Interfacial Reaction Characteristics of a Bi-20Sb-10Cu-0.3Ni Pb-free Solder Alloy on Cu Pad (Bi-10Cu-20Sb-0.3Ni 고온용 무연 솔더와 Cu와의 계면 반응 특성)

  • Kim, Ju-Hyung;Hyun, Chang-Yong;Lee, Jong-Hyun
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.17 no.1
    • /
    • pp.1-7
    • /
    • 2010
  • Interfacial reaction characteristics of a Bi-10Cu-20Sb-0.3Ni Pb-free alloy on Cu pad was investigated by reflow soldering at $430^{\circ}C$. The thickness of interfacial reaction layers with respect to the soldering time was also measured. After the reflow soldering, it was observed that a $(Cu,Ni)_2Sb$, a $Cu_4Sb$ intermetallic layer, and a haze layer, which is consisted of Bi and $Cu_4Sb$ phases, were successively formed at the Bi-10Cu-20Sb-0.3Ni/Cu interface. The total thickness of the reaction layers was found to be linearly increased with increasing of the reflow soldering time up to 120 s. As the added Ni element did not participate in the formation of the thickest $Cu_4Sb$ interfacial layer, suppression of the interfacial growth was not observed.

Characterisitics of the over current of Bi-2223 HTS tape (Bi-2223 고온초전도선의 과전류 통전특성)

  • Kim, Jae-Ho;Sim, Ki-Deok;Cho, Jeon-Wook;Kim, Hae-Jun;Kwag, Dong-Soon;Seong, Ki-Chul;Kim, Hae-Jong
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.284-285
    • /
    • 2005
  • Bi-2223 High-Temperature Superconducting(HTS) tape is one of the most widely used HTS tape for power application. Characteristics of the over current of HTS tape with different sheath are described. This paper presents the basic properties such as temperature and resistivity rise of the Bi-2223 HTS tape which is exposed to the over current. It is expected that results from this study can be utilized as basic data in designing superconducting power devices.

  • PDF

Thermoelectric Properties of N-type 90% $Bi_2Te_3$+10% $Bi_2Se_3$ Thermoelectric Materials Produced by Melt spinning method and Sintering (Melt spinning법에 의한 n형 90% $Bi_2Te_3$+10% $Bi_2Se_3$ 열전소결체의 열전특성)

  • 김익수
    • Journal of Powder Materials
    • /
    • v.5 no.1
    • /
    • pp.50-56
    • /
    • 1998
  • A new process using rapid solidification (melt spinning method) followed by pressing and sintering was investigated to produce the n-type thermoelectric ribbons of 90% $Bi_2Te_3$+10% $Bi_2Se_3$ doped with $CdCl_2$. Quenched ribbons are very brittle and consisted of homogeneous $Bi_2Te_3-Bi_2Se_3$ pseudo-binary solid solutions. Property variations of the materials was investigated as a function of variables, such as dopant $CdCl_2$ quantity and sintering temperature. When the process parameters were optimized, the maximum figure of merit was $2.146{\times}10^{-3}K^{-1}$.

  • PDF

Distribution Behavior of Bi and Pb Between Molten PbO-SiO2 Slag and Bi (용융(熔融) PbO-SiO2계(系) 슬래그와 Bi 사이의 Bi와 Pb의 분배거동(分配擧動))

  • Kim, Se-Jong;Kim, Eung-Jin;Sohn, Ho-Sang
    • Resources Recycling
    • /
    • v.21 no.5
    • /
    • pp.65-71
    • /
    • 2012
  • The equilibrium distribution of bismuth and lead between molten PbO-$SiO_2$ slag and bismuth phase was studied in the temperature range of $775^{\circ}C$ to $850^{\circ}C$ in a MgO crucible. The oxygen partial pressure of atmosphere was controlled by $P_{CO2}/P_{CO}$ ratio. The value of $(%PbO)_{slag}/[%Pb]_{metal}$ increased with increasing $SiO_2$ content of slag, and the value of $(%Bi_2O_3)_{slag}/[%Bi]_{metal}$ decreased with increasing $SiO_2$ content of slag. The concentration of Pb in metal increased with increasing temperature. These experimental results agreed well with the thermodynamic prediction.

The mechanism of Bi$_{0.5}Pb_3Sr_2Ca_2CuO_{\delta}$ and (Ca,Sr)$_2$(BiPb)O$_4$ phase as a flux-pinning center in (Bi,Pb)$_2Sr_2Ca_2CuO_{10}$ superconductor ((Bi,Pb)$_2Sr_2Ca_2CuO_{10}$ 초전도체에l서 flux-pinning center로서 Bi$_{0.5}Pb_3Sr_2Ca_2CuO_{\delta}$ 및 (Ca,Sr)$_2$(BiPb)O$_4$ 상의도입 기구)

  • Chung, Jun-Ki;Kim, Cheol-Jin;Lee, Sang-Hee;Yoo, Jae-Moo;Kim, Hae-Doo;Koh, Jae-Woong
    • 한국초전도학회:학술대회논문집
    • /
    • v.9
    • /
    • pp.300-304
    • /
    • 1999
  • To tap the feasibility of exploiting the 2$^{nd}$ phases as flux-pinning centers in the (Bi,Pb)$_2Sr_2Ca_2CuO_{10}$ superconductor, the size and the distribution of the precipitates have been controlled by changing reaction temperature and time, oxygen partial pressure Po$_2$ and annealing condition. Various annealing heat treatments were also conducted on the as-received 61 filament Bi-2223 tapes with Bi$_{1.8}Pb_{0.4}Sr_2Ca_{2.2}Cu_3O_8$ starting composition and annealed specimen were analyzed with XRD, SEM, EDS and TEM.. The grain size of (Ca,Sr)$_2$(BiPb)O$_4$ or Bi$_{0.5}Pb_3Sr_2Ca_2CuO_{\delta}$ was controllable by optimizing the heat treatment condition and critical current density (J$_c$) showed dependence on the size of the 2$^{nd}$ phases.

  • PDF

Properties and Structures of Bi2O3-B2O3-ZnO Glasses for Application in Plasma Display Panels Rib (PDP Rib용 Bi2O3-B2O3-ZnO계 유리의 물성과 구조)

  • Jin, Young-Hun;Jeon, Young-Wook;Lee, Byung-Chul;Ryu, Bong-Ki
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.2
    • /
    • pp.184-189
    • /
    • 2002
  • This study, compared with data of PbO-base glass system is a part of new glass composition design with Bi-base composition for PDP Rib. As $Bi_2O_3-B_2O_3-ZnO$ glass composition including Bi, which have similar density value and work facility to PbO, properties of softening point, thermal expansion coefficient, chemical durability, dielectric constant, and structural changing by XPS were investigated. $Bi_2O_3-B_2O_3-ZnO$ glass system, added 50∼80 wt% $Bi_2O_3$ widely, were presented 400∼480$^{\circ}C$ softening temperature, $68{\sim}72{\times}10^{-7}/^{\circ}C$ thermal expansion coefficient and 13∼25 dielectric constant. These results were showed similar physical properties with Pb-base glass system of same composition content, application possibility as starting composition of rib material was identified through micro-control of components and physical properties. The bonding energy of $O_{1s}$ as the $Bi_2O_3$ content decreasing was increased and full width at half-maximum (FWHM) was decreased, which is caused by non-bridging oxygen increasing.

Ferroelectric and Magnetic Properties of BiFeO3 Thin Films Deposited on SrTiO3 Substrate (SrTiO3기판 위에 증착한 BiFeO3박막의 강유전 및 자기적 특성)

  • Lee, Eun-Gu;Kim, Sun-Jae;Lee, Jae-Gab
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.6
    • /
    • pp.358-362
    • /
    • 2008
  • $BiFeO_3$ films were hetero-epitaxially grown on $SrTiO_3$ substrate with a various orientation by pulse laser deposition. $BiFeO_3$ films grown on (111) $SrTiO_3$ substrate have a rhombohedral structure, identical to that of single crystals. On the other hand, films grown on (110) or (001) $SrTiO_3$ substrate are monoclinically distorted from the rhombohedral structure due to the epitaxial constraint. The easy axis of spontaneous polarization is close to [111] for the variously oriented films. Dramatically enhanced polarization and magnetization have been found for $BiFeO_3$ thin films grown on $SrTiO_3$ substrate comparing to that of $BiFeO_3$ crystals. The results are explained in terms of an epitaxially-induced transition between cycloidal and homogeneous spin states, via magneto-electric interactions.

Microstructures and Magnetic Properties of Multiferroic BiFeO3 Thin Films Deposited by RF Magnetron Sputtering Method (RF 마그네트론 스퍼터링법으로 증착된 Multiferroic BiFeO3 박막의 미세구조 및 자기적 특성)

  • Song, Jong-Han;Nam, Joong-Hee;Kang, Dae-Sik;Cho, Jung-Ho;Kim, Byung-Ik;Choi, Duck-Kyun;Chun, Myoung-Pyo
    • Journal of the Korean Magnetics Society
    • /
    • v.20 no.6
    • /
    • pp.222-227
    • /
    • 2010
  • $BiFeO_3$ (BFO) thin films were deposited on Pt/Ti/$SiO_2$/Si(100) substrates by RF magnetron sputtering method at room temperature. The influence of the flow rate of $O_2$ gas on the preparation of $BiFeO_3$ thin films was studied. XRD results indicate that the $BiFeO_3$ thin films were crystallized to the perovskite structure with the presence of small amount of impurity phases. The flow rate of $O_2$ gas has great affect on the microstructures and magnetic properties of $BiFeO_3$ thin films. As flow rate of $O_2$ gas increased, roughness and grain size of the thin films increased. $BiFeO_3$ thin films exhibited weak ferromagnetic behavior at room temperature. The PFM images revealed correlation between the surface morphology and the piezoresponse, indicating that the piezoelectric coefficient is related to microstructure.

Synthesis and M$\ddot{o}$ssabuer Spectroscopy Studies of $Nd_{1-x}Bi_xY_2Fe_5O_{12}$ Nano-Particles

  • Uhm, Young Rang;Lee, Jae-Gwang;Kim, Chul Sung
    • Journal of Magnetics
    • /
    • v.5 no.1
    • /
    • pp.16-18
    • /
    • 2000
  • The garnets $Nd_{1-x}Bi_xY_2Fe_5O_{12}$ ($\chi$=0.0, 0.25, 0.5, 0.75 and 1.0) have been studied by x-rays, electron microscopy, ferromagnetic resonance, vibrating sample magnetometer and Mossbauer spectroscopy, Ultra-fine polycrystalline cubic samples have been prepared by a melt-salt routed sol-gel method. The Mossbauer spectra consist of two sets of six-line patterns corresponding to $Fe^{3+}$ at the tetrahedral 24(d) and octahedral 16(a) sites. Magnetic hyperfine fields of $Nd_{0.5}Bi_{0.5}Y_2Fe_5O_{12}$ at 12 K are found to be 548 kOe (octahedral site) and 475 kOe (tetrahedral site), respectively, It is found that Debye temperatures for the tetrahedral and octahedral sites of $Nd_{0.75}Bi_{0.25}Y_2Fe_5O_{12}$ are $\theta_{tet}=436$ K and $\theta_{oct}=285$ K, respectively, The iron ions at both sites are highly covalent ferric. The Nel temperature decreases linearly with Bi concentration, from 630 K fur $\chi$=0.0 to 600 K for $\chi$=1.0, suggesting that the superexchange interaction for the Nd-O-Fe link is stronger than that for the Bi-O-Fe link. As a consequence, the coercivity of $Nd_{1-x}Bi_xY_2Fe_5O_{12}$ drastically decreases and the magnetization remains almost constant as x increases.

  • PDF

Significance and Application of Digital Breast Tomosynthesis for the BI-RADS Classification of Breast Cancer

  • Cai, Si-Qing;Yan, Jian-Xiang;Chen, Qing-Shi;Huang, Mei-Ling;Cai, Dong-Lu
    • Asian Pacific Journal of Cancer Prevention
    • /
    • v.16 no.9
    • /
    • pp.4109-4114
    • /
    • 2015
  • Background: Full-field digital mammography (FFDM) with dense breasts has a high rate of missed diagnosis, and digital breast tomosynthesis (DBT) could reduce organization overlapping and provide more reliable images for BI-RADS classification. This study aims to explore application of COMBO (FFDM+DBT) for effect and significance of BI-RADS classification of breast cancer. Materials and Methods: In this study, we selected 832 patients who had been treated from May 2013 to November 2013. Classify FFDM and COMBO examination according to BI-RADS separately and compare the differences for glands in the image of the same patient in judgment, mass characteristics display and indirect signs. Employ Paired Wilcoxon rank sum test was used in 79 breast cancer patients to find differences between two examine methods. Results: The results indicated that COMBO pattern is able to observe more details in distribution of glands when estimating content. Paired Wilcoxon rank sum test showed that overall classification level of COMBO is higher significantly compared to FFDM to BI-RADS diagnosis and classification of breast (P<0.05). The area under FFDM ROC curve is 0.805, while that is 0.941 in COMBO pattern. COMBO shows relation of mass with the surrounding tissues, the calcification in the mass, and multiple foci clearly in breast cancer tissues. The optimal sensitivity of cut-off value in COMBO pattern is 82.9%, which is higher than that in FFDM (60%). They share the same specificity which is both 93.2%. Conclusions: Digital Breast Tomosynthesis (DBT) could be used for the BI-RADS classification in breast cancer in clinical.