• Title/Summary/Keyword: LiTaO$_3$

Search Result 153, Processing Time 0.017 seconds

Effect of Sintering Time on the Piezoelectric Properties of (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics ((Na,K,Li)(Nb,Sb,Ta)O3계 세라믹스의 소성시간이 압전특성에 미치는 영향)

  • Kim, Seung-Won;Yoo, Ju-Hyun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.30 no.4
    • /
    • pp.218-222
    • /
    • 2017
  • In this paper, in order to develop excellent composition ceramics for a piezoelectric energy- harvesting device, we synthesized $0.99(Na_{0.52}\;K_{0.443}\;Li_{0.037})(Nb_{0.883}\;Sb_{0.08}\;Ta_{0.037})O_3$ + $0.01(Sr_{0.95}Ca_{0.05})TiO_3$ + $0.3\;wt%\;Bi_2O_3\;+\;0.3\;wt%\;Fe_2O_3\;+\;0.3\;wt%\;CuO$ (abbreviated as NKN-SCT) ceramics with different sintering times, using the ordinary solid-state reaction method. The effect of sintering time on the microstructure and piezoelectric properties was investigated. The ceramics with the sintering time of 7 h have the optimum values of the piezoelectric constant ($d_{33}$), piezoelectric voltage constant ($g_{33}$), planar piezoelectric coupling coefficient (kp), mechanical quality factor (Qm), and dielectric constant (${\varepsilon}r$): $d_{33}=314[pC/N]$, $g_{33}=20.07[10^{-3}mV/N]$, kp = 0.442, Qm = 93, ${\varepsilon}r=1,768$, all being suitable for a piezoelectric energy-harvesting device.

Effect of Na2CO3 Addition on Piezoelectric Properties in (Na0.5K0.5)NbO3-LiTaO3 Ceramics (Na2CO3 첨가에 따른 (Na0.5K0.5)NbO3-LiTaO3 세라믹스의 압전 특성)

  • Kim, Mi-Soo;Oh, Seok;Lee, Dae-Su;Park, Eon-Cheol;Jeong, Soon-Jong;Song, Jae-Sung
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.11
    • /
    • pp.1025-1028
    • /
    • 2006
  • Dense $0.95(Na_{0.5}K_{0.5})NbO_3-0.05LiTaO_3$ (NKN-5LT) ceramics were developed by conventional sintering process. Sintering temperature was lowered by adding $Na_2CO_3$ as a sintering aid. The electrical properties of NKN-5LT ceramics were investigated as a function of $Na_2CO_3$ concentration. When the sample sintered at $1000^{\circ}C$ for 4 h with the addition of 1 mol% $Na_2CO_3$, electro-mechanical coupling factor $(k_p)$ and piezoelectric coefficient $(d_{33})$ of NKN-5LT ceramics were found to reach the highest values of 0.43 and 190 pC/N, respectively.

A Study on the CMP of Lithium Tantalate Wafer (Lithium Tantalate (LiTaO3) 웨이퍼의 CMP에 관한 연구)

  • Lee, Hyun-Seop;Park, Boum-Young;Seo, Heon-Deok;Chang, One-Moon;Jeong, Hae-Do
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.29 no.9 s.240
    • /
    • pp.1276-1281
    • /
    • 2005
  • Compound semiconductors are the semiconductors composed of more than two chemical elements. Lithium Tantalate$K_I$ wafer is used for several optical devices, especially surface acoustic wave(SAW) device. Because of the lithography in SAW device process, $LiTaO_3$ polishing is needed. In this paper, the commercial slurries $(NALC02371^{TM},\; ILD1300^{TM},\;ceria slurry)$ used for chemical mechanical polishing(CMP) were tested, and the most suitable slurry was selected by measuring material removal rate and average centerline roughness$(R_a)$. From these result, it was proven that $ILD1300^{TM}$ was the most suitable slurry for $LiTaO_3$ wafer CMP due to the chemical reaction between solution in slurry and material.

Dielectric and Piezoelectric Properties of Low Temperature Sintering (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics Doped with SnO2 (SnO2가 첨가된 저온소결 (Na,K,Li)(Nb,Sb,Ta)O3계 세라믹스의 유전 및 압전 특성)

  • Lee, Gwang-Min;Yoo, Ju-Hyun;Lee, Ji-Young
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.28 no.11
    • /
    • pp.690-693
    • /
    • 2015
  • In this paper, in order to develop excellent Pb-free composition ceramics for ultrasonic sensor. The $SnO_2$-doped ($Na_{0.525}K_{0.443}Li_{0.037})(Nb_{0.883}Sb_{0.08}Ta_{0.037})O_3$)(abbreviated as NKL-NST) ceramics have been synthesized using the ordinary solid state reaction method. The effect of $SnO_2$-doping on their dielectric and piezoelectric properties was investigated. The ceramics doped with 0 wt% $SnO_2$ have the optimum values of piezoelectric constant($d_{33}$), piezoelectric figure of merit($d_{33}.g_{33}$), planar piezoelectric coupling coefficient($k_p$) and density : $d_{33}=195[pC/N]$, $d_{33}.g_{33}=5.62pm^2/N.kp=0.40$, $density=4.436[g/cm^3]$. suitable for duplex ultrasonic sensor application.

Effect of Ta Substitution on the Dielectric and Piezoelectric Properties of (Li0.04(Na0.54K0.46)0.96(Nb0.96-xTaxSb0.04)O3Ceramics (Ta 치환이 (Li0.04(Na0.54K0.46)0.96(Nb0.96-xTaxSb0.04)O3 세라믹스의 유전 및 압전 특성에 미치는 영향)

  • Noh, Jung-Rae;Yoo, Ju-Hyun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.24 no.8
    • /
    • pp.627-631
    • /
    • 2011
  • [ $[Li_{0.04}(Na_{0.54}K_{0.46})_{0.96}](Nb_{1-0.04-X}TaxSb_{0.04})O_3$ ]lead-free piezoelectric ceramics have been prepared by normal sintering at $1,100^{\circ}C$ for 5 h. X-ray diffraction analysis indicated that specimens demonstrate orthorhombic symmetry when $Ta\leq5$ mol%. While transforming into tetragonal symmetry when $x\geq20$ mol%. These suggest that the orthorhombic and tetragonal phases co-exist in the ceramics with 5 mol% $cm^3$. As the result of SEM images, the grain growth was decreased with the increase of Ta substitution. The ceramics become 'softening', leading to improvements in $k_p$, $\varepsilon_r$ and $d_{33}$, but a decrease in $Q_m$. Excellent properties of $k_p$= 0.46, $d_{33}$= 293 pC/N, ${\varepsilon}_r$= 1,583 and Tc= $340^{\circ}C$ were obtained when Ta= 15 mol%.

Effect of Sintering Temperature on the Dielectric and Piezoelectric Properties of (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics (소성 온도가 (Na,K,Li)(Nb,Sb,Ta)O3 세라믹스의 유전 및 압전 특성에 미치는 영향)

  • Kim, You-Seok;Yoo, Ju-Hyun;Hong, Jae-Il;Lee, Jie-Young
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.26 no.11
    • /
    • pp.806-809
    • /
    • 2013
  • In this study, $(Na_{0.525}K_{0.443}Li_{0.037})(Nb_{0.883}Sb_{0.08}Ta_{0.037})O_3+0.10\;wt%Bi_2O_3+0.35\;wt%B_2O_3$ ceramics were prepared by conventional soild-state sintering process. The specimens were sintered at temperature range from $1,060^{\circ}C$ to $1,100^{\circ}C$. XRD (X-ray diffractron), SEM (scanning electron microscope) were used to analyze the crystal structure and microstructural sproperties of specimens. And also, $T_{O-T}$, TC were observed by the mesurement of temperature dependence of dielectric constant. Excellect physical properties of the piezoelectric constant $d_{33}$= 170 pC/N, electromechanical coupling factor kp= 0.312, Tc= $315^{\circ}C$ were obtained, respectively, from the specimen sintered at $1,080^{\circ}C$.

Dielectric and Piezoelectric Properties of (Na,K,Li)(Nb,Ta,Sb)O3 Ceramics Manufactured Using Columbite Methods with Calcination Temperature (Columbite법으로 제조된 (Na,K,Li)(Nb,Ta,Sb)O3 세라믹스의 하소온도에 따른 유전 및 압전 특성)

  • Ra, Cheol-Min;Yoo, Ju-Hyun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.29 no.3
    • /
    • pp.159-163
    • /
    • 2016
  • In this paper, in order to develop optimum composition ceramics with excellent piezoelectric properties, $(Na_{0.525}K_{0.443}Li_{0.037})(Nb_{0.823}Sb_{0.08}Ta_{0.037})O_3+0.3wt%Bi_2O_3+0.4wt%Fe_2O_3$ lead-free piezoelectric ceramics were synthesized by conventional soild-state method. The calcination temperature of columbite precursors were fabricated at temperature range from $950^{\circ}C$ to $1,150^{\circ}C$ and sintering aids with low melting point were added to densify these ceramics. Effect of calcination temperature on dielectric and piezoelectric properties of ceramics were investigated. the ceramics with B-site columbite precursors at temperature of $1,100^{\circ}C$ obtained the optimal values of $d_{33}=272$ [pC/N], $k_p=0.51$, $Q_m=102$, ${\varepsilon}_r=978$.

X-Ray Fluorescence Analysis of $Ta_2O_5, Nb_2O_5, TiO_2, SnO_2$ and $Zr_O2$ in Tin-Slags (주석-슬랙 중 $Ta_2O_5, Nb_2O_5, TiO_2, SnO_2$, 및 $ZrO_2$의 X-선 형광분석)

  • Young-Sang Kim;Chong Wook Lee
    • Journal of the Korean Chemical Society
    • /
    • v.27 no.4
    • /
    • pp.273-278
    • /
    • 1983
  • With the synthetic standards, valuable metals $(Ta_2O_5, Nb_2O_5, TiO_2, SnO_2$, and $ZrO_2$) in the tin slags have been determined by the x-ray fluorescence spectrometry. The powder sample and the standards are homogeneously mixed with anhydrous $Li_2B_4O_7$ and La_2O_3$ in weight ratio of 15 : 42 : 3 respectively. The mixed material is fused at $1,150^{\circ}C$ for 30 minutes to be changed into the glass bead. The bead is ground to (-) 325 mesh size and pelletized. The analytical results obtained in this work are consistent with the data obtained by other common methods within allowable error range. The standard deviation for $Ta_2O_5$ in PTS-H sample is 0.12 % at level of 3.40 % content.

  • PDF

Crystal chemistry and growth of$La_3Ga_5SiO_{14}$ for the applications of filter and resonator (필터와 레죠네이터 응용을 위한 $La_3Ga_5SiO_{14}$ 의 결정화학 및 성장)

  • Jung, Il-Hyoung;Joo, Kyung;Shim, Kwang-Bo;Auh, Keun-Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.9 no.1
    • /
    • pp.74-79
    • /
    • 1999
  • Langasite($La_3Ga_5SiO_14$) is a new piezoelectric material which is similar to quartz, LN($LiNbO_3$) and LT($LiTaO_3$) in its acoustic behavior. In this study, pure Langasite and Lagnasite family groups were synthesized by the solid state reactions in air. The diffusion species for synthesis were investigated and the sintered body was studied on dielectric property to comparison of characteristics. Also, Langasite single crystals were grown by self-designed Czochralski system and characterized.

  • PDF