Al-Cu-Mg 합금에 있어서의 2차 결함조직 (The Secondary Defect Structure in Al-Cu-Mg Alloy)

  • 조현기;우기도
    • Applied Microscopy
    • /
    • 제16권2호
    • /
    • pp.14-24
    • /
    • 1986
  • The interrelation of secondary defects, intermediate S' phase and aging condition in Al-2.0 wt% Cu-1.1 wt% Mg alloy is studied by transmission electron microscope. The results obtained in this study are as follows. 1. High density of dislocation loops, helices and stacking faults are observed in this specimen with aging treatment. 2. The number of dislocation loops and the width of loop free zone (LFZ) are increased with aging time. 3. The intermediate S' phase precipitates and grows on the dislocations and secondary defects. 4. The misfit dislocations are formed around intermediate S' phase. 5. It is thought that the helices appear to be produced by the climb of screw dislocations, while the dislocation loops appear to be formed both by condensation of vacancies into collapsed discs and by interaction of helices with screw of opposite sign.

  • PDF

SiC 입자강화 Al-Si 복합재료의 내마멸성에 미치는 Cu , Mg의 영향 (Effects of Cu and Mg on Wear Properties of SiC Particulate Reinforced Al-Si Metal Matrix Composites)

  • 심상한;정용근;박익민
    • 한국주조공학회지
    • /
    • 제10권1호
    • /
    • pp.43-49
    • /
    • 1990
  • The influences of Cu and Mg addition on wear properties of SiC particulate reinforced Al-Si metal(alloy) matrix composites were investigated. Metal matrix composites were prepared by combination of compocasting and hot pressing techniques. The main results obtained are as follows : 1) The composite with Mg addition exhibits letter wear resistance than that with Cu addition. It is considered that Mg addition improved wettability of matal matrix composite by the strong segregation to the SiC / Al matrix interface. 2) After homogenization treatment, it was found that the interfacial segregation of Mg was predominant, while that of Cu was not detected. 3) The SiC / Al-11Si eutectic composite exhibits better wear resistance than the SiC / Al-6Si hypoeutectic composite does. 4) It seems that the increase in the amount of Mg addition affects on the uniform dispersion of SiC particulates, on the refinement of microstructure and on age hardening and these effects cause wear resistance improvement of composites.

  • PDF

Al-Cu-Mg합금의 일방향응고시 로온도에 따른 응고거동변화 (Effects of the Furnace Temperature on the Growth Behavior of Directionally Solidified Al-Cu-Mg Alloy)

  • 문철희
    • 한국주조공학회지
    • /
    • 제17권6호
    • /
    • pp.545-551
    • /
    • 1997
  • 14 cm length Al-15Cu-1Mg alloys have been directionally solidified in 3 mm diameter alumina tubes in a furnace moved with a constant velocity V=12 cm/hr under various furnace temperatures of 660, 710 and $760^{\circ}C$. By analysing the evolution of the temperature profiles along the alloy length during the solidification, the growth characteristics such as the position of the solid/liquid interface, the local growth velocity (R) and the temperature gradient at the solid/liquid interface (G) have been determined. The effects of the furnace temperature on the growth behavior have been investigated by the comparison of R and G values for each temperature. Under the furnace temperature of $760^{\circ}C$, steady state growth region was observed for the latter half of the growth period.

  • PDF

Al-Zn-Mg 계 합금의 Creep 거동에 관한 연구 (A Study on the Creep Behaviour of Al-Zn-Mg Alloy)

  • 박종건;최재하
    • 열처리공학회지
    • /
    • 제6권2호
    • /
    • pp.79-88
    • /
    • 1993
  • The static creep mechanism and behaviour of Al-Zn-Mg alloy have been investigated under condition of constant stress tension creep test in the temperature and stress range of $170-260^{\circ}C$ and 5-12.5 $kg/mm^2$ respectively. The experimental result are follows : The stress exponent value for creep was observed to about 7.3-6.43 and the activation energy for creep deformation was 44-41 kcal/mol. Larson-Miller parameter P for the crept specimens under the creep condition was obtained as P = (T + 460) (log $t_r$ + 8.6). Emperical equation for the creep rate was obtained by the computer simulation as follows. $${\varepsilon}\;=\;\exp[(-5.519{\times}10^{-4}{\sigma}+2.33{\times}10^{-2})T-6.98{\sigma}+18.295]{\times}{\sigma}^{-0.0142+10.18}\exp[\frac{(-6{\sigma}+47.8)1000}{RT}]$$ Fracture was dominated by intergranular mechanism over the experimental range.

  • PDF

Al-Li-Cu-Mg합금의 조직과 기계적 성질에 미치는 가공열처리의 영향 (Effect of Thermomechanical Treatments on Microstructure and Mechanical Properties in Al-Li-Cu-Mg Alloy)

  • 우기도;조현기
    • 열처리공학회지
    • /
    • 제3권1호
    • /
    • pp.8-16
    • /
    • 1990
  • Effects of thermomechanical treatments(TMT) on the microstructures and mechanical properties in Al-2.27%, Li-1.28%, Cu-0.63%, Mg-0.12%, Zr alloy were investigated. The TMT process improved the tensile strength. Growth of ${\delta}^{\prime}$, S' and $T_1$ phases was restrained by TMT processes while the density of ${\delta}^{\prime}$, S' and $T_1$ phases was increased by TMT processes. The TMT treated specimens tend to fail in inter-subboundary mode. The increases of strength by the T-HA processes were compared to those of the T-AHA processes.

  • PDF

용탕단조한 Al-7%Si-0.3% Mg합금 봉상시료의 편석거동 (Segregation of Squeeze Cast Al-7% Si-0.3% Mg Alloy Bars)

  • 김기영;기석도;박종락
    • 한국주조공학회지
    • /
    • 제13권1호
    • /
    • pp.71-80
    • /
    • 1993
  • Squeeze casting has advantages to improve mechanical properties of nonferrous castings without losing high productivity. Sound pore free structure makes it possible to be subjected to heat treatment and welding. This process became popular to produce lighter automobile parts alternating cast iron parts. It has, however, two disadvantages of segregation and scattered structure due to the solidified layers in sleeve. In this study segregation behavior of squeeze cast Al-7%Si-0.3%Mg alloy bars was investigated using HVSC machine under various injection conditions. Degree of segregation decreased with injection pressure and effect of injection velocity on it was small. Segregation mode of solute was strongly governed by solidification mode and flow pattern.

  • PDF

DIAGNOSTICS OF PLASMA INDUCED IN Nd:YAG LASER WELDING OF ALUMINUM ALLOY

  • Kim, Jong-Do;Lee, Myeong-Hoon;Kim, Young-Sik;Seiji Katayama;Akira Matsunawa
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.612-619
    • /
    • 2002
  • The dynamic behavior of Al-Mg alloys plasma was very unstable and this instability was closely related to the unstable motion of keyhole during laser irradiation. The keyhole fluctuated both in size and shape and its fluctuation period was about 440 ${\mu}{\textrm}{m}$. This instability has been estimated to be caused by the evaporation phenomena of metals with different boiling point and latent heats of vaporization. Therefore, the authors have conducted the spectroscopic diagnostics of plasma induced in the pulsed YAG laser welding of Al-Mg alloys in air and argon atmospheres. In the air environment, the identified spectra were atomic lines of Al, Mg, Cr, Mn, Cu, Fe and Zn, and singly ionized Mg line, as well as strong molecular spectrum of AlO, MgO and AIH. It was confirmed that the resonant lines of Al and Mg were strongly self-absorbed, in particular in the vicinity of pool surface. The self-absorption of atomic Mg line was more eminent in alloys containing higher Mg. These facts showed that the laser-induced plasma was relatively a low temperature and high density metallic vapor. The intensities of molecular spectra of AlO and MgO were different each other depending on the power density of laser beam. Under the low power density irradiation condition, the MgO band spectra were predominant in intensity, while the AlO spectra became much stronger in higher power density. In argon atmosphere the band spectra of MgO and AlO completely vanished, but AlH molecular spectra was detected clearly. The hydrogen source was presumably the hydrogen solved in the base Metal, absorbed water on the surface oxide layer or H$_2$ and $H_2O$ in the shielding gas. The temporal change in spectral line intensities was quite similar to the fluctuation of keyhole. The time average plasma temperature at 1 mm high above the surface of A5083 alloy was determined by the Boltzmann plot method of atomic Cr lines of different excitation energy. The obtained electron temperature was 3, 280$\pm$150 K which was about 500 K higher than the boiling point of pure aluminum. The electron number density was determined by measuring the relative intensities of the spectra1lines of atomic and singly ionized Magnesium, and the obtained value was 1.85 x 1019 1/㎥.

  • PDF

SKD 11 금형 표면처리에 따른 AZ31 판재 마찰 특성 연구 (Study on the Friction Characteristics for AZ31 Sheet as Various Surface Treatment of SKD11)

  • 장성호;신광호;김흥규;전용준;허영무
    • 소성∙가공
    • /
    • 제19권7호
    • /
    • pp.429-434
    • /
    • 2010
  • The material used is a commercial magnesium based alloy AZ31(Mg-3Al-1Zn) sheet with a thickness of 0.8 mm. Friction tests at various temperatures(R.T. to $200^{\circ}C$) and at various holding forces in the 4 type molds were carried out to investigate the coefficient of friction. A warm drawing process with a local heating and cooling technique was developed in the Mg alloy sheet forming to improve formability because it is very difficult for Mg alloy to deform at room temperature by the conventional method. So, the coefficient of friction at various mold surface treatment conditions in this study was needed to develop the Mg alloy sheet forming technology.

Al-20Si-5.5Fe-1.2Mg-0.5Mn 합금분말의 치밀화에 미치는 소결온도와 분위기의 영향 (Effects of Sintering Temperature and Atmosphere on Densification of Hypereutectic Al-Si Alloy Powders)

  • 이재욱;박상빈;양상선;김용진
    • 한국분말재료학회지
    • /
    • 제15권3호
    • /
    • pp.196-203
    • /
    • 2008
  • The densification behavior of Al-20Si-5.5Fe-1.2Mg-0.5Mn powders was investigated through micro-structure analysis of sintered specimens. The specimens sintered in vacuum or in high purity (99.999%) nitrogen showed porous near-surface microstructures. The densification of near-surface part was enhanced by means of ultra-high purity (99.9999%) nitrogen atmosphere. The relationship between slow densification and oxide surfaces of Al alloy powders was discussed. And the effects of Mg addition, nitrogen gas, and humidity on densification were discussed. In addition, the rapid growth of primary Si crystals above the critical temperature was reported.

전기전도도를 이용한 Al-Si-Cu-Mg 합금 품의 기계적 압축 특성 평가 (Evaluation of Mechanical Compressive Properties of Al-Si-Cu-Mg Alloy Foams Using Electrical Conductivity)

  • 이창훈;김엄기;하산;남승훈;조성석
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.377-381
    • /
    • 2004
  • Electrical conductivity of Al-Si-Cu-Mg alloy foams of various density produced in powder metallurgical method has been measured using two probe electrical conductivity measurement method. Compressive mechanical properties such as elastic modulus and plastic plateau stress of foams were evaluated from electrical conductivity using power law relation and scaling laws of foam properties. Uni-axial compression test was also performed. Experimentally measured elastic modulus and plastic plateau stress were compared with the values evaluated from electrical conductivity. The computed values were in good agreement with the experimental result.