Comparison of Bonding Strength by Cleaning Method of Pediatric Zirconia Crown Contaminated with Saliva or Blood

타액 및 혈액오염 시 유치 지르코니아 기성관 내면의 세척 방법에 따른 결합강도의 비교

  • Kim, Jaeyong (Department of Pediatric Dentistry, Oral Science Research Center, College of Dentistry, Gangneung-Wonju National University) ;
  • Park, Howon (Department of Pediatric Dentistry, Oral Science Research Center, College of Dentistry, Gangneung-Wonju National University) ;
  • Lee, Juhyun (Department of Pediatric Dentistry, Oral Science Research Center, College of Dentistry, Gangneung-Wonju National University) ;
  • Seo, Hyunwoo (Department of Pediatric Dentistry, Oral Science Research Center, College of Dentistry, Gangneung-Wonju National University)
  • 김재용 (강릉원주대학교 치과대학 소아치과학교실 및 구강과학연구소) ;
  • 박호원 (강릉원주대학교 치과대학 소아치과학교실 및 구강과학연구소) ;
  • 이주현 (강릉원주대학교 치과대학 소아치과학교실 및 구강과학연구소) ;
  • 서현우 (강릉원주대학교 치과대학 소아치과학교실 및 구강과학연구소)
  • Received : 2017.09.26
  • Accepted : 2017.10.26
  • Published : 2018.05.31

Abstract

The objective of this study was to compare the shear bonding strength of zirconia after cleaning the crown contaminated by saliva or blood and determine the effect of thermocycling. 180 specimens were embedded in acrylic resin. 20 Specimens in the positive control group were bonded with resin cement without contamination. 20 Specimens in the negative control group were washed with water for 20 seconds and then dried for 10 seconds. 120 Specimens contaminated by saliva or blood were cleaned by using three cleaning methods: 37% phosphoric acid gel, commercial cleanse, and 2.5% NaOCl. All samples were bonded with resin cement and divided into two subgroups: One was not aged, and the other was tested with 30,000 thermocycling. In both groups contamination by saliva and blood, no statistically significant difference was not found in control, groups cleansed by commercial cleanser and 2.5% NaOCl. When the groups cleansed with water and 37% phosphate gel were compared with the control, significantly low shear bond strength was shown. Thermocycling group showed statistically significantly low shear bond stress compared to the groups without thermocycling. When zirconia was contaminated by saliva or blood, its original shear bond strength could be obtained if it was cleaned with commercial cleanser or 2.5% NaOCl.

본 연구의 목적은 타액이나 혈액에 오염된 유치 지르코니아 기성관의 내면을 다양한 세척 방법으로 세척 한 뒤, 레진 시멘트와의 결합력을 비교하고, 열 순환이 결합력에 미치는 효과를 평가하였다. 지르코니아 기성관의 내면과 유사한 상태의 지르코니아 절편($5mm{\times}3mm$)을 아크릴릭 레진에 매몰하였다(n=180). 이 중 160개의 시편을 무작위로 두 군으로 나누어 타액 오염과 혈액 오염을 시행하였다. 양성 대조군은 오염 과정을 거치지 않고 resin cement로 접착을 시행하였고, 음성 대조군은 오염 후 dental unit chair 상의 물로 20초간 세척 후 10초간 건조를 시행하였다. 타액 오염된 시편과 (n=60) 혈액 오염된 시편(n=60)은 각각 세 가지 방법의 세척을 시행하였다. 37% 인산 젤, 상용 세척제(Ivoclean), 2.5% NaOCl을 각 시편에 20초간 적용 후 10초간 물로 세척하고 건조를 시행하였다. 이 후 모든 시편(n=160)에 접착을 시행하였다. 대조군과 각 실험군을 모두 절반으로 나누어 절반은 바로 전단응력을 측정하였고, 절반은 열 순환 과정 후 전단응력을 측정하였다. 타액오염과 혈액오염을 시행한 군 모두에서, 양성 대조군과 상용 세척제, 2.5% NaOCl으로 세척한 군에서 통계학적으로 유의한 차이는 존재하지 않았다. 음성 대조군과 37% 인산 젤로 세척한 군의 전단 결합 강도는 양성 대조군과 비교하였을 때, 유의하게 감소하였다. 열 순환 시행 시 타액 오염을 시행한 군과 혈액 오염을 시행한 모든 군에서 열 순환을 시행하지 않은 군보다 통계적으로 유의하게 낮은 전단 응력 간도를 나타내었다. 유치 지르코니아 기성관 내부의 타액 오염이나 혈액 오염 시, 상용 세척제나 2.5% NaOCl로 세척을 시행하면 원래의 전단응력 값을 얻을 수 있다. 열 순환 시행 시 모든 군에서 유의하게 낮은 전단 응력 값을 보였다.

Keywords

References

  1. Komine F, Tomic M, Gerds T, Strub JR : Influence of different adhesive resin cements on the fracture strength of aluminum oxide ceramic posterior crowns. J Prosthet Dent, 92:359-364, 2004. https://doi.org/10.1016/j.prosdent.2004.07.018
  2. Piconi C, Maccauro G : Zirconia as a ceramic biomaterial. Biomaterials, 20:1-25, 1999. https://doi.org/10.1016/S0142-9612(98)00010-6
  3. Denry I, Kelly JR : State of the art of zirconia for dental applications. Dent Mater, 24:299-307, 2008. https://doi.org/10.1016/j.dental.2007.05.007
  4. Thompson JY, Stoner BR, Piascik JR, Smith R : Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now? Dent Mater, 27:71-82, 2011. https://doi.org/10.1016/j.dental.2010.10.022
  5. Amaral R, Ozcan M, Valandro LF, et al. : Effect of conditioning methods on the microtensile bond strength of phosphate monomer-based cement on zirconia ceramic in dry and aged conditions. J Biomed Mater Res B Appl Biomater, 85:1-9, 2008.
  6. Blatz MB, Sadan A, Kern M : Resin-ceramic bonding: a review of the literature. J Prosthet Dent, 89:268-274, 2003. https://doi.org/10.1067/mpr.2003.50
  7. Phark JH, Duarte S, Jr., Blatz M, Sadan A : An in vitro evaluation of the long-term resin bond to a new densely sintered high-purity zirconium-oxide ceramic surface. J Prosthet Dent, 101:29-38, 2009. https://doi.org/10.1016/S0022-3913(08)60286-3
  8. El Zohairy AA, De Gee AJ, Hassan FM, Feilzer AJ : The effect of adhesives with various degrees of hydrophilicity on resin ceramic bond durability. Dent Mater, 20:778-787, 2004. https://doi.org/10.1016/j.dental.2003.05.010
  9. Hahn P, Attin T, Grofke M, Hellwig E : Influence of resin cement viscosity on microleakage of ceramic inlays. Dent Mater, 17:191-196, 2001. https://doi.org/10.1016/S0109-5641(00)00067-1
  10. Yang B, Lange-Jansen HC, Scharnberg M, et al. : Influence of saliva contamination on zirconia ceramic bonding. Dent Mater, 24:508-513, 2008. https://doi.org/10.1016/j.dental.2007.04.013
  11. Yang B, Wolfart S, Scharnberg M, et al. : Influence of contamination on zirconia ceramic bonding. J Dent Res, 86:749-753, 2007. https://doi.org/10.1177/154405910708600812
  12. Aboush YE : Removing saliva contamination from porcelain veneers before bonding. J Prosthet Dent, 80:649-653, 1998. https://doi.org/10.1016/S0022-3913(98)70050-2
  13. Zhang Y, Lawn BR, Malament KA, et al. : Damage accumulation and fatigue life of particle-abraded ceramics. Int J Prosthodont, 19:442-448, 2006.
  14. Zhang Y, Lawn BR, Rekow ED, Thompson VP : Effect of sandblasting on the long-term performance of dental ceramics. J Biomed Mater Res B Appl Biomater, 71:381-386, 2004.
  15. Souza RO, Valandro LF, Melo RM, et al. : Air-particle abrasion on zirconia ceramic using different protocols: effects on biaxial flexural strength after cyclic loading, phase transformation and surface topography. J Mech Behav Biomed Mater, 26:155-163, 2013. https://doi.org/10.1016/j.jmbbm.2013.04.018
  16. El-Korashy DI, El-Refai DA : Mechanical properties and bonding potential of partially stabilized zirconia treated with different chemomechanical treatments. J Adhes Dent, 16:365-376, 2014.
  17. Kim DH, Son JS, Jeong SH, et al. : Efficacy of various cleaning solutions on saliva-contaminated zirconia for improved resin bonding. J Adv Prosthodont, 7:85-92, 2015. https://doi.org/10.4047/jap.2015.7.2.85
  18. Ishii R, Tsujimoto A, Takamizawa T, et al. : Influence of surface treatment of contaminated zirconia on surface free energy and resin cement bonding. Dent Mater J, 34:91-97, 2015. https://doi.org/10.4012/dmj.2014-066
  19. Boehm RF : Thermal environment of teeth during openmouth respiration. J Dent Res, 51:75-78, 1972. https://doi.org/10.1177/00220345720510013401
  20. Palmer DS, Barco MT, Billy EJ : Temperature extremes produced orally by hot and cold liquids. J Prosthet Dent, 67:325-327, 1992. https://doi.org/10.1016/0022-3913(92)90239-7
  21. Quaas AC, Yang B, Kern M : Panavia F 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures. Dent Mater, 23:506-512, 2007. https://doi.org/10.1016/j.dental.2006.03.008
  22. Gale MS, Darvell BW : Thermal cycling procedures for laboratory testing of dental restorations. J Dent, 27:89-99, 1999. https://doi.org/10.1016/S0300-5712(98)00037-2
  23. Luthy H, Loeffel O, Hammerle CH : Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater, 22:195-200, 2006. https://doi.org/10.1016/j.dental.2005.04.016
  24. Zhang S, Kocjan A, Lehmann F, et al. : Influence of contamination on resin bond strength to nano-structured aluminacoated zirconia ceramic. Eur J Oral Sci, 118:396-403, 2010. https://doi.org/10.1111/j.1600-0722.2010.00752.x
  25. Barakat MM, Powers JM : In vitro bond strength of cements to treated teeth. Aust Dent J, 31:415-419, 1986. https://doi.org/10.1111/j.1834-7819.1986.tb01243.x
  26. Song JY, Park SW, Lee K, et al. : Fracture strength and microstructure of Y-TZP zirconia after different surface treatments. J Prosthet Dent, 110:274-280, 2013. https://doi.org/10.1016/S0022-3913(13)60376-5
  27. Angkasith P, Burgess JO, Bottino MC, Lawson NC : Cleaning Methods for Zirconia Following Salivary Contamination. J Prosthodont, 25:375-379, 2016. https://doi.org/10.1111/jopr.12441
  28. Siqueira JF, Jr., Guimaraes-Pinto T, Rocas IN : Effects of chemomechanical preparation with 2.5% sodium hypochlorite and intracanal medication with calcium hydroxide on cultivable bacteria in infected root canals. J Endod, 33:800-805, 2007. https://doi.org/10.1016/j.joen.2006.11.023