• 제목/요약/키워드: Marginal discrepancy

검색결과 61건 처리시간 0.023초

Co-Cr-Ti 합금으로 제작한 conical telescope 외관의 변연적합도와 유지력에 관한 연구 (MARGINAL DISCREPANCY AND RETENTION FORCE OF CONICAL TELESCOPE OUTER CROWN WITH CO-CR-TI ALLOY)

  • 정희찬;정창모;전영찬;임장섭
    • 대한치과보철학회지
    • /
    • 제38권2호
    • /
    • pp.214-225
    • /
    • 2000
  • The purpose of this study was to investigate the effects of investing conditions on the marginal discrepancy of conical telescope outer crown with Co-Cr-Ti alloy(Dentitan) and to compare the marginal discrepancy and the retention force of outer crowns using different pattern materials(plastic foil, casting wax, pattern resin). To evaluate the effects of investing conditions on the marginal discrepancy, patterns with plastic foil were invested under three different liquid/powder ratio conditions using phosphate bonded investment(Univest-nonprecious): standard, 10% decreased and 10% increased. At each liquid/powder ratio condition, metal ring was lined with single or double layers of ceramic ring liner. The marginal discrepancy of outer crown at different investing conditions was measured by ${\times}100$ compact measuring microscope(STM5, Olympus, Japan). For measurement of the marginal discrepancy and the retention force of outer crown using different pattern materials, the investing condition of 10% decreased liquid/powder ratio and double layers of ring liner was selected because this investing condition resulted in the best fit of outer crown. Marginal discrepancy was measured in the same way above and retention force on universal testing machine. Under the conditions of this study, the following conclusions were drawn: 1. The thickness of ring liner had more influence on the marginal discrepancy of outer crown than the liquid/powder ratio, and the acceptable marginal fitness could not be expected at the investing condition directed by investment manufacturer 2. There were no differences in the marginal discrepancy of outer crown among three different pattern materials(P>0.05). 3. Casting wax showed the greatest retention force(1640g) of outer crown, followed by pattern resin(1110g), plastic foil(820g). However, there was no significant difference between plastic foil and pattern resin(P>0.05). 4. Plastic foil showed the least variation in marginal discrepancy and retention force.

  • PDF

개별 치아 트레이의 재료와 형태에 따른 인상체의 정밀성에 관한 연구 (A STUDY ON THE ACCURACY OF THE IMPRESSION BODY ACCORDING TO MATERIALS AND FORMS OF THE INDIVIDUAL TOOTH TRAY)

  • 류덕우;임주환;조인호
    • 대한치과보철학회지
    • /
    • 제38권2호
    • /
    • pp.242-254
    • /
    • 2000
  • Accurate impression is very important to achieve desirable prosthesis and there are many factors in taking a good impression. For example, types of impression material, types of impression tray, impression taking methods and so on. Recently individual tooth tray technique is accepted as obtaining good impression that can be applied to multiple abutment impression, heavy salivated patient, to minimize the effect of natural teeth s undercuts and to reduce pain during cord packing procedures. The purpose of this study was to compare the accuracy according to materials and forms of the individual tooth tray which is clinically applied nowadays. Used materials in experiment were divided into 3 types (acrylic resin. $Futar^{(R)}$ occlusion. $Blu-mousse^{(R)}$) and forms were divided into 2 types (forming occlusal vent hole or not and forming marginal vent space or not). Stone master model from impression body and metal master model were measured by $X-PLAN360d^{(R)}$ to compare occlusal surface discrepancy and marginal discrepancy. The results were as follows: 1. In comparison of occlusal surface discrepancy and marginal discrepancy according to materials, groups with three materials showed no statistical difference 2. In comparison of occlusal surface discrepancy and marginal discrepancy according to occlusal vent hole, groups with occlusal vent hole showed significantly less marginal discrepancy than groups with no occlusal vent hole(p<0.05). 3. In comparison of occlusal surface discrepancy and marginal discrepancy according to 0.5mm-marginal-vent-space, groups with no 0.5mm-marginal-vent-space showed significantly less marginal discrepancy than groups with 0.5mm-marginal-vent-space (p<0.05). In summary these results suggest that individual tooth tray made of 3 types of materials with occlusal vent hole and individual tooth tray made of acrylic resin with no marginal vent space showed good accuracy of impression. In addition, individual tooth tray which is made of bite registration materials may be more useful because of advantage in facility and timesaving aspect of fabrication.

  • PDF

Vent의 형성이 도재전장 비귀금속합금 주조체의 변연부 적합도에 미치는 영향 (The effect of vent on the marginal discrepancy of the PFM base metal castings)

  • 김태석;이성욱;오세윤;김웅철;김지환;유진호
    • 대한치과기공학회지
    • /
    • 제23권1호
    • /
    • pp.45-53
    • /
    • 2001
  • This study was performed to investigate the effect of vent on the marginal discrepancy of PFM base metal castings. Eighteen identical wax patterns of a maxillary 3 unit anterior bridge were fabricated. Nine cases out of them were vented with $\phi$2.5mm sprue wax, for direct comparison as to the marginal discrepancy of the castings with the other non vented 9 ones. The mean value of marginal discrepancies of the vented castings was $85.02{\pm}25.57{\mu}m$, and that of the non vented was $163.21{\pm}69.88{\mu}m$ respectively. Statistical analysis revealed that marginal discrepancy of the vented casting was significantly reduced(p<0.05).

  • PDF

도재용 코발트-크롬 금속관의 변연적합도 비교 (Comparison of the Marginal Fitness of Ceramic Co-Cr Metal Crown)

  • 전병욱;김부섭
    • 대한치과기공학회지
    • /
    • 제37권2호
    • /
    • pp.69-76
    • /
    • 2015
  • Purpose: In this study, the marginal fitness of ceramic Co-Cr metal crown made by precision casting, milling, and selective laser melting method were compared. Methods: The ceramic Co-Cr metal crown manufactured by precision casting used the lost wax(LC specimen) method. The abutment were scanned and then made by milling(CM specimen), selective laser melting(CS specimen) method. The specimen were cut bucco-lingual and mesio-distal, and absolute marginal discrepancy and marginal gap were measured using a digital microscope. The surface roughness of the crown was also observed. Results: On the bucco-lingual axial, absolute marginal discrepancy was the LC specimen $31.72({\pm}4.58){\mu}m$, the CM specimen $78.29({\pm}3.28){\mu}m$ and the CS specimen $143.13({\pm}3.83){\mu}m$, respectively. On the bucco-lingual axial, marginal gap was the LC specimen $22.70({\pm}1.46){\mu}m$, the CM specimen $22.70({\pm}1.49){\mu}m$ and CS specimen $99.60({\pm}1.57){\mu}m$, respectively. Conclusion: For ceramic Co-Cr metal crowns, LC specimen was superior for absolute marginal discrepancy and marginal gap. The surface of metal crowns by selective laser melting were the roughest.

Evaluation of marginal discrepancy in metal frameworks fabricated by sintering-based computer-aided manufacturing methods

  • Kaleli, Necati;Ural, Cagri;Us, Yesim Olcer
    • The Journal of Advanced Prosthodontics
    • /
    • 제12권3호
    • /
    • pp.124-130
    • /
    • 2020
  • PURPOSE. The aim of this in vitro study was to evaluate the effect of sintering procedures on marginal discrepancies of fixed partial metal frameworks fabricated using different sintering-based computer-aided design and computer/aided manufacturing (CAD/CAM) techniques. MATERIALS AND METHODS. Forty resin die models of prepared premolar and molar abutment teeth were fabricated using a three-dimensional (3D) printer and divided into four groups (n = 10) according to the fabrication method of metal frameworks used: HM (via hard milling), SM (via soft metal milling), L25 (via direct metal laser melting [DMLM] with a 25 ㎛ layer thickness), and L50 (via direct DMLM with a 50 ㎛ layer thickness). After the metal frameworks were fabricated and cemented, five vertical marginal discrepancy measurements were recorded in each site (i.e., buccal, facing the pontic, lingual, and facing away from the pontic) of both abutment teeth under a stereomicroscope (×40). Data were statistically analyzed at a significance level of 0.05. RESULTS. No statistically significant differences (P>.05) were found among the four axial sites of metal frameworks fabricated by sintering-based CAD/CAM techniques. The HM and L25 groups showed significantly (P<.001) lower marginal discrepancy values than the SM and L50 groups. CONCLUSION. Marginal discrepancy in the sites facing the pontic was not influenced by the type of sintering procedure. All fabrication methods exhibited clinically acceptable results in terms of marginal discrepancies.

Comparative clinical study of the marginal discrepancy of fixed dental prosthesis fabricated by the milling-sintering method using a presintered alloy

  • Kim, Mijoo;Kim, Jaewon;Mai, Hang-Nga;Kwon, Tae-Yub;Choi, Yong-Do;Lee, Cheong-Hee;Lee, Du-Hyeong
    • The Journal of Advanced Prosthodontics
    • /
    • 제11권5호
    • /
    • pp.280-285
    • /
    • 2019
  • PURPOSE. The present study was designed to examine the clinical fit of fixed dental prosthesis fabricated by the milling-sintering method using a presintered cobalt-chromium alloy. MATERIALS AND METHODS. Two single metal-ceramic crowns were fabricated via milling-sintering method and casting method in each of the twelve consecutive patients who required an implant-supported fixed prosthesis. In the milling-sintering method, the prosthetic coping was designed in computer software, and the design was converted to a non-precious alloy coping using milling and post-sintering process. In the casting method, the conventional manual fabrication process was applied. The absolute marginal discrepancy of the prostheses was evaluated intraorally using the triple-scan technique. Statistical analysis was conducted using Mann-Whitney U test (${\alpha}=.05$). RESULTS. Eight patients (66.7%) showed a lower marginal discrepancy of the prostheses made using the milling-sintering method than that of the prosthesis made by the casting method. Statistically, the misfit of the prosthesis fabricated using the milling-sintering method was not significantly different from that fabricated using the casting method (P=.782). There was no tendency between the amount of marginal discrepancy and the measurement point. CONCLUSION. The overall marginal fit of prosthesis fabricated by milling-sintering using a presintered alloy was comparable to that of the prosthesis fabricated by the conventional casting method in clinical use.

In-vitro evaluation of marginal and internal fit of 3-unit monolithic zirconia restorations fabricated using digital scanning technologies

  • Ozal, Cise;Ulusoy, Mutahhar
    • The Journal of Advanced Prosthodontics
    • /
    • 제13권6호
    • /
    • pp.373-384
    • /
    • 2021
  • PURPOSE. This study aimed to compare the marginal and internal fit of 3-unit monolithic zirconia restorations that were designed by using the data obtained with the aid of intraoral and laboratory scanners. MATERIALS AND METHODS. For the fabrication of 3-unit monolithic zirconia restorations using impressions taken from the maxillary master cast, plaster cast was created and scanned in laboratory scanners (InEos X5 and D900L). The main cast was also scanned with different intraoral scanners (Omnicam [OMNI], Primescan [PS], Trios 3 [T3], Trios 4 [T4]) (n = 12 per group). Zirconia fixed partial dentures were virtually designed, produced from presintered block, and subsequently sintered. Marginal and internal discrepancy values (in ㎛) were measured by using silicone replica method under stereomicroscope. Data were statistically analyzed by using 1-way ANOVA and Kruskal Wallis tests (P<.05). RESULTS. In terms of marginal adaptation, the measurements on the canine tooth indicated better performance with intraoral scanners than those in laboratory scanners, but there was no difference among intraoral scanners (P<.05). In the premolar tooth, PS had the lowest marginal (86.9 ± 19.2 ㎛) and axial (92.4 ± 14.8 ㎛), and T4 had the lowest axio-occlusal (89.4 ± 15.6 ㎛) and occlusal (89.1 ± 13.9 ㎛) discrepancy value. In both canine and premolar teeth, the D900L was found to be the most marginally and internally inconsistent scanner. CONCLUSION. Within the limits of the study, marginal and internal discrepancy values were generally lower in intraoral scanners than in laboratory scanners. Marginal discrepancy values of scanners were clinically acceptable (< 120 ㎛), except D900L.

열가압성형도재의 사용이 금속도재관 치경부 변연적합도에 미치는 영향 (The effect of heat and press-on-metal technique on marginal fit of metal-ceramic crown)

  • 김지은;김세연;이청희
    • 대한치과보철학회지
    • /
    • 제52권2호
    • /
    • pp.90-96
    • /
    • 2014
  • 연구 목적: 이 연구의 목적은 열가압성형기법이 금속도재관의 치경부 변연적합도에 미치는 영향을 확인하는 것이다. 연구 재료 및 방법: 실험에 앞서, 4개의 금속 주모형을 형성하였다. 각 모형은 각각chamfer, heavy chamfer, shoulder with bevel, shoulder (collarless)변연을 형성하였다. 각 변연당 10개씩의 금관을 제작하여, 총 40개를 제작하였다. Coping 단계에서, 그리고 금속도재관 완성 단계에서 주모형과 금관 사이의 변연간극은 100배율의 광학현미경 관찰을 통하여 측정되었다. Data분석은 paired t-test along with one-way ANOVA와 Duncan multiple comparison test를 이용하여 이루어졌다. 결과: 변연간극의 평균과 표준편차를 분석한 결과, 금속 코핑과 그 후 완성된 금속도재관, 모든 경우에서 변연부 간격은 임상적 허용범위 안에 있었다. Chamfer 변연 실험군의 경우 Heavy chamfer 변연 실험군에 비하여 금속도재관 완성 후 변연부 간격의 유의한 증가가 있었다. 그리고Shoulder 변연 실험군에서 도재로 처리된 변연이 Chamfer와 Shoulder변연 실험군의 금속변연에 비하여 변연부 간격이 유의하게 작게 나타났다. 결론: 열가압성형기법을 통하여 제작한 금속도재수복물의 변연적합도는 전통적인 방법으로 제작한 금속도재수복물의 변연적합도와 유의한 차이점이 없었다. 제작과정의 효율성으로, 열가압성형기법은 임상에서의 효과적인 사용법으로 고려될 수 있다.

절삭 및 적층 가공법으로 제작된 3본 고정성 국소의치의 변연 및 내면 적합도에 관한 연구 (Marginal and internal discrepancy of 3-unit fixed dental prostheses fabricated by subtractive and additive manufacturing)

  • 최재원
    • 대한치과보철학회지
    • /
    • 제58권1호
    • /
    • pp.7-13
    • /
    • 2020
  • 목적: 본 연구의 목적은 절삭 가공법 및 적층 가공법에 의해 제작된 3본 고정성 국소의치의 변연 및 내면 적합도를 비교하는 것이다. 재료 및 방법: 상악 좌측 제2소구치가 상실된 3본 고정성 국소의치 지대치를 제작하고(주모형), 구강 스캐너를 이용해 주모형 스캔 데이터를 얻었다. 3본 고정성 보철물은 다음과 같은 3가지 방법으로 제작하였다: Milled 3-unit fixed dental prostheses (FDP) (MIL군), digital light processing (DLP) 3D printed 3-unit FDP (D3P군), stereolithography apparatus (SLA) 3D printed 3-unit FDP (S3P군). 보철물의 변연 및 내면 적합도와 내면 정밀도 평가하기 위해 각각 triple-scan protocol과 콤비네이션 수식을 사용하여 스캔 데이터를 중첩하였다. 3차원 분석 프로그램(Geomagic control X)을 사용하여 root mean square (RMS) 값과 color difference map 통해 정량 및 정성 분석 시행하였다. Kruskal-Wallis test (α = .05)와 Mann-Whitney U test 및 Bonferroni correction (α = .05/3 = .017)을 이용하여 통계 분석하였다. 결과: S3P군의 변연 적합도는 MIL군과 D3P군에 비해 우수하였으며, MIL군과 D3P군은 비슷한 수준을 보였다. D3P군과 S3P군은 MIL군에 비해 상대적으로 우수한 내면 적합도를 보였으며, D3P군과 S3P군 사이에는 유의한 차이가 없었다. 한편, MIL군, S3P군, 그리고 D3P군 순으로 우수한 정밀도를 보였다. 결론: 본 연구의 한계 내에서 적층 가공법으로 제작된 3본 고정성 보철물은 절삭 가공법으로 제작된 3본 고정성 보철물에 비해 우수한 변연 및 내면 적합도를 보인 반면 정밀도는 떨어지는 것으로 나타났다.

Precision of the milled full-arch framework fabricated using pre-sintered soft alloy: A pilot study

  • Woo, Hyun-Wook;Cho, Sung-Am;Lee, Cheong-Hee;Lee, Kyu-Bok;Cho, Jin-Hyun;Lee, Du-Hyeong
    • The Journal of Advanced Prosthodontics
    • /
    • 제10권2호
    • /
    • pp.128-131
    • /
    • 2018
  • PURPOSE. This study aimed to evaluate the marginal discrepancy of full-arch frameworks in implant-supported prostheses fabricated using pre-sintered soft alloy (PSA). MATERIALS AND METHODS. Full-arch metal frameworks were fabricated on the edentulous implant model using casting alloy (CA), fully-sintered hard alloy (FHA), and PSA (n = 4 in each group). To evaluate the misfit of the framework to the abutments, the absolute marginal discrepancy (AMD) values of the frameworks were measured in cross-sectional images that had been drawn as part of the triple-scan protocol. The AMD values were compared among the tested alloy groups using the Kruskal-Wallis test, with a post hoc Mann-Whitney U test (${\alpha}=.05$). RESULTS. The FHA and PSA groups showed lower marginal discrepancies than the CA group (P<.001). However, the FHA group did not differ significantly from the PSA group. CONCLUSION. Soft alloy milling is comparable to hard alloy milling, and it is more precise than casting in terms of the marginal fit of implant-supported, full-arch prostheses.