본 연구에서는 마그네트론 스퍼터링 법으로 제작한 Mn-Ir/Ni-Fe/Buffer/Si 다층막에서 다양한 하지층과 적층구조에 따른 교환이방성과 미세구조에 대하여 고찰하였다. Ni-Fe 위에 Mn-Ir을 증착한 Top 구조의 경우에서는 (111) 우선방위에 상관없이 165 Oe 이상의 높은 Hex 값을 얻을수 있었다. 또한 Mn-Ir/Ni-Fe 계면에서 grain-to-grain epitaxy가 발생함을 알 수 있었다. 따라서 Mn-Ir/Ni-Fe 다층박막의 Hex는 Mn-Ir/Ni-Fe 계면에서의 Mn-Ir의 결정립 크기와 grain-to-grain epitaxy에 의존하며 Hc는 Mn-Ir/Ni-Fe의 계면거칠기에 의존한다는 것을 알 수 있었다.
An ion-exchanged reaction of $MnCl_2$ with Al-incorporated solid core/mesoporous shell silica (AlSCMS) followed by calcinations generated manganese species, where average oxidation state of manganese ion is 3+, in the mesoporous materials. Dehydration results in the formation of $Mn^{2+}$ ion species, which can be characterized by electron spin resonance (ESR). The chemical environments of the manganese centers in Mn-AlSCMS were investigated by diffuse reflectance, UV-VIS and ESR spectroscopic methods. Upon drying at 323 K, part of manganese is oxidized to higher oxidation state ($Mn^{3+}$ and $Mn^{4+}$) and further increase in (average) oxidation state takes place upon calcinations at 823 K. It was found that the manganese species on the wall of the Mn-AlSCMS were transformed to tetrahedral $Mn^{3+}$ or $Mn^{4+}$ and further changed to square pyramid by additional coordination to water molecules upon hydration. The oxidized $Mn^{3+}$ or $Mn^{4+}$ species on the surfaces were reversibly reduced to $Mn^{2+}$ or $Mn^{3+}$ species or lower valances by thermal process. Mn(II) species I with a well resolved sextet was observed in calcined, hydrated Mn-AlSCMS, while Mn (II) species II with g = 5.1 and 3.2 observed in dehydrated Mn-AlSCMS. Both species I and II are considered to be non-framework Mn(II).
본 연구에서는 열벽 적층 성장법으로 GaAs(100) 기판 위에 $Zn_{1-x}Mn_{x}Te$ 에피층을 성장하여 그 특성을 조사하였다. $Zn_{1-x}Mn_{x}Te$ 에피층의 Mn 조성비는 x = 0.97까지 얻을 수 있었으며 성장된 시료의 결정구조는 징크브랜드이었다. 성장된 면은 GaAs (100) 기판과 동일한 방향으로 성장되었다. 성장시 기판 온도가 $350^{\circ}C$에서 $400^{\circ}C$로 증가함에 따라 Mn 조성비 x는 0.02에서 0.23으로 증가하였다. $Zn_{1-x}Mn_{x}Te$ 에피층의 격자상수는 Mn 조성비 x가 증가할수록 선형으로 증가하였고 띠 간격 에너지는 x에 대하여 비선형으로 증가하였다.
The effects of Mn2O3 and Y2O3 additives on the microstructure and dielectric properties of Sr(Zr, Ti)O3 have been investigated. Powders with Sr(Zr1-xTix)O3(0$\leq$x$\leq$0.1) composition were prepared by the conventional solid state processing from commercial TiO2 and precipitation-processed ZrO2. The powders containing sintering additives of Mn2O3 and Y2O3 were compacted and then sintered at 1,55$0^{\circ}C$ for 4 h to get>97% relative density. Mn2O3 suppressed the grain growth and Y2O3 enhanced the density of sintered body. The oxidation state of Mn ions were determined by a chemical wet method and EPR spectroscopy. Mn ions were present as Mn2+ and Mn4+ in SrZrO3, while as Mn3+ and Mn4+ in Ti-substituted Sr(Zr, Ti)O3. With the substitution of Ti, the lattice parameters of SrZrO3 decreased and its dielectric constant increased with remarkable decrease in Q value. The dielectric constant of Sr(Zr, Ti)O3 was in the range of 30 to 40, Q values 1,200~5,400 at 6 GHz and temperature coefficient of resonant frequency -67~100 ppm/K.
양이온 결손 La0.970Mn0.970O3의 x-ray photoemission spectroscopy를 온도를 함수로 측정하였다. 온도의 변화에 따라서 Mn 2p와 3d core level의 화학적 변동 및 이동이 관측되었다. 즉 Mn 2p 3/2와 1/2 및 La 3d core 스펙트럼은 온도의 증가와 함께 저 결합 에너지 측으로 이동이 관측되었다. 이러한 XPS 관측 결과는 Mn3+의 localization의 강도 변화에 의한 것으로 사료되며, Mn3+에 의한 Jahn-Teller효과 이외에도 conventional random potential 효과 역시 La0.790Mn0.970O3의 전도 carrier의 localization에 기여하는 것으로 사료된다.
[ $LiMn_2O_4$ ] $Mn^{2+}$이온 용출현상 연구를 위한 간단하고 신속한 전기화학적 $Mn^{2+}$이온 분석법을 정립하였다. 이 분석법은 완충용액에서 $Mn^{2+}$이온이 $Mn^{4+}(MnO_2)$로 산화되는 원리를 이용한다. 최적조건 (pH 8.9 0.04 M $NH_3-NH_4Cl$ 완충용액 및 glassy carbon 작업전극)에서, Linear sweep voltammetry(LSV) 측정에 대해 $5{\mu}M-100{\mu}M$ (0.275-5.5 ppm) $Mn^{2+}$이온 범위에서, differential pulse voltammetry (DPV) 측정에 대해 $0.2{\mu}M-10{\mu}M$ (0.011-0.55 ppm) 범위에서 선형적 응답 특성을 확인하였다. 또한, 측정용액에 리튬 이차전지용 전해액 ($LiPF_6$, EC, EMC)이 첨가할 경우, 첨가량에 비례하여 $Mn^{2+}$ 이온의 산화 전류 감소하였는데, 이러한 감소의 주요 원인은 EMC보다는 $LiPF_6$와 EC성분임을 확인하였다.
Manganese dependent peroxidase (MnP) is the most ubiquitous enzyme produced by white-rot fungi, MnP is known to be involved in lignin degradation, biobleaching and oxidation of hazardous organopollutants. Bjerkandera fumosa is a nitrogen-unregulated white-rot fungus, which produces high amounts of MnP in the excess of N-nutrients due to increased biomass yield. The objective of this study was to optimize the MnP production in N-sufficient cultures by varying different physiological factors such as Mn concentration, culture pH, and incubation temperature. The growth of fungus was optimal in pH 4.5 at $30^{\circ}C$, $N_2$-unregulated white-rot fungus produces high amounts of MnP in the excess N-nutrients. The fungus produced the highest level of MnP (up to $1000U/{\ell}$) with $0.25g/{\ell}$ asparagine and $1g/{\ell}$$NH_4Cl$ as N source at 1.5 mM $MnCl_2$ concentration, pH value of 4.5 at $30^{\circ}C$. Purification of MnP revealed the existence of two isoforms: MnPl and MnP2. The molecular masses of the purified MnPl and MnP2 were in the same range of 42~45 kDa. These isoforms of B. fumosa strictly require Mn to oxidize phenolic substrates. Concerned to kinetic constants of B. fumosa MnPs, B. fumosa has similar Km value and Vmax compared to the other white-rot fungi.
Half-metallic Heusler alloys (NiMnSb, ppdMnSb, pptMnSb) have attracted much attention due to their unique electronic and magnetic structures. Sppin-ppolarized band structure calculation ppredicts metallic behavior for the majority sppin states and semiconductor behavior for the minority sppin states. We have studied the electronic structures of these half-metallic Heusler alloys by core-level pphotoemission sppectroscoppy of Mn 2pp and 3s XppS sppectra. We found large intensities of Mn 2pp satellites and 3s exchange spplitting comppared with other metal Mn-alloys. These satellite structure can be understood by applying Anderson imppurity model. This fact supports the calculated sppin pprojected ppartial density of states which suggests that the valence electrons be highly sppin ppolarized near Fermi level and that the electrons involved with charge-transfer be mainly minority sppin ones which have semiconducting band structure. The trend of charge transfer energies Δ from ligands (Sb 5pp) to Mn 3d, obtained from our model fitting, is consistent with that calculated from sppin pprojected ppartial density of state. Also the trend of d-d electron correlation energies U calculated from Mn Auger line L3 VV by Mg $K\alpha$ source is comppatible with that resulted from our model fitting. We fitted the Mn 3s curve in the same way as for insulating Mn comppounds by using the same pparameters calculated from Mn 2pp curve fitting exceppt for the Coulomb interaction energy Q between core hole and d-electrons. The 3s sppectra were analyzed by combing the charge transfer model and a simpple model taking into account the configuration mixing effect due to the intra-shell correlation. We found that the exchange interaction between 3s hole and 3d electrons is mainly respponsible for the satellite of Mn 3s sppectra. This is consistent with the neutron scattering data, which suggests local 3d magnetic moment. We find that the XppS analysis results of Mn 2pp and 3s satellite structures of half-metallic Heusler alloys are very similar to those of insulating transition metal comppounds.
Alumina added with Mn3O4 up to 7.5 cat% of Mn was prepared by conventional ceramic processing, and the sintering behavior and the optical properties of which were studied as functions of Mn content. Densification and grain growth of alumina were enhanced by Mn addition up to 0.75 cat% but was leveled off at higher concentrations. XRD revealed that $Al_2MnO_4$(galaxite) was formed as a second phase in the specimens with more than 0.75 cat% of Mn. Thus it is believed that either the solid solution effect of Mn or the Zener effect of $Al_2MnO_4$ becomes predominant in the sintering of Mn-added $Al_2O_3$ according to the additive concentration. UV-VIS reflectivity(SCI) spectra of Mn-added $Al_2O_3$ consisted of smooth bottoms in 300~550 nm wavelength range and plateaus at wavelengths longer than 650 nm. The reflectivity spectrum continuously moved downward, and the specimen color became darker and thicker with increasing Mn content. The CIELAB color change with respect to standard white was also dependent on the amount of Mn added: ${\Delta}L^*$(D65) negatively increased and ${\Delta}E_{ab}^*$(D65) positively increased with increasing Mn content, probably due to Mn substitution to Al and/or the mixing effect of black $Al_2MnO_4$ as a second phase.
본 연구에서는 Mn-PC 촉매와 상압유통식 반응장치를 이용하여 $200{\sim}380^{\circ}C$ 범위에서 VOCs(아세트알데히드, 프로피온알데히드, 톨루엔) 연소반응을 수행하였다. 촉매 전처리(air, $450^{\circ}C$, 1 hr, 60 cc/min) 전 후의 물리화학적 특성변화 조사는 TGA (Thermogravimetric Analyzer), BET (Brunauer Emmett Teller), EA (Elemental Analyzer), XRD (X-ray Diffractometer) 및 SEM (Scanning Electronic Microscope)을 이용하여 파악하였다. TGA 분석결과 Mn-PC의 열중량(공기 분위기) 감소는 $419^{\circ}C$에서 88 wt.%를 나타내었으며, 전처리 후 비표면적은 크게 증가하는 것으로 확인되었다. EA 분석결과 전처리를 통해서 유기물 성분은 분해 또는 연소되어 거의 관찰되지 않는 것으로 파악되었다. 또한 XRD분석을 통해 Mn-PC 촉매가 전처리 후 새로운 형태의 산화물인 $Mn_3O_4$로 전이됨을 확인하였다. 그리고 SEM 분석결과 전처리 과정에서 많은 micropore가 생성된 것으로 관찰되었다. 프로피온알데히드 연소의 경우 전처리한 Mn-PC는 $Mn_3O_4$와 fresh한 Mn-PC 보다 우수한 촉매활성을 나타내었다. 전처리된 Mn-PC상에서 VOCs 연소 효과는 톨루엔 < 아세트알데히드 < 프로피온알데히드 순서로 나타났다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.