Kim, Sang-Sup;Lee, Sun-Jea;Park, Yong-Jun;Lee, Myung-Hoo;Han, Min-Cheol;Han, Cheon-Goo
Proceedings of the Korean Institute of Building Construction Conference
/
2015.11a
/
pp.120-121
/
2015
In this research, to evaluate the influence of using non-KS aggregate on concrete performance, the engineering properties of normal strength concrete were assessed depending on the KS aggregate and non-KS aggregate from various sources in mid-Korea. From the experiment, when the non-KS aggregate was used, low compressive strength was achieved with increased water-to-cement ratio caused by increased unit water due to high absorption rate of the non-KS aggregate.
Journal of the Korea Institute of Building Construction
/
v.17
no.6
/
pp.499-506
/
2017
This study is to present empirical data about the needs for quality security of aggregate by randomly selecting aggregate from 4 major locations including A, B, C, D province in Korea, by investigating its quality status in terms of physical properties and particle distribution based on Korean industrial standards(KS). The test results indicated that wide variance in quality, and some of aggregate samples were far below the standard, still many of them are not satisfying KS standards. In addition, the current aggregate manufacturing process that does not include inspection of particle size distribution by sieving and fineness modulus, can induce a possibility of non-KS aggregate's distribution; this provide that the current status of aggregate quality security of Korea is seriously threatened. Thus, it is important to secure each aggregate's quality level under KS standards.
Journal of the Korean Recycled Construction Resources Institute
/
v.4
no.2
/
pp.125-135
/
2016
The objective of this paper is to provide integrated Korea industrial standards(KS) for concrete aggregates, which has been separately provided with ten kinds of KS, in order to improve the way of quality management of concrete aggregate and to prevent distribution of unsuitable aggregates. For the sequences of the paper, typical foreign standards related to concrete aggregates including ASTM for US, EN for EU, JIS for Japan are reviewed and compared to provide necessities and feasibilities of the paper. Based on the analysis above results, existing KS for concrete aggregates, which have been separately provided with ten kinds being lack of correlation between each KS is integrated to KS F 2526 "Aggregates for concrete" in this paper. By doing this, in terms of terminology, the expression of the aggregate, which has been currently classified into specified terminologies of aggregates depending on sources, manufacturing methods of each aggregates, is able to be integrated to single expression of the aggregate for concrete. It is believed that integrated KS presented herein provides more desirable way in terms of its better accessibility, easier revision and closer connection between each aggregate kinds.
Jo, Man-Ki;Song, Yuan-Lou;Park, Young-Jun;Lee, Hong-Kyu;Han, Min-Cheol;Han, Cheon-Goo
Proceedings of the Korean Institute of Building Construction Conference
/
2015.11a
/
pp.145-146
/
2015
When using non KS aggregate muck pile in general, compared to when using KS aggregate, when obtaining an identical slump a high unit quantity of water was confirmed, and when designing the concrete mix the compressive strength of concrete decreased due to an increase in W/B. Therefore because the use of non KS aggregate decreases the liquidity, strength and durability etc. qualities of concrete from an overall performance point of view, there is a need for the used of KS aggregate and when using aggregate that does not adhere to KS standards, it is determined there is a need for appropriate concrete mix design and care.
Proceedings of the Korea Concrete Institute Conference
/
2008.04a
/
pp.465-468
/
2008
This study investigated the best condition when mixed sand with a river and crushed sand was used though the experiment for the properties of the concrete corresponding to the control of fine aggregate ratio to apply the mixed sand and properties of the fine aggregate at the ready-mixed concrete factory on Yeongnam and Honam. The physical properties of Yeongnam and Honam is satisfied with KS F 2526 and KS F 2527 except fineness modulus and passing amount of 8mm sieve. And, the mixed sand above two types which were incongruent to use individually was being used at each factory, and it was managed in accordance with KS. The flowabillity of the mixture proportion of concrete which was estimated by method of unit volume weight according to the fine aggregate ratio at each factory on Yeongnam and Honam was higher than existing mixture proportion. It was analyzed that the residual water due to decline of the surface area caused by reducing fine aggregate ratio was increased relatively. Accordingly, it was considered that the effect on the economic mixture proportion and improvement of durability might be possible.
Proceedings of the Korean Institute of Building Construction Conference
/
2016.05a
/
pp.181-182
/
2016
We developed eco-friendly lightweight concrete in order to apply eco-friendly lightweight concrete into structural wall or slab of shallow depth urban railway system. However, since lightweight aggregate has different structural feature of porous and it has been overvalued at current KS standard when applied, we did compare the characteristics of freezing and thawing of normal weight aggregate concrete by comparative test method(KS, ASTM). According to test method, there was a big difference of dynamic elastic modulus in lightweight concrete rather than in normal weight aggregate concrete. The big absorption factor in lightweight aggregate is main reason for that. For more detail, in KS law in which only 14 days water curing is carried out, the big amount of moisture in lightweight aggregate is frozen and high heaving pressure occurs and finally that lead to destruction of lightweight concrete. Therefore, it is considered that in case of lightweight concrete, resistibility against freezing and thawing has been undervalued in domestic KS law compared to ASTM law, which is overseas standard. So, a variety of examination about testing criteria and rule would be necessary for exact assessment of lightweight concrete.
Chemical experiment KS F 2545 and Physical experiment ASTM C 1260 has been accomplished to estimate the potential of alkali aggregate. Used for testing aggregate samples are forest aggregate and recycled aggregate which collected in Gangwon province Samcheok and Pyeongchang, Jeollabuk province Gimje and Kochang, and Gyeongsangnam province Goryeong. As the results of chemical experiment confirmed that if silicate rock and carbonate rock are mixed, reduction in alkalinity is increase. So it has been identified that case makes a disturb at the result of alkali aggregate reaction. In 9 out of the 62 aggregate samples check dissolved silica exceeding 100 mmol/ℓ. and mortar bar length increase rate confirmed that 5 of 9 chemical method aggregates were 0.1~0.2% and 2 aggregates were 0.2%. As a result of the alkaline aggregate reaction test using the chemical method and the mortar bar method, the aggregates showing alkali aggregate reaction are sandstone and tuff aggregates. Therefore, Alkali aggregate reaction tests are required to use clastic sedimentary rocks and volcanic pyroclastic rocks aggregates.
Kim, Se-Hwan;Kim, Sang-Heon;Lee, Soo-Hyung;Jeon, Hyun-Kyu;Seo, Chee-Ho
Journal of the Korea Institute of Building Construction
/
v.13
no.3
/
pp.202-208
/
2013
The method used to test lightweight aggregate concrete for its resistance to freezing and thawing is different in each country. In Korea, the method of KS F 2456 on normal concrete is adopted for lightweight aggregate concrete, while the testing method of ASTM C 330 lightweight aggregates for structural concrete is used in the majority of overseas countries. In this study, we identified differences between KS F 2456 and ASTM C 330 in terms of the testing method for freezing and thawing resistance, and we studied the influence of this on the freezing and thawing resistance of lightweight aggregate concrete. The results of this study were as follows: Blocked lightweight aggregates had a slight collapse of shape and lost weight by repeated freezing and thawing, but unblocked lightweight aggregates were badly collapsed. And while the freezing and thawing resistance tests of normal concrete showed similar results despite the difference in the KS and ASTM testing method, the results for lightweight aggregate concrete were very different. So the KS test method shows evaluation results that are much lower than the ASTM test method.
Journal of the Korean Recycled Construction Resources Institute
/
v.7
no.2
/
pp.101-108
/
2019
This study is analysis of the utilization as a concrete fine aggregate on CGS, a by-product of Integrated coal gasification combined cycle(IGCC). That is, in KS F 2527 "Concrete aggregate," properties of 1~12times to CGS were evaluated, focusing on quality items corresponding to natural aggregate sand(NS) and melted slag aggregate sand(MS). As a result, the distribution of grain shape, safety and expansion were all satisfied with KS standards by physical properties, but the quality was unstable at 7~12times of water absorption ratio and absolute dry density. The particle size distribution was unstable due to asymmetry distribution of coarse particles, and particles were too thick for 7~12times. The passing ratio of 0.08mm sieve was also out of the KS standard at part factor of 7~12times, but chloride content, clay contents, coal and lignite were all satisfactory. Meanwhile, chemical composition was satisfactory except for $SO_3$ in 1~6times, and content and amount of harmful substances were all within the specified value except for F in 7~12times. As a result of SEM analysis, the surface quality and porosity were 7~12times more than 1~6times, and it was the quality was degraded. Therefore, it is necessary to reduce the quality deviation by using separate measures in order to utilize it as concrete aggregate in the future, and if it is premixed with fine quality aggregate, it will contribute positively to solve aggregate supply shortage and utilize circulation resources.
Proceedings of the Korea Concrete Institute Conference
/
2004.05a
/
pp.368-371
/
2004
It analyzes the quality of the fine aggregate which is reproduced through a dry production process with cyclone and a wet production process. The conclusions of the study are as follows. 1. The recycled fine aggregate through the dry production process with cyclone shows the low rate of absorption and impurity content after the cyclone process. It shows that its density is 2.37, absorption rate is 4.8 and stability is $5.1\%$ and less. Therefore, it satisfies the standards of KS F 2573(recycled aggregate for concrete) as the first grade. 2. The recycled fine aggregate through the wet production process shows the low rate of absorption and foreign substance content after the process of wash and dehydration. It shows that its density is 2.40, absorption rate is 3.12 and stability is $3.2\%$ and less. Therefore, it satisfies the standards of KS F 2573(recycled aggregate for concrete) as the first grade.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.