재료학회지
    • /
    • 제14권4호
    • /
    • pp.261-264
    • /
    • 2007
  • The electromagnetic wave (EM) absorption properties of various particle size have been investigated in a sheet-type absorber using the $Fe_{73}Si_{16}B_{7}Nb_{3}Cu_{1}$ alloy powder. With decreasing the average particle size, the complex permeability (${\mu}_{r}$) and permittivity (${\varepsilon}_{r}$) increased and the matching frequency is shifted toward lower frequency. The fabricated EM wave absorbers showed permeability $2{\sim}6$, permittivity $17{\sim}23$ for a $-325{\sim}+400$ mesh sample, and the calculated power absorption was as high as 80% in the frequency range over 2 GHz.

철기(Fe Based) 나노결정질 합금 분말코어의 코팅제 및 입도가 연자기적 특성에 미치는 영향 (Influence of Coating Agent and Particle Size on the Soft Magnetic Properties of Fe Based Nano Crystalline Alloy Powder Core)

  • 장세종;최영진;김상욱;전병서;이태행;송창빈;남궁정
    • 한국자기학회지
    • /
    • 제25권3호
    • /
    • pp.67-73
    • /
    • 2015
  • 본 연구는 철기(Fe based) $Fe_{73.5}Si_{13.5}B_9Nb_3Cu_1$ 나노결정 합금의 분말코어(powder core)의 연자기적 특성 향상을 위한 기초연구로서, 절연 코팅제의 첨가량 및 분말입도에 따른 투자율, 코어손실 및 DC 바이어스 특성을 주로 조사하였다. 우선 합금조성을 PFC 장치를 이용하여 비정질 합금리본을 제조한 후, 열처리, 미분쇄 및 분급하여 얻어진 합금분말에 절연 코팅제(PEI)의 첨가량을 0.5, 1.0, 2.0, 2.5 wt%로 변화시켜 $16ton/cm^2$으로 압축성형 및 결정화 열처리하여 제조한 토로이달 나노결정 분말코어($OD12.7mm{\times}ID7.62mm{\times}H4.75mm$)는 절연 코팅제 함량이 증가할수록 투자율은 감소하였지만, 코어손실 및 DC 바이어스 특성은 향상됨을 확인하였다. 이러한 이유는 합금분말 절연 코팅제 첨가량이 증가할수록 비정질 합금분말 입자가 적어져 분말코어의 성형밀도가 낮아지기 때문으로 추정되었으며, 절연 코팅제의 함량은 1 wt%가 가장 적합한 것으로 판단되었다. 또한 절연 코팅제 함량을 1 wt%로 고정하고, 합금분말의 입도에 따라 제조한 분말코어의 경우, 실효투자율 및 코어손실은 입도가 클수록 우수하였지만, DC 바이어스 특성은 인가자장이 증가함에 따라 더욱 나빠짐을 확인하였다. 그 이유는 합금분말 표면의 코팅층 두께 차이에 의한 절연효과, 잔류기공 혹은 분말코어의 성형밀도 차이 등에 기인하는 것으로 추정되었다.