• 제목/요약/키워드: Nb content

검색결과 278건 처리시간 0.023초

스파크플라즈마 소결에 의한 Ti-Nb-Zr-Mo-CPP 생체복합재의 기계적 성질 및 생체적합성 (Mechanical Properties and Biocompatibility of Ti-Nb-Zr-Mo-CPP Biomaterial Fabricated by Spark Plasma Sintering)

  • 우기도;김상미;김동건;김대영;강동수
    • 한국재료학회지
    • /
    • 제23권2호
    • /
    • pp.135-142
    • /
    • 2013
  • The Ti-6Al-4V extra low interstitial (ELI) alloy has been widely used as an orthopedic implant material because of its excellent mechanical properties and biocompatibility. However, it still has many problems, including a high elastic modulus and toxicity of the Al and V elements. Therefore, non-toxic biomaterials with a low elastic modulus need to be developed. A high energy mechanical milling (HEMM) process is introduced to improve the effect of sintering. Rapid sintering of spark plasma sintering (SPS) under pressure was used to make an ultra fine grain of Ti-25 wt.%Nb-7 wt.%Zr-10 wt.%Mo-(10 wt.%CPP) composites with bio-attractive elements for increasing strength. These composites were fabricated by SPS at $1000^{\circ}C$ at 60 MPa using HEMM powders. During the sintering process, $CaTiO_3$, TixOy, and CaO were formed because of the reaction between Ti and CPP. The effects of CPP content on the physical and mechanical properties of the sintered Ti-Nb-Zr-Mo-CPP composites were investigated. The biocompatibility and corrosion resistance of the Ti-Nb-Zr-Mo alloys were improved by the addition of CPP.

Doping Effect of Yb2O3 on Varistor Properties of ZnO-V2O5-MnO2-Nb2O5 Ceramic Semiconductors

  • Nahm, Choon-Woo
    • 한국재료학회지
    • /
    • 제29권10호
    • /
    • pp.586-591
    • /
    • 2019
  • This study describes the doping effect of $Yb_2O_3$ on microstructure, electrical and dielectric properties of $ZnO-V_2O_5-MnO_2-Nb_2O_5$ (ZVMN) ceramic semiconductors sintered at a temperature as low as $900^{\circ}C$. As the doping content of $Yb_2O_3$ increases, the ceramic density slightly increases from 5.50 to $5.54g/cm^3$; also, the average ZnO grain size is in the range of $5.3-5.6{\mu}m$. The switching voltage increases from 4,874 to 5,494 V/cm when the doping content of $Yb_2O_3$ is less than 0.1 mol%, whereas further doping decreases this value. The ZVMN ceramic semiconductors doped with 0.1 mol% $Yb_2O_3$ reveal an excellent nonohmic coefficient as high as 70. The donor density of ZnO gain increases in the range of $2.46-7.41{\times}10^{17}cm^{-3}$ with increasing doping content of $Yb_2O_3$ and the potential barrier height and surface state density at the grain boundaries exhibits a maximum value (1.25 eV) at 0.1 mol%. The dielectric constant (at 1 kHz) decreases from 592.7 to 501.4 until the doping content of $Yb_2O_3$ reaches 0.1 mol%, whereas further doping increases it. The value of $tan{\delta}$ increases from 0.209 to 0.268 with the doping content of $Yb_2O_3$.

Microwave Dielectric Properties of (Pb0.4Ca0.6)[(Fe1/2Nb1/2)1-x(Mg1/3Nb2/3)x]O3 Ceramics

  • Kim, Eung-Soo;Han, Ki-Moon;Kim, Jong-Hee;Yoon, Ki-Hyun
    • 한국세라믹학회지
    • /
    • 제40권4호
    • /
    • pp.323-327
    • /
    • 2003
  • Microwave dielectric properties of (P $b_{0.4}$C $a_{0.6}$)[($Fe_{\frac{1}{2}}$N $b_{\frac{1}{2}}$)$_{1-x}$ (M $g_{1}$ 3/N $b_{2}$ 3/)x] $O_3$ (PCFMN) ceramics were investigated as a function of (M $g_{1}$ 3/N $b_{2}$ 3/)$^{4+}$ content (0.1$\leq$x$\leq$0.8). A single perovskite phase with the cubic structure was obtained through the given composition range. The unit cell volume was increased with (M $g_{1}$ 3/N $b_{2}$ 3/)$^{4+}$, due to the larger average ionic size of (M $g_{1}$ 3/N $b_{2}$ 3/)$^{4+}$ than that of ($Fe_{\frac{1}{2}}$N $b_{\frac{1}{2}}$)$^{4+}$ for B-site ion. Dielectric constant (K) and Temperature Coefficient of Resonant Frequency(TCF) of PCFMN ceramics were dependent on (M $g_{1}$ 3/N $b_{2}$ 3/)$^{4+}$ content due to the decrease of ionic polarizability and B-site bond valence, respectively. Qf value was decreased with (M $g_{1}$ 3/N $b_{2}$ 3/)$^{4+}$ content due to the decrease of grain size. Typically, K of 73.56, Qf of 5,074 GHz and TCF of -6.45 ppm/$^{\circ}C$ were obtained for the specimens with x=0.4 sintered at 125$0^{\circ}C$ for 3 h.125$0^{\circ}C$ for 3 h.

양이온성 ${\eta}^3$-알릴 팔라듐 촉매를 사용한 폴리(5-헥실-2-노보넨-co-5-메틸에스터-2-노보넨)의 비닐 부가 중합 거동 (Vinyl Addition Polymerization Behavior of Poly(5-hexyl-2-norbornene-co-5-methylester-2-norbornene)s Using Cationic ${\eta}^3$-Allyl Palladium Catalyst)

  • 안재철;박기홍
    • 폴리머
    • /
    • 제28권3호
    • /
    • pp.245-252
    • /
    • 2004
  • 5-헥실-2-노보넨 (HNB)과 5-메틸에스터-2-노보넨 (MES-NB)을 양이온 ${\eta}^3$-알릴 팔라듐 촉매인 [(${\eta}^3$-allyl) palladium(tricyclohexylphosphine) trifluoroacetate]와 리튬계 조촉매 [lithium tetrakis(pentafluorophenyl( borate${\cdor}$2.5etherate]를 사용하여 비닐 부가형의 폴리노보넨 공중합체를 합성하였다. 에스터기를 과량 함유한 폴리노보넨을 제조하기 위한 최적 중합 조건을 조사하기 위하여 여러가지 중합조건에 따른 분자량변화와 수율의 변화를 알아보았다. 팔라듐 촉매의 함량이 많을수록 수득율은 증가하는 한편, 분자량은 감소하였으며, 리튬조촉매의 함량은 많을수록 분자량과 수득율이 동시에 증가하였다. 사슬이동체를 이용하여 분자량을 조절할 수 있었고, 사슬이동제의 길이가 긴 1-데센과 1-옥텐이 1-헥센보다 분자량을 더 감소시키는 역할을 하였다. 한편 사슬이동제의 양은 수율에 큰 영향을 미치지 않았다. HNB/MES-NB(투입비 40/60 mol%)의 공종합체의 $^1$H-NMR 과 GPC 분석으로부터, 실제 에스터 함유량으 약 25mol%인 고분자량 (M$_{w}$ : 270,000)의 폴리노보넨 공중합체가 얻어짐을 알 수 있었다.

RF마그네트론 스퍼터링 법에 의해 증착된 SrBi2Nb2O9 박막의 Bi 량의 조절에 따른 특성분석 (Characteristics of the SrBi2Nb2O9 Thin Films Deposited by RF Magnetron Sputtering with Controlling of Bi Contents)

  • 이종한;최훈상;성현주;임근식;권영석;최인훈;손창식
    • 한국재료학회지
    • /
    • 제12권12호
    • /
    • pp.962-966
    • /
    • 2002
  • The $SrBi_2$$Nb_2$$O_{9}$ (SBN) thin films were deposited with $SrNb_2$$O_{6}$ / (SNO) and $Bi_2$$O_3$ targets by co-sputtering method. For the growth of SBN thin films, we adopted the various power ratios of two targets; the power ratios of the SNO target to $Bi_2$$O_3$ target were 100 W : 20 W, 100 W : 25 W, and 100 W : 30 W during sputtering the SBN films. We found that the electrical properties of SBN films were greatly dependent on Bi content in films. The $Bi_2$Pt and $Bi_2$$O_3$ phase as second phases occurred at the films with excess Bi content greater than 2.4, resulting in poor ferroelectric properties. The best growth condition of the SBN films was obtained at the power ratio of 100 W : 25 W for the two targets. At this condition, the crystallinity and electrical properties of the films were improved at even low annealing temperature as $700^{\circ}C$ for 1h in oxygen ambient and the Sr, Bi and Nb component in the SBN films were about 0.9, 2.4, and 1.8 respectively. From the P-E and I-V curves for the specimen, the remnant polarization value ($2P_{r}$) of the SBN films was obtained about 6 $\mu$C/c $m^2$ at 250 kV/cm and the leakage current density of this thin film was $2.45$\times$10^{-7}$ $A/cm^2$ at an applied voltage of 3 V.V.

Enhanced Piezoelectric Properties of Lead-Free La and Nb Co-Modified Bi0.5(Na0.84K0.16)0.5TiO3-SrTiO3 Ceramics

  • Malik, Rizwan Ahmed;Hussain, Ali;Maqbool, Adnan;Zaman, Arif;Song, Tae Kwon;Kim, Won Jeong;Kim, Myong Ho
    • 한국재료학회지
    • /
    • 제25권6호
    • /
    • pp.288-292
    • /
    • 2015
  • New lead-free piezoelectric ceramics $0.96[\{Bi_{0.5}(Na_{0.84}K_{0.16})_{0.5}\}_{1-x}La_x(Ti_{1-y}Nb_y)O_3]-0.04SrTiO_3$ (BNKT-ST-LN, where $x=y=0.00{\leq}(x=y){\leq}0.015)$ were synthesized using the conventional solid-state reaction method. Their crystal structure, microstructure, and electrical properties were investigated as a function of the La and Nb (LN) content. The X-ray diffraction patterns revealed the formation of a single-phase perovskite structure for all the LN-modified BNKT-ST ceramics in this study. The temperature dependence of the dielectric curves showed that the maximum dielectric constant temperature ($T_m$) shifted towards lower temperatures and the curves became more diffuse with an increasing LN content. At the optimum composition (LN 0.005), a maximum value of remnant polarization ($33C/cm^2$) with a relatively low coercive field (22 kV/cm) and high piezoelectric constant (215 pC/N) was observed. These results indicate that the LN co-modified BNKT-ST ceramic system is a promising candidate for lead-free piezoelectric materials.

Analysis of surface characteristics of (Y, Nb)-TZP after finishing and polishing

  • Seong-keun, Yoo;Ye-Hyeon, Jo;In-Sung Luke, Yeo;Hyung-In, Yoon;Jae-Hyun, Lee;Jin-Soo, Ahn;Jung-Suk, Han
    • The Journal of Advanced Prosthodontics
    • /
    • 제14권6호
    • /
    • pp.335-345
    • /
    • 2022
  • PURPOSE. This in vitro study aimed to evaluate the surface characteristics of a full veneer crown fabricated chairside (CS) from a (Y, Nb)-TZP zirconia block in response to conventional zirconia grinding and polishing. MATERIALS AND METHODS. Zirconia crowns (n = 40) were first prepared and divided into two groups of materials: Labside (LS) and CS, after which each specimen went through a five-step grinding and polishing procedure. Following each surface treatment, surface characteristics were analyzed using confocal laser microscopy (CLSM), average surface roughness (Ra) values were processed from the profile data through Gaussian filtering, and X-ray diffraction pattern analysis was performed to evaluate the monoclinic (M) phase content. Then, a representative specimen was selected for field-emission scanning electron microscopy (FE-SEM), followed by a final analysis of the roughness and X-ray diffraction of the specimens using the independent t-test and repeated measures analysis of variance (RM-ANOVA). RESULTS. In every group, polishing significantly reduced the Ra values (P < .001). There was no significant difference in Ra between the polished state CS and LS. Furthermore, CLSM and FE-SEM investigations revealed that even though grain exposure was visible in CS specimens throughout the as-delivered and ground states, the exposure was reduced after polishing. Moreover, while no phase transformation was visible in the LS, phase transformation was visible in CS after every surface treatment, with the M phase content of the CS group showing a significant reduction after polishing (P < .001). CONCLUSION. Within the limits of this study, clinically acceptable level of surface finishing of (Y, Nb)-TZP can be achieved after conventional zirconia polishing sequence.

Biochemical Attributes of Mature Female Gonads of Different Strains and Hybrid of Mulberry Silkmoth, Bombyx mori L.(Lepidoptera : Bombycidae)

  • A.K. Saha;A. Chaudhuri;N. Krishnan;A.K. Sengupta;M. Shamsuddin;S.K. Sen;B. Saratchandra
    • 한국잠사곤충학회지
    • /
    • 제40권1호
    • /
    • pp.27-32
    • /
    • 1998
  • One indigenous polyvoltine strain (Nistari) and two bivoltine strains viz. P5 and NB18 along with one bivoltine hybrid (P5$\times$NB18) were subjected for studies on the differences on some physiologically important biomolecules like protein, nucleic acids and cholesterol. Ovarian protein and RNA content remained significantly high in the bivoltine races and their hybrid over multivoltine breed, while, DNA and cholesterol content remained significantly low in all the breeds and the hybrid as compared to Nistari strain. However, the ovarian weight was higher in both the bivoltine breeds and their hybrid than that of Nistari. Higher ovarian weight together with more protein and RNA concentrations reflect the preparatory phase for production of diapausing eggs by the bivoltine silknoths and their hybrid. The variations in biochemical parameters studied herein, thus establish a distinct difference in the overt reproductive physioiogy between multivoltine and bivoltine silkworms.

  • PDF

$MnO_2$가 첨가된 PSN-PNN-PT세라믹스의 전기적인 특성 (Electrical properties of $MnO_2$doped PSN-PNN-PT ceramics)

  • 이종덕;박상만;박기엽
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.959-962
    • /
    • 2001
  • In this study, the piezoelectric and dielectric properties and Temperature stability of resonant frequency with MnO$_2$doped 0.36Pb(Sc$_{1}$2/Nb$_{1}$2/)O$_3$- 0.25Pb(Ni$_{1}$3/Nb$_{2}$3/)O$_3$-0.39PbTiO$_3$(hereafter PSNNT) were investigated. The tetagonality of crystal structure was developed with increasing MnO$_2$additive content. With increasing MnO$_2$additive content, the electromechanical coupling factor and quality factor were increased. Electromechanical coupling k$_{p}$ and quality factor Q$_{m}$ at MnO$_2$doped with 2.0mol% were showed highest value of 55.6% and 252. In the case of specimen for MnO$_2$doped with 2mol%, temperature dependance of resonant frequency had a good properties.ies.

  • PDF