The magneto-transport properties of an individual single crystalline Bi nanowire grown by a spontaneous growth method are reported. A four-terminal device based on an individual 400-nm-diameter nanowire was successfully fabricated using a plasma etching technique that removed an oxide layer that had formed on the surface of the nanowire. Large transverse ordinary magnetoresistance (1401%) and negative longitudinal ordinary magnetoresistance (-38%) were measured at 2 K. It was observed that the period of Shubnikov-de Haas oscillations in transverse geometry was $0.074^{T-1}$, $0.16^{T-1}$ and $0.77^{T-1}$, which is in good agreement with those of bulk Bi. However, it was found that the period of SdH oscillation in longitudinal geometry is $0.24^{T-1}$, which is larger than the value of $0.16^{T-1}$ reported for bulk Bi. The deviation is attributable to the spatial confinement arising from scattering at the nanowire surface boundary.
미크론 자성비드 검출용 바이오센서에 활용하는 GMR-SV 박막을 이온빔 스퍼터링 증착법으로 glass/Ta(5.8 nm)/NiFe(5 nm)/Cu(t nm)/NiFe(3 nm)/FeMn(12 nm)/Ta(5.8 nm)의 구조를 갖도록 증착하였다. 비자성체 Cu의 두께가 3.0 nm에서 2.2 nm까지 얇아질수록 교환결합력은 증가하였고 자기저항비는 다소 감소하였다. 비자성체의 두께가 얇으면 반강자성체의 층간 교환작용이 강자성체의 고정층뿐만 아니라 자유층의 스핀배열에도 영향을 주고 있음을 확인할 수 있었다. 또한 리소그래피 공정 과정을 거쳐 GMR-SV 소자를 제작하여 미크론 자기비드를 검출하였다. 여기서 자기비드를 떨어뜨리기 전과 후의 자기저항비, 교환결합력, 보자력은 각각 0.9%, 3Oe, 2 Oe의 값을 나타내었다. 이러한 결과로 나노 단위의 바이오센서에 활용할 수 있는 가능성을 보여주었다.
고감도 바이오센서용 거대자기저항-스핀밸브(Giant magnetoresistance-spin valve; GMR-SV) 박막소자의 미세패턴 공정으로 인한 교환결합력과 보자력 약화 문제를 해결하고자 전자사이크로트론 공명(Electron Cyclotron Resonance) Ar-이온 밀링을 이용하여 GMR-SV 박막에 지름 $35{\mu}m$인 원형 모양의 홀(Hole)을 패턴닝 하였다. GMR-SV를 4-단자법으로 측정한 자기저항 곡선으로부터 홀 개수가 많아질수록 자기저항비와 자장감응도는 홀이 없을 때 측정된 초기값과 같은 값을 유지하였고, 교환결합세기와 보자력은 120 Oe에서 190 Oe, 10 Oe에서 41 Oe로 크게 향상되었다. 이러한 현상은 GMR-SV 박막내의 자화용이축과 같은 방향을 띄고 센싱 전류의 방향과 수직인 공간에 위치하는 용이 자구영역(Easy magnetic domain; EMD)의 역할에 기인하는 결과를 보여주었다. GMR-SV 바이오 소자 제작시 폭을 넓게 하고 소자내부에 홀의 개수를 증가시켜 발생하는 EMD 효과가 자기저항특성을 향상시킬 수 있었다.
우리는 증기전달법(vapor transport method)으로 성장된 $Cr_5S_6$ 단결정의 자기저항 효과를 연구하였다. 상온에서의 X-선 회절 (X-ray diffraction) 연구는 삼방구조(trigonal structure)를 가지는 단결정의 상 형성을 보여주었다. 5 K~400 K 온도영역에서 온도의 함수로 자기장(0.1 T, 5 T)을 걸어주면서 자화를 측정하였다. 자화의 온도의존성 결과로부터 $Cr_5S_6$의 두 가지 상태변화를 확인 할 수 있었다. 첫 번째는 150 K 근처에서 반강자성에서 준강자성으로의 전이가 일어나고, 두 번째는 준강자성에서 상자성으로의 전이가 300 K 근처에서 일어난다. 0 T와 5 T의 자기장에서 측정한 온도에 따른 저항의 변화는 150 K 근처에서 반강자성-준강자성 전이를 보여주면서 금속성을 보여주었다. 자기장의 변화에 따른 자화의 변화를 고정된 온도(100 K, 150 K, 200 K, 그리고 300 K)에서 측정하였다. 200 K과 300 K에서는 M-H 이력 현상을 잘 보여주는 반면에, 100 K과 150 K에서는 이력 현상을 보여주지 않았다. 150 K, 즉 반강자성 전이온도에서 $Cr_5S_6$는 5 T의 자기장 하에서 약 -2%의 음의 자기저항(magnetoresistance)이 관찰되었다.
d.c.magnetron sputtering 방법으로 제작된 Fe/[NiFe/Cu] 다층박막을 Fe 기저층의 두께, 적층횟수 및 열처리 온도 변화에 따라 자기저항비가 계면 거칠기 및 우선 배향에 미치는 영향에 대하여 조사하였다. Fe 기저층의 두께가 증가함에 따라 (200) 우선 배향의 세기라 증가하였으며, 자기저항비는 Fe70$\AA$의 두께어서 최대값 4.7%를 보이며 이때 자장감응도도 최대를 나타낸다. Fe 기저층의 두께를 70$\AA$ 으로 고정시키고 적층횟수를 변화시켰을 때 40층에서 최대값 5.3%를 보였다. 열처리 온도에 따른 자기저항비는 $300^{\circ}C$이하에서는 커다란 변화가 없으며, $300^{\circ}C$이상에서는 크게 감소하였는데, 이는 Cu의 확산에 의한 상자성 혼합층의 증가와 반강자성석으로 결함된 자성층간의 배열의 변화가 그 원인이다.
나노옥사이드(nato-oxide layer, NOL) 층이 고정층에 첨가된 스펙큘라 스핀밸브(specular spin valve)와 NOL이 없는 기본 스핀 밸브를 UHV 스퍼터 시스템에서 FeMn 반강자성층을 사용하여 탑 및 바텀 형 스핀밸브를 제조하였으며, 제조한 시료의 열처리 온도에 따른 자기저항 특성 및 교환바이어스 특성을 비교 분석하였다. 탑 형 스핀밸브에서는 NOL이 있는 경우 25$0^{\circ}C$ 열처리에서 9.2%의 자기저항비를 얻을 수 있었으며, 바텀 형 스핀밸브에서는 25$0^{\circ}C$ 열처리에서 10.1%의 자기저항비를 얻을 수 있었다. 따라서 바텀 형 스핀밸브가 탑 형 스핀밸브보다 고정층에 첨가된 NOL의 스펙큘라 반사 효과가 높아 자기저항비가 증가함을 확인하였다. 또한 바텀 형 스핀밸브에서 25$0^{\circ}C$ 이상의 열처리시 NOL이 있는 경우가 NOL이 없는 경우보다 28 % 이상의 교환바이어스 증가를 보였다. 이와 같은 원인은 NOL이 첨가된 고정층의 자기모멘트의 감소와 X-선 회절 분석 결과로부터 NOL의 첨가에 따른 강화된 (111) FeMn집합조직 때문이라고 판단된다.
Dc 마그네트론 스퍼터링법으로 자기저항비 5.0 %와 자장감응도 1.5 %/Oe를 갖는 glass/Ta(5.8 nm)/NiFe(5 nm)/Cu(2.3 nm)/NiFe(3 nm)/IrMn(12 nm)/Ta(5.8 nm) 다층구조 GMR-SV 박막을 증착하였다. 광 리소그래피 공정으로 적혈구 직경 크기인 $7{\mu}m{\sim}8{\mu}m$ 이내의 선폭인 GMR-SV 소자를 제작하였다. 직경 $1{\mu}m$ 크기인 여러 개의 자성비드가 결합된 적혈구를 자기저항비 1.06 % 자장감응도 0.3 %/Oe를 갖는 GMR-SV 소자에 떨어뜨려 -0.6 Oe 부근에서 약 $0.4{\Omega}$과 약 0.15 %의 변화를 관찰하였다. 본 연구로부터 미크론 크기의 선폭을 갖는 GMR-SV 소자가 자성비드를 결합한 적혈구내 헤모글로빈의 새로운 자성 특성을 분석하는 바이오센서로 활용할 수 있음을 보여주었다.
FeMn에 의해 교환 바이어스된 Synthetic antiferromagnet(CoFe/Ru/CoFe)을 가진 Top Ta/NiFe/CoFe/Cu/CoFe/Ru/CoFe/FeMm/Ta 스핀밸브 구조를 마그네트론 스퍼터링 법으로 제조하여 유효 교환이방성 및 자기저항 특성을 조사하였다. FeMn 반강자성층의 두께가 100$\AA$정도일 때 자기저항비와 유효 교환바이어스 자장이 최대값을 나타내었으며, 100 $\AA$ 이상 두께 증가시 FeMn층을 통한 션팅 전류에 의한 자기저항 효율의 저하로 자기저항이 점점 감소하였다. 자유층의 두께가 40 $\AA$일 때 7.5% 이상의 최대 자기저항비가 얻어졌으며, 자유층의 두께 감소에 따라 자기저항비는 감소하였다. Synthetic antiferrormagnet 구조에서 Cu층에 인접한 CoFe(Pl)층의 두께를 증가시키고 FeMn층에 인접한 CoFe(P2)층의 두께를 감소시켜 그 두께 차이가 증가할수록 자기저항비는 증가하였고 반면 유효 교환 바이어스 자장은 감소하였다. 자기저항특성의 증가는 Pl층 두께 증가로 인한 스핀의존산란 효율의 증가로 이해되었으며, 유효 교환 바이어스 자장의 감소는 최소에너지 모델의 이론적 계산을 통해 감소경향을 검증할 수 있었다.
Local magnetization reversal in the exchange-biased NiFe/FeMn and $[Pd/Co]_5/FeMn$ multilayers with in-plane and out-of-plane magnetic anisotropy was achieved by using laser annealing. The local annealed NiFe/FeMn film under the opposite magnetic field shows a magnetoresistance (MR) curve having two symmetric peaks at the positive and negative exchange biasing field (${\pm}H_{ex}$). The intensity of the nucleated MR peak rises as the exposed area extends during the laser annealing process, and the peak disappears under the reverse magnetic field. In the case of [Pd/Co]/FeMn films, the local magnetization reversal increased gradually as the laser power increases. The locally reversed magnetization was restored under the opposite magnetic field.
미시자기모델과 Stoner-Wohlfarth 모델을 이용하여 미크론 크기로 패터닝(patterning) 된 퍼멀로이 박막의 자기소거장 효과를 분석하였다. 또한 20 $\mu\textrm{m}$$\times$(40 $\mu\textrm{m}$~200 $\mu\textrm{m}$) 크기의 퍼멀로이 박막 시료를 DC 마그네트론 스퍼터링과 광 리소그라피(photo littlography)로 제작하였고, 제작된 시료의 자기저항 특성과 전산시늉에 의한 결과를 비교하였다. 미시자기모델에 의한 결과가 Stoner-Wohlfarth모델에 의한 결과보다 측정 데이터에 더 잘 일치하였다. 전산시늉 결과 미크론 크기로 패터닝 된 자기박막 시료의 경우 Stoner-Wohlfarth 모델에서의 자기소거장 근사식이 수정되어야함을 제안하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.