A simulation study of a current-mode direct current (DC)-DC boost converter is presented in this paper. This converter, with a fully-integrated power module, is implemented by using bipolar complementary metal-oxide semiconductor (BiCMOS) technology. The current-sensing circuit has an op-amp to achieve high accuracy. With the sense metal-oxide semiconductor field-effect transistor (MOSFET) in the current sensor, the sensed inductor current with the internal ramp signal can be used for feedback control. In addition, BiCMOS technology is applied to the converter, for accurate current sensing and low power consumption. The DC-DC converter is designed with a standard 0.35 ${\mu}m$ BiCMOS process. The off-chip inductor-capacitor (LC) filter is operated with an inductance of 1 mH and a capacitance of 12.5 nF. Simulation results show the high performance of the current-sensing circuit and the validity of the BiCMOS converter. The output voltage is found to be 4.1 V with a ripple ratio of 1.5% at the duty ratio of 0.3. The sensing current is measured to be within 1 mA and follows to fit the order of the aspect ratio, between sensing and power FET.
Journal of the Microelectronics and Packaging Society
/
v.18
no.4
/
pp.33-38
/
2011
The p-type $(Bi_{0.2}Sb_{0.8})_2Te_3$ powers were fabricated by mechanical alloying and hot-pressed at temperatures of $350{\sim}550^{\circ}C$. Themoelectric properties of the hot-pressed $(Bi_{0.2}Sb_{0.8})_2Te_3$ were characterized as a function of the hot-pressing temperature. With increasing the hot-pressing temperature from $350^{\circ}C$ to $550^{\circ}C$, the Seebeck coefficient and the electrical resistivity decreased from 237 ${\mu}V/K$ to 210 ${\mu}V/K$ and 2.25 $m{\Omega}-cm$ to 1.34 $m{\Omega}-cm$, respectively. The power factor of the hot-pressed $(Bi_{0.2}Sb_{0.8})_2Te_3$ became larger from $24.95{\times}10^{-4}W/m-K^2$ to $32.85{\times}10^{-4}W/m-K^2$ with increasing the hot-pressing temperature from $350^{\circ}C$ to $550^{\circ}C$. Among the specimens hot-pressed at $350{\sim}550^{\circ}C$, the $(Bi_{0.2}Sb_{0.8})_2Te_3$ hot-pressed at $500^{\circ}C$ exhibited the maximum dimensionless figure-of-merit of 1.09 at $25^{\circ}C$ and 1.2 at $75^{\circ}C$.
Kim, Jongho;Jun, DongSan;Jeong, Seyoon;Cho, Sukhee;Choi, Jin Soo;Kim, Jinwoong;Ahn, Chieteuk
ETRI Journal
/
v.34
no.5
/
pp.753-758
/
2012
As the next-generation video coding standard, High Efficiency Video Coding (HEVC) has adopted advanced coding tools despite the increase in computational complexity. In this paper, we propose a selective bi-prediction method to reduce the encoding complexity of HEVC. The proposed method evaluates the statistical property of the sum of absolute differences in the motion estimation process and determines whether bi-prediction is performed. A performance comparison of the complexity reduction is provided to show the effectiveness of the proposed method compared to the HEVC test model version 4.0. On average, 50% of the bi-prediction time can be reduced by the proposed method, while maintaining a negligible bit increment and a minimal loss of image quality.
This article aims at presenting multi objective optimization of parameters that affect crashworthiness characteristics of bi-tubular structures using Taguchi method with grey relational analysis. To design the experiments, the $L_9$ orthogonal array has been used and based on that, the inner tubes have been fabricated by varying the three influence factors such as reference diameter, length difference and numbers of sides of the polygon with three levels, but all the outer cylinders have the same diameter and length 90 mm and 135 mm respectively. Then, the tailor made bi-tubular steel structures were subjected into quasi static axial compression. From the test results it is found that the crushing behaviors of bi-tubular structures with different combinations were fairly significant. The important responses (crashworthiness indicators) specific energy absorption and crush force efficiency have been evaluated from load - displacement curve. Finally optimal levels of parameters were identified using grey relational analysis, and significance of parameters was determined by analysis of variance. The optimum crashworthiness parameters are reference diameter 80 mm, length difference 0 mm and number of sides of polygon is 3, i.e., triangle within the selected nine bi-tube combinations.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.28
no.9
/
pp.577-580
/
2015
In this paper, in order to develop the composition ceramics with the outstanding piezoelectric properties, $Pb(Mg_{1/2}W_{1/2})_{0.03}(Ni_{1/3}Nb_{2/3})_{0.09}(Zr_{0.5}Ti_{0.5})_{0.88}O_3$ ceramics substituted with $BiFeO_3$ were prepared by the conventional solid-state reaction method. The addition of small amount of $Li_2CO_3$ and $CaCO_3$ as sintering aids decreased the sintering temperature of the ceramics. The effects of $BiFeO_3$ substitution on their piezoelectric and dielectric properties were investigated. when 0.015 mol $BiFeO_3$ was substituted, the optimal physical properties of $d_{33}=590pC/N$, $E_c=8.78kV/mm$ were obtained.
Homogeneous and fine powders for Bi-2223 tape were prepared by ultrasonic spray pyrolysis (SP) method from an aqueous solution of metal nitrates. Bi-2223 precursor powders were synthesized with various solutes concentration and pyrolysis temperature. The synthesized precursor powders had a narrow particle size distribution and an average particle size was $\~{\cal}um$. The reactivity of precursor powder by SP method is very high, attributed to the fine and narrow particle size distribution. Bi-2223/Ag tape was prepared using PIT method and followed by various sintering conditions. The precursor powder by SP method promoted a very quick formation of the Bi-2223 phase for short sintering time while the secondary phase such as large AEC phase and $Ca_2PbO_4$ were minimized for SP tapes.
Steady-state sublimation vapour pressures of anhydrous bismuth trichloride have been measured by the continuous gravimetric Knudsen effusion method from 370.6 to 488.8 K. Additional effusion measurements have also been made from 438.2 to 495.7 K by the torsion effusion method. Based on a correlation of ${\Delta}_H0298$.15 and ${\Delta}_H0298$.15, a recommended p(T) equation has been obtained for BiCl3(s); log(p/Pa)=-C/(T/K)-2.838log(T/K)-8.097${\times}$10-2(K/T)2+22.588, where p is in Pa, T in Kelvin and ${\Delta}_H0298$.15 in kJmo1-1 and C=(${\Delta}_H0298$.15+5.9988)/1.9146${\times}$10-2. Condensation coefficients and their temperature dependence have been derived from the effusion measurements.
Proceedings of the Korean Vacuum Society Conference
/
2011.08a
/
pp.183-183
/
2011
Multiferroic materials have been widely studied in recent years, because of their abundant physics and potential applications in the sensors, data storage, and spintronics. $BiFeO_3$ is one of the well-known single-phase multiferroic materials with $ABO_3$ structure and G-type antiferromagnetic behavior below the Neel temperature $T_N$ ~ 643 K, but the ferroelectric behavior below the Curie temperature $T_c$~1,103 K. In this study, the $BiFe_{1-x}Ni_xO_3$ (x=0 and 0.05) bulk ceramics were prepared by solid-state reaction and rapid sintering with high-purity $Bi_2O_32$, $Fe_3O_4$ and NiO powders. The powders of stoichiometric proportions were mixed, as in the previous investigations, and calcined at 450$^{\circ}C$ for $BiFe_{1-x}Ni_xO_3$ for 24 h. The obtained powders were grinded, and pressed into 5-mm-thick disks of 1/2-inch diameter. The disks were directly put into the oven, which has been heated up to 800$^{\circ}C$ and sintered in air for 20 min. The sintered disks were taken out from the oven and cooled to room temperature within several min. The phase of samples was checked at room temperature by powder x-ray diffraction using a Rigaku Miniflex diffractometer with Cu K${\alpha}$ radiation. The Raman measurements were carried out by employing a hand-made Raman spectrometer with 514.5-nm-excitation $Ar^+$ laser source under air ambient condition on a focused area of 1-${\mu}m$ diameter. The field-dependent magnetization measurements were performed with a superconducting quantum-interference-device magnetometer.
Park, Jung Soo;Lee, Ku Tak;Cho, Jeong Ho;Jeong, Young Hun;Paik, Jong Hoo;Yun, Ji Sun
Journal of the Korean Ceramic Society
/
v.51
no.6
/
pp.527-532
/
2014
$0.97Bi_{0.5+x}(Na_{0.78}K_{0.22})_{0.5-3x}TiO_3-0.03LaFeO_3$ lead-free piezoelectric ceramics were fabricated by a solid state reaction method. $LaFeO_3$ additives were added to $Bi_{0.5}(Na_{0.78}K_{0.22})_{0.5}TiO_3$ for volatile compensation of bismuth and sodium ions in the sintering process. To create A-site vacancies, the mole ratio and charge valence of A-site ions ($Bi^{3+}$, $Na^+$ and $K^+$) were controlled. The improved piezoelectric properties were observed by addition of $LaFeO_3$ and control of A-site vacancies. In particular, a $d_{33}^*(S_{max}/E_{max})$ value of 614pm/V and an electric field induced strain of 0.33% was observed in $0.97Bi_{0.505}(Na_{0.78}K_{0.22})_{0.485}TiO_3-0.03LaFeO_3$ ceramic.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.11
no.2
/
pp.111-120
/
1998
In this paper, the $(SrPb)(CaMg)TiO_3$ ceramics with paraelectric properties were fabricated by the mixed oxide method. It was investigated that which the variation of contents of $Bi_2O_3{\cdot}3TiO_2$ effects on structural, dielectrical and electrical properties of specimens. As a result, the grain size were grown with increasing the contents of $Bi_2O_3{\cdot}3TiO_2$. The relative dielectric constants were increased up to 4[mol%] of $Bi_2O_3{\cdot}3TiO_2$, and decreased more or less at a low temperature in the specimens which had more than. But the temperature coefficient. of capacitance were showed ${\pm}25$[%]. The dielectric loss were less than 0.05 in all specimens which had more than 4[mol%] of $Bi_2O_3{\cdot}3TiO_2$. In order to investigate the behavior of charged particles, the characteristics of electrical conduction were measured. As a result, the conduction current was divided into the three steps as a function of DC electric field. The first step was Ohmic region due to ionic conduction, below 15[kV/cm]. The second step was showed a saturation which seems to be related to a depolarizing field occuring in field-enforced ferroelectric phase, between 15[kV/cm] and 40[kV/cm]. The third step was attributed to Child's law related to space charge which injected from electrode, above 40[kV/cm].
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.