The effect of cleaning methods on bond strength of zirconia after saliva contamination (타액으로 오염된 지르코니아 수복물의 접착강도에 세척 방법들이 미치는 영향)

  • Shim, Young-Bo;Choi, An-Na;Son, Sung-Ae;Jung, Kyoung-Hwa;Kwon, Yong Hoon;Park, Jeong-Kil
    • Korean Journal of Dental Materials
    • /
    • v.44 no.1
    • /
    • pp.61-68
    • /
    • 2017
  • This study evaluated the effects of various cleaning methods on the shear bond strength of zirconia ceramics after saliva contamination. Eighty zirconia disk specimens were divided into 8 groups. All groups were treated with one coat of MDP primer. All specimens (except the negative control) were contaminated with human saliva on the zirconia surface. The positive control went through the bonding procedure immediately after contamination without any cleaning procedure. With the exception of control groups, the remaining six groups were rinsed with water and either applied with MDP recoating (WATER+MDP) or without MDP recoating (WATER). While some were cleaned with a Ivoclean with MDP recoating (IVOCLEAN+MDP) or not applied with MDP recoating(IVOCLEAN), others were cleaned with a 1% NaOCl solution with MDP recoating (NaOCl+MDP) or without MDP recoating (NaOCl). The shear bond strength of all specimens were measured after being stored in distilled water at $37^{\circ}C$ for 24 hours. The data was analyzed statistically by an analysis of ANOVA, Tukey's post hoc test and Student's t-test was used to compare the shear bond strength according to the re-coating of MDP after the cleaning procedure. The positive control group showed the lowest shear bond strength value, and the WATER group and NaOCl group showed no significant difference when compared to the positive control group. The IVOCLEAN group showed significantly higher shear bond strength when compared to Water group and NaOCl group but not with the group of negative control. After rinsing with water or the NaOCl solution, the comparison of the single coating of MDP and re-coating of MDP showed different shear bond strengths but there was no significant difference to the negative control. After rinsing with Ivoclean, there was no significant difference to the negative control regardless of the recoating of MDP. In conclusion, the shear bond strength was affected by the cleansing procedure and Ivoclean was found to be effective regardless of the re-coating of MDP. When water or the NaOCl solution is used to remove surface contaminants, the re-coating of MDP provides a positive effect on cementation.

Efficacy of various cleaning solutions on saliva-contaminated zirconia for improved resin bonding

  • Kim, Da-Hye;Son, Jun-Sik;Jeong, Seong-Hwa;Kim, Young-Kyung;Kim, Kyo-Han;Kwon, Tae-Yub
    • The Journal of Advanced Prosthodontics
    • /
    • v.7 no.2
    • /
    • pp.85-92
    • /
    • 2015
  • PURPOSE. This study aimed to investigate the efficacy of cleaning solutions on saliva-contaminated zirconia in comparison to air-abrasion in terms of resin bonding. MATERIALS AND METHODS. For saliva-contaminated air-abraded zirconia, seven cleaning methods)-no contamination (NC), water-spray rinsing (WS), additional air-abrasion (AA), and cleaning with four solutions (Ivoclean [IC]; 1.0 wt% sodium dodecyl sulfate [SDS], 1.0 wt% hydrogen peroxide [HP], and 1.0 wt% sodium hypochlorite [SHC])-were tested. The zirconia surfaces for each group were characterized using various analytical techniques. Three bonded resin (Panavia F 2.0) cylinders (bonding area: $4.5mm^2$) were made on one zirconia disk specimen using the Ultradent jig method [four disks (12 cylinders)/group; a total of 28 disks]. After 5,000 thermocycling, all specimens were subjected to a shear bond strength test with a crosshead speed of 1.0 mm/minute. The fractured surfaces were observed using an optical and scanning electron microscope (SEM). RESULTS. Contact angle measurements showed that groups NC, AA, IC, and SHC had hydrophilic surfaces. The X-ray photoelectron spectroscopy (XPS) analysis showed similar elemental distributions between group AA and groups IC and SHC. Groups IC and SHC showed statistically similar bond strengths to groups NC and AA (P>.05), but not groups SDS and HP (P<.05). For groups WS, SDS, and HP, blister-like bubble formations were observed on the surfaces under SEM. CONCLUSION. Within the limitations of this in vitro study, some of the cleaning solutions (IC or SHC) were effective in removing saliva contamination and enhancing the resin bond strength.

Microshear bond strength of dual-cure resin cement in zirconia after different cleaning techniques: an in vitro study

  • Atoche-Socola, Katherine Joselyn;Arriola-Guillen, Luis Ernesto;Lopez-Flores, Ana Isabel;Garcia, Isadora Martini;Huertas-Mogollon, Gustavo;Collares, Fabricio Mezzomo;Leitune, Vicente Castelo Branco
    • The Journal of Advanced Prosthodontics
    • /
    • v.13 no.4
    • /
    • pp.237-245
    • /
    • 2021
  • PURPOSE. This study aimed to compare the microshear bond strength (µSBS) of dual-cure resin cement in CAD-CAM zirconia after different cleaning techniques. MATERIALS AND METHODS. Fifty discs of zirconia-based ceramic from Ivoclar Vivadent were embedded in acrylic resin. The discs were divided into five groups according to the cleaning methods used: Group 1: drying with spraying + sandblasting with Al2O3; Group 2: washed with water and dried with spraying + sandblasting with Al2O3;Group 3: washed with distilled water and dried with spraying + sandblasting with Al2O3 + zirconium oxide (Ivoclean); Group 4: washed with distilled water and dried with spraying + sandblasting with Al2O3 + potassium hydroxide (Zirclean); and Group 5: washed with distilled water and dried with spraying + sandblasting with Al2O3 + 1% NaClO. All of the groups were contaminated with artificial saliva for 1 minute and then cleaned. Statistical analyses were performed using ANOVA and Tukey's tests. RESULTS. There were statistically significant differences among all groups for µSBS (P < .05). The group treated with zirconium oxide (Group 3) showed the highest µSBS (18.75 ± 0.23 MPa). CONCLUSION. When applied to zirconia, the cleaning methods affected the bonding with resin cement differently.

Comparison of Bonding Strength by Cleaning Method of Pediatric Zirconia Crown Contaminated with Saliva or Blood (타액 및 혈액오염 시 유치 지르코니아 기성관 내면의 세척 방법에 따른 결합강도의 비교)

  • Kim, Jaeyong;Park, Howon;Lee, Juhyun;Seo, Hyunwoo
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.45 no.2
    • /
    • pp.185-194
    • /
    • 2018
  • The objective of this study was to compare the shear bonding strength of zirconia after cleaning the crown contaminated by saliva or blood and determine the effect of thermocycling. 180 specimens were embedded in acrylic resin. 20 Specimens in the positive control group were bonded with resin cement without contamination. 20 Specimens in the negative control group were washed with water for 20 seconds and then dried for 10 seconds. 120 Specimens contaminated by saliva or blood were cleaned by using three cleaning methods: 37% phosphoric acid gel, commercial cleanse, and 2.5% NaOCl. All samples were bonded with resin cement and divided into two subgroups: One was not aged, and the other was tested with 30,000 thermocycling. In both groups contamination by saliva and blood, no statistically significant difference was not found in control, groups cleansed by commercial cleanser and 2.5% NaOCl. When the groups cleansed with water and 37% phosphate gel were compared with the control, significantly low shear bond strength was shown. Thermocycling group showed statistically significantly low shear bond stress compared to the groups without thermocycling. When zirconia was contaminated by saliva or blood, its original shear bond strength could be obtained if it was cleaned with commercial cleanser or 2.5% NaOCl.