• Title/Summary/Keyword: Mg 입자

Search Result 716, Processing Time 0.033 seconds

Grain Refining and Age Hardening of Mg-Zn Alloys by Addition of Cu and Si (Cu 및 Si첨가에 의한 Mg-Zn합금계의 입자미세화 및 시효경화)

  • Hwang, Jin-Hwan;Nam, Tae-Hyeon;An, In-Seop;Kim, Yu-Gyeong;Heo, Gyeong-Cheol;Heo, Bo-Yeong
    • Korean Journal of Materials Research
    • /
    • v.5 no.6
    • /
    • pp.682-689
    • /
    • 1995
  • In order to refine the grain size of Mg-Zn alloy 0.5 to 6wt.%Cu or Si elements were added. Alloy ingot was made under vacuum atmosphere of 4 ${\times}$ 10$\^$-4/ Torr in the quartz tube coated by BN. Grain size and hardness were measured after solution treatment for 8 hours at 435$^{\circ}C$. Optimal condition for grain size refining effect was obtained at the minimum composition of 2wt.%Cu or 1.5wt.%Si addition to Mg-6wt%Zn alloy. Age hardening behavior was experimented at the optimal compositions of the Mg-6wt.%Zn, Mg-6wt.% Zn-2wt.%Cu and Mg-6wt.% Zn-1.5wt.%Si. The hardness increment due to fine grain size was higher at the Mg-Zn-Cu alloy system, but that due to age hardening was higher at the Mg-Zn-Si alloy system.

  • PDF

Hydrogenation Study of Mg-based Alloys by mechanical Grinding Reaction for Hydrogen Storage of Fuel Cell (연료전지의 수소저장용 마그네슘계 합금의 기계적 분쇄 반응에 의한 수소화 특성 평가)

  • Kim, Ho-Sung;Suh, Hee-Seok;Cha, Jae-Sang
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.20 no.6
    • /
    • pp.69-74
    • /
    • 2006
  • The effects of mechanical grinding(MG) treatment on the hydrogen storage of $Mg_2Ni$ alloy and $Mg_2Ni$ composite alloy($Mg_2Ni+graphite$) were investigated by pressure-composition-temperature(PCT) measurement, the micro-electrode technique of electrochemistry and etc, in which PCT was measured at high temperature(around $300[^{\circ}C]$) of gas phase and a carbon-filament micro-electrode for electrochemical evaluation was manipulated to make electrical contact with the particle in 1M KOH aqueous solution. It was found that the hydrogenation properties of $Mg_2Ni$ and graphite composite particle were greatly improved by the mechanical grinding treatment by which the $Mg_2Ni$ and graphite composite alloys could be changed into microstructure and nano-level particles. namely; the hydrogen dissociation pressure of PCT measurement was decreased from 0.55[MPa] to 0.42[MPa] and hydrogenation peaks by micro-electrode were also observed more clearly on the same sample.

Removal of Red Tide Organisms -1. flocculation of Red Tide Organisms by Using IOSP- (적조생물의 구제 -1. IOSP에 의한 적조생물의 응집제거-)

  • KIM Sung-Jae;CHO Kyu-Dae
    • Korean Journal of Fisheries and Aquatic Sciences
    • /
    • v.33 no.5
    • /
    • pp.448-454
    • /
    • 2000
  • This study was to examine the physicochemical characteristics of coagulation reaction between ignited oyster shell powder (IOSP) and red tide organisms (RTO), and its feasibility, in developing a technology for the removal of RTO bloom in coastal sea,IOSP was made from oyster shell and its physicochemical characteristics were examined for particle size distribution, surface characteristic by scanning electron microscope, zeta potential, and alkalinity and pH variations in sea water. Two kinds of RTO that were used in this study, Cylindrotheca closterium and Skeletonema costatum, were sampled in Masan bay and were cultured in laboratory. Coagulation experiments were conducted using various c(Incentrations of IOSP, RTO, and a jar tester. The supernatant and RTO culture solution were analyzed for pH, alkalinity, RTO cell number, IOSP showed positive zeta potentials of $11.1{\~}50.1\;mV\;at\;pH\;6.2{\~}12.7$, A positive zeta potential of IOSP slowly decreased with decreasing pNa 4,0 to 2,0. When pNa reached zero, the zeta potential approached zero, When a pMg value was decreased, the positive zeta potential of IOSP increased until pMg 3.0 and decreased below pMg 3.0. IOSP showed 4.8 mV of positive zeta potential while RTO showed -9.2 mV of negative zeta potential in sea water. A positive-negative EDL (electrical double-layer) interaction occurred between $Mg(OH)_2$ adsorption layer of IOSP and RTO in sea water so that EDL attractive force always worked between them. Hence, their coagulation reaction occurred at primary minimum on which an extreme attractive force acted because of charge neutralization by $Mg(OH)_2$ adsorption layer of IOSP. As a result, the coagulation reaction was rapidly processed and was irreversible according to DLVO (Deriaguin-Landau-Verwey-Overbeek) theory. Removal rates of RTO were exponentially increased with increasing both IOSP concentration and G-value. The removal rates were steeply increased until 50 mg/l of IOSP and reached $100{\%}\;at\;400\;mg/l$ of IOSP. Removal rates of RTO were $70.5,\;70.5,\;81.7,\;85.3{\%}$ for G-values of $1,\;6,\;29,\;139\;sec^(-1)$at IOSP 100 mg/l, respectively. This indicated that mixing (i.e., collision among particles) was very important for a coagulation reaction.

  • PDF

Settling Characteristics of Natural Loess Particles in Seawater (해수 중에서 자연상태 황토입자의 침강특성)

  • KIM Sung-Jae
    • Korean Journal of Fisheries and Aquatic Sciences
    • /
    • v.32 no.6
    • /
    • pp.706-712
    • /
    • 1999
  • PSD (particle size distribution) for 2,000 mg/$\ell$ natural loess in seawater showed normal distribution cure at 0 minute settling time, accompanying with very large particle distribution range with its mean particle diameter of 31.6 $\mu$m and coencient of variance of $72.6\%$, With elapsed time it showed that the PSD was rapidly changed from normal distribution cure to abnormal distribution curve, steepened the right-hand side of it and its coefficient of variance was getting increased because of rapid settling of large size particles, Cumulative weight distribution showed that 2,000 mg/$\ell$ natural loess in seawater was almost $100\%$ constituted of particles bigger than 20 $\mu$m in diameter. Ratio of $V_s/(D_{bm})^{1/2}$ for loess particles in seawater was increased with increase of particle size in geometrical progression. Almost all loess particles in seawater had Stokes settling velocity not less than 2,255 times of Brownian diffusion coefficient, There was almost to EDL (about 0.4 nm) around natural loess particles in seawater, Thus, there was always LVDW attractive force between loess particles approaching each other in seawater, and almost no EDL repulsive force. Loess particles were not always in the condition of easy floe formation. Concentration of natural loess in seawater increasing from 400 mg/$\ell$ to 10,000 mg/$\ell$, characteristics of the settling was changed from Type I settling (discrete settling) to Type II settling (flocculation settling). PVD (particle volume distribution) showed that natural loess particles in seawater were largely constituted of two types of particles, such as rapidly settling particles and suspended and dispersed particles for a long time. Amount of the latter was much less than that of the former.

  • PDF

Function Layer가 적용된 AC-PDP에서 지속방전으로 재형성 된 MgO 나노 입자의 음극선 분광 분석

  • Lee, Gyeong-Ae;Choe, Jun-Ho;Son, Chang-Gil;Choe, Eun-Ha
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.02a
    • /
    • pp.419-419
    • /
    • 2010
  • 최근 AC-PDP의 효율향상을 위해 MgO Protective Layer 위에 별도의 기능막(Functional Layer)을 적용하고 있으며 기능막의 재료로는 MgO 나노 입자를 사용하고 있다. 그러나 장시간 구동시 AC-PDP Panel 내에서 Plasma 방전에 의하여 MgO Protective Layer와 기능막이 방전 공간에 형성 된 이온에 의해 Sputtering 또는 재 증착 될 수 있다. 본 실험에서는 기능막이 적용된 AC-PDP Test Panel을 제작하여 장시간 구동 후 MgO Protective Layer와 기능막인 MgO 나노 입자의 재형성된 형태를 주사 전자 현미경(Scanning Electron Microscope)을 통해 Surface Profile 및 구조의 변화를 분석하고, 또한 음극선 분광 분석(Cathodoluminascence)을 통하여 방전 영역과 비방전 영역의 delay time, 방전전압 및 효율 등의 전기 광학적 특성과의 관계를 분석하고자 한다.

  • PDF

Toxicity Evaluation of Metals and Metal-oxide Nanoparticles based on the Absorbance, Chlorophyll Content, and Cell Count of Chlorella vulgaris (Chlorella vulgaris의 흡광도, 클로로필 및 개체수 통합 영향에 근거한 중금속 및 나노입자 독성 조사)

  • Jang, Hyun Jin;Lee, Mun Hee;Lee, Eun Jin;Yang, Xin;Kong, In Chul
    • Clean Technology
    • /
    • v.23 no.1
    • /
    • pp.27-33
    • /
    • 2017
  • In this study, toxicities of seven metals (Cu, Cd, Cr, As(III), As(V), Zn, Ni) and five metal oxide nanoparticles (NPs: CuO, ZnO, NiO, $TiO_2$, $Fe_2O_3$) were evaluated based on the growth of Chlorella vulgaris. Effect on algae growth was evaluated by integrating the results of absorption, chlorophyll content, and cell count. The toxicity rankings of metals was observed as Cr ($0.7mgL^{-1}$) > Cu ($1.7mgL^{-1}$) > Cd ($3.2mgL^{-1}$) > Zn ($3.9mgL^{-1}$) > Ni ($13.2mgL^{-1}$) > As(III) ($17.8mgL^{-1}$) ${\gg}$ As(V) (> $1000mgL^{-1}$). Slightly different orders and sensitivities of metal toxicity were examined depending on endpoints of algal growth. In case of NPs, regardless of endpoints, similar toxicity rankings of NPs ($TEC_{50}$) were observed, showing ZnO ($2.4mgL^{-1}$) > NiO ($21.1mgL^{-1}$) > CuO ($36.6mgL^{-1}$) > $TiO_2$ ($62.5mgL^{-1}$) > $Fe_2O_3$ ($82.7mgL^{-1}$). These results indicate that an integrating results of endpoints might be an effective strategy for the assessment of contaminants.

Evaluation of Absorbed Dose According to the Gold Nanoparticle Density in Prostate Cancer Brachytherapy (전립선암의 근접치료 시 금 나노입자 밀도에 따른 흡수선량평가)

  • Lee, Deuk-Hee;Kim, Jung-Hoon
    • Journal of the Korean Society of Radiology
    • /
    • v.13 no.2
    • /
    • pp.247-252
    • /
    • 2019
  • This study was evaluated absorbed dose according to the gold nanoparticle density in prostate brachytherapy which was constantly occurred in Korean men. Absorbed dose evaluation was using MCNPX program which was applied Monte Carlo simulation. Source were applied $^{192}Ir$ which was temporary insertion source and $^{103}Pd$ which was permanently insertion source. And gold nanoparticle density was applied 0 mg, 7 mg, 18 mg and 30 mg. The prostate absorbed dose was increased in proportion to the density 2.95E-14 Gy/e to 4.42E-14 Gy/e in $^{192}Ir$ and showed the same tendency in $^{103}Pd$. And surrounding organ absorbed dose was inversely proportional to the density. Therefore using nanoparticle in brachytherapy was increased therapeutic ratio.

Comparison of Magnesium Hydroxide Particles by Precipitation and Hydrothermal Treatment for Flame Retardant Application to Low Density Polyethylene and Ethylene-Co-Vinyl Acetate Resin (침전법과 수열처리로 제조된 수산화마그네슘 비교와 이의 저밀도 폴리에틸렌-에틸렌 비닐 아세테이트 수지 난연제 적용)

  • Hyun, Mi Kyung;Lim, Hyung Mi;Yoon, Joonho;Lee, Dong Jin;Lee, Seung-Ho;Whang, Chin Myung;Jeong, Sang Ok
    • Applied Chemistry for Engineering
    • /
    • v.20 no.2
    • /
    • pp.234-240
    • /
    • 2009
  • $Mg(OH)_2$ particles were prepared by precipitation and a hydrothermal treatment to examine the effect of $MgCl_2$ concentration, alkali type and concentration, temperature, hydrothermal treatment on the formation of $Mg(OH)_2$ particles using full factorial design, as one of DOE (Design of experiment) methods. The primary particle size is similar to the secondary particle size for the samples after the hydrothermal treatment, where the average particle size of $Mg(OH)_2$ increased with increasing the concentration of $MgCl_2$ and hydrothermal temperature and decreasing alkali/Mg molar ratio. On the other hand, for the samples prepared from precipitation, the secondary particle size is larger than the primary particles due to aggregation. The difference in alkaline source is that the particles prepared from $NH_4OH$ exhibit the larger size with better dispersion than those from NaOH. Low density polyethylene and ethylene-co-vinyl acetate (LDPE-EVA) resin composed of the smaller secondary particle size of $Mg(OH)_2$ shows a higher limited oxygen index (LOI) at 50 and 55% loading, but the smaller primary particle size may result in a better grade in UL-94 tests. At the high loading of 60%, all samples with any preparation methods exhibit V-0 grade but the LOI value depends on not only primary particle size but also dispersion state.

Preparation of Dextran Microparticles by Using the SAS Process (초임계 반용매 재결정 공정을 이용한 Dextran 입자의 제조)

  • Kang, Dong-Yuk;Min, Byoung-Jun;Rho, Seon-Gyun;Kang, Choon-Hyoung
    • Korean Chemical Engineering Research
    • /
    • v.46 no.5
    • /
    • pp.958-964
    • /
    • 2008
  • In this work, micro-sized dextran particles, which have recently been focused as one of the candidate materials for the Drug Delivery System(DDS), were prepared by means of the Supercritical Antisolvent (SAS) process with $CO_2$. With dimethyl sulfoxide(DMSO) as the solvent, effects of the operating variables such as temperature (308.15~323.15 K), pressure(90~130 bar), solute concentration(10~20 mg/ml), and the molecular weight of the solute(Mw=37,500, 450,000) on the size and morphology of the resulting particles were thoroughly observed. The higher solute concentration led to the larger particles, however, the injection velocity of the solution and pressure did not show significant effects on the resulting particle size. With dextran of the lower molecular weight, the smallest particles were obtained at 313.15 K. On the other hand, the size of the particles from the high molecular weight dextran ranged between $0.1{\sim}0.5{\mu}m$ with an incremental effect of the temperature and pressure. For the solute concentration of 5 mg/ml, the lower molecular weight dextran did not form discrete particles while aggregation of the particles appeared when the solute concentration exceeded 15 mg/ml for the higher molecular weight dextran. It is believed that if the solute concentration is too low, the degree of the supersaturation in the recrystallization chamber would not be sufficient for initiation of the nucleation and growth mechanism. Instead, the spinodal decomposition mechanism leads to formation of the island-like phase separation which appears similar to aggregation of the discrete particles. This effect would be more pronounced for the smaller molecular weight polymer system due to the narrower phase-splitting region.

AC-PDP에서 지속방전으로 재형성 된 MgO 나노 입자의 음극선 분광 분석

  • Lee, Gyeong-Ae;Choe, Jun-Ho;Kim, Yong-Hui;Son, Chang-Gil;Choe, Eun-Ha
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.08a
    • /
    • pp.109-109
    • /
    • 2010
  • 최근 AC-PDP에서 MgO Protective Layer 위에 별도의 기능막(Functional Layer)을 사용하고 있는데, 이 기능막인 MgO 나노 입자는 장시간 구동시 AC_PDP panel내에서 plasma 방전에 의하여 MgO Protective Layer와 기능막이 방전 공간에 형성 된 이온에 의해 Sputtering 또는 재 증착 될 수 있다. 본 실험에서는 조성이 다른 기능막이 적용된 AC-PDP Test panel을 제작하여 장시간 구동 후 기능막인 두 가지 다른 MgO 나노 입자의 재형성된 형태를 주사 전자 현미경(Scanning Electron Microscope)을 통해 Surface Profile 및 구조의 변화를 분석하고, 또한 음극선 분광 분석(Cathodoluminascence)을 통하여 방전 영역과 비방전 영역의 delay time, 방전전압 및 효율 등의 전기 광학적 특성과의 관계를 분석하고자 한다.

  • PDF