천이액상확산접합에 의한 합금공구강의 접합특성 (Joinability of Tool Steels by TLP Bonding)

  • 권병대;이원배;김봉수;홍태환;서창제;정승부
    • Journal of Welding and Joining
    • /
    • 제21권4호
    • /
    • pp.69-74
    • /
    • 2003
  • The mechanical properties of STD11 Joints by using TLP (Transient Liquid Phase Diffusion) bonding method employing MBF-30 and MBF-80 insert metals were investigated with concerning to the microstructural change. TLP bonding of STD 11 was carried out at 1323∼1423K for 0.6ks∼3.6ks in vacuum. The microstructure and the element distribution of the interlayer between tool steels and insert metals showed specific feature with bonding conditions. It was found that the width of the interlayer increased at initial bonding stage. However, the width of interlayer showed nearly constant value during the isothermal solidification. After isothermal solidification was completed, the joint showed homogeneous element distribution and similar microstructure with base metal because of the grain boundary migration to the bonded interlayer. The bonding strength measured by a tensile test has been varied with the bonding conditions. The maximum joint strength, 760MPa, was obtained with the condition of 1423K for 1.2ks using MBF30 insert metal in this experiment.

일방향응고 Ni기초내열합금 GTD-111의 천이액상확산접합(III) - 미세조직 및 기계적 성질에 미치는 균질화처리 및 시효처리의 영향 - (Transient Liquid Phase Bonding of Directionally Solidified Ni Base Superalloy, GTD-111(III) - The Effect of Homogenizing and Aging on the Microstructures and Mechanical Properties -)

  • 강정윤;황형철;김인배;김대업;우인수
    • Journal of Welding and Joining
    • /
    • 제21권3호
    • /
    • pp.78-84
    • /
    • 2003
  • The changes of microstructure and hardness of TLP bonds of directionally solidified Ni base superalloy, GTD-111, with variation of homogenizing and aging treatment were investigated. The specimens were bonded at 1403K for 7.2ks using different insert metals such as MBF-50, MBF-80 and MBF-90 and they were homogenized at 1393K with various holding time. At center of bonded interlayer homogenized for hold time 30h, the contents of aluminum and titanium were approximately 90% and 95% of base metal, respectively. In this study, aging was performed at three different kinds : one step aging ; 1113K $\times$ 16h, two step aging ; 1113K $\times$ 10h ⇒ 1103K $\times$ 10h, three step aging ; 1113K $\times$ 10h ⇒ 1103K $\times$ 8h ⇒ 922K $\times$ 24h. ${\gamma}$' volume fraction and hardness of joints were high in the sequence of one step, two step and three step aging, whereas ${\gamma}$' volume fraction and hardness of joints obtained by three step aging treatment were higher than those of raw material. Tensile properties of joints bonded with MBF-80 and MBF-90, homogenized at 1393K for 30h and then three step aged became excellent than those of raw material, however, joint bonded with MBF-50 was poor.

$^{13}N$-암모니아 PET에서 반정량적 심근관류 점수와 절대적 심근혈류량의 상관관계 (Correlation between Semiquantitative Myocardial Perfusion Score and Absolute Myocardial Blood Flow in $^{13}N-Ammonia$ PET)

  • 이병일;김계훈;김정영;김수진;이재성;민정준;송호천;범희승
    • Nuclear Medicine and Molecular Imaging
    • /
    • 제41권3호
    • /
    • pp.194-200
    • /
    • 2007
  • 목적: $^{13}N$-암모니아는 심근혈류 측정에 유용한 방사성의 약품으로 최근 국내에 도입된 PET/CT를 이용하여 비침습적으로 정량적인 검사를 시행 할 수 있다. 이 연구에서는 $^{13}N$-암모니아를 이용한 동적 영상으로부터 얻은 심근혈류정보와 정적 영상으로부터 얻은 심근관류정보의 상관관계를 살펴봄으로써 심장핵의학 검사의 유용성을 알아보고자 하였다. 방법: 심혈관질환이 의심되어 핵의학 심근관류 검사를 시행한 12명(남 11명, 여 1명, 평균나이 $57.9{\pm}8.6$세)을 대상으로 $^{13}N$-암모니아 검사를 시행하였다. 휴식기와 부하기에서 영상획득을 위하여 $^{13}N$ 암모니아 0.3 mCi/kg를 15초간 순간주사하면서 동시에 동적영상을 6분간(5초씩 12회, 10초씩 6회, 20초씩 3회, 30초씩 6회) 획득하고 이어서 게이트 영상을 13분간 각각 획득하였다. 심근혈류의 측정은 기저부 4분절, 중간부 4분절, 그리고 심첨부로 구성된 9분절 모델을 이용하였으며, 추출한 시간-방사능곡선과 추적자 모델을 사용하여 정량화 하였다. 심근관류는 정량화 분석 소프트웨어를 사용하여 구하였다. 20분절 모델을 9분절 모델과 비교하기 위하여 최기저부 6분절은 제외하고 인접분절의 값을 평균하여 사용하였다. 결과: 심근혈류량(휴식기, 0.18-2.38 ml/min/g; 부하기, 0.4-4.95 ml/min/g)과 심근섭취율(휴식기, 22-91%; 부하기, 14-90%) 간에는 약한 상관관계가 있었으며, 휴식기 보정된 심근관류와 혈류의 상관이 부하기에서보다 더 컸다(휴식기 r=0.59, 부하기 r=0.80). 수축기 심근두꺼워짐이 좋을수록 보정된 관상동맥 혈류예비능과 심근관류 예비능이 상관관계를 보였다. 결론: $^{13}N$-암모니아를 이용한 관류값을 특성에 따라 보정하고 해석하였을 때, 동적영상에서 절대값으로 구한 심근혈류와 좋은 상관관계를 보였다. 따라서 심근관류가 심근혈류를 잘 반영하는 지표임을 보였으므로 심장질환에서의 PET-CT 검사를 유용하게 활용할 수 있을 것으로 기대한다.

Myocardial Coverage and Radiation Dose in Dynamic Myocardial Perfusion Imaging Using Third-Generation Dual-Source CT

  • Masafumi Takafuji;Kakuya Kitagawa;Masaki Ishida;Yoshitaka Goto;Satoshi Nakamura;Naoki Nagasawa;Hajime Sakuma
    • Korean Journal of Radiology
    • /
    • 제21권1호
    • /
    • pp.58-67
    • /
    • 2020
  • Objective: Third-generation dual-source computed tomography (3rd-DSCT) allows dynamic myocardial CT perfusion imaging (dynamic CTP) with a 10.5-cm z-axis coverage. Although the increased radiation exposure associated with the 50% wider scan range compared to second-generation DSCT (2nd-DSCT) may be suppressed by using a tube voltage of 70 kV, it remains unclear whether image quality and the ability to quantify myocardial blood flow (MBF) can be maintained under these conditions. This study aimed to compare the image quality, estimated MBF, and radiation dose of dynamic CTP between 2ndDSCT and 3rd-DSCT and to evaluate whether a 10.5-cm coverage is suitable for dynamic CTP. Materials and Methods: We retrospectively analyzed 107 patients who underwent dynamic CTP using 2nd-DSCT at 80 kV (n = 54) or 3rd-DSCT at 70 kV (n = 53). Image quality, estimated MBF, radiation dose, and coverage of left ventricular (LV) myocardium were compared. Results: No significant differences were observed between 3rd-DSCT and 2nd-DSCT in contrast-to-noise ratio (37.4 ± 11.4 vs. 35.5 ± 11.2, p = 0.396). Effective radiation dose was lower with 3rd-DSCT (3.97 ± 0.92 mSv with a conversion factor of 0.017 mSv/mGy∙cm) compared to 2nd-DSCT (5.49 ± 1.36 mSv, p < 0.001). Incomplete coverage was more frequent with 2nd-DSCT than with 3rd-DSCT (1.9% [1/53] vs. 56% [30/54], p < 0.001). In propensity score-matched cohorts, MBF was comparable between 3rd-DSCT and 2nd-DSCT in non-ischemic (146.2 ± 26.5 vs. 157.5 ± 34.9 mL/min/100 g, p = 0.137) as well as ischemic myocardium (92.7 ± 21.1 vs. 90.9 ± 29.7 mL/min/100 g, p = 0.876). Conclusion: The radiation increase inherent to the widened z-axis coverage in 3rd-DSCT can be balanced by using a tube voltage of 70 kV without compromising image quality or MBF quantification. In dynamic CTP, a z-axis coverage of 10.5 cm is sufficient to achieve complete coverage of the LV myocardium in most patients.

액상확산접합한 Ni기 초내열합금의 등온응고거동에 미치는 모재결정입계의 영향 (The Effect of Base Metal Grain Boundary on Isothermal Solidification Phenomena during TLP Bonding of Ni Base Superalloys)

  • 김대업
    • Journal of Welding and Joining
    • /
    • 제19권3호
    • /
    • pp.325-333
    • /
    • 2001
  • The effect of base metal grain size on isothermal solidification behavior of Ni-base superalloy, CMSX-2 during transient liquid phase (TLP) bonding was investigated employing MBF-80 insert metal. TLP-bonding of single crystal. coarse-grained and fine-grained CMSX-2 was carried out at 1373∼1548k for various holding time in vacuum. The eutectic width diminished linearly with the square root of holding time during isothermal solidification process for single crystal, coarse-grained and fine-grained base metals. The completion time for isothermal solidification decreased in the order ; single crystal, coarse-grained and fine-grained base metals. The difference of isothermal solidification rates produced when bonding the different base metals could be explained quantitatively by the effect of base metal grain boundaries on the apparent average diffusion coefficient of boron in CMSX-2.

  • PDF

Ni기 초내열합금의 액상확산접합부 생성상의 금속조직학적 검토 (Metallurgical Study of Microconstituents in Transient Liquid Phase Bended Joints of Ni Base Superalloy)

  • 김대업
    • Journal of Welding and Joining
    • /
    • 제19권1호
    • /
    • pp.75-81
    • /
    • 2001
  • The metallurgical study of microconstituents in transient liquid phase bonded joints of Ni-base single crystal superalloys, CMSX-2 and CMSX-4 was investigated employing MBF-80 insert metal. TLP bonding of specimens was carried out at 1,373~1,523K for 0~19.6ks in vacuum. Three types of microconstituents ; needle-like constituent, dot-like constituent and abnormal shape constituent were formed in the bonded interlayer during TLP bonding operation. All these microconstituents were identified as boride. Microconstituents contain a large percentage of Cr in the early stage of bonding. As increasing the holding time, the amount of Cr was decreased and the amount of W, Co and Re were increased. From the analysis results of electron diffraction pattern by TEM, composition of elements in microconstituents were into MBlongrightarrowM$_{5}$B$_3$longrightarrowM$_2$B type with the increased in holding time. It can be explained by the fact that the relative amount of boron in microconstituents was decreased when the holding time was increased.d.

  • PDF

액상확산접합한 Ni기 단결정 초내열합금의 크리프 파단 및 피로특성 (Creep-Rupture and Fatigue Properties of Transient Liquid Phase Bonded Joints of Ni-Base Single Crystal Superalloy)

  • 김대업
    • Journal of Welding and Joining
    • /
    • 제19권1호
    • /
    • pp.82-87
    • /
    • 2001
  • The creep-rupture and low cycle fatigue properties of transient liquid phase bonded joints of Ni-base single crystal superalloy, CMSX-2 was investigated using MBF-80 insert metal. The (100) orientation of bonded specimen was aligned perpendicular to the joint interface. CMSX-2 was bonded at 1523K for 1.8ks in vacuum, optimum bonding condition. The creep rupture strength and rupture lives of the joints were the almost identical to ones of the base metal. SEM observation of the fracture surfaces of joints after creep rupture test revealed that the fracture surfaces classified three types of region, ductile fracture surface, cleavage fracture surface and interfacial fracture surface. The low cycle fatigue properties of the joints were also the same level as those of base metal. The elongation and reduction of area values of joints were comparable to those of base metal while fell down on creep rupture condition of high temperature.

  • PDF

고성능 단결정 초내열합금 CMSX-4의 액상확산접합현상 (Bonding Phenomena during Transient Liquid Phase Bonding of CMSX-4, High Performance Single Crystal Superalloy)

  • 김대업
    • Journal of Welding and Joining
    • /
    • 제19권4호
    • /
    • pp.423-428
    • /
    • 2001
  • The bonding phenomena of Ni base single crystal superalloy. CMSX-4 during transient liquid phase(TLP) bonding was investigated using MBF-80 insert metal. Bonding of CMSX-4 was carried out at 1,373∼1,548K for 0∼19.6ks in vacuum. The (001) orientation of each test specimen was aligned perpendicular to the bonding interface. The dissolution width of base metal was increased when the bonding temperature and holding time were increased. The eutectic width diminished linearly with the square root of holding time during isothermal solidification process. Borides were formed in the bonded layer during TLP bonding operation. The solid phase grew epitaxially into the liquid phase from substrates and single crystallization could be readily achieved during the isothermal solidification.

  • PDF

Computer-Aided Alloy Design of Insert Metal for Transient Liquid Phase Bonding of High Aluminum Ni-base Superalloys

  • Nishimotd, Kazutoshi;Saida, Kazuyoshi
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.803-808
    • /
    • 2002
  • A computer-aided alloy-designing technique to develop the insert metal for transient liquid phase (TLP) bonding was applied to high aluminum Ni-base superalloys. The main procedure of a mathematical programming method was to obtain the optimal chemical composition through rationally compromising the plural objective performances of insert metal by a grid-search which involved data estimation from the limited experimental data using interpolation method. The objective function Z which was introduced as an index of bonding performance of insert metal involved the melting point, hardness (strength), formability of brittle phases and void ratio (bonding defects) in bond layer as the evaluating factors. The contour maps of objective function Z were also obtained applying the interpolation method. The compositions of Ni-3.0%Cr-4.0%B-0.5%Ce (for ${\gamma}$/${\gamma}$/${\beta}$ type alloy) and Ni3.5%Cr-3.5%B-3%Ti (for ${\gamma}$/${\gamma}$ type alloy) which optimized the objective function were determined as insert metal. SEM observations revealed that the microstructure in bond layers using the newly developed insert metals indicated quite sound morphologies without forming microconstituents and voids. The creep rupture properties of both joints were much improved compared to a commercial insert metal of MBF-80 (Ni-15.5%Cr-3.7%B), and were fairly comparable to those of base metals.